CN110284402A - A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement - Google Patents

A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement Download PDF

Info

Publication number
CN110284402A
CN110284402A CN201910443575.3A CN201910443575A CN110284402A CN 110284402 A CN110284402 A CN 110284402A CN 201910443575 A CN201910443575 A CN 201910443575A CN 110284402 A CN110284402 A CN 110284402A
Authority
CN
China
Prior art keywords
spraying
layer
ultra micro
basal plane
construction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910443575.3A
Other languages
Chinese (zh)
Inventor
蔡海军
郁讳讳
沈峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Fu Optical Engineering Technology Co Ltd
NANTONG FULUNLI NEW MATERIAL CO Ltd
Original Assignee
Jiangsu Fu Optical Engineering Technology Co Ltd
NANTONG FULUNLI NEW MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Fu Optical Engineering Technology Co Ltd, NANTONG FULUNLI NEW MATERIAL CO Ltd filed Critical Jiangsu Fu Optical Engineering Technology Co Ltd
Priority to CN201910443575.3A priority Critical patent/CN110284402A/en
Publication of CN110284402A publication Critical patent/CN110284402A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of ultra micro spray coating constructing techniques of Colorful Asphalt Pavement.On the advantages of the present invention are mainly reflected in areas small, irregular basal plane, especially on coloury square, park, and the non-motorized lane etc. in region is divided, can accomplish reply freely, it is flexible and changeable.It is most suitable for sport and body-building, stroll, shares and rides, and antiskid effect is obvious, and big harm will not be caused to ambient enviroment, it is most important that construction is fast, high-efficient, traffic delay caused by effectively reducing because of construction.

Description

A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement
Technical field
The invention belongs to colours to emulsify decoloration pitch field, and in particular to a kind of ultra micro spraying application of Colorful Asphalt Pavement Technique.
Background technique
Color asphalt also known as chromatic cementing agent are one kind of road-making material, are widely used in green road, cycle track, gardens In the slow-vehicle systems such as landscape road, the Heavy Traffics road such as bus special lane, crossing, Expressway Service can also be applied to Face.There are two types of common color asphalt is current: the first is with colourless cementitious matter additive color powder, and colourless cementitious matter can be by pitch It decolourizes and obtains, can also be deployed and be obtained by low color polymers such as Petropols, pass through form of construction work identical with the heated bitumen that paves To realize;Be for second, by special emulsifying process, be prepared into emulsification decoloration pitch using colourless cementitious matter as raw material, then To its modified addition mill base, to be modulated into the color emulsified asphalt of various colors, final colored road surface is sealed by thin pulp The mode that layer vehicle pave, manually scratches or sprays is realized.Color emulsified asphalt it is in bright gay color, at present have it is red, yellow, blue, Several big colour systems such as green, grey.Currently, the colour asphalt pavement of mainstream is defined as decolourizing pitch and various colors building stones, The materials such as colorant and additive mix mix within specified temperatures, that is, can be configured to the asphalt of various colours, then pass through It crosses and paves, rolls and form the colour asphalt pavement with some strength and pavement performance.But it is this specific At a temperature of mix the mode of mix and can not increasingly adapt to social progress, Visual Aesthetics and the requirement of people is being constantly progressive, and is The beauty of road or partition functionality area or the requirement for embodying road are different, such as distinguish the road of pedestrian and motor-driven vehicle going, Or be used in school, court, the different zones such as amusement of having a rest, the diversity of color, construction in terms of, it will quilt The mode of cold mixing cold-application replaces.
Summary of the invention
Goal of the invention: the present invention provides a kind of manual operations, flexible and changeable, and high efficiency can reduce difficulty of construction and cost, Service life is long, a kind of brightly painted ultra micro spray coating constructing technique of Colorful Asphalt Pavement.
