water
add
dispersing agent
sulphuric acid
coal
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510304155.9A
Other languages
English (en)
Inventor
李全灵
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510304155.9A priority Critical patent/CN106281511A/zh
Publication of CN106281511A publication Critical patent/CN106281511A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Liquid Carbonaceous Fuels (AREA)
  • Emulsifying, Dispersing, Foam-Producing Or Wetting Agents (AREA)

Abstract

水煤浆分散剂,本发明涉及建筑材料技术领域,它的组成成分为:工业萘100-200kg、98%的浓硫酸290-430kg、水200-300kg、37%的甲醛90-100kg、300g/L的氢氧化钠60-90kg、石灰水30-50kg、聚丙烯酰胺90-150kg。它结构稳定,不分层,不沉淀,且分散效果好,没有废物排放,环保经济。

Description

水煤浆分散剂
技术领域
本发明涉及建筑材料技术领域,具体涉及水煤浆分散剂。
背景技术
分散剂按离解与否可分为离子型与非离子型两大类。离子型又可按电荷的属性分为阴离子型、阳离子型和两性型三类。两性型是指当溶液呈碱性时显示阴离子特性,呈酸性时显示阳离子特性。阴离子、非离子、阳离子、及两性分散剂的国际价格比为 1:2:3:4。制浆分散剂多选择阴离子型。阴离子型分散剂主要有萘磺酸盐、木质素磺酸盐、磺化腐值酸盐、聚羧酸系等。
分散剂的作用机理有:(1) 提高煤表面的亲水性,分散剂是一种可促进分散相(水煤浆中的煤粒)在分散介质(水煤浆中的水)中均匀分散的化学药剂,煤炭主体是非极性的碳氢化合物,属疏水性物质,煤炭的润湿性可按水在其表面的接触角大小分成四等,按触角为零者,称强亲水性煤炭,小于 40°者称弱水性煤炭;40°~90°者,称疏水性煤炭;超过90°者称强疏水性煤炭,各种煤炭的表面均显疏水性; (2) 增强煤粒间的静电斥力,胶体颗粒稳定分散的先决条件是颗粒间的静电斥力超过颗粒间的范氏引力,离子型分散剂除能改善煤表面的亲水性外,还能增强其静电斥力,进一步促使煤粒分散于水介质中; (3) 空间隔离位阻效应,水化膜中的水与体系中的“自由水”不同,它因受到表面电场的吸引而呈定向排列,当颗粒相互靠近时,水化膜受挤压变形,引力则力图恢复原来的定向,这样就使水化膜表现出一定的弹性,使煤粒均匀分散,且颗粒表面的分散剂具有一定的厚度,当两个带吸附层的颗粒相互重叠时,由于吸附层分散剂分子运动的自由度受到阻碍,吸附分子的熵减少,因为体系的熵总是自发地向增加方向发展,所以颗粒有再次分开的倾向,避免颗粒聚集,当分散剂为大分子时,被吸附分子有长的亲水链,在煤表面形成三维水化膜,当颗粒相互接近时,产生较强的排斥力,导致煤粒分散悬浮,该斥力即为空间隔离位阻或立体障碍。
现有的水煤浆分散剂稳定性不好,容易分层和沉淀,且分散效果不好,有废物排出。
发明内容
本发明的目的在于针对现有技术的缺陷和不足,提供水煤浆分散剂,结构稳定,不分层,不沉淀,且分散效果好,没有废物排放,环保经济。
为实现上述目的,本发明采用的技术方案是:它的组成成分为:工业萘100-200kg、98%的浓硫酸290-430kg、水200-300kg、37%的甲醛90-100kg、300g/L的氢氧化钠60-90kg、石灰水30-50kg、聚丙烯酰胺90-150kg。
本发明的制作流程如下:
一、在1000L反应釜中,加入100-200kg工业萘,加热熔化,升温到 120℃时启动搅拌,然后升温到150℃,开始缓慢加入98%浓硫酸140-180kg,在搅拌状态下于160~165℃下恒温2~3小时,进行磺化反应;
二、反应结束后,降温至120℃,加水100-150kg,于110~120℃水解50分钟,然后补加浓硫酸150-250kg,使总酸度维持在30%左右;
三、反应物降温至90℃左右时,在2小时内增滴加完37%甲醛90-100kg后,在100~105℃下进行缩合反应2小时;
四、缩合反应完毕时加入100-150kg的水搅拌均匀,再加300g/L的NaOH溶液60-90kg,搅拌均匀,用石灰水30-50kg调PH值至7~9,然后加入90-150kg的聚丙烯酰胺,溶解,搅拌30分钟,进行真空抽滤,将滤液浓缩到50%,喷雾干燥即制得棕色粉末装产品,或者浓缩到一定的浓度得到液体产品。
采用上述结构后,本发明有益效果为:本发明所述的水煤浆分散剂,结构稳定,不分层,不沉淀,且分散效果好,没有废物排放,环保经济。
具体实施方式
具体实施方式一:
本具体实施方式采用的技术方案是:它的组成成分为:工业萘120-180kg、98%的浓硫酸290-430kg、水200-300kg、37%的甲醛90-98kg、300g/L的氢氧化钠65-80kg、石灰水30-50kg、聚丙烯酰胺95-110kg。
本发明的制作流程如下:
一、 在1000L反应釜中,加入120-180kg工业萘,加热熔化,升温到 120℃时启动搅拌,然后升温到150℃,开始缓慢加入98%浓硫酸140-180kg,在搅拌状态下于160~165℃下恒温2~3小时,进行磺化反应;
二、反应结束后,降温至120℃,加水100-150kg,于110~120℃水解50分钟,然后补加浓硫酸150-250kg,使总酸度维持在30%左右;
三、反应物降温至90℃左右时,在2小时内增滴加完37%甲醛90-98kg后,在100~105℃下进行缩合反应2小时;
四、缩合反应完毕时加入100-150kg的水搅拌均匀,再加300g/L的NaOH溶液65-80kg,搅拌均匀,用石灰水30-50kg调PH值至7~9,然后加入95-110kg的聚丙烯酰胺,溶解,搅拌30分钟,进行真空抽滤,将滤液浓缩到50%,喷雾干燥即制得棕色粉末装产品,或者浓缩到一定的浓度得到液体产品。
本发明有益效果为:本发明所述的水煤浆分散剂,结构稳定,不分层,不沉淀,且分散效果好,没有废物排放,环保经济。
具体实施方式二:
本具体实施方式采用的技术方案是:它的组成成分为:工业萘150kg、98%的浓硫酸300kg、水220kg、37%的甲醛95kg、300g/L的氢氧化钠70.8kg、石灰水40kg、聚丙烯酰胺100kg。
本发明的制作流程如下:
一、在1000L反应釜中,加入150kg工业萘,加热熔化,升温到 120℃时启动搅拌,然后升温到150℃,开始缓慢加入98%浓硫酸152kg,在搅拌状态下于160~165℃下恒温2~3小时,进行磺化反应;
二、反应结束后,降温至120℃,加水120kg,于110~120℃水解50分钟,然后补加浓硫酸148kg,使总酸度维持在30%左右;
三、反应物降温至90℃左右时,在2小时内增滴加完37%甲醛95kg后,在100~105℃下进行缩合反应2小时;
四、缩合反应完毕时加入100kg的水搅拌均匀,再加300g/L的NaOH溶液70.8kg,搅拌均匀,用石灰水40kg调PH值至7~9,然后加入100 kg的聚丙烯酰胺,溶解,搅拌30分钟,进行真空抽滤,将滤液浓缩到50%,喷雾干燥即制得棕色粉末装产品,或者浓缩到一定的浓度得到液体产品。
以上所述仅用以说明本发明的技术方案而非限制,本领域普通技术人员对本发明的技术方案所做的其它修改或者等同替换,只要不脱离本发明技术方案的精神和范围,均应涵盖在本发明的权利要求范围当中。

