DE3579315D1 - Elektroden-herstellungsverfahren. - Google Patents
Elektroden-herstellungsverfahren.Info
- Publication number
- DE3579315D1 DE3579315D1 DE8585308642T DE3579315T DE3579315D1 DE 3579315 D1 DE3579315 D1 DE 3579315D1 DE 8585308642 T DE8585308642 T DE 8585308642T DE 3579315 T DE3579315 T DE 3579315T DE 3579315 D1 DE3579315 D1 DE 3579315D1
- Authority
- DE
- Germany
- Prior art keywords
- electrode manufacturing
- electrode
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/10—Fuel cells with solid electrolytes
- H01M8/12—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte
- H01M8/1213—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte characterised by the electrode/electrolyte combination or the supporting material
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/86—Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M4/90—Selection of catalytic material
- H01M4/9016—Oxides, hydroxides or oxygenated metallic salts
- H01M4/9025—Oxides specially used in fuel cell operating at high temperature, e.g. SOFC
- H01M4/9033—Complex oxides, optionally doped, of the type M1MeO3, M1 being an alkaline earth metal or a rare earth, Me being a metal, e.g. perovskites
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/86—Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M4/90—Selection of catalytic material
- H01M4/9041—Metals or alloys
- H01M4/905—Metals or alloys specially used in fuel cell operating at high temperature, e.g. SOFC
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/86—Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M4/90—Selection of catalytic material
- H01M4/9041—Metals or alloys
- H01M4/905—Metals or alloys specially used in fuel cell operating at high temperature, e.g. SOFC
- H01M4/9066—Metals or alloys specially used in fuel cell operating at high temperature, e.g. SOFC of metal-ceramic composites or mixtures, e.g. cermets
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/30—Hydrogen technology
- Y02E60/50—Fuel cells
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P70/00—Climate change mitigation technologies in the production process for final industrial or consumer products
- Y02P70/50—Manufacturing or production processes characterised by the final manufactured product
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
- Y10T29/00—Metal working
- Y10T29/49—Method of mechanical manufacture
- Y10T29/49002—Electrical device making
- Y10T29/49108—Electric battery cell making
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
- Y10T29/00—Metal working
- Y10T29/49—Method of mechanical manufacture
- Y10T29/49002—Electrical device making
- Y10T29/49108—Electric battery cell making
- Y10T29/49115—Electric battery cell making including coating or impregnating
Landscapes
- Chemical Kinetics & Catalysis (AREA)
- Life Sciences & Earth Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Sustainable Development (AREA)
- Sustainable Energy (AREA)
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Inert Electrodes (AREA)
- Fuel Cell (AREA)
- Measuring Oxygen Concentration In Cells (AREA)
- Electrodes For Compound Or Non-Metal Manufacture (AREA)
- Chemical Vapour Deposition (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US06/716,865 US4597170A (en) | 1985-03-28 | 1985-03-28 | Method of making an electrode |
Publications (1)
Publication Number | Publication Date |
---|---|
DE3579315D1 true DE3579315D1 (de) | 1990-09-27 |
Family
ID=24879769
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DE8585308642T Expired - Fee Related DE3579315D1 (de) | 1985-03-28 | 1985-11-28 | Elektroden-herstellungsverfahren. |
Country Status (5)
Country | Link |
---|---|
US (1) | US4597170A (de) |
EP (1) | EP0196388B1 (de) |
JP (1) | JPS61225778A (de) |
CA (1) | CA1236352A (de) |
DE (1) | DE3579315D1 (de) |
Families Citing this family (45)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US5549850A (en) * | 1984-11-02 | 1996-08-27 | The Boeing Company | LaMnO3 -coated ceramics |
US6333000B1 (en) | 1984-11-02 | 2001-12-25 | The Boeing Company | Process for making LaMnO3-coated ceramics |