Technical solution: a kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement, basal plane be divided into asphalt concrete pavement and Cement concrete pavement;
The ultra micro spray coating constructing technique of the bituminous concrete basal plane is as follows:
Step 1: to improve interfacial adhesion, base should cleaning and inspection: be gone through before being laid with chromatic bitumen mixture The quality of layer ensures solid, smooth, clean, especially drosses such as pollutant, mortar of cleaning basal plane, at the same cope with generator, Air compressor machine, miniature hand pulling type mixing plant, miniature hand pulling type ultra micro spraying equipment working condition checked, wherein it is small-sized Hand propelled spice bucket has fully demonstrated the flexibility of spice, miniature hand pulling type ultra micro spraying equipment has fully demonstrated the flexible of construction Property, it saves labour turnover, improves construction efficiency;
Step 2: construction area confirmation and unwrapping wire, and edge is put up along the line put well with 10-15 centimeters of paper self-adhesive tape, with And prepare 2-3 block spraying baffle (baffle dimensions: high 1.2m* long 2m), the splashing in spraying is prevented, environment is polluted;
Step 3: layering spraying: according to road using object, design thickness, roughness etc. using layering spraying, i.e., first Sprayed layer undercoat can up spray one layer on the basis of bottom again as needed, and interlayer must be perfectly dry, and keep uninterrupted one Secondary property forms to form a complete level, to guarantee that color is consistent, particle is uniform, beautiful;Before spraying, it is necessary to first adjust water Dosage, the dilute consistency of the mixture mixed and stirred out is moderate, i.e., need to be through strainer mistake without oilstone segregation phenomenon and the mixture mixed and stirred Filter, is sending to flush coater charging basket, can guarantee easily smooth when spraying;When starting spraying, met the requirements in strict accordance with thickness, Ensure to spray continuous;
Step 4: roller coating seal protection layer: with the uniform roller coating surface layer protective agent of the roller that becomes mildewed, the bright-coloured journey of color is promoted Degree, enhancing anti-aging property;
Step 5: throwing off paper self-adhesive tape after dry, cleans road surface, it is ensured that it is clear that the complete material of work uses up place;
Step 6: open to traffic: close traffic health in 12 hours is answered after construction, forbids all vehicles and pedestrians;
The ultra micro spray coating constructing technique of the cement concrete basal plane is as follows:
Step 1: to improve interfacial adhesion, base should cleaning and inspection: be gone through before spraying chromatic bitumen mixture The quality of layer ensures solid, smooth, clean, especially drosses such as pollutant, mortar of cleaning basal plane, at the same cope with generator, Air compressor machine, napper, miniature hand pulling type mixing plant, miniature hand pulling type ultra micro spraying equipment working condition checked, such as Fruit cement basal plane has had grey dusting phenomenon, it is necessary to be removed with sander or shot-blasting machine, wherein the abundant body of miniature hand pulling type spice bucket Showed the flexibility of spice, miniature hand pulling type ultra micro spraying equipment fully demonstrated construction flexibility, save labour turnover, mention High construction efficiency;
Step 2: construction area confirmation and unwrapping wire, and edge is put up along the line put well with 10-15 centimeters of paper self-adhesive tape, with And prepare 2-3 block spraying baffle (baffle dimensions: high 1.2m* long 2m), the splashing in spraying is prevented, environment is polluted;
Step 3: basal plane plucking: since former road surface is cement concrete layer, smooth surface is deep almost without construction Degree, first need to doing hair pulling treatment to cement concrete layer, (plucking depth is in 1mm-2mm, spacing
2mm-3mm), to obtain corresponding construction depth (imitating bituminous concrete basal plane), to enhance basal plane and spraying Bottom inlays power, increase accordingly sprayed layer undercoat and basal plane contact area, improves interfacial adhesion;
Step 4: infiltration solidification: since former road surface is cement concrete layer, cement concrete layer that need to be good to plucking is carried out Infiltration solidification processing, can increase the surface strength of cement concrete, while can also consolidate the fine ash etc. of concrete surface, under Very big effect is played on the adhesive property of procedure;It is required that roller coating is uniform, no accumulation, according to the infiltration feelings of cement concrete Condition needs disposable infiltration solidification in place, can not overcoating after hardening;
Step 5: layering spraying: according to road using object, design thickness, roughness etc. using layering spraying, i.e., first Sprayed layer undercoat can up spray one layer on the basis of bottom again as needed, and interlayer must be perfectly dry, and keep uninterrupted one Secondary property forms to form a complete level, to guarantee that color is consistent, particle is uniform, beautiful.Before spraying, it is necessary to first adjust water Dosage, the dilute consistency of the mixture mixed and stirred out is moderate, i.e., need to be through strainer mistake without oilstone segregation phenomenon and the mixture mixed and stirred Filter, is sending to flush coater charging basket, can guarantee easily smooth when spraying.When starting spraying, met the requirements in strict accordance with thickness, Ensure to spray continuous;
Step 6: roller coating seal protection layer: with the uniform roller coating surface layer protective agent of the roller that becomes mildewed, the bright-coloured journey of color is promoted Degree, enhancing anti-aging property;
Step 7: throwing off paper self-adhesive tape after dry, cleans road surface, it is ensured that it is clear that the complete material of work uses up place;
Step 8: open to traffic: close traffic health in 12 hours is answered after construction, forbids all vehicles and pedestrians.