Claims (2)

1.水煤浆分散剂,其特征在于:它的组成成分为:工业萘100-200kg、98%的浓硫酸290-430kg、水200-300kg、37%的甲醛90-100kg、300g/L的氢氧化钠60-90kg、石灰水、聚丙烯酰胺90-150kg。
2.水煤浆分散剂,其特征在于:它的制作流程如下:
(一)、在1000L反应釜中,加入100-200kg工业萘,加热熔化,升温到 120℃时启动搅拌,然后升温到150℃,开始缓慢加入98%浓硫酸140-180kg,在搅拌状态下于160~165℃下恒温2~3小时,进行磺化反应;
(二)、反应结束后,降温至120℃,加水100-150kg,于110~120℃水解50分钟,然后补加浓硫酸150-250kg,使总酸度维持在30%左右;
(三)、反应物降温至90℃左右时,在2小时内增滴加完37%甲醛90-100kg后,在100~105℃下进行缩合反应2小时;
(四)、缩合反应完毕时加入100-150kg的水搅拌均匀,再加300g/L的NaOH溶液60-90kg,搅拌均匀,用石灰水30-50kg调PH值至7~9,然后加入90-150kg的聚丙烯酰胺,溶解,搅拌30分钟,进行真空抽滤,将滤液浓缩到50%,喷雾干燥即制得棕色粉末装产品,或者浓缩到一定的浓度得到液体产品。
CN201510304155.9A 2015-06-08 2015-06-08 水煤浆分散剂 Pending CN106281511A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510304155.9A CN106281511A (zh) 2015-06-08 2015-06-08 水煤浆分散剂

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510304155.9A CN106281511A (zh) 2015-06-08 2015-06-08 水煤浆分散剂

