CN110184767A - A kind of cashmere sweater washes contracting technique - Google Patents
A kind of cashmere sweater washes contracting technique Download PDFInfo
- Publication number
- CN110184767A CN110184767A CN201910415777.7A CN201910415777A CN110184767A CN 110184767 A CN110184767 A CN 110184767A CN 201910415777 A CN201910415777 A CN 201910415777A CN 110184767 A CN110184767 A CN 110184767A
- Authority
- CN
- China
- Prior art keywords
- contracting
- fabric
- cashmere sweater
- technique
- washes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to a kind of cashmere sweaters to wash contracting technique, includes the following steps, pretreatment: fabric outer is cleaned up, clothing is turned over, fabric is cleaned up;It washes contracting processing: warm soft water (38 DEG C -40 DEG C) being added into shampoo, fulling agent is added into shampoo, stirs evenly, fabric is put into and carries out washing contracting in shampoo;Dehydration cleaning: the fabric that contracting is completed will be washed and dried, then cleaned twice with warm soft water (38 DEG C -40 DEG C), finally dried, contracting technique is washed in completion.The present invention has preferable fulling milling effect to cashmere sweater.
Description
Technical field
The present invention relates to contracting technique is washed, in particular to a kind of cashmere sweater washes contracting technique.
Background technique
Under wet heat condition, the repeated action through mechanical external force, fiber assembly gradually tapers up closely wool fibre, and mutually
It is interspersed to tangle, it hands over and compiles felting.This performance is known as the feltability of wool fibre, and the processing work of cashmere sweater is handled using this characteristic
Skill is known as cashmere sweater and washes contracting technique.It is thick to be mainly used in cashmere, camel hair, the rabbit hair, Feng Zaimao, Xue Telanmao etc. for fulling process at present
It spins in class cashmere sweater, spinning class cashmere sweater also often makees washing dressing with room temperature, short time or light fulling milling is arranged to improve appearance.
Cashmere sweater washes the purpose of contracting technique primarily to improving the inherent quality and appearance effect of cashmere sweater product
Fruit, one side fulling milling can make fabric texture close, and length shortening, weight per square meter and thickness increase, and strength improves, elasticity and guarantor
Warm property enhancing;On the other hand go out one layer of villus by washing the cashmere sweater of contracting technique its surface open, make attractive appearance, feel is abundant
Softness, color are soft;Villus certain faults original to woollen sweater that the generation of contracting technique is washed in terms of third play desalination and cover
Lid effect, makes it that will not significantly be exposed to fabric surface.
Current cashmere sweater washes the conventional flowsheet of contracting technique are as follows: contracting processing-cleaning-drying is washed in prewashing-, and each step is main
By personal experience, the result for washing contracting technique is affected by human factors larger, and it is undesirable cashmere sweater fulling milling effect usually occur
Problem.
Summary of the invention
The purpose of the present invention is to provide a kind of cashmere sweaters to wash contracting technique, has preferable fulling milling effect to cashmere sweater.
Above-mentioned purpose of the invention has the technical scheme that a kind of cashmere sweater washes contracting technique, including
Following steps,
Pretreatment: fabric outer is cleaned up, clothing is turned over, fabric is cleaned up;
It washes contracting processing: warm soft water (38 DEG C -40 DEG C) being added into shampoo, fulling agent is added into shampoo, stirs evenly,
Fabric is put into and carries out washing contracting in shampoo;
Dehydration cleaning: will wash the fabric that contracting is completed and dry, then cleaned twice with warm soft water (38 DEG C -40 DEG C), finally dried, complete
At washing contracting technique.
By using above-mentioned technical proposal, after pretreatment, the inside and outside equal energy reliable contacts fulling milling of cashmere sweater
Agent, under the mechanical external force repeated action that shampoo provides, fiber assembly is gradually tapered up closely, and is mutually interted and tangled, and is handed over
Felting is compiled, reaches preferable fulling milling effect inside and outside cashmere sweater, then by dehydration cleaning removal fulling agent.Technical process
In for warm soft water (38 DEG C -40 DEG C) temperature have accurate restriction, the influence of human factor is reduced, so that cashmere
The controllability that shirt washes contracting technique is more preferable, and fulling milling effect is more preferable.
The present invention is further arranged to: being washed in contracting processing step, when fabric to be put into shampoo, first with hand by fabric
It holds wet, then impregnates again 10-15 minutes, then start to wash contracting.
