DE3002949A1 - Hydraulic viscous flow damping agent - has carrier liq. contg. suspended carbon black of particle size below one micron - Google Patents
Hydraulic viscous flow damping agent - has carrier liq. contg. suspended carbon black of particle size below one micronInfo
- Publication number
- DE3002949A1 DE3002949A1 DE19803002949 DE3002949A DE3002949A1 DE 3002949 A1 DE3002949 A1 DE 3002949A1 DE 19803002949 DE19803002949 DE 19803002949 DE 3002949 A DE3002949 A DE 3002949A DE 3002949 A1 DE3002949 A1 DE 3002949A1
- Authority
- DE
- Germany
- Prior art keywords
- viscous flow
- particle size
- carbon black
- flow losses
- damping
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
Description
Dämpfungamaase für hydraulische Dämpfer mit viskosenDamping mamaase for hydraulic dampers with viscous
Strömungsverluaten Die Erfindung bezieht sich auf Dämpfungamassen für hydraulische Dämpfer mit viskosen Strömungsverlusten. Flow losses The invention relates to damping masses for hydraulic dampers with viscous flow losses.
Hydraulische Dämpfer mit viskosen Strdmungsverlusten sind bekanntlich Stoß- Prall- oder Schwingungsdämpfer, in welchen vorwiegend viskositätsbedingte Strömungsverluste, die meistens durch eine laminare Kanalströmung einer hochviskosen Flüssigkeit erzeugt werden, in Wärme umgesetzt werden.Hydraulic dampers with viscous flow losses are known Shock, impact or vibration dampers, in which mainly viscosity-related Flow losses, which are mostly caused by a laminar channel flow of a highly viscous Liquid can be generated, converted into heat.
Um die gewünschten viskositätebedingten Strömungsverluste in möglichst kurzen Strömungskanälen zu erzeugen, verwendet man Flüssigkeiten, die durch die Beimischung on Feststoffen zu einer Trägerflüasigkeit sehr hochviskos gemacht werden. Bekannt ist die Beimischung mineralischer Feststoffe wie Graphit oder Talk.In order to achieve the desired viscosity-related flow losses as far as possible To create short flow channels, one uses liquids flowing through the Admixture of solids to a carrier liquid can be made very highly viscous. The admixture of mineral solids such as graphite or talc is known.
Der Nachteil dieser mineralischen Feststoffe ist, daß sie nur mit unwirtschaftlich großem Aufwand zu so feinen und gleichmäßigen Korngrößen zerkleinert werden können, daß eine für die Trägerflüssigkeit und die kleinsten vorhandenen Korngrößen ausreichends Dichtung der Suspension im Dämpfer erreicht werden kann.The disadvantage of these mineral solids is that they only contain Uneconomically large effort comminuted to such fine and uniform grain sizes can be that one for the carrier liquid and the smallest available Grain sizes sufficient sealing of the suspension in the damper can be achieved.
Ein weiterer Nachteil dieser Suspensionen ist, daß sie nicht stabil sind, weil die hohe Dichte der Mineralien und die große Korngröße des Füllstoffes bei längerer Ruhe zu einer Phasentrennung von Füllstoff und Trägerflüssigkeit führen.Another disadvantage of these suspensions is that they are not stable are because of the high density of the minerals and the large grain size of the filler lead to phase separation of filler and carrier liquid if left idle for a longer period of time.
Darüberhinaus wird bei dynamischen Dichtungen an der Dichtstelle ein Film der Trägerflüssigkeit ausgetragen, sodaß eine Flüssigkeitsverarmung der Suspension im Dämpfer eintritt, die mit einer starken Visknsitätsänderung einhergeht. Durch die Viskositätsänderung werden aber die viskositätsbedingten Strömungsverluste in den Stramungsknälen erhöht, sodaß sich die Dämpfeigenschaften des Stoßdämpfers ändern.In addition, in the case of dynamic seals, a Film of the carrier liquid discharged, so that a liquid depletion of the suspension occurs in the damper, which is accompanied by a sharp change in viscosity. By the viscosity change but the viscosity-related flow losses in the tension buckles increased, so that the damping properties of the shock absorber change.
Der Erfindung liegt die Aufgabe zugrunde, dieee Nachteile zu vermeiden. Dies geschisht erfindungsgemäß dadurch, daß man der Trägerflüssigkeit als Füllstoff Ruß zufügt.The invention is based on the object of avoiding these disadvantages. According to the invention, this is achieved by using the carrier liquid as a filler Adds soot.
Ruß hat nämlich mit 1,8 g/cm3 eine erheblich niedrigere Dichte als mineralische Füllstoffe, sodaß eine Sedimentation langsamer verläuft.At 1.8 g / cm3, soot has a significantly lower density than mineral fillers, so that sedimentation is slower.
Die Teilchengröße preiswerten, handelsüblichen Rußes liegt in der GröSenordnung von 10'8 m und damit im Bereich der Teilchengröße der Feststoffe kolloidaler Systeme. Sie ist um zwei Größenordnungen kleiner als die für dynamische Dichtstsllen in der Hydraulik übliche Oberflächenrauhigkeit.The particle size of inexpensive, commercially available carbon black is in Order of magnitude of 10'8 m and thus in the range of the particle size of the colloidal solids Systems. It is two orders of magnitude smaller than that for dynamic sealing joints Surface roughness common in hydraulics.
Deshalb wird durch den Dichtspalt dynamischer Dichtstellen nicht die Trägerflüssigkeit allein, sondern allenfalls kolloide Dämpfungemasse ausgetragen. Die Flüsslgkeitsverarmung der Dämpfungamaase und die damit verbundene \Jiskoeitätsänderung findet deshalb nicht statt.Therefore, through the sealing gap of dynamic sealing points, the Carrier liquid alone, but at most colloidal damping mass discharged. The fluid depletion of the dampening masseuse and the associated change in viscosity therefore does not take place.
Besonders vorteilhaft verwendet man Ruße mit geringen Veraschungsrückständen, weil sie die geringste abrasive Wirkung zeigen.It is particularly advantageous to use carbon blacks with low incineration residues, because they show the least abrasive effect.
Es ist ferner vorteilhaft, der Dämpfungsmasse Kieselsäure als Additiv in geringen Mengen beizufügen. Man erreicht damit nämlich nicht nur eine Erhöhung der Viskosität, sondern auch eine weit höhere Stabilität der Viskosität über einen weiten Temperaturbereich. Dadurch wird die Dämpfcharakteristik des Dämpfers temperaturunabhängiger.It is also advantageous to use silica as an additive to the damping compound to be enclosed in small quantities. You don't just get an increase the viscosity, but also a much higher stability of the viscosity over a wide temperature range. This makes the damping characteristics of the damper more temperature-independent.
Vorzugeweise verwendet man pyrogene Kieselsäure mit möglichst geringer TeilchengröAe. Insbesondere soll die TeiLchengröße der Kieselsäure kleiner als die des Rußes sein, weil dadurch die abrasive Wirkung der harten Kieselsäure sich nicht stark auswirken kann.It is preferable to use fumed silica with as little as possible Particle size. In particular, the particle size of the silica should be smaller than the of the soot, because this does not reduce the abrasive effect of the hard silica can have a strong impact.
Darüberhinaus können der Dämpfungamasse auch noch andere Additive beispielsweise zur Erhöhung der Alterungsbeständigkeit oder zur Erzielung besonderer rheologischer Eigenschaften zugesetzt werden.In addition, the damping compound can also contain other additives for example to increase the aging resistance or to achieve special ones rheological properties are added.
Claims (6)