US4702971A (en) * | 1986-05-28 | 1987-10-27 | Westinghouse Electric Corp. | Sulfur tolerant composite cermet electrodes for solid oxide electrochemical cells |
US4812329A (en) * | 1986-05-28 | 1989-03-14 | Westinghouse Electric Corp. | Method of making sulfur tolerant composite cermet electrodes for solid oxide electrochemical cells |
US4767518A (en) * | 1986-06-11 | 1988-08-30 | Westinghouse Electric Corp. | Cermet electrode |
JP2601821B2 (ja) * | 1987-05-29 | 1997-04-16 | 日本原子力研究所 | 水蒸気の電解装置 |
JPS63303088A (ja) * | 1987-05-30 | 1988-12-09 | Japan Atom Energy Res Inst | 固体電解質水蒸気電解装置 |
JPH088105B2 (ja) * | 1987-08-12 | 1996-01-29 | 三菱重工業株式会社 | 固体電解質形燃料電池 |
US4847172A (en) * | 1988-02-22 | 1989-07-11 | Westinghouse Electric Corp. | Low resistance fuel electrodes |
US4849254A (en) * | 1988-02-25 | 1989-07-18 | Westinghouse Electric Corp. | Stabilizing metal components in electrodes of electrochemical cells |
US4895576A (en) * | 1988-04-15 | 1990-01-23 | Westinghouse Electric Corp. | Method of doping interconnections for electrochemical cells |
US4971830A (en) * | 1990-02-01 | 1990-11-20 | Westinghouse Electric Corp. | Method of electrode fabrication for solid oxide electrochemical cells |
US5035962A (en) * | 1990-03-21 | 1991-07-30 | Westinghouse Electric Corp. | Layered method of electrode for solid oxide electrochemical cells |
US5132352A (en) * | 1990-04-27 | 1992-07-21 | Westinghouse Electric Corp. | Tape method of forming a thin layer of doped lanthanum chromite particles and of bonding such on an electrode |
US5080689A (en) * | 1990-04-27 | 1992-01-14 | Westinghouse Electric Co. | Method of bonding an interconnection layer on an electrode of an electrochemical cell |
US5106654A (en) * | 1990-07-20 | 1992-04-21 | Westinghouse Electric Corp. | Method of forming a dense, high temperature electronically conductive composite layer on a porous ceramic substrate |
JP2513920B2 (ja) * | 1990-09-26 | 1996-07-10 | 日本碍子株式会社 | 固体電解質燃料電池の燃料電極及びその製造方法 |
US5085742A (en) * | 1990-10-15 | 1992-02-04 | Westinghouse Electric Corp. | Solid oxide electrochemical cell fabrication process |
DE4203245C2 (de) * | 1991-02-07 | 1994-03-24 | Yoshida Kogyo Kk | Festelektrolytbrennstoffzelle |
US5474800A (en) * | 1991-06-20 | 1995-12-12 | Tokyo Gas Company, Ltd. | Method for preparing anode for solid oxide fuel cells |
US5342703A (en) * | 1991-07-19 | 1994-08-30 | Ngk Insulators, Ltd. | Solid electrolyte type fuel cell and method for producing the same |
US5141825A (en) * | 1991-07-26 | 1992-08-25 | Westinghouse Electric Corp. | Method of making a cermet fuel electrode containing an inert additive |
JP3281925B2 (ja) * | 1991-08-06 | 2002-05-13 | 大阪瓦斯株式会社 | サーメット電極及びその製造方法 |
US5445903A (en) * | 1993-09-09 | 1995-08-29 | Technology Management, Inc. | Electrochemical apparatus |
US5589285A (en) * | 1993-09-09 | 1996-12-31 | Technology Management, Inc. | Electrochemical apparatus and process |
US5413879A (en) * | 1994-02-08 | 1995-05-09 | Westinghouse Electric Corporation | Integrated gas turbine solid oxide fuel cell system |
US5391440A (en) * | 1994-02-14 | 1995-02-21 | Westinghouse Electric Corporation | Method of forming a leak proof plasma sprayed interconnection layer on an electrode of an electrochemical cell |
US5389456A (en) * | 1994-02-14 | 1995-02-14 | Westinghouse Electric Corporation | Method and closing pores in a thermally sprayed doped lanthanum chromite interconnection layer |
US5426003A (en) * | 1994-02-14 | 1995-06-20 | Westinghouse Electric Corporation | Method of forming a plasma sprayed interconnection layer on an electrode of an electrochemical cell |
US5516597A (en) * | 1994-11-07 | 1996-05-14 | Westinghouse Electric Corporation | Protective interlayer for high temperature solid electrolyte electrochemical cells |
US5955039A (en) * | 1996-12-19 | 1999-09-21 | Siemens Westinghouse Power Corporation | Coal gasification and hydrogen production system and method |
US5989634A (en) * | 1997-06-25 | 1999-11-23 | Isenberg; Arnold O. | Process of manufacturing solid oxygen ion conducting oxide layers |
US5908713A (en) * | 1997-09-22 | 1999-06-01 | Siemens Westinghouse Power Corporation | Sintered electrode for solid oxide fuel cells |