By using above-mentioned technical proposal, holds wet rear fabric and be not easy to float to upper layer, it can be with reliable contacts fulling agent;Together
When be soaked for a period of time and can also promote the effect for washing contracting.
The present invention is further arranged to: washing contracting bath raio is 1:30.
By using above-mentioned technical proposal, washes contracting bath raio and refer to cashmere sweater weight and fulling milling liquid weight ratio.Woollen sweater contracting
Bath raio when suede should be appropriate, and when bath raio is too small, the friction between cashmere sweater increases, and the degree of irregularity of friction and active force increases
Add, therefore leads to the uneven of fulling milling.When bath raio is excessive, mechanicals efforts are opposite to be reduced, and the friction between woollen sweater slows down, contracting agent
Consumption increases, and the fulling milling time lengthens.Appropriate fulling milling bath raio is 1:25~35.
The present invention is further arranged to: it further includes soft treatment that cashmere sweater, which washes contracting technique, and warm soft water soft treatment: is added
(38 DEG C -40 DEG C) are added softening agent according to the 7% of fabric weight and stir evenly, fabric is impregnated 40 minutes, is dried, drying
Moisture content afterwards is 30%, is then dried.
By using above-mentioned technical proposal, in actual use, cashmere sweater is after washing contracting technique, and texture is too hard for wool fibre,
It will affect comfort level when wearing.For this purpose, it further includes soft treatment that cashmere sweater, which washes contracting technique, after soft treatment, cashmere sweater
Wool fibre becomes more soft, more comfortable when wearing.
The present invention is further arranged to: it further includes drying and processing that cashmere sweater, which washes contracting technique, drying and processing: is by moisture content
30% fabric, which is put into dryer, is dried, and the temperature of drying is no more than 80 DEG C.
By using above-mentioned technical proposal, fabric can be quickly made to become drying using the heat of dryer, at promotion
Manage efficiency.
The present invention is further arranged to: in drying and processing step, being blown after drying with cold wind, is completed treatment process after cooling.
By using above-mentioned technical proposal, use cold front heavy rain that can fabric be quickly cooled down, so that wool fibre is not easy
Deformation, and then ensure that preferable fulling milling effect.
In conclusion the invention has the following advantages:
1. the inside and outside equal energy reliable contacts fulling agent of cashmere sweater is outer in the machinery that shampoo provides after pretreatment
Under power repeated action, fiber assembly is gradually tapered up closely, and is mutually interted and tangled, and is handed over and is compiled felting, inside and outside cashmere sweater
Reach preferable fulling milling effect, then cleaned by dehydration and remove fulling agent, for (38 DEG C -40 of soft water of warm in technical process
DEG C) temperature have accurate restriction, the influence of human factor is reduced, so that cashmere sweater washes the controllability of contracting technique more
Good, fulling milling effect is more preferable;
2. increasing soft treatment step: so that the wool fibre of cashmere sweater becomes more soft, it is more comfortable when wearing;
3. increasing drying and processing step: being unlikely to deform wool fibre while promoting treatment effeciency, and then ensure that preferably
Fulling milling effect.
Specific embodiment
Embodiment
A kind of cashmere sweater washes contracting technique, includes the following steps,
Pretreatment: fabric outer is cleaned up, clothing is turned over, fabric is cleaned up;
It washes contracting processing: warm soft water (38 DEG C -40 DEG C) being added into shampoo, fulling agent is added into shampoo, stirs evenly,
Fabric is put into and carries out washing contracting in shampoo;
Dehydration cleaning: will wash the fabric that contracting is completed and dry, then cleaned twice with warm soft water (38 DEG C -40 DEG C), finally dried, complete
At washing contracting technique.
After pretreatment, the inside and outside equal energy reliable contacts fulling agent of cashmere sweater, in the machinery that shampoo provides
Under external force repeated action, fiber assembly is gradually tapered up closely, and is mutually interted and tangled, and is handed over and is compiled felting, inside and outside cashmere sweater
Reach preferable fulling milling effect, then by dehydration cleaning removal fulling agent.In technical process for warm soft water (38 DEG C-
40 DEG C) temperature have accurate restriction, the influence of human factor is reduced, so that cashmere sweater washes the controllability of contracting technique more
Good, fulling milling effect is more preferable.
In order to promoted wash contracting processing effect, when fabric is put into shampoo, first fabric is held with hand it is wet, then again
It impregnates 10-15 minutes, then starts to wash contracting.