As a preferred solution: spraying is applied speed and was calculated with 8 hours, and 2000-4000 can be completed in the layering spraying ㎡, whole color is consistent after spraying, the available guarantee of flatness, avoids blade coating bring scratch, influences beauty.
As a preferred solution: the colorful bituminous pavement structure spray coating is according to pavement usage object, it can extension set motor-car Road: coarse grain formula bottom and particulate formula surface layer;Non-motorized lane: single layer coarse grain formula surface layer or single layer particulate formula surface layer.
The utility model has the advantages that the invention discloses a kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement, advantage of the invention It is mainly reflected in that area is small, on irregular basal plane, especially on coloury square, park, and divides the non-machine in region Motor-car road etc. can accomplish reply freely, flexible and changeable.It is most suitable for sport and body-building, stroll, shares and rides, and antiskid effect is bright It is aobvious, big harm will not be caused to ambient enviroment, it is most important that construction is fast, high-efficient, effectively reduces because construction causes Traffic delay.
Specific embodiment
The technical scheme in the embodiments of the invention will be clearly and completely described below, so that the technology of this field Personnel can better understand advantages and features of the invention, to make apparent boundary to protection scope of the present invention It is fixed.Embodiment described in the invention is only a part of the embodiment of the present invention, instead of all the embodiments, based on the present invention In embodiment, those of ordinary skill in the art's every other implementation obtained without making creative work Example, shall fall within the protection scope of the present invention.
Embodiment
The technical scheme in the embodiments of the invention will be clearly and completely described below, so that the technology of this field Personnel can better understand advantages and features of the invention, to make apparent boundary to protection scope of the present invention It is fixed.Embodiment described in the invention is only a part of the embodiment of the present invention, instead of all the embodiments, based on the present invention In embodiment, those of ordinary skill in the art's every other implementation obtained without making creative work Example, shall fall within the protection scope of the present invention.
Specific embodiment 1
A kind of construction technology of Colorful Asphalt Pavement is motor vehicle using object, and basal plane is newly-built dark asphalt concrete, About 3000 ㎡ of area.It mainly comprises the steps that
Step 1: first day, close traffic cleaned road surface;Check generator, air compressor machine, miniature hand pulling type agitator, small The working condition of the equipment such as type hand propelled ultra micro flush coater;
Step 2: unwrapping wire simultaneously puts up edge line with 10-15cm paper self-adhesive tape, determines construction area, and prepares the spraying of 2-3 block Baffle (baffle dimensions: high 1.2m* long 2m) prevents the splashing in spraying, pollutes environment;
Step 3: it is equidistant to stack corresponding raw material according to the dosage of unit area colorful asphalt emulsion and mixture, A certain amount of colorful asphalt emulsion is first weighed by construction proportion to be added in miniature hand pulling type agitator, then weighs coarse grain formula mixture It is slowly added into agitator, while suitable water is added according to dilute consistency, it is ensured that be not demulsified, do not isolate in whipping process, count Measure the dosage of water.The coarse grain formula mixture mixed is first being inclined with filter screen filtration into clean bucket according to the demand of spraying In in hand propelled flush coater charging basket, by lasting spice, persistently spray in a manner of promote.During spraying painting, baffle is sprayed It needs to follow spray gun synchronizing moving, spraying is avoided to splash, pollute environment.
