Prior art keywords
welded
direct
steel
utility
steel jaw
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 02268640
Other languages
Chinese (zh)
Inventor
李学信
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 02268640 priority Critical patent/CN2561798Y/en
Application granted granted Critical
Publication of CN2561798Y publication Critical patent/CN2561798Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Bulkheads Adapted To Foundation Construction (AREA)

Abstract

The utility model discloses a direct-blast welded cast steel jaw, which is characterized in that a transition connector made of aluminum sheet is directly welded with the steel jaw through direct-blast welding. The utility model has unique proposal that, due to the transition connector (aluminum sheet) being directly welded on the steel jaw through the direct-blast welding method, steel panel can be eliminated in ordinary connectors in ordinary blast welding process; in actual use, a guide bar only needs to be welded with the aluminum sheet on the steel jaw; the conductive area can reach 100 percent, so as to greatly enlarge the conductive performance and effectively lower the electric energy consumption in aluminum electrolyzing; therefore, the ecnomic effects are quite considerable.

Description

Straight quick-fried formula casting steel claw
Affiliated technical field
The utility model belongs to aluminium cell electrode casting steel claw technical field, and what relate generally to is a kind of straight quick-fried formula casting steel claw.
Background technology
Existing aluminium cell electrode casting steel claw, (as shown in Figure 1) be aluminum steel blast welding block, its crossover sub 1 all must could be welded to connect with steel pawl 3 behind the steel plate welding sequence, because the direct conductive area of general quick-fried its steel plate of weldering crossover sub and steel pawl is a peripheral welds 2, only accounts for about 6% of the total area, all the other 94% are indirect conductive area, like this, will increase resistance, reduce conductivity, make the production current consumption of electrolytic aluminum big, production cost occupies high-leveled and difficult following.
Summary of the invention
The purpose of this utility model promptly produces thus, proposes a kind of straight quick-fried formula casting steel claw.This steel pawl can not only strengthen conductivity, and can reduce the production cost of electrolytic aluminum, saves electric energy.
For achieving the above object, the utility model is achieved through the following technical solutions: its crossover sub that will constitute by aluminium sheet directly with steel pawl quick-fried being welded to connect directly.
Design of the present utility model is unique, because it adopts the method for direct explosive welding that crossover sub (aluminium sheet) directly is welded on the steel pawl, deducted the steel plate in the common explosive welding crossover sub, only need during use the aluminium sheet seam on guide rod and the steel pawl is got final product, its conductive area reaches 100%, strengthened its conductivity greatly, effectively reduced the current consumption of electrolytic aluminum, the economic benefit highly significant.
Description of drawings
Accompanying drawing 1 is the structural representation of existing steel pawl.
Accompanying drawing 2 is the utility model structural representation.
Among the figure, 1, crossover sub, 2, weld seam, 3, the steel pawl.
Embodiment
In conjunction with the accompanying drawings, it is as follows to provide embodiment of the present utility model:
As shown in Figure 2, the present embodiment crossover sub 1 direct explosive welding that will be made of aluminium sheet is on steel pawl 3.Concrete welding process is: crossover sub (aluminium sheet) 1 adopts straight quick-fried formula weldprocedure welding with steel pawl 3, and guide rod and crossover sub (aluminium sheet) 1 adopts aluminium-aluminium weldering to get final product.

Claims (1)

1, a kind of straight quick-fried formula casting steel claw comprises crossover sub (1) and steel pawl (3), it is characterized in that: the direct explosive welding of the described crossover sub that is made of aluminium sheet (1) is on steel pawl (3).
CN 02268640 2002-08-02 2002-08-02 Cast steel claw welded by direct explosion process Expired - Fee Related CN2561798Y (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 02268640 CN2561798Y (en) 2002-08-02 2002-08-02 Cast steel claw welded by direct explosion process

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 02268640 CN2561798Y (en) 2002-08-02 2002-08-02 Cast steel claw welded by direct explosion process

Publications (1)

Publication Number Publication Date
CN2561798Y true CN2561798Y (en) 2003-07-23

Family

ID=33734041

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 02268640 Expired - Fee Related CN2561798Y (en) 2002-08-02 2002-08-02 Cast steel claw welded by direct explosion process

