DE3316134C2 - Method and device for the production of protective tubes with a flat cross-section for concrete reinforcing bars - Google Patents
Method and device for the production of protective tubes with a flat cross-section for concrete reinforcing barsInfo
- Publication number
- DE3316134C2 DE3316134C2 DE19833316134 DE3316134A DE3316134C2 DE 3316134 C2 DE3316134 C2 DE 3316134C2 DE 19833316134 DE19833316134 DE 19833316134 DE 3316134 A DE3316134 A DE 3316134A DE 3316134 C2 DE3316134 C2 DE 3316134C2
- Authority
- DE
- Germany
- Prior art keywords
- section
- mandrel
- pipe
- cross
- tube
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
Verfahren und Vorrichtung zum Herstellen von Schutzrohren mit flachem Querschnitt für Betonbewehrungsstäbe. In ein Rohr mit kreisförmigem Querschnitt, insbesondere ein gewelltes Rohr, wird ein Dorn von im wesentlichen rechteckigem Querschnitt eingelegt, worauf das Rohr in seiner gesamten Länge vorzugsweise in einem einzigen Preßvorgang bis zum Anliegen gegenüberliegender Wandteile am Dorn breitgedrückt wird. Hierzu dienen zwei zu- und voneinander bewegbare Preßbalken (2, 3), deren wirksame Länge zumindest gleich der Länge des zu verformenden Rohres ist, sowie in einem Dorn (4), welcher vor dem Pressen des Rohres in dieses einschiebbar ist.Method and device for the production of protective tubes with a flat cross-section for concrete reinforcing bars. In a pipe with a circular cross-section, in particular a corrugated pipe, a mandrel with a substantially rectangular cross-section is inserted, whereupon the entire length of the pipe is expanded, preferably in a single pressing process, until opposing wall parts rest against the mandrel. Two press bars (2, 3) which can be moved towards and from one another are used for this purpose, the effective length of which is at least equal to the length of the pipe to be deformed, and in a mandrel (4) which can be pushed into the pipe before it is pressed.
Description
Die Erfindung betrifft ein Verfahren nach dem Oberbegriff des Patentanspruches i.The invention relates to a method according to the preamble of claim i.
Einen weiteren Gegenstand der vorliegenden Patentanmeldung bildet eine Vorrichtung zur Durchführung dieses Verfahrens.Another object of the present patent application is a device for implementation this procedure.
Es ist üblich, Betonbewehrungen, welche nach dem Erhärten des Betons gespannt werden, in Schutzrohren zu verlegen, um eine Berührung zwischen Beton und Bewehrungsstab zu vermeiden und um dadurch die freie und unbehinderte Dehnung des Stabes beim Spannen zu sichern.It is common to place concrete reinforcements, which are tensioned after the concrete has hardened, in protective pipes to be laid in order to avoid contact between the concrete and the reinforcement bar and thereby the free and to ensure unhindered elongation of the rod during tensioning.
Außer den Bewehrungsstäben mit kreisförmigem Querschnitt oder Bündeln solcher Stäbe stehen auch Flachstäbe als Bewehrung in Verwendung, und es ist auch, in vielen Fällen aus Gründen des verfügbaren Platzes innerhalb des zu bewehrenden Trägers, gebräuchlich, mehrere Bewehrungsstäbe mit kreisförmigem Querschnitt nebeneinander im gleichen Rohr zu verlegen. Die hierfür verwendeten Rohre haben flachen, dem Stab entsprechend angepaßten Querschnitt und wurden durch Flachdrücken von Blechrohren hergestellt. Diese Blechrohre wurden durch schraubenlinienförmiges Wickeln über einen Dorn eines Blechstreifens, dessen Ränder einander überlappten und durch Punktschweißen miteinander verbunden wurden erzeugt. Die Blechstreifen konnten hierbei einen leicht gewellten Querschnitt haben.In addition to the reinforcing bars with a circular cross-section or bundles of such bars are also available Flat bars are in use as reinforcement, and also, in many cases, for reasons of availability Space within the girder to be reinforced, common, several reinforcing bars with circular Cross-section to be laid next to each other in the same pipe. The tubes used for this have flat, The cross-section corresponding to the rod and were produced by flattening sheet metal tubes. These sheet metal tubes were made by helically winding a sheet metal strip over a mandrel, the edges of which overlapped each other and were connected to each other by spot welding. the Sheet metal strips could have a slightly corrugated cross-section.