US6063517A (en) * | 1997-10-16 | 2000-05-16 | Southwest Research Institute | Spiral wrapped cylindrical proton exchange membrane fuel cells and methods of making same |
US6139985A (en) * | 1998-07-24 | 2000-10-31 | Siemens Westinghouse Power Corporation | Electrode electrolyte interlayers containing cerium oxide for electrochemical fuel cells |
US6248468B1 (en) | 1998-12-31 | 2001-06-19 | Siemens Westinghouse Power Corporation | Fuel electrode containing pre-sintered nickel/zirconia for a solid oxide fuel cell |
US6655325B1 (en) | 1999-02-01 | 2003-12-02 | Delphi Technologies, Inc. | Power generation system and method with exhaust side solid oxide fuel cell |
US6230494B1 (en) | 1999-02-01 | 2001-05-15 | Delphi Technologies, Inc. | Power generation system and method |
CN1336016A (zh) | 1999-10-08 | 2002-02-13 | 全球热电公司 | 用于固态电化学装置的复合电极 |
JP2004513500A (ja) | 2000-11-08 | 2004-04-30 | グローバル サーモエレクトリック インコーポレイテッド | 電気化学電池の連結装置 |
CA2431231A1 (en) * | 2001-01-12 | 2002-07-18 | Global Thermoelectric Inc. | Redox solid oxide fuel cell |
US6580191B2 (en) * | 2001-05-29 | 2003-06-17 | Gimbie Enterprises Ltd. | Fuel cell powered magnetically driven shaft assembly |
US6984467B2 (en) * | 2002-09-24 | 2006-01-10 | Siemens Westinghouse Power Corporation | Plasma sprayed ceria-containing interlayer |
US8211587B2 (en) * | 2003-09-16 | 2012-07-03 | Siemens Energy, Inc. | Plasma sprayed ceramic-metal fuel electrode |
US9642192B2 (en) * | 2011-08-04 | 2017-05-02 | Fuelcell Energy, Inc. | Method and manufacturing assembly for sintering fuel cell electrodes and impregnating porous electrodes with electrolyte powders by induction heating for mass production |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3915119A (en) * | 1972-10-27 | 1975-10-28 | Us Energy | Apparatus for fabricating composite ceramic members |
US4242426A (en) * | 1979-11-05 | 1980-12-30 | General Electric Company | Process for electrolyte structure with strontium titanate matrix for molten carbonate fuel cells |
US4499663A (en) * | 1983-10-12 | 1985-02-19 | The United States Of America As Represented By The United States Department Of Energy | Method of fabricating a monolithic core for a solid oxide fuel cell |
-
1985
- 1985-03-28 US US06/716,865 patent/US4597170A/en not_active Expired - Lifetime
- 1985-11-19 CA CA000495711A patent/CA1236352A/en not_active Expired
- 1985-11-28 EP EP85308642A patent/EP0196388B1/de not_active Expired - Lifetime
- 1985-11-28 DE DE8585308642T patent/DE3579315D1/de not_active Expired - Fee Related
- 1985-11-28 JP JP60269217A patent/JPS61225778A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
US4597170A (en) | 1986-07-01 |
JPS61225778A (ja) | 1986-10-07 |
CA1236352A (en) | 1988-05-10 |
EP0196388A3 (en) | 1988-01-07 |
JPH0558235B2 (de) | 1993-08-26 |
EP0196388A2 (de) | 1986-10-08 |
EP0196388B1 (de) | 1990-08-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3579315D1 (de) | Elektroden-herstellungsverfahren. | |
DE3676744D1 (de) | Leiterplattenherstellungsverfahren. | |
DE3580981D1 (de) | Ionenselektive elektrode. | |
DE3689533T3 (de) | Plasmaphorese-verfahren | |
NO863154L (no) | Biocid blanding. | |
IT8622048A0 (it) | Elettrodo defibrillatore. | |
DE3789898D1 (de) | Referenzelektrode. | |
DE3777503D1 (de) | Elektrodenaufbau. | |
KR870700615A (ko) | 감마-부티로락톤의 제조방법 | |
DE3689354D1 (de) | Herzschrittmacher. | |
NO864935D0 (no) | Elektrode for fast-polymer-elektrolytt. | |
DE3676140D1 (de) | Herzschrittmacherelektrode. | |
DE3675364D1 (de) | Elektrode. | |
DE3689347D1 (de) | Herzschrittmacher. | |
NO159616C (no) | L smutter. | |
DE3579980D1 (de) | Elektroerosionselektrode. | |
DK78186A (da) | Elektrokardiografisk elektrode | |
DE3583697D1 (de) | Ionenselektivelektrode. | |
NO853376L (no) | Broenn-testemetode. | |
FI862890A (fi) | Elektrisk klaemlist. | |
DE3874996D1 (de) | Chloridionenselektive elektrode. | |
FI860180A (fi) | Polycykliska salter. | |
DE3650261D1 (de) | Herzschrittmacher. | |
DE3579483D1 (de) | Kaliionenselektive elektrode. | |
DE3676753D1 (de) | Stranggiessverfahren. |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
8364 | No opposition during term of opposition | ||
8339 | Ceased/non-payment of the annual fee |