CN206154792U - Glass cover plate - Google Patents

Glass cover plate Download PDF

Info

Publication number
CN206154792U
CN206154792U CN201621029837.XU CN201621029837U CN206154792U CN 206154792 U CN206154792 U CN 206154792U CN 201621029837 U CN201621029837 U CN 201621029837U CN 206154792 U CN206154792 U CN 206154792U
Authority
CN
China
Prior art keywords
glass
substrate
cover
woven wire
glass substrate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201621029837.XU
Other languages
Chinese (zh)
Inventor
吴广剑
黄晓辉
乔传方
吴小三
仲云华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinhu Yu Di Optical Co Ltd
Original Assignee
Jinhu Yu Di Optical Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jinhu Yu Di Optical Co Ltd filed Critical Jinhu Yu Di Optical Co Ltd
Priority to CN201621029837.XU priority Critical patent/CN206154792U/en
Application granted granted Critical
Publication of CN206154792U publication Critical patent/CN206154792U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model relates to a glass cover plate, including glass substrate (1), glass substrate (1) tow sides all are provided with woven wire (2), woven wire (2) outside still is provided with one deck substrate glass (3), be located high -refractive -index medium layer (4) and semi reflecting layer (5) have set gradually on glass substrate (1) positive substrate glass (3), be located strengthening film layer (6) and glue film (7) have set gradually on substrate glass (3) of glass substrate (1) reverse side. The utility model discloses set up woven wire between substrate glass and glass substrate, strengthened glass cover plate's intensity, made it not fragile.

Description

A kind of cover-plate glass
Technical field
The utility model is related to a kind of mobile phone screen glass, and in particular to a kind of cover-plate glass.
Background technology
Mobile phone is a kind of very big communication products of consumption figure, meets the needs of people's communication.With sending out for smart mobile phone Exhibition, mobile phone screen is increasing, and the glass demand of Mobile phone screen is also increasing.The quality of Mobile phone screen quality is directly connected to Mobile phone quality and cost of manufacture.Common mobile phone panel glass is not enough on anti-soil and intensity, or relatively costly.Exploitation is a kind of Low cost and stain resistance are strong, not breakable mobile phone panel glass is needs.
In view of above-mentioned defect, the design people, positive research and innovation in addition, to founding a kind of cover plate of new structure Glass so as to more the value in industry.
The content of the invention
To solve above-mentioned technical problem, the purpose of this utility model is to provide a kind of hand-set lid glass of high intensity.
Power technology scheme of the present utility model is as follows:
A kind of cover-plate glass, including glass substrate (1), glass substrate (1) tow sides are provided with woven wire (2), woven wire (2) outside is additionally provided with one layer of substrate glass (3);Positioned at the positive substrate of the glass substrate (1) High refractive index medium layer (4) and semi-reflective layer (5) are disposed with glass (3);Positioned at the lining of the glass substrate (1) reverse side Reinforcing film layer (6) and glue-line (7) are disposed with bottom glass (3).
Further:The tow sides etching of the glass substrate (1) is fluted, positioned at the glass substrate (1) front Groove in set gradually the woven wire (2), the substrate glass (3), high refractive index medium layer (4) and semi-reflective layer (5) woven wire (2), the substrate glass (3), institute, are set gradually in the groove of the glass substrate (1) reverse side State reinforcing film layer (6) and the glue-line (5).
Further:The groove is dovetail groove.
Further:The glass substrate (1) is aluminum based metallic glass.
Further:The glass substrate (1) is sapphire material.
Further:The woven wire (2) is crisscross woven wire.
Further:The thickness of the glass substrate (1) is 0.5-0.8mm.
Further:Reinforcing film layer (6) is polyamide adipose membrane, and the thickness of the reinforcing film layer (6) is that 10-20 is micro- Rice.
Further:The substrate glass (2) is silica glass, and its thickness is 0.3-0.5mm.
By such scheme, the utility model at least has advantages below:
1) the utility model is provided with woven wire between substrate glass and glass substrate, increases the intensity of glass, It is hardly damaged it;
2) the utility model makes additional other assemblies on the glass substrate be positioned at glass substrate by etched recesses On, groove is dovetail groove, it is possible to achieve more preferable locating effect.
Described above is only the general introduction of technical solutions of the utility model, in order to better understand skill of the present utility model Art means, and being practiced according to the content of specification, with preferred embodiment of the present utility model and coordinate accompanying drawing detailed below Describe in detail bright as after.
Description of the drawings
Fig. 1 is the structural representation of high strength cap glass sheet disclosed in the utility model;
In figure:1- glass substrates;2- woven wires;3- substrate glass;4- high refractive index medium layers;5- semi-reflective layers;6- Reinforcing film layer;7- glue-lines.
Specific embodiment
With reference to the accompanying drawings and examples, specific embodiment of the present utility model is described in further detail.Below Embodiment is used to illustrate the utility model, but is not limited to scope of the present utility model.
Referring to Fig. 1, the preferred embodiment of the utility model one
A kind of cover-plate glass, including glass substrate 1, the tow sides of glass substrate 1 are provided with woven wire 2, wire The outside of net 2 is additionally provided with one layer of substrate glass 3;High index of refraction is disposed with the positive substrate glass 3 of glass substrate 1 Dielectric layer 4 and semi-reflective layer 5;Reinforcing film layer 6 and glue-line 7 are disposed with the substrate glass 3 of the reverse side of glass substrate 1.
By arranging woven wire 2, the intensity of mobile phone glass is enhanced, by arranging high refractive index medium layer 4, reduced The thickness of mobile phone glass, by arranging semi-reflective layer 5, to realize reaching stable reflectivity in wide wave-length coverage and penetrate Rate is combined, and by arranging reinforcing film layer 6, increases mobile phone glass plastic property, by arranging glue-line 7, makes mobile phone glass and hand Machine screen is relatively fixed.
For optimum position effect, the tow sides etching of glass substrate 1 is fluted, positioned at the recessed of the reverse side of glass substrate 1 Woven wire 2, substrate glass 3, high refractive index medium layer 4 and glue-line 5 are set gradually in groove, it is positive positioned at glass substrate 1 Woven wire 2, substrate glass 3, semi-reflective layer 6, reinforcing film layer 7, radiation protective layer 8 and scratch resistant layer 9 are set gradually in groove.
Above-mentioned groove is dovetail groove.
Glass substrate 1 is aluminum based metallic glass or sapphire material.
Woven wire 2 is crisscross woven wire.
The thickness of glass substrate 1 is 0.5-0.8mm.
Reinforcing film layer 6 is polyamide adipose membrane, and the thickness for strengthening film layer 6 is 10-20 microns.
Substrate glass 2 is silica glass, and its thickness is 0.3-0.5mm.
The utility model at least has advantages below:
The utility model is provided with woven wire between substrate glass and glass substrate, increases the strong of cover-plate glass Degree so as to be hardly damaged.
The above is only preferred embodiment of the present utility model, is not limited to the utility model, it is noted that For those skilled in the art, on the premise of without departing from the utility model know-why, can also do Go out some improvement and modification, these are improved and modification also should be regarded as protection domain of the present utility model.