Beim Flachdrücken dieser unter der Bezeichnung »Spiralrohr« allgemein bekannten Erzeugnisse ergab sich aber der Nachteil, daß das ursprünglich kreisförmigen Querschnitt aufweisende Rohr nicht einen flachen Querschnitt erhielt, der aus zwei zueinander parallelen Geraden und zwei diese verbindenden Bögen bestand, sondern eine Querschnittsform zeigte, die einer Biskotte entsprach, d. h. die beiden Seiten waren zueinander oder ins Innere des Querschnittes hin gebogen oder eingebeult Dieser unerwünschten Verformung mußte Rechnung getragen werden, und das Flachdrücken konnte nur soweit vorgenommen werden, daß der freie Abstand der eingebeulten Seiten das Einführen des oder der Bewehrungsstäbe noch erlaubte. Anders ausgedrückt, man war gezwungen, ein Rohr mit an sich zu großen Durchmesser nur teilweise nachzudrücken, um ίο die vorgesehenen Bewehrungsstäbe im verformten Rohr unterbringen zu können; eine entsprechende Kostenüberhöhung war damit zwangsläufig verbunden.When flattening these products, which are generally known under the designation "spiral tube", resulted but there is the disadvantage that the tube, which was originally circular in cross section, is not flat Received a cross-section, which consisted of two parallel straight lines and two arcs connecting them, but showed a cross-sectional shape corresponding to a biscuit, i.e. H. the two sides were to each other or bent or dented into the interior of the cross-section. This undesirable deformation had to be taken into account be carried, and the flattening could only be done so far that the free space the dented sides still allowed the introduction of the reinforcing bar (s). Expressed differently, one was forced to push back a pipe with a diameter that was too large in itself only partially in order to ίο to be able to accommodate the intended reinforcing bars in the deformed pipe; a corresponding cost inflation was inevitably connected with it.
Die Erfindung hat sich zum Ziel gesetzt, die angegebenen Nachteile zu vermeiden und erreicht dieses Ziel bei dem Verfahren der eingangs umrissenen Art durch die Maßnahme nach dem kennzeichnenden Teil des Patentanspruches 1.The invention has set itself the goal of avoiding the specified disadvantages and achieves this goal in the method of the type outlined above by the measure according to the characterizing part of the patent claim 1.
Die erfindungsgemäße Vorrichtung zur Durchführung dieses Verfahrens besteht aus den Merkmalen des Anspruches 2.The inventive device for performing this method consists of the features of Claim 2.
Weitere Vorteile der erfindungsgemäßen Vorrichtung ergeben sich aus den Merkmalen der Patentansprüche 3 und 4.Further advantages of the device according to the invention result from the features of the patent claims 3 and 4.
Die Erfindung wird im folgenden an Hand der Zeichnung erläutert. Es zeigen dieThe invention is explained below with reference to the drawing. It show the
F i g. 1 und 2 die bisher übliche Verfahrensweise zum Flachdrücken eines Schutzrohres aus Blech und dieF i g. 1 and 2 the previously common procedure for flattening a protective tube made of sheet metal and the
F i g. 3 und 4 den Vorgang des Verformens gemäß der Erfindung.F i g. 3 and 4 show the deformation process according to the invention.
Die F i g. 1 und 2 lassen deutlich erkennen, daß ein Blechrohr 1 mit ursprünglich kreisförmigem Querschnitt beim Flachdrücken zwischen einem ebenen Pressentisch 2 und einem ebenfalls ebenen PreßstempelThe F i g. 1 and 2 clearly show that a sheet metal tube 1 with an originally circular cross-section when pressing flat between a flat press table 2 and a likewise flat ram
3 einen biskottenartigen Querschnitt erhält, dessen geringste Höhe H so groß sein muß, daß ein Bewehrungsstab noch hinreichend leicht eingeschoben werden kann.3 receives a biscottel-like cross-section, the lowest height H of which must be so large that a reinforcing bar can still be pushed in with sufficient ease.