Step 4: second day, after particulate formula mixture is completely dried, with same spice and spraying method, spraying was thin Grain formula chromatic bitumen mixture.
Step 5: third day, with roller roller coating seal protection agent of becoming mildewed, using crossing method, it is ensured that the uniform nothing of roller coating Accumulation, no color differnece.Paper self-adhesive tape is removed, place cleaning, exhaustive is pollution-free.Keep traffic closed state.
Step 6: the 4th day, open to traffic.
Specific embodiment 2
A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement, is motor vehicle using object, and basal plane is that rigid health terminates Cement concrete, about 2000 ㎡ mainly comprise the steps that
Step 1: first day, close traffic cleaned road surface;Check that generator, air compressor machine, napper, miniature hand pulling type stir Mix the working condition of the equipment such as bucket, miniature hand pulling type ultra micro flush coater;
Step 2: unwrapping wire simultaneously puts up edge line with 10-15cm paper self-adhesive tape, determines construction area, and prepares the spraying of 2-3 block Baffle (baffle dimensions: high 1.2m* long 2m) prevents the splashing in spraying, pollutes environment;
Step 3: basal plane plucking: since former road surface is cement concrete layer, smooth surface is deep almost without construction Degree needs first to do hair pulling treatment (plucking depth is in 1mm-2mm, spacing 2mm-3mm) to cement concrete layer, to obtain corresponding structure Make depth (imitate bituminous concrete basal plane), so that enhance basal plane and sprayed layer undercoat inlays power, increase accordingly sprayed layer undercoat with Basal plane contact area improves interfacial adhesion;
Step 4: roller coating infiltration solidification agent repeats roller coating in roller coating and increases use according to the infiltration situation of cement basal plane Amount, can not the overcoating after one-step solidification.The same day completes all infiltration solidification work.
Step 5: second day, equidistant to stack accordingly according to the dosage of unit area colorful asphalt emulsion and mixture Raw material first weigh a certain amount of colorful asphalt emulsion by construction proportion and are added in miniature hand pulling type agitator, then weigh particulate Formula mixture is slowly added into agitator, while suitable water is added according to dilute consistency, it is ensured that is not demulsified in whipping process, no Isolation, measures the dosage of water.The coarse grain formula mixture mixed according to spraying demand, first with filter screen filtration to clean bucket In, be poured into hand propelled flush coater charging basket, by lasting spice, persistently spray in a manner of promote.During spraying painting, spray It applies baffle to need to follow spray gun synchronizing moving, spraying is avoided to splash, pollute environment.
Step 6: third day, after coarse grain formula mixture is completely dried, with same spice and spraying method, spraying is thin Grain formula chromatic bitumen mixture.
Step 7: the 4th day, with roller roller coating seal protection agent of becoming mildewed, using crossing method, it is ensured that the uniform nothing of roller coating Accumulation, no color differnece.Paper self-adhesive tape is removed, place cleaning, exhaustive is pollution-free.Keep traffic closed state.,
Step 8: the 5th day, open to traffic.
