CN201807706U - 一种空心铸锭用双段式结晶器 - Google Patents
一种空心铸锭用双段式结晶器 Download PDFInfo
- Publication number
- CN201807706U CN201807706U CN2010205433285U CN201020543328U CN201807706U CN 201807706 U CN201807706 U CN 201807706U CN 2010205433285 U CN2010205433285 U CN 2010205433285U CN 201020543328 U CN201020543328 U CN 201020543328U CN 201807706 U CN201807706 U CN 201807706U
- Authority
- CN
- China
- Prior art keywords
- crystallizer
- cast
- pouring
- conventional cylindrical
- section type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型属于金属合金化铸造设备技术领域,涉及一种空心铸锭用双段式结晶器,由芯头构件、常规圆筒形结晶器(3)两部分构成;所述芯头构件具有浇注池(1),浇注池(1)外侧套置有保护作用的金属套(2),浇注池(1)与成型芯头(4)上部螺纹连接;所述芯头构件通过浇注池(1)与常规圆筒形结晶器(3)卡接连接,芯头构件的成型芯头(4)与常规圆筒形结晶器(3)之间构成环形浇注腔室;所述浇注池(1)底面具有浇注口,浇注口与芯头上部的浇注通道(5)连接,浇注通道(5)与成型芯头(4)、常规圆筒形结晶器(3)之间的环形浇注腔室连通。本实用新型具有结构简单、操作方便、成本低、使用效果好的特点。
Description
技术领域
本实用新型属于金属合金化铸造设备技术领域,主要涉及一种空心铸锭用双段式结晶器,用于立式铸造空心铜合金铸锭。
背景技术
目前,铜合金铸造中多采用无芯的结晶器来铸造实心铜合金铸锭。若要铸造空心铸锭,必然要设计新型结构的结晶器,用以适应空心铸锭的生产。铸造空心铜合金铸锭的技术现在国内并不多见,仅有水平铸造空心锭的技术,此技术不能铸造大规格的空心铸锭。
要实现大规格铜合金空心铸锭的生产,结晶器是技术的难点和关键。由于大规格空心铜合金铸锭在结晶冷却中释放大量的热量,及时冷却、带走热量十分重要。空心锭结晶冷却收缩快,为了解决熔液补给及时、成型下拉不断芯头、内部组织晶粒均匀无缺陷,表面无瘤疤等三方面的工艺与质量问题,需要结合空心锭的铸造技术实际,研制适合生产、满足工艺与质量要求的结晶器。
发明内容
本实用新型的目的是提出一种空心铸锭用双段式结晶器,使铸造金属合金产品的内部晶粒细化、均匀,内部组织的强度和性能大幅提高,有效控制铸造空心铜合金铸锭的内、外表面缺陷。
本实用新型完成其发明任务所采用如下技术方案是:
一种空心铸锭用双段式结晶器,由芯头构件、常规圆筒形结晶器两部分构成;所述芯头构件具有浇注池,浇注池外侧套置有保护作用的金属套,浇注池与成型芯头上部螺纹连接,构成芯头构件;所述芯头构件通过浇注池与常规圆筒形结晶器卡接连接,芯头构件的成型芯头与常规圆筒形结晶器之间构成环形浇注腔室;所述浇注池底面具有浇注口,浇注口与芯头上部的浇注通道连通,浇注通道与成型芯头、常规圆筒形结晶器之间的环形浇注腔室连通。
所述的成型芯头具有≤10°的锥度。
由于采用如上所述的技术方案,本实用新型具有如下优越性:
该结晶器与现有技术相比,具有结构简单、操作方便、成本低、使用效果好的优点,能够使铸造金属合金产品的内部晶粒细化、均匀,内部组织的强度和性能大幅提高,铸造空心铜合金铸锭的内、外表面缺陷得到有效控制。
附图说明
图1是空心铸锭用双段式结晶器的结构示意图。
图中:1、浇注池;2、金属套,3、常规圆筒形结晶器,4、成型芯头,5、浇注通道。
具体实施方式
下面结合附图和实施例对本实用新型作进一步详细说明。
如图1所示,一种空心铸锭用双段式结晶器,由芯头构件、常规圆筒形结晶器3两部分构成构成;所述芯头构件具有浇注池1,本实施例的浇注池为石墨材料制成,浇注池1外侧套置有保护作用的金属套2,保护浇注池1在温差较大的浇铸条件下不出现皲裂,安全铸造;浇注池1与成型芯头4上部螺纹连接,构成芯头构件;成型芯头4为石墨材质;所述芯头构件通过浇注池1与常规圆筒形结晶器3卡接连接,常规圆筒形结晶器3为普通的圆筒形浇注结晶器,用以单独使用时,实现常规的实心铸造。芯头构件的成型芯头4与常规圆筒形结晶器3之间构成环形浇注腔室;所述浇注池1底面具有浇注口,浇注口与芯头上部的浇注通道5连通,浇注通道5与成型芯头4、常规圆筒形结晶器3之间的环形浇注腔室连通。成型芯头具有≤10°的锥度,空心锭在铸造冷却中会向中心收缩,收缩形成的抱芯力很大,笔直的芯头在铸造中不容易向下脱模,更严重的会发生抱断芯头的情况,所以,芯头具有适度的锥度是必要的,为了保证空心锭内表面的光滑和笔直,根据实验情况成型芯头的锥度不大于10°。
使用时,把芯头构件与常规结晶器3卡接连接,铸造熔液浇注到浇注池1内,通过浇注池1的浇注口进入成型芯头4上部的浇注通道5内,经浇注通道5流入成型芯头4与常规圆筒形结晶器3之间构成的环形浇注腔室内,在环形浇注腔室内进行冷却铸造,由于成型芯头4具有一定斜度的成型空心,空心铜合金铸锭与成型芯头4之间可自由滑动,铸造拉锭阻力较小,铸造过程成型充分,铸锭质量良好。
Claims (2)
1.一种空心铸锭用双段式结晶器,其特征是:结晶器由芯头构件、常规圆筒形结晶器(3)两部分构成;所述芯头构件具有浇注池(1),浇注池(1)外侧套置有保护作用的金属套(2),浇注池(1)与成型芯头(4)上部螺纹连接,构成芯头构件;所述芯头构件通过浇注池(1)与常规圆筒形结晶器(3)卡接连接,芯头构件的成型芯头(4)与常规圆筒形结晶器(3)之间构成环形浇注腔室;所述浇注池(1)底面具有浇注口,浇注口与芯头上部的浇注通道(5)连通,浇注通道(5)与成型芯头(4)、常规圆筒形结晶器(3)之间的环形浇注腔室连通。
2.根据权利要求1所述的空心铸锭用双段式结晶器,其特征是:所述的成型芯头(4)具有≤10°的锥度。