CN1318687C - 毛用阳离子染料的染色方法 - Google Patents

毛用阳离子染料的染色方法 Download PDF

Info

Publication number
CN1318687C
CN1318687C CNB2004100411522A CN200410041152A CN1318687C CN 1318687 C CN1318687 C CN 1318687C CN B2004100411522 A CNB2004100411522 A CN B2004100411522A CN 200410041152 A CN200410041152 A CN 200410041152A CN 1318687 C CN1318687 C CN 1318687C
Authority
CN
China
Prior art keywords
dye
dyeing
liquid
wool
add
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNB2004100411522A
Other languages
English (en)
Other versions
CN1594723A (zh
Inventor
肖学俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Kede Education Technology Co ltd
Original Assignee
SUZHOU DONGWU DYESTUFF CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU DONGWU DYESTUFF CO Ltd filed Critical SUZHOU DONGWU DYESTUFF CO Ltd
Priority to CNB2004100411522A priority Critical patent/CN1318687C/zh
Publication of CN1594723A publication Critical patent/CN1594723A/zh
Application granted granted Critical
Publication of CN1318687C publication Critical patent/CN1318687C/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本发明涉及一种毛用阳离子染料的染色方法,采用专用染料,染料用量为待染物重量的0.01-3%,按待染物重量的30~100倍加入水,加醋酸或液碱调整pH在2-8,搅匀后,将经过洗净的毛类、蚕丝纤维或织物放入染缸中,用泵使染液循环10-30分钟,再按1-2℃/分钟的升温速度使染液温度升至98-100℃,保温30-60分钟,冷却至常温,残液放至残液存放容器。再洗掉被染物上的浮色,甩干、烘干即可。本方法除加入专用染料和调整pH的酸碱外,无需额外加入其他助剂,因而染整残液可保存待下次染色时套用,不仅染色工艺简单,而且改善对环境的污染,可用于毛类、蚕丝织物,毛腈混浊纺织物及皮毛的染色。