Wet rear fabric is held to be not easy to float to upper layer, it can be with reliable contacts fulling agent;Being soaked for a period of time simultaneously can also be with
Promote the effect for washing contracting.
Washing contracting bath raio is 1:30.It washes contracting bath raio and refers to cashmere sweater weight and fulling milling liquid weight ratio.When woollen sweater fulling milling
Bath raio should be appropriate, and when bath raio is too small, the friction between cashmere sweater increases, and the degree of irregularity of friction and active force increases, therefore leads
Cause the uneven of fulling milling.When bath raio is excessive, mechanicals efforts are opposite to be reduced, and the friction between woollen sweater slows down, and contracting agent consumption increases
Greatly, the fulling milling time lengthens.Appropriate fulling milling bath raio is 1:25~35.
In actual use, cashmere sweater is after washing contracting technique, and texture is too hard for wool fibre, will affect comfort level when wearing.For
This, it further includes soft treatment that cashmere sweater, which washes contracting technique,.
Soft treatment: being added warm soft water (38 DEG C -40 DEG C), and softening agent is added according to the 7% of fabric weight and stirs equal
It is even, fabric is impregnated 40 minutes, drying, the moisture content after drying is 30%, is then dried.
Softening agent is quiet, dynamic friction coefficient the chemical substance that can change fiber.When changing confficient of static friction, feel touching
Smooth sense is touched with, is easy to move on fiber or fabric;Fine structure when changing dynamic friction coefficient, between fiber and fiber
Be easy to be mutually shifted, that is, fiber or fabric it is easily deformable.The comprehensive of the two feels to be exactly soft.By soft treatment
Afterwards, the wool fibre of cashmere sweater becomes more soft, more comfortable when wearing.
In actual use, its natural drying spent time is longer after cashmere sweater soft treatment, in order to further increase
The efficiency of cashmere sweater concentration technology carries out drying and processing to the cashmere sweater after soft treatment.
Drying and processing: the fabric that moisture content is 30% being put into dryer and is dried, and the temperature of drying is no more than 80
DEG C, it is blown after drying with cold wind, completes treatment process after cooling.
Quickly fabric can be made to become drying using the heat of dryer in this way;Use cold front heavy rain that can make fabric
It is quickly cooled down, while promoting treatment effeciency wool fibre is unlikely to deform, and then ensure that preferable fulling milling effect.
The embodiment of present embodiment is present pre-ferred embodiments, not limits protection model of the invention according to this
Enclose, therefore: the equivalence changes that all structures under this invention, shape, principle are done, should all be covered by protection scope of the present invention it
It is interior.
Claims (6)
1. a kind of cashmere sweater washes contracting technique, it is characterised in that: include the following steps,
Pretreatment: fabric outer is cleaned up, clothing is turned over, fabric is cleaned up;
It washes contracting processing: warm soft water (38 DEG C -40 DEG C) being added into shampoo, fulling agent is added into shampoo, stirs evenly,
Fabric is put into and carries out washing contracting in shampoo;
Dehydration cleaning: will wash the fabric that contracting is completed and dry, then cleaned twice with warm soft water (38 DEG C -40 DEG C), finally dried, complete
At washing contracting technique.
2. a kind of cashmere sweater according to claim 1 washes contracting technique, it is characterised in that: wash in contracting processing step, will knit
When object is put into shampoo, first fabric is held with hand wet, then impregnates again 10-15 minutes, then start to wash contracting.
3. a kind of cashmere sweater according to claim 2 washes contracting technique, it is characterised in that: washing contracting bath raio is 1:30.
4. a kind of cashmere sweater according to claim 1 or 3 washes contracting technique, it is characterised in that: cashmere sweater is washed contracting technique and also wrapped
Soft treatment is included, soft treatment: warm soft water (38 DEG C -40 DEG C) is added, softening agent is added according to the 7% of fabric weight and stirred
Uniformly, fabric is impregnated 40 minutes, drying, the moisture content after drying is 30%, is then dried.
5. a kind of cashmere sweater according to claim 4 washes contracting technique, it is characterised in that: it further includes drying that cashmere sweater, which washes contracting technique,
Dry-cure, drying and processing: the fabric that moisture content is 30% being put into dryer and is dried, and the temperature of drying is no more than 80
℃。
6. a kind of cashmere sweater according to claim 5 washes contracting technique, it is characterised in that: in drying and processing step, after drying
It is blown with cold wind, completes treatment process after cooling.