Gemäß dem erfindungsemäßen Verfahren wird in das Rohr 1 ein Dorn 4 von im wesentlichen rechteckigem Querschnitt eingeschoben. Die Dicke des Domes 4 entspricht vorzugsweise der Dicke (Höhe) der zu verwendenden Bewehrung, vermehrt um einen geringen Betrag, um das leichte Einführen der Bewehrung in das flachgedrückte Rohr 1' zu ermöglichen, und die Breite des Domes 4 ist so groß, daß der Dorn in das noch unverformte Rohr gerade noch ohne wesentlichen Widerstand eingeschoben werden kann. Das mit dem DornAccording to the method according to the invention, a mandrel 4 of an essentially rectangular shape is inserted into the tube 1 Cross-section inserted. The thickness of the dome 4 preferably corresponds to the thickness (height) of the one to be used Reinforcement, increased by a small amount, to allow the reinforcement to be easily inserted into the To enable flattened tube 1 ', and the width of the dome 4 is so large that the mandrel in the still undeformed pipe can just be pushed in without significant resistance. The one with the thorn
4 versehene Rohr 1 wird auf den Presnentisch 2 aufgelegt und der Preßstempel 3 wird dann vorzugsweise mittels einer hydraulischen Vorrichtung soweit abgesenkt, bis die einander gegenüberliegenden Wandteile \" und V" satt am Dorn 4 anliegen. Das verformte Rohr Γ hat dabei einen aus Fig.4 ersichtlichen flachen bzw. ovalen Querschnitt erhalten. Nach Anheben des Preßstempels 3 wird der Dorn 4 z. B. von einer nicht gezeigten Ausziehvorrichtung erfaßt und aus dem flachgedrückten Rohr 1' ausgezogen.4 provided tube 1 is placed on the press table 2 and the ram 3 is then lowered, preferably by means of a hydraulic device, until the opposing wall parts \ " and V \" are in full contact with the mandrel 4. The deformed tube Γ has been given a flat or oval cross-section which can be seen in FIG. After lifting the ram 3, the mandrel 4 z. B. detected by an extractor, not shown, and pulled out of the flattened tube 1 '.
Der Preßtisch 2 und der Preßstempel 3 bestehen beim vorliegenden Ausführungsbeispiel der Preßvorrichtung aus je einem I-Träger, dessen Länge zumindest gleich der Länge des zu verformenden Rohres 1 ist, so daß dieses in einem einzigen Preßvorgang entlang seiner gesamten Länge verformt wird. Der Preßstempel 3 wird von zumindest zwei Kolben 5 eines hydraulischen Preßzylinders 6 getragen, welcher auf einem Ständer 7 befestigtist. The press table 2 and the press ram 3 exist in the present embodiment of the press device each from an I-beam, the length of which is at least equal to the length of the tube 1 to be deformed, so that this is deformed in a single pressing process along its entire length. The ram 3 is carried by at least two pistons 5 of a hydraulic press cylinder 6 which is mounted on a stand 7.
Selbstverständlich können im Rahmen der Erfindung verschiedene konstruktive Änderungen vorgenommen werden. So besteht die Möglichkeit die PreßvorrichtungOf course, various design changes can be made within the scope of the invention will. So there is the possibility of the pressing device
aus einem oberen fixen Preßbalken und einem unteren hydraulischen heb- und senkbaren Preßbalken auszubilden. to be formed from an upper fixed press beam and a lower hydraulic press beam that can be raised and lowered.
Der Dorn 4 kann an seinem in das Rohr einzuschiebenden Ende seitlich konisch ausgeführt sein, um das 5 Einschieben des Domes in das Rohr zu erleichtern.The mandrel 4 can be laterally conical at its end to be pushed into the tube in order to To facilitate pushing the dome into the pipe.
Weiters kann der Dorn in seiner Längsrichtung geteilt und seine beiden Teile können gegeneinander verstellbar sein, wodurch der Dorn an verschiedenen Rohrdurchmessern anpaßbar ist. 10Furthermore, the mandrel can be divided in its longitudinal direction and its two parts can be adjusted relative to one another be, whereby the mandrel is adaptable to different pipe diameters. 10
Hierzu 1 Blatt Zeichnungen1 sheet of drawings
1515th
2020th
2525th
3030th
4545
5050
5555
6060
Claims (4)