Description

毛用阳离子染料的染色方法
技术领域
本发明涉及用于毛类(羊毛、兔毛)、蚕丝的毛用阳离子染料的染色方法。
背景技术
目前,可通过酸性染料,弱酸性染料,中性染料,铬媒染料,1∶1型金属络合染料,1∶2型金属络合染料,活性染料,在不同助剂(如匀染剂,媒染剂,柔软剂,扩散剂,渗透剂),不同酸度的条件下进行染色。近年也有人提出通过不同助剂,用阳离子染料和分散染料对毛类(羊毛,兔毛)、蚕丝进行染色,在染色工艺上也存在以水为介质条件和在表面活性剂、发泡剂条件下进行染色的溶剂染色工艺和泡沫染色工艺,这些染色方法都不同程度地存在着各种短处和不足,如染色牢度差,过强的酸性染浴对纤维造成损伤;很多酸性染料都属禁用染料,不仅要排放大量的有色废水.而且废水中还含有大量的对环境造成有毒、有害的化学物质。对于多种纤维混纺织物的染色,这些方法和工艺就显得更加的不足,复杂,和困难。
这些问题都影响毛纺行业的发展。因此发展适合毛类、蚕丝染色的专用染料的染色新方法,越发显得重要和迫切。
发明内容
为解决当前不同染料不同染色工艺所存在的问题,本发明的目的是提出一种可用于染整毛类、蚕丝纤维纺织品及毛腈混纺纤维纺织品,也可用于染整皮毛的染料进行染色的方法,其染色方法工艺简单,操作方便,染整质量好,成本低,所排放的有色污水大幅度减少,污水中的有害物质相对当前的同类染色工艺也有大幅度的下降,大大减少印染行业对环境所造成的危害。
本发明的染色方法采用具有以下结构通式的毛用阳离子染料:
其中,
R1:选自F、Cl中的一种元素;
R2:选自萘氨基、萘氧基、苯氨基、苯氧基及具有氨基或羟基的化合物;
D+:选自阳离子染料中的任意一种阳离子;
按以下步骤染色:染缸中加入水,水量为待染物重量的30~100倍,开启循环泵对缸内水搅动,在大于10℃的常温下,以待染物重量的0.01-3%的量加入专用染料,再加醋酸或液碱,调整PH在2-8,搅匀后,将经过洗净的毛类、蚕丝纤维或织物放入染缸中,继续用泵使染液循环10-30分钟,再按1-2℃/分钟的升温速度使染液温度升至98-100℃,并保温30-60分钟,然后冷却至常温,将染缸残液放出至残液存放容器,染缸中加入常温清水,洗涤染织物2-3次,洗掉浮色,再将被染物甩干、烘干、处理。
上述方法中以PH为4-7时效果更好。
当进行下一批毛类、蚕丝纤维或织物染色时,将上一批的染色缸残液放入染缸中,添加水,以调整缸内水量为待染物的30-100倍,添加染料,以达到被染物的染色深度0.01-3.00%,再加入醋酸或液碱,调整pH在2-8之间,再加入待染的毛类、蚕丝纤维或织物,继续用泵使染液循环10-30分钟.再按1-2℃/分钟的升温速度进行升温,当温度升至98-100℃,保温30-60分钟,然后冷却至常温,放出染缸残液至残液存放容器,再加入常温清水洗被染物,经过2-3次的洗涤,把浮色洗掉.再将被染物进行甩干、烘干处理。
本发明的染色方法在染整过程中除加入专用染料和调整PH的酸碱外,无需额外加入其他助剂,如匀染剂、扩散剂、渗透剂,由此可以降低染整成本。染整残液可以套用是该发明的主要特点之一,染色过程中除加入专用染料和调整pH的酸碱外,无需用加入其他化合物。因此,染整残液可继续利用,即残液经添加适量的染料和水,调整好染色深度,并控制酸碱量达适当的pH值后即可以套用,这不仅可以大大降低染整成本,还可以减少大量废水排放.缩小对环境的负面影响。
本发明不仅适用于单色染色,对于毛晴混纺也可以采用一浴法染色,大大地缩短工艺和减化工序。
具体实施方式
实施例1:
500ml的染缸中加入450g水,加入毛用阳离子染料0.05g(兰色),调整pH为5,搅拌均匀,加入洗涤过的5g羊毛布,关闭染缸,启动搅拌,升温速度为1℃/分,升至98度后,保温(98-100度)60分钟。保温结束,降温至常温打开染缸倒出残液用于下次套用。染好的羊毛布用清水洗至洗水无色,取出羊毛布,经甩干、烘干即完成染色。染色质量指标例于表一
表一:羊毛染色牢度检测结果。
项目 单位 试验方法   纺织工业一等品标准
检测数据
  耐水洗(37±2℃)   色泽变化   GB/T5713   不低于3     4
  毛布沾色   GB/T5713   不低于3     3-4
  棉布沾色   GB/T5713   不低于3     3
  耐皂洗(40±2℃)   色泽变化   GB/T3921.1   不低于3     3
  毛布沾色   GB/T3921.1   不低于3     4
  棉布沾色   GB/T3921.1   不低于3     4-5
耐汗渍(37±2℃) 色泽变化   GB/T3922酸 不低于3-4     4
  GB/T3922碱     4
毛布沾色   GB/T3922酸 不低于3     2-3
  GB/T3922碱     2
棉布沾色   GB/T3922酸 不低于3     3-4
  GB/T3922碱     3-4
耐摩擦   干摩擦   GB/T3920   不低于3-4     4
  湿摩擦   GB/T3920   不低于2-3     3
  耐热压(200℃)   色泽变化   GB/T6152     4-5
  棉布沾色   GB/T6152     4-5
  耐光   氙弧   GB/T8427   不低于3-4     3
实例2
除5g羊毛布改为2g晴纶和3g羊毛纤维的混纺布外,其他操作过程同实例1.染色质量指标例于表二.
表二.毛腈混纺织物中腈纶纤维上的染色牢度检测结果
项目   单位     试验方法 本发明检测等级
耐皂洗(60±2℃)     色泽变化   级     GB/3921.3 4-5
    棉布沾色   级     GB/3921.3 4-5
    腈纶沾色   级     GB/3921.3 4-5
耐汗渍(37±2℃) 色泽变化     GB/T3922酸 4
    GB/T3922碱 4
棉布沾色     GB/T3922酸 4-5
    GB/T3922碱 4-5
腈纶沾色     GB/T3922酸 4-5
    GB/T3922碱 4-5
耐摩擦     干摩擦   级     GB/T3920 4-5
    湿摩擦   级     GB/T3920 4
耐热压(200℃)     色泽变化   级     GB/T6152 4
    棉布沾色   级     GB/T6152 4-5
耐光     氙弧   级     GB/T8427 5

Claims (3)

1.毛用阳离子染料的染色方法,其特征是采用具有以下结构通式的毛用阳离子染料:
其中,
R1:选自F、Cl中的一种元素;
R2:选自萘氨基、萘氧基、苯氨基、苯氧基;
D+:选自阳离子染料中的任意一种阳离子;
按以下步骤染色:染缸中加入水,水量为待染物重量的30~100倍,开启循环泵对缸内水搅动,在大于10℃的常温下,以待染物重量的0.01-3%的量加入专用染料,再加醋酸或液碱,调整pH在2-8,搅匀后,将经过洗净的毛类、蚕丝纤维或织物放入染缸中,继续用泵使染液循环10-30分钟,再按1-2℃/分钟的升温速度使染液温度升至98-100℃,并保温30-60分钟,然后冷却至常温,放出染缸残液至残液存放容器,加入常温清水洗涤染织物2-3次,洗掉浮色,再将被染物甩干、烘干、处理。
2.根据权利要求1所述的的毛用阳离子染料的染色方法,其特征是将上一批的染色残液,放入染缸中,添加入水和染料,以调整缸内水量为待染物的30-100倍,被染物的染色深度0.01-3.00%,再加入醋酸或液碱,调整pH在2-8,加入毛类、蚕丝纤维或织物进行新一轮染色。
3.根据权利要求1或2所述的毛用阳离子染料的染色方法,其特征是所说的pH为4-7。
CNB2004100411522A 2004-07-02 2004-07-02 毛用阳离子染料的染色方法 Expired - Lifetime CN1318687C (zh)