CN2747055Y - 高白亮度涂层膜 - Google Patents
高白亮度涂层膜 Download PDFInfo
- Publication number
- CN2747055Y CN2747055Y CN 200420094667 CN200420094667U CN2747055Y CN 2747055 Y CN2747055 Y CN 2747055Y CN 200420094667 CN200420094667 CN 200420094667 CN 200420094667 U CN200420094667 U CN 200420094667U CN 2747055 Y CN2747055 Y CN 2747055Y
- Authority
- CN
- China
- Prior art keywords
- layer
- titanium dioxide
- coated film
- transparent resin
- whitening agent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种高白亮度涂层膜,其特点是至少具有三层结构,由底层至面层分别是树脂纤维层、钛白粉填料层和透明树脂层,在透明树脂层内混入有荧光增白剂。由于荧光增白剂与钛白粉位于不同的分层,而且荧光增白剂所在的透明树脂层位于钛白粉填料层的上方,因此钛白粉对紫外光的吸收作用不会影响荧光增白剂的充分激发,使得荧光增白剂能起到有效的消黄作用,无需再利用蓝色颜料来消黄,由此又能使钛白粉充分发挥提高亮度的作用,使涂层膜兼具有高亮度和高白度的效果。
Description
技术领域
本实用新型涉及涂层膜的结构,特别是在广告、家居装修、影视制作等场合作为白场背景使用的涂层膜。
背景技术
在广告、家居装修、影视制作等场合,常需要利用白场背景来衬托前景。优良的白场背景应当在常规光源下具有高白、高亮度,如此才能使前景在背景下获得优良的复视效果。目前人们常用一种涂层膜作为白场背景。这种涂层膜是在一层纤维层上涂覆一层聚氯乙烯。为了使涂层膜具有高亮度的效果,在聚氯乙烯层内加入有钛白粉,以提高涂层膜对光的反射作用,达到高亮度的效果。但钛白粉色温在4500K以下,色相偏黄,因此在聚氯乙烯层内还需加入荧光增白剂,其目的是利用荧光增白剂发出的蓝光与钛白粉所反射的偏黄光混合形成色温在5000K~6500K的白光,以提高涂层膜的白度。但不巧的是荧光增白剂需要紫外光来激发,而钛白粉恰好对紫外光有很强的吸收作用,因此荧光增白剂起到的作用非常有限,并不能达到消黄的目的。为此,已有技术还需在聚氯乙烯层内加入蓝色颜料,以提高消黄效果,但这样又会降低亮度。由此可见,已有技术始终无法使涂层膜兼具有高亮度和高白度的效果。
发明内容
本实用新型的目的是提供一种兼具有高亮度和高白度效果的涂层膜。
本实用新型是这样实现的:涂层膜至少具有三层结构,由底层至面层分别是树脂纤维层、钛白粉填料层和透明树脂层,在透明树脂层内混入有荧光增白剂。由于荧光增白剂与钛白粉位于不同的分层,而且荧光增白剂所在的透明树脂层位于钛白粉填料层的上方,因此钛白粉对紫外光的吸收作用不会影响荧光增白剂的充分激发,使得荧光增白剂能起到有效的消黄作用,无需再利用蓝色颜料来消黄,由此又能使钛白粉充分发挥提高亮度的作用,使涂层膜兼具有高亮度和高白度的效果。
本实用新型的优点是能够有效地利用荧光增白剂发出的蓝光与钛白粉所反射的偏黄光混合形成色温在5000K~6500K的白光,使涂层膜具有人眼最喜爱的5000~6500K色温,以该涂层膜作为白场背景可增强人眼对“白”的感觉,使前景在白场背景下获得优良的复视效果。
附图说明
图1是涂层膜实施例的横截面结构示意图。
具体实施方式
参见图1,本实施例的涂层膜具有四层结构,由底层至面层分别是树脂纤维层1、钛白粉填料层2、图案颜料层3和透明树脂层4,在透明树脂层4内混入有荧光增白剂5。荧光增白剂5可采用荧光增白剂OB或者OB-1。树脂纤维层1是树脂和纤维的混合物,起到保护其他各层的作用。图案颜料层3的作用是使涂层膜具有图案。如果涂层膜不需要图案,则可将图案颜料层3省去。图案颜料层3所用的颜料可采用普通的印刷油墨,也可采用各种具射光性的颜料,如珠光素、金银粉、镭射粉等等,使图案具有闪闪发光的效果。钛白粉填料层2可用胶水与钛白粉混合,并加入碳酸钙、滑石粉等填料6混合而成,其中胶水起粘合作用,碳酸钙、滑石粉等填料起填充作用,以降低成本。由于碳酸钙、滑石粉的反射光通常会略带黄色,因此相应地在钛白粉填料层2内最好再混入荧光增白剂7。虽然钛白粉会影响荧光增白剂的效果,但由于碳酸钙、滑石粉的反射光只是略微偏黄,因此在钛白粉填料层内加入荧光增白剂仍能起到对填料进行消黄的作用。
作为最佳实施方式,本实施例的钛白粉填料层2的上表面为凹凸不平的表面,如此可增加该层的反光面积,而且能增强与上一层的粘结强度。同理,钛白粉填料层2的下表面也是凹凸不平的表面,以此增强钛白粉填料层与下一层的粘结强度。为了提高涂层膜的耐用性以及保光、保色性,最底层的树脂纤维层1所用的树脂,以及最上层的透明树脂层4最好采用丙稀酸类树脂。涂层膜的制作方法可采用逐层叠加的方式,首先在树脂纤维层1的上表面涂覆一层以胶水、荧光增白剂7和填料6混合而成的糊状钛白粉填料层2,待钛白粉填料层2干固后,再于其上表面涂覆颜料,构成所需要的图案,最后再往已干固的图案颜料层3上涂覆混入有荧光增白剂5的透明树脂,待透明树脂干固后便形成透明树脂层4,至此完成涂层膜的制作。在上述制作过程中,各层之间已能自然粘结成一体。
Claims (6)
1、一种高白亮度涂层膜,其特征是:涂层膜至少具有三层结构,由底层至面层分别是树脂纤维层、钛白粉填料层和透明树脂层,在透明树脂层内混入有荧光增白剂。
2、如权利要求1所述的高自亮度涂层膜,其特征是:在钛白粉填料层与透明树脂层之间设置有图案颜料层。
3、如权利要求1所述的高白亮度涂层膜,其特征是:在钛白粉填料层内混合有碳酸钙和滑石粉。
4、如权利要求3所述的高白亮度涂层膜,其特征是:在钛白粉填料层内混合有荧光增白剂。
5、如权利要求1所述的高白亮度涂层膜,其特征是:钛白粉填料层的上表面为凹凸不平的表面。
6、如权利要求5所述的高白亮度涂层膜,其特征是:钛白粉填料层的下表面为凹凸不平的表面。