CN202201993U - 一种电积镍的阴极结构 - Google Patents
一种电积镍的阴极结构 Download PDFInfo
- Publication number
- CN202201993U CN202201993U CN2011202679131U CN201120267913U CN202201993U CN 202201993 U CN202201993 U CN 202201993U CN 2011202679131 U CN2011202679131 U CN 2011202679131U CN 201120267913 U CN201120267913 U CN 201120267913U CN 202201993 U CN202201993 U CN 202201993U
- Authority
- CN
- China
- Prior art keywords
- nickel
- electro deposited
- deposited nickel
- cathode
- cathode structure
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种镍精炼生产的电积镍的阴极结构。其阴极结构包括为镍始极片的阴极,其特征在于在其结构还包括由一水平条板和两个分别垂直固接于水平条板端头的重直条板形成“U”型框体,在“U”型框体内侧开有能嵌入为镍始极片的阴极的凹槽。本实用新型制作工艺简单、使用寿命长、操作方便的特点,解决了电积镍生产中存在的技术难题,对提升电积镍质量、降低隔膜袋消耗、降低职工劳动强度、提高劳动生产率具有重要意义。
Description
技术领域
本实用新型涉及一种镍精炼生产的电积镍的阴极结构。
背景技术
目前,镍电积通常采用不溶阳极隔膜电解生产工艺,阳极为Pb-Ca-Sr-Ag四元铅合金阳极板,阴极为镍始极片,两块阳极对应一块阴极。在生产中由于阴阳极边部电力线比较密集,局部电流密度偏高,导致电积镍边部形成结粒,影响产品质量;另一方面由于电积槽同极距小,电积镍生产过程中易出现粘袋、增加隔膜袋消耗,使电积镍加工成本上升,同时增加职工劳动强度,影响产品质量。
发明内容
本实用新型的目的就是针对上述已有技术存在的不足,提供一种能有效解决不溶阳极电积生产中电积镍易长边部结粒及粘袋现象,提高电积镍物理外观质量,优化操作,提高劳动生产率的电积镍的阴极结构。
本实用新型的目的是通过以下技术方案实现的。
一种电积镍的阴极结构,其阴极结构包括为镍始极片的阴极,其特征在于在其结构还包括由一水平条板和两个分别垂直固接于水平条板端头的重直条板形成的“U” 型框体,在“U” 型框体内侧开有能嵌入为镍始极片的阴极的凹槽。
本实用新型的一种电积镍的阴极结构,能有效改善阴极电力线分布,使阴极各处电力线均匀分布,杜绝电积镍边部结粒、粘袋现象,提高产品质量,优化操作,提高劳动生产率。有效解决产品物理外观质量缺陷、粘袋及劳动强度大等问题,并为电镍产品的剪切和包装创造良好条件。
附图说明
图1为本实用新型的结构示意图。
图2为图1的俯视图。
图3为图1的A—A剖面图。
具体实施方式
一种电积镍的阴极结构,其阴极结构包括为镍始极片的阴极1,其特征在于在其结构还包括由一水平条板和两个分别垂直固接于水平条板端头的重直条板形成的“U” 型框体2,在“U” 型框体内侧开有能嵌入为镍始极片的阴极的凹槽。
操作时,将“U” 型框体置于镍电积槽阴极室隔膜袋内,再将为镍始极片的阴极嵌入“U” 型框体内侧的凹槽。“U” 型框体改善了阴极电力线分布,解决了电积镍边部结粒、阴极粘袋、劳动强度大等问题,取得了良好效果。此新材料的开发和应用,提高了电积镍物理外观质量,降低隔膜袋消耗,优化了生产操作,提高了劳动生产率。
Claims (1)
1.一种电积镍的阴极结构,其阴极结构包括为镍始极片的阴极,其特征在于在其结构还包括由一水平条板和两个分别垂直固接于水平条板端头的重直条板形成的“U” 型框体,在“U” 型框体内侧开有能嵌入为镍始极片的阴极的凹槽。