Claims (9)

1. a kind of cover-plate glass, it is characterised in that:Including glass substrate (1), glass substrate (1) tow sides are provided with Woven wire (2), woven wire (2) outside is additionally provided with one layer of substrate glass (3);Positioned at the glass substrate (1) just High refractive index medium layer (4) and semi-reflective layer (5) are disposed with the substrate glass (3) in face;Positioned at the glass substrate (1) Reinforcing film layer (6) and glue-line (7) are disposed with the substrate glass (3) of reverse side.
2. a kind of cover-plate glass according to claim 1, it is characterised in that:The tow sides erosion of the glass substrate (1) Groove is carved with, the woven wire (2), the substrate glass are set gradually in the positive groove of the glass substrate (1) (3), high refractive index medium layer (4) and semi-reflective layer (5), in the groove of the glass substrate (1) reverse side institute is set gradually State woven wire (2), the substrate glass (3), reinforcing film layer (6) and the glue-line (7).
3. a kind of cover-plate glass according to claim 2, it is characterised in that:The groove is dovetail groove.
4. a kind of cover-plate glass according to claim 1, it is characterised in that:The glass substrate (1) is aluminium based metal glass Glass.
5. a kind of cover-plate glass according to claim 1, it is characterised in that:The glass substrate (1) is sapphire material.
6. a kind of cover-plate glass according to claim 1, it is characterised in that:The woven wire (2) is crisscross Woven wire.
7. a kind of cover-plate glass according to claim 1, it is characterised in that:The thickness of the glass substrate (1) is 0.5- 0.8mm。
8. a kind of cover-plate glass according to claim 1, it is characterised in that:Reinforcing film layer (6) is polyamide adipose membrane, The thickness of reinforcing film layer (6) is 10-20 microns.
9. a kind of cover-plate glass according to claim 1, it is characterised in that:The substrate glass (3) is silica glass Glass, its thickness is 0.3-0.5mm.
CN201621029837.XU 2016-08-31 2016-08-31 Glass cover plate Expired - Fee Related CN206154792U (en)