Publications (1)

Publication Number Publication Date
CN106281511A true CN106281511A (zh) 2017-01-04

Family

ID=57658699

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510304155.9A Pending CN106281511A (zh) 2015-06-08 2015-06-08 水煤浆分散剂

Country Status (1)

Country Link
CN (1) CN106281511A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109233923A (zh) * 2018-11-26 2019-01-18 萍乡市乐乐腐植酸厂 一种粗品腐殖酸制备腐殖酸分散剂的方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101543745A (zh) * 2009-05-06 2009-09-30 北京华中新工贸有限公司 一种制备扩散剂方法及扩散剂
CN101735870A (zh) * 2009-12-16 2010-06-16 北京海淀华煤水煤浆技术开发中心 一种水煤浆添加剂及其制备方法与应用
CN102250655A (zh) * 2011-06-10 2011-11-23 天津市双盛化学助剂工贸有限公司 一种高流动性气化水煤浆分散剂的制备方法
CN103509617A (zh) * 2013-01-17 2014-01-15 湖南东盈煤化工技术开发有限公司 一种煤气化专用的复合水煤浆添加剂

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101543745A (zh) * 2009-05-06 2009-09-30 北京华中新工贸有限公司 一种制备扩散剂方法及扩散剂
CN101735870A (zh) * 2009-12-16 2010-06-16 北京海淀华煤水煤浆技术开发中心 一种水煤浆添加剂及其制备方法与应用
CN102250655A (zh) * 2011-06-10 2011-11-23 天津市双盛化学助剂工贸有限公司 一种高流动性气化水煤浆分散剂的制备方法
CN103509617A (zh) * 2013-01-17 2014-01-15 湖南东盈煤化工技术开发有限公司 一种煤气化专用的复合水煤浆添加剂

Non-Patent Citations (3)

* Cited by examiner, † Cited by third party
Title
何国锋: "《水煤浆新技术研发及实践》", 29 February 2012 *
徐江华 等: ""萘磺酸甲醛缩合物的合成及其在水煤浆添加剂中的应用"", 《淮南矿业学院学报》 *
马宝岐等: "《煤焦油制燃料油品》", 31 January 2011 *

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109233923A (zh) * 2018-11-26 2019-01-18 萍乡市乐乐腐植酸厂 一种粗品腐殖酸制备腐殖酸分散剂的方法

Similar Documents

Publication Publication Date Title
WO2021204210A9 (zh) 以水泥和"三废"为原料的微纳米材料系列产品及合成工艺
CN103535376A (zh) 一种具有抗菌与吸附功能的纳米氧化锌-竹炭复合粒子的制备方法
CN102583973A (zh) 一种空心玻璃微球软化学制备方法和所制空心玻璃微球及其应用
CN103086415A (zh) 水热条件下贝壳制备片状文石结构碳酸钙粉体的方法
CN108160338B (zh) 一种胶磷矿脱镁反浮选捕收剂及其制备方法
CN101905861A (zh) 一种纳米层状复合金属氢氧化物的制备方法
WO2014181346A4 (en) A process for manufacturing of boehmite particulate material
CN104386726A (zh) 一种室温固相反应制备球霰石型碳酸钙微球的方法
CN111362607A (zh) 一种轻质固废免烧陶粒及其制备方法
CN104194847B (zh) 一种含腰果酚磺酸盐的水煤浆添加剂及其应用
CN106281511A (zh) 水煤浆分散剂
CN103804617A (zh) 苯酚改性减水剂
CN109133775B (zh) 锂渣混配砂砾型水泥混凝土及其制备方法
KR20100014349A (ko) 탄산기 함유 수산화마그네슘 입자 및 그 제조 방법
CN110040987B (zh) 一种菱镁矿浮选尾矿制备轻烧镁砂的方法
CN113788635B (zh) 一种不带入污染性铬元素的通用水泥生产方法
CN101597078A (zh) 一种片状α-Al2O3颗粒粉体的制备方法
CN110423379A (zh) 一种氢氧化镁/石墨烯薄片复合阻燃剂及其制备方法
CN109775734A (zh) 一种低比表面积碱式碳酸镁的制备方法
WO2019019844A1 (zh) 钙铁榴石一步碱热法处理拜耳法赤泥生产4a沸石的方法
CN109824309B (zh) 一种利用地质聚合反应制备耐酸矿石团聚体的方法
CN101804332B (zh) 用煤矸石、聚乙烯亚胺制备二氧化碳捕捉材料的方法
CN111063502B (zh) 一种稳定性可调的磁流体及其制备与回收方法
CN1328202C (zh) 一种具有抑制碱骨料反应效能的高效减水剂及其制备方法
CN110052332B (zh) 一种铜基配位聚合物及其制备方法和作为脉石矿物抑制剂在铜镍硫化矿浮选中的应用

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20170104

RJ01 Rejection of invention patent application after publication