CN1712244A - 一种标牌及装饰画的制作工艺 - Google Patents
一种标牌及装饰画的制作工艺 Download PDFInfo
- Publication number
- CN1712244A CN1712244A CN 200510050309 CN200510050309A CN1712244A CN 1712244 A CN1712244 A CN 1712244A CN 200510050309 CN200510050309 CN 200510050309 CN 200510050309 A CN200510050309 A CN 200510050309A CN 1712244 A CN1712244 A CN 1712244A
- Authority
- CN
- China
- Prior art keywords
- paper
- decoration painting
- ultrapas
- manufacture craft
- label
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种标牌及装饰画的制作工艺,主要包括如下步骤:1)将选择好的图形按装饰画需要的规格制版,在专用纸上印刷;2)将印刷好的装饰图片以40-70度的温度固定在三聚氢胺浸渍纸上形成粘贴有图案的结合层;3)压板:压板时先铺装平衡纸,然后放置高密度木质基材,再把粘贴有图案的结合层平铺到基材上并按基准线定位,最后铺装表面防护层,各层材料组合完成后热压成型;4)开板:按需要的规格加工成适合的尺寸;5)铣型:将适合加工尺寸的小板在铣型机上将边缘处理平滑。本发明有益的效果是:可以将装饰层牢固的粘贴在高密度纤维板上,具有一定的耐刻划性,耐光照性能增强,不易褪色。有较强的防潮性,因此可用于户外。
Description
技术领域
本发明涉及一种标牌及装饰画领域,尤其是一种标牌及装饰画的制作工艺,适应于户内、户外各种标牌、指示牌、装饰画、广告宣传图片的制作以及照片的装裱制作。
背景技术
目前的标牌和装饰画,大多在成型的材质上直接进行印制,雕刻等工艺,其不足在于在光照下易褪色,工艺复杂。本发明的着眼点在于在图形印制工序嵌入到制作标牌及装饰画的过程中去,来解决普通工艺的一些缺陷。
发明内容
本发明要解决上述所述的不足,提供一种耐光照不易褪色、美观、安装方便、成本低、无污染的标牌及装饰画的制作工艺。
本发明解决其技术问题所采用的技术方案。这种标牌及装饰画的制作工艺,主要包括如下步骤:1)、将选择好的图形按装饰画需要的规格制版,在专用纸上印刷;2)、将印刷好的装饰图片以40-70度的温度固定在三聚氢胺浸渍纸上形成粘贴有图案的结合层;3)、压板:压板时先铺装平衡纸,然后放置高密度木质基材,再把粘贴有图案的结合层平铺到基材上并按基准线定位,最后铺装表面防护层,各层材料组合完成后热压成型,压好后的大板进行散热、养生;4)、开板:按需要的规格加工成适合的尺寸;5)、铣型:将适合加工尺寸的小板在铣型机上将边缘处理平滑;6)、将抛光后的装饰画按需要装裱。
本发明有益的效果是:1、三聚氢胺浸渍纸具有很强的结合力,可以将装饰层牢固的粘贴在高密度纤维板上。高密度纤维板具有一定的强度,因此牢固耐用。2、在表面采用含三氧化二铝的三聚氢胺浸渍纸保护层,使产品具有一定的耐刻划性,同时因含三氧化二铝的三聚氢胺浸渍纸保护层具有良好的密闭性,因而使产品耐光照性能增强,不易褪色。3、正反面采用三聚氢胺浸渍纸,三聚氢胺浸渍纸经热压固化后结合紧密,具备较强的防潮性,因此可用于户外。在户外应用时周边采用防水材料对木质层进行封闭。
具体实施方式
下面结合实施例对本发明作进一步描述。
这种标牌及装饰画的制作工艺,主材料:高密度纤维板、三聚氢胺浸渍纸、表面防护层、装饰纸(印刷),主要包括如下步骤:
1、将选择好的图形按装饰画(标牌图案、照片)需要的规格制版。
2、在专用纸上印刷。(例如加工规格为290mm*210mm的装饰画)
3、将印刷好的装饰图片(标牌图案,照片)以60度的温度固定在三聚氢胺浸渍纸上。
4、压板:压板时先铺装三聚氢胺浸渍纸(平衡纸),然后放置高密度木质基材,再把粘贴有图案的结合层(三聚氢胺浸渍纸)平铺到基材上并按基准线定位,最后铺装表面防护层(含三氧化二铝的三聚氢胺浸渍纸保护层)。各层材料组合完成后,在压机上以200℃的温度,1200吨的压力热压20秒钟,压好后的大板进行散热、养生。
5、开板:按需要的规格加工成适合的尺寸。
6、铣型:将适合加工尺寸的小板在铣型机上将边缘处理平滑。
7、将抛光后的装饰画(标牌图案,照片)按需要装裱。
标牌及装饰画的制做采用五层结构:(至上而下)第一层:表面防护层(含三氧化二铝的三聚氢胺浸渍纸);第二层:印刷图案层;第三层:结合层(三聚氢胺浸渍纸);第四层:高密度纤维板;第五层:平衡层(三聚氢胺浸渍纸)。
Claims (5)
1、一种标牌及装饰画的制作工艺,其特征在于,主要包括如下步骤:
1)、将选择好的图形按装饰画需要的规格制版,在专用纸上印刷;
2)、将印刷好的装饰图片以40-70度的温度固定在三聚氢胺浸渍纸上形成粘贴有图案的结合层;
3)、压板:压板时先铺装平衡纸,然后放置高密度木质基材,再把粘贴有图案的结合层平铺到基材上并按基准线定位,最后铺装表面防护层,各层材料组合完成后热压成型,压好后的大板进行散热、养生;
4)、开板:按需要的规格加工成适合的尺寸;
5)、铣型:将适合加工尺寸的小板在铣型机上将边缘处理平滑;
6)、将抛光后的装饰画按需要装裱。
2、根据权利要求1所述的标牌及装饰画的制作工艺,其特征在于,印刷好的装饰图片以60度的温度固定在三聚氢胺浸渍纸上。
3、根据权利要求1所述的标牌及装饰画的制作工艺,其特征在于,所述的平衡纸采用三聚氢胺浸渍纸。
4、根据权利要求1所述的标牌及装饰画的制作工艺,其特征在于,表面防护层采用含三氧化二铝的三聚氢胺浸渍纸保护层。
5、根据权利要求1所述的标牌及装饰画的制作工艺,其特征在于,在步骤3)中:各层材料组合完成后,在压机上以200℃的温度,1200吨的压力热压20秒钟。