CN205575939U - Anti -oxidation laminated glass that comes unstuck - Google Patents

Anti -oxidation laminated glass that comes unstuck Download PDF

Info

Publication number
CN205575939U
CN205575939U CN201620003005.4U CN201620003005U CN205575939U CN 205575939 U CN205575939 U CN 205575939U CN 201620003005 U CN201620003005 U CN 201620003005U CN 205575939 U CN205575939 U CN 205575939U
Authority
CN
China
Prior art keywords
glass
layer
ground floor
thickness
laminated glass
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201620003005.4U
Other languages
Chinese (zh)
Inventor
王祥甫
陈�峰
潘国华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xiangyang Fodico Photoelectric Technology Co Ltd
Original Assignee
Xiangyang Fodico Photoelectric Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xiangyang Fodico Photoelectric Technology Co Ltd filed Critical Xiangyang Fodico Photoelectric Technology Co Ltd
Priority to CN201620003005.4U priority Critical patent/CN205575939U/en
Application granted granted Critical
Publication of CN205575939U publication Critical patent/CN205575939U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides an anti -oxidation laminated glass that comes unstuck. It includes first layer glass, second floor glass and presss from both sides locates the hollow layer between first layer glass and the second floor glass, the side surface has the rete in the first layer glass, the rete is the transparent film structure, and its area equals the area of side surface in the first layer glass the periphery of rete is provided with the round layer of borduring, compresses tightly at first layer glass edge the rete is sealed, and the width on the layer of borduring is less than 10mm, and thickness is less than hollow layer's thickness. The device of the utility model is simple in structure, the structure is wrapped by adoption limit portion, reduces the oxidation rate of coming unstuck, does not influence the light percent of pass simultaneously.

Description

Anti-oxidation degumming laminated glass
Technical field
This utility model relates to the furnace equipment technical field in glass processing, particularly relates to a kind of anti-oxidation degumming laminated glass.
Background technology
Coated laminated glass is usually used in building curtain wall, building decoration, automotive window, etc., it is the novel glass of a kind of energy-conservation environmental protection again.Being only limited to white glass interlayer in the market, its function only has sound insulation, anti-fragment to drop.For increasing function, form function plated film, so that laminated glass not only has sound insulation, a function that anti-fragment drops, but also possess that color is diversified, heat insulation, the gear function such as ultraviolet, selective transmitance.
Laminated glass, sometimes referred to as compound glass, as the term suggests, at least including layer glass, glass is bonded by viscose glue between layers, for some function, such as, heat insulation, the gear functional requirement such as ultraviolet, sound insulation, transmitance selection, on the surface of glassy layer, there is functional film layer.In existing laminated glass structure, viscose glue generally bonds with functional film layer.But, can start inwardly to engender oxidation from the film layer of edge during glass sandwich, cause interlayer degumming.
Accordingly, it is desirable to provide a kind of new laminated glass, with the problem of the interlayer degumming that edge oxidation after solving tradition low radiation coated glass interlayer causes.
Summary of the invention
Technical problem to be solved in the utility model is the technical deficiency for above-mentioned existence, it is provided that a kind of simple in construction, uses edge binding structure for binding, reduces oxidation degumming rate, does not affect the anti-oxidation degumming laminated glass of light percent of pass simultaneously.
This utility model solves its technical problem and be the technical scheme is that
Anti-oxidation degumming laminated glass, it is characterized in that: it includes ground floor glass, second layer glass and is located in the hollow layer between ground floor glass and second layer glass, described ground floor glass inner side surface has film layer, described film layer is hyaline membrane structure, its area is equal to the area on described ground floor glass inner side surface, periphery at described film layer is provided with a circle edging layer, film layer is sealed and is pressed on ground floor glass edge, the width of edging layer is less than 10mm, and thickness is less than the thickness of hollow layer.
In such scheme, the thickness range of described hollow layer is 2mm-5mm.
In such scheme, described ground floor glass and the marginal portion of second layer glass are for sealing structure.
In such scheme, the gross thickness of described laminated glass between 6mm-15mm, described ground floor glass, second layer glass thickness respectively between 2mm-5mm, the thickness of described film layer is between 60nm-300nm.
Of the present utility model mainly provide the benefit that:
This utility model apparatus structure is simple, uses edge binding structure for binding, reduces oxidation degumming rate, does not affect light percent of pass simultaneously.
Accompanying drawing explanation
Fig. 1 is this utility model example structure figure
In figure: 1, ground floor glass;2, second layer glass;3, hollow layer;4, film layer;5, edging layer.
Detailed description of the invention
Below in conjunction with detailed description of the invention, this utility model embodiment is further described:
Anti-oxidation degumming laminated glass as shown in Figure 1, it includes ground floor glass 1, second layer glass 2 and the hollow layer 3 being located between ground floor glass 1 and second layer glass 2, described ground floor glass 1 inner surface has film layer 4, described film layer 4 is hyaline membrane structure, its area is equal to the area of described ground floor glass 1 inner surface, periphery at described film layer 4 is provided with a circle edging layer 5, film layer 4 is sealed and is pressed on ground floor glass edge, the width of edging layer 5 is less than 10mm, and thickness is less than the thickness of hollow layer 3.
In the present embodiment, the thickness range 5mm of described hollow layer 3.
In the present embodiment, described ground floor glass 1 and the marginal portion of second layer glass 2 are for sealing structure.
In the present embodiment, the gross thickness of described laminated glass is 15mm, and described ground floor glass 1, the thickness of second layer glass 2 are 5mm, and the thickness of described film layer is 100nm.
Protection domain of the present utility model is not limited to the above embodiments, it is clear that those skilled in the art can carry out various change and deformation without deviating from scope and spirit of the present utility model to this utility model.If these are changed and deformation belongs in the range of this utility model claim and equivalent technologies thereof, intention the most of the present utility model also comprises these and changes and deformation.

Claims (4)

  1. The most anti-oxidation degumming laminated glass, it is characterized in that: it includes ground floor glass, second layer glass and is located in the hollow layer between ground floor glass and second layer glass, described ground floor glass inner side surface has film layer, described film layer is hyaline membrane structure, its area is equal to the area on described ground floor glass inner side surface, periphery at described film layer is provided with a circle edging layer, film layer is sealed and is pressed on ground floor glass edge, the width of edging layer is less than 10mm, and thickness is less than the thickness of hollow layer.
  2. Anti-oxidation degumming laminated glass the most as claimed in claim 1, it is characterised in that the thickness range of described hollow layer is 2mm-5mm.
  3. Anti-oxidation degumming laminated glass the most as claimed in claim 1, it is characterised in that described ground floor glass and the marginal portion of second layer glass are for sealing structure.
  4. Anti-oxidation degumming laminated glass the most as claimed in claim 1, it is characterized in that, the gross thickness of described laminated glass between 6mm-15mm, described ground floor glass, second layer glass thickness respectively between 2mm-5mm, the thickness of described film layer is between 60nm-300nm.
CN201620003005.4U 2016-01-05 2016-01-05 Anti -oxidation laminated glass that comes unstuck Expired - Fee Related CN205575939U (en)