Country Status (1)

Country Link
CN (1) CN2561798Y (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101787550A (en) * 2010-03-30 2010-07-28 云南铝业股份有限公司 Connecting structure of aluminum electrolytic prebaked anode guide bar and steel jaw and preparation method thereof
CN102139410A (en) * 2011-03-14 2011-08-03 哈尔滨正晨焊接切割设备制造有限公司 Friction welder and method for repairing defective shunting of electrolytic aluminum anode
CN103769772A (en) * 2014-01-15 2014-05-07 王会智 Welding agent and welding method for welding anode steel claw
CN111453608A (en) * 2019-10-30 2020-07-28 国家电投集团黄河上游水电开发有限责任公司 Aluminum anode steel claw body erecting hanger

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101787550A (en) * 2010-03-30 2010-07-28 云南铝业股份有限公司 Connecting structure of aluminum electrolytic prebaked anode guide bar and steel jaw and preparation method thereof
CN101787550B (en) * 2010-03-30 2011-12-07 云南铝业股份有限公司 Connecting structure of aluminum electrolytic prebaked anode guide bar and steel jaw and preparation method thereof
CN102139410A (en) * 2011-03-14 2011-08-03 哈尔滨正晨焊接切割设备制造有限公司 Friction welder and method for repairing defective shunting of electrolytic aluminum anode
CN102139410B (en) * 2011-03-14 2015-09-09 哈尔滨正晨焊接切割设备制造有限公司 Repair friction-welding machine and the restorative procedure of electrolytic aluminium anode shunting badness
CN103769772A (en) * 2014-01-15 2014-05-07 王会智 Welding agent and welding method for welding anode steel claw
CN103769772B (en) * 2014-01-15 2016-04-27 王会智 A kind of anode steel claw welding method
CN111453608A (en) * 2019-10-30 2020-07-28 国家电投集团黄河上游水电开发有限责任公司 Aluminum anode steel claw body erecting hanger
CN111453608B (en) * 2019-10-30 2022-07-12 国家电投集团黄河上游水电开发有限责任公司 Aluminum anode steel claw body erecting hanger

Similar Documents

Publication Publication Date Title
CN2889597Y (en) Aluminium parent metal mould for fusion casting and welding
CN2869044Y (en) Stainless steel cathode material conducting structure for copper, nickel electrolytic refining or electrodeposition
CN202430299U (en) Combined anode steel talon welded by steel plate
CN201962378U (en) Anode conducing device for aluminum electrolytic cell
CN2561798Y (en) Cast steel claw welded by direct explosion process
CN201388025Y (en) Bolt locking-catch type intensive bus duct
CN201220320Y (en) Cathode steel bar welding device
CN2851290Y (en) Device for use in short circuit power failure in aluminium electrolytic tank
CN2700343Y (en) Cathode connecting device of aluminium cell
CN203229576U (en) Composite steel claw for aluminum electrolysis
CN201924092U (en) Embedded welding type electrolysis cathode plate
CN2685354Y (en) Connecting apparatus for aluminium electrolytic tank cathode steel bar and cathode aluminium bus
CN2806505Y (en) Anode structure for small-scale prebaked aluminum electrolytic cell
CN2716289Y (en) Aluminum-aluminum compression joint device of aluminum-electrolytic cell cathode soft bus bar
CN201340914Y (en) Copper-aluminum composite wire clamp
CN2883401Y (en) Dual-side aluminum/steel composite concave crossing cathode steel rod conductive joint
CN2615149Y (en) Cathode steel bar and bus connector of aluminium cell
CN2615148Y (en) Aluminium electrolytic cell crimp connector between cathode steel bar and cathode soft strip
CN207904381U (en) A kind of connection structure of aluminum cell cathode steel bar and slot surrounding cathode busbar
CN202576608U (en) Copper conductive stick stainless steel permanent negative electrode plate internally injected with copper solution
CN201793757U (en) Sodium chlorate electrolytic bath
CN204885841U (en) Low -voltage distribution cabinet section bar assembly structure
CN206706219U (en) A kind of anode rod component
CN201439187U (en) Special tool for body-in-white fender construction bolt
CN204980791U (en) Shrouding about door of detachable elevator glass layer

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee