Prior art keywords
aluminum foil
flakeboard
curing paint
ultraviolet photo
particieboard
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008200895100U
Other languages
English (en)
Inventor
丁乃今
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNU2008200895100U priority Critical patent/CN201179675Y/zh
Application granted granted Critical
Publication of CN201179675Y publication Critical patent/CN201179675Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Paints Or Removers (AREA)
  • Laminated Bodies (AREA)

Abstract

紫外线光固化漆铝箔饰面刨花板,现有市场上的各种装饰板存在很多问题。紫外线光固化漆铝箔饰面刨花板,其组成包括:刨花板(1),所述的刨花板上下面复合经过光固化漆淋涂的铝箔(2)。本产品用作建筑装饰板材。

Description

紫外线光固化漆铝箔饰面刨花板
技术领域:
本实用新型涉及一种与淋涂紫外线光固化漆的铝箔复合的防火饰面板,具体涉及一种紫外线光固化漆铝箔饰面刨花板。
背景技术:
现有市场上的各种装饰板存在很多问题,如华丽板、宝丽板防火性能差,不坚韧;刨花板、中密度纤维板表面粗糙、甲醛释放量不符合室内环保要求,各种树脂和溶剂制作的装饰材料和涂饰材料有毒有害;装饰材料的表面强度和硬度差等。
发明内容:
本实用新型的目的是提供一种与淋涂紫外线光固化漆铝箔复合的紫外线光固化漆铝箔饰面刨花板,防水、防潮、无毒害。
上述的目的通过以下的技术方案实现:
紫外线光固化漆铝箔饰面刨花板,其组成包括:刨花板,所述的刨花板上下面复合经过光固化漆淋涂的铝箔。
所述的紫外线光固化漆铝箔饰面刨花板,所述的刨花板与铝箔之间具有夹层板材。
本实用新型的有益效果:
1.本产品是用金属铝箔覆盖在刨花板表面,使刨花板内的有毒有害物质无法释放,并把金属的高强度、高硬度和防火性能与刨花板的质轻、坚挺结合起来,同时采用的光固化漆解决了采用含苯、甲醛或其它芳香烃溶剂油漆涂饰挥发固化释放出的有毒物质对人体的毒害。
2.解决了刨花板表面粗糙,不防水、易吸潮,不环保的缺点,扩大了刨花板的应用范围。
3.铝箔可制成各种颜色和印刷逼真的珍贵天然树种木纹,来替代昂贵薄木和浸渍胶膜纸饰面材料,具有防火、强度高的特点,并用紫外线光固化漆淋涂铝箔表面,提高了金属对人体皮肤的亲和力。
4.传统漆面涂抹后,在24小时内固化90%,在3个月至一年完全固化,占用场地大,要求条件高,工人劳动环境差;而本产品可完全实现日班化连续生产,无有害气体,改善劳动环境和使用环境,提高了劳动生产率,是无毒无害的绿色环保装饰板材。
5.本实用新型板材提供了一种新的完全绿色无污染装饰板材,装饰后马上可以入住,室内无任何异味,有益于装璜工作者及居家人士身体健康。
6.本实用新型板材饰面材料和漆膜阻燃,装修的房屋可以阻止火势蔓延,延长火苗进入房间的时间,从而给人带来宝贵时间。
7.本实用新型板材外观坚韧靓丽,硬度高耐磨性能好,淋涂光固化漆后能使铝箔上的色彩和花纹更加艳丽、丰满、逼真,并彰显金属饰面材料的雍荣华贵。
附图说明:
附图1是本产品的结构示意图。
具体实施方式:
实施例1:
紫外线光固化漆铝箔饰面刨花板,其组成包括:刨花板1,所述的刨花板上下面复合经过光固化漆淋涂的铝箔2,所述的铝箔为素箔、上色箔或印刷铝箔。
所述的紫外线光固化漆铝箔饰面刨花板,具有三层漆面,使得漆面层平整饱满均匀,保证漆面连续稳定不脱层。先把铝箔背面涂上金属胶合剂待其无压固化后再把刨花板涂上酚醛树脂胶粘剂,再把铝箔已固化的涂胶面贴覆在已经涂上胶的刨花板基材上,然后用附着力极强的光固化一道底漆辊涂,光固化半分于后再辊涂上第二道底漆,保证了漆面平整,为淋面漆作好了有效过渡,能避免剥落掉漆,最后淋第三层面漆,通过前面涂层的稳固结合,使第三层漆能具有坚固的附着力,淋漆后通过80℃的热流平机使得漆面更加平整,晶莹剔透,提高其光感和强度,经检验符合要求后用紫外线光固化,由此保证了在铝箔上形成稳定坚固而且美丽的漆面。
实施例2:
紫外线光固化漆铝箔饰面刨花板,其组成包括:刨花板1,所述的刨花板上下面复合经过光固化漆淋涂的铝箔2,所述的铝箔为素箔、上色箔或印刷铝箔。
所述的紫外线光固化漆铝箔饰面刨花板,所述的刨花板与铝箔之间具有夹层板材3。

Claims (2)

1.一种紫外线光固化漆铝箔饰面刨花板,其组成包括:刨花板,其特征是:所述的刨花板上下面复合经过光固化漆淋涂的铝箔。
2.根据权利要求1所述的紫外线光固化漆铝箔饰面刨花板,其特征是:所述的刨花板与铝箔之间具有夹层板材。
CNU2008200895100U 2008-03-18 2008-03-18 紫外线光固化漆铝箔饰面刨花板 Expired - Fee Related CN201179675Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNU2008200895100U CN201179675Y (zh) 2008-03-18 2008-03-18 紫外线光固化漆铝箔饰面刨花板

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNU2008200895100U CN201179675Y (zh) 2008-03-18 2008-03-18 紫外线光固化漆铝箔饰面刨花板

Publications (1)

Publication Number Publication Date
CN201179675Y true CN201179675Y (zh) 2009-01-14

Family

ID=40249178

Family Applications (1)

Application Number Title Priority Date Filing Date
CNU2008200895100U Expired - Fee Related CN201179675Y (zh) 2008-03-18 2008-03-18 紫外线光固化漆铝箔饰面刨花板

Country Status (1)

Country Link
CN (1) CN201179675Y (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2009146589A1 (zh) * 2008-06-06 2009-12-10 Ding Naijin 紫外线光固化漆铝箔饰面刨花板及其制作方法
CN101549506B (zh) * 2008-04-02 2012-09-05 丁乃今 紫外线光固化漆铝箔饰面刨花板及其制作方法
CN106003271A (zh) * 2016-05-18 2016-10-12 詹雄光 一种阻燃高强度立体实木板材及其制备方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101549506B (zh) * 2008-04-02 2012-09-05 丁乃今 紫外线光固化漆铝箔饰面刨花板及其制作方法
WO2009146589A1 (zh) * 2008-06-06 2009-12-10 Ding Naijin 紫外线光固化漆铝箔饰面刨花板及其制作方法
CN106003271A (zh) * 2016-05-18 2016-10-12 詹雄光 一种阻燃高强度立体实木板材及其制备方法

Similar Documents

Publication Publication Date Title
CN206201638U (zh) 一种无机高压防火耐磨装饰板
CN201179675Y (zh) 紫外线光固化漆铝箔饰面刨花板
US20210010203A1 (en) Stainable decorative board
CN101549506B (zh) 紫外线光固化漆铝箔饰面刨花板及其制作方法
CN201179676Y (zh) 紫外线光固化漆pvc饰面刨花板
CN102529290A (zh) 一种装饰板材的制备方法
CN2933783Y (zh) 淋涂紫外线光固漆实木皮复合的胶合板
CN202318502U (zh) 一种替换天然木皮的复合木板
WO2009146589A1 (zh) 紫外线光固化漆铝箔饰面刨花板及其制作方法
CN200945667Y (zh) 与淋涂紫外线光固漆实木皮复合的防火板
CN201002282Y (zh) 三聚氰胺浸渍实木皮
CN2933781Y (zh) 三聚氰胺浸渍实木皮复合刨花板
CN2933776Y (zh) 紫外线光固树脂漆薄木饰面密度板复合细木工板
CN205522780U (zh) 铝纸复合轻质防火板
CN202862322U (zh) 三聚氰胺浸渍实木皮复合中密度板
CN2933785Y (zh) 三聚氰胺浸渍实木皮复合防火板
CN205531147U (zh) 一种具有炫彩视觉效果的板材
CN2933773Y (zh) 紫外线光固树脂漆薄木饰面细木工板
CN202899510U (zh) 钢制面板复合防火内墙裙装饰板
CN205348681U (zh) 一种双面环保型实木整芯生态板
CN2933784Y (zh) 三聚氰胺浸渍实木皮贴面的中密度细木工复合板
CN202727027U (zh) 实木皮复合防火板
CN202727031U (zh) 实木皮复合的淋涂紫外线光固漆层胶合板
CN202727026U (zh) 紫外线光固树脂漆中密度板
RU2780737C2 (ru) Пригодная для травления поверхность

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C17 Cessation of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20090114

Termination date: 20100318