Specific embodiment 3
A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement is non-motor vehicle using object, and basal plane is dark asphalt Concrete, color is red and green color, wherein red area is 1500 ㎡, green areas is 400 ㎡.It mainly include following step It is rapid:
Step 1: first day, close traffic cleaned road surface;Check generator, air compressor machine, miniature hand pulling type agitator, small The working condition of the equipment such as type hand propelled ultra micro flush coater;
Step 2: unwrapping wire simultaneously puts up edge line with 10-15cm paper self-adhesive tape, determines construction area, and prepares the spraying of 2-3 block Baffle (baffle dimensions: high 1.2m* long 2m) prevents the splashing in spraying, pollutes environment;
Step 3: first day, the spraying of 1500 ㎡ red single layer structure coarse grain formulas is first completed.According to unit area color asphalt The dosage of lotion and mixture, it is equidistant to stack corresponding raw material, a certain amount of color asphalt cream is first weighed by construction proportion Liquid is added in miniature hand pulling type agitator, then weighs particulate formula mixture and be slowly added into agitator, while being added according to dilute consistency Enter suitable water, it is ensured that be not demulsified, do not isolate in whipping process, measure the dosage of water.The coarse grain formula mixture mixed by According to the demand of spraying, first with filter screen filtration into clean bucket, it is being poured into hand propelled flush coater charging basket, persistently to mix Material, the mode persistently sprayed promote.During spraying painting, spraying baffle needs to follow spray gun synchronizing moving, and spraying is avoided to fly It splashes, pollutes environment.Complete the spraying of 400 ㎡ green single layer structure particulate formulas in the same way again.
Step 4: second day, with roller roller coating seal protection agent of becoming mildewed, using crossing method, it is ensured that the uniform nothing of roller coating Accumulation, no color differnece.Paper self-adhesive tape is removed, place cleaning, exhaustive is pollution-free.Keep traffic closed state.
Step 5: third day, open to traffic.
On the advantages of the present invention are mainly reflected in areas small, irregular basal plane, especially on coloury square, public affairs Garden, and the non-motorized lane etc. in region is divided, it can accomplish reply freely, it is flexible and changeable.Be most suitable for sport and body-building, stroll, It is shared to ride, and antiskid effect is obvious, and big harm will not be caused to ambient enviroment, it is most important that construction is fast, high-efficient, Traffic delay caused by effectively reducing because of construction.

Claims (3)

1. a kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement, it is characterised in that: basal plane be divided into asphalt concrete pavement and Cement concrete pavement;
The ultra micro spray coating constructing technique of the bituminous concrete basal plane is as follows:
Step 1: to improve interfacial adhesion, base should cleaning and inspection: be gone through before being laid with chromatic bitumen mixture Quality ensures solid, smooth, clean, especially drosses such as pollutant, mortar of cleaning basal plane, while coping with generator, pneumatics Machine, miniature hand pulling type agitator, miniature hand pulling type ultra micro spraying equipment working condition checked, wherein miniature hand pulling type Spice bucket has fully demonstrated the flexibility of spice, miniature hand pulling type ultra micro spraying equipment has fully demonstrated the flexibility constructed, section Less manpower cost improves construction efficiency;
Step 2: construction area confirmation and unwrapping wire, and edge, Yi Jizhun are put up along the line put well with 10-15 centimeters of paper self-adhesive tape Standby 2-3 block spraying baffle (baffle dimensions: high 1.2m* long 2m), prevents the splashing in spraying, pollutes environment;
Step 3: it layering spraying: is first sprayed using object, design thickness, roughness etc. using layering spraying according to road Bottom can up spray one layer on the basis of bottom again as needed, and interlayer must be perfectly dry, and keep uninterrupted disposable Molding forms a complete level, to guarantee that color is consistent, particle is uniform, beautiful;Before spraying, it is necessary to first adjust the use of water Amount, the dilute consistency of the mixture mixed and stirred out is moderate, i.e., without oilstone segregation phenomenon and the mixture mixed and stirred need to through strainer filtering, It is sending to flush coater charging basket, can guarantee easily smooth when spraying;When starting spraying, met the requirements in strict accordance with thickness, really It is continuous to protect spraying;
Step 4: with the uniform roller coating surface layer protective agent of the roller that becomes mildewed, bright-coloured degree, the increasing of color roller coating seal protection layer: are promoted Strong anti-aging property;
Step 5: throwing off paper self-adhesive tape after dry, cleans road surface, it is ensured that it is clear that the complete material of work uses up place;
Step 6: open to traffic: close traffic health in 12 hours is answered after construction, forbids all vehicles and pedestrians;
The ultra micro spray coating constructing technique of the cement concrete basal plane is as follows:
Step 1: to improve interfacial adhesion, base should cleaning and inspection: be gone through before spraying chromatic bitumen mixture Quality ensures solid, smooth, clean, especially drosses such as pollutant, mortar of cleaning basal plane, while coping with generator, pneumatics Machine, napper, miniature hand pulling type agitator, miniature hand pulling type ultra micro spraying equipment working condition checked, if cement Basal plane has had grey dusting phenomenon, it is necessary to be removed with sander or shot-blasting machine, wherein miniature hand pulling type spice bucket, which has fully demonstrated, to be mixed The flexibility of material, miniature hand pulling type ultra micro spraying equipment have fully demonstrated the flexibility of construction, save labour turnover, and improve construction Efficiency;
Step 2: construction area confirmation and unwrapping wire, and edge, Yi Jizhun are put up along the line put well with 10-15 centimeters of paper self-adhesive tape Standby 2-3 block spraying baffle (baffle dimensions: high 1.2m* long 2m), prevents the splashing in spraying, pollutes environment;
Step 3: basal plane plucking: since former road surface is cement concrete layer, smooth surface needs almost without construction depth Hair pulling treatment (plucking depth is in 1mm-2mm, spacing 2mm-3mm) first is done to cement concrete layer, it is deep to obtain corresponding construction Degree (imitate bituminous concrete basal plane) increase accordingly sprayed layer undercoat and basal plane so that enhance basal plane and sprayed layer undercoat inlays power Contact area improves interfacial adhesion;
Step 4: infiltration solidification: since former road surface is cement concrete layer, cement concrete layer that need to be good to plucking permeates Curing process can increase the surface strength of cement concrete, while can also consolidate the fine ash etc. of concrete surface, with lower road work Very big effect is played on the adhesive property of sequence;It is required that roller coating is uniform, no accumulation is needed according to the infiltration situation of cement concrete Disposable infiltration solidification in place, can not overcoating after hardening;
Step 5: it layering spraying: is first sprayed using object, design thickness, roughness etc. using layering spraying according to road Bottom can up spray one layer on the basis of bottom again as needed, and interlayer must be perfectly dry, and keep uninterrupted disposable Molding forms a complete level, to guarantee that color is consistent, particle is uniform, beautiful.Before spraying, it is necessary to first adjust the use of water Amount, the dilute consistency of the mixture mixed and stirred out is moderate, i.e., without oilstone segregation phenomenon and the mixture mixed and stirred need to through strainer filtering, It is sending to flush coater charging basket, can guarantee easily smooth when spraying.When starting spraying, met the requirements in strict accordance with thickness, really It is continuous to protect spraying;
Step 6: with the uniform roller coating surface layer protective agent of the roller that becomes mildewed, bright-coloured degree, the increasing of color roller coating seal protection layer: are promoted Strong anti-aging property;
Step 7: throwing off paper self-adhesive tape after dry, cleans road surface, it is ensured that it is clear that the complete material of work uses up place;
Step 8: open to traffic: close traffic health in 12 hours is answered after construction, forbids all vehicles and pedestrians.
2. the ultra micro spray coating constructing technique of Colorful Asphalt Pavement as described in claim 1, it is characterised in that: the layering spray Tu Zhong, spraying are applied speed and were calculated with 8 hours, and 2000-4000 ㎡ can be completed, whole color is consistent after spraying, flatness can be with It is guaranteed, avoids blade coating bring scratch, influence beauty.
3. the ultra micro spray coating constructing technique of Colorful Asphalt Pavement as described in claim 1, it is characterised in that: the colored drip Green pavement structure spray coating can divide car lane according to pavement usage object: coarse grain formula bottom and particulate formula surface layer;Non-motor vehicle Road: single layer coarse grain formula surface layer or single layer particulate formula surface layer.
CN201910443575.3A 2019-05-27 2019-05-27 A kind of ultra micro spray coating constructing technique of Colorful Asphalt Pavement Pending CN110284402A (en)