CN106170027A CN201610192656.7A CN201610192656A CN106170027A CN 106170027 A CN106170027 A CN 106170027A CN 201610192656 A CN201610192656 A CN 201610192656A CN 106170027 A CN106170027 A CN 106170027A
Authority
CN
China
Prior art keywords
glass
mobile phone
carried out
touch screen
manufacture method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610192656.7A
Other languages
Chinese (zh)
Inventor
程先本
张平
陈盘石
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI VOWBO PHOTOELECTRIC MATERIAL Co Ltd
Original Assignee
ANHUI VOWBO PHOTOELECTRIC MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI VOWBO PHOTOELECTRIC MATERIAL Co Ltd filed Critical ANHUI VOWBO PHOTOELECTRIC MATERIAL Co Ltd
Priority to CN201610192656.7A priority Critical patent/CN106170027A/en
Publication of CN106170027A publication Critical patent/CN106170027A/en
Pending legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H04ELECTRIC COMMUNICATION TECHNIQUE
    • H04MTELEPHONIC COMMUNICATION
    • H04M1/00Substation equipment, e.g. for use by subscribers
    • H04M1/02Constructional features of telephone sets
    • H04M1/0202Portable telephone sets, e.g. cordless phones, mobile phones or bar type handsets
    • H04M1/026Details of the structure or mounting of specific components
    • H04M1/0266Details of the structure or mounting of specific components for a display module assembly
    • CCHEMISTRY; METALLURGY
    • C03GLASS; MINERAL OR SLAG WOOL
    • C03BMANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
    • C03B27/00Tempering or quenching glass products
    • CCHEMISTRY; METALLURGY
    • C03GLASS; MINERAL OR SLAG WOOL
    • C03BMANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
    • C03B33/00Severing cooled glass
    • C03B33/02Cutting or splitting sheet glass or ribbons; Apparatus or machines therefor
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P40/00Technologies relating to the processing of minerals
    • Y02P40/50Glass production, e.g. reusing waste heat during processing or shaping
    • Y02P40/57Improving the yield, e-g- reduction of reject rates

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Organic Chemistry (AREA)
  • Signal Processing (AREA)
  • Physics & Mathematics (AREA)
  • Thermal Sciences (AREA)
  • Laminated Bodies (AREA)
  • Joining Of Glass To Other Materials (AREA)

Abstract

The present invention relates to the manufacture method of a kind of mobile phone capacitive touch screen cover-plate glass, belong to mobile phone glass cover plate production field.Large stretch of glass-cutting is become than product the specification of big 20 30mm, enters next process;According to having design drawing, the glass after sawing sheet is carried out trimming, fluting, edge grinding;Glass is carried out plain grinding again, improves surface smoothness;Then glass is carried out tempering process;Then, after glass is carried out the wire mark of one side, high-temperature baking is carried out;Anti-radiation film is plated again at glass another side;Finally the above-mentioned product completed is tested.

Description

A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass
Technical field
The present invention relates to the manufacture method of a kind of mobile phone capacitive touch screen cover-plate glass, belong to hand-set lid glass manufacture Field.
Background technology
Cover-plate glass is called again protection glass, is an important component part as touch-control parts, and its main task is Protection LCD, light transmission is good and the effect of device touch-control parts.As the cover-plate glass of mobile phone, need printed ink area overleaf Greatly, the substantial amounts of bad product of the as easy as rolling off a log generation of secondary operation, such as defects such as pin hole light leak, variable color or edge blackouts.
Summary of the invention
The technical problem to be solved is: provide a kind of mobile phone capacitive touch screen lid improving product yield The manufacture method of glass sheet.The technical problem to be solved takes techniques below scheme to realize:
The manufacture method of a kind of mobile phone capacitive touch screen cover-plate glass, said method comprising the steps of:
A. sawing sheet: large stretch of glass-cutting is become the specification of 20-30mm bigger than product, enters next process;
B. molding: according to having design drawing, carries out trimming, fluting, edge grinding to the glass after sawing sheet;
C. plain grinding: glass carries out plain grinding, improves surface smoothness;
D. tempering: glass is carried out tempering process;
F. wire mark: after glass is carried out the wire mark of one side, carry out high-temperature baking;
G. plated film: plate anti-radiation film at glass another side;
H. inspection: the above-mentioned product completed is tested.
Preferably, rank or punching can be begined a theatrical performance with finishing impression after described step B molding.
Preferably, described D step tempering is to use the glass after plain grinding is put into heating furnace, and heating makes its 600 degrees Celsius, Again it is carried out high pressure cooling air and be cooled to room temperature rapidly.
Preferably, the wire mark of described F step is to use the mode of three superpositions to print, first to glass glass one side Carry out impurity cleaning, then carry out wire mark color sample for the first time, carry out 60-80 degree Celsius of baking 30min-50min, then carry out Wire mark color sample for the second time, rebake 30min-50min, after room temperature again after transparent protective film of net, at baking 10min- 20min。
Preferably, electrostatic precipitation operation will be entered before described each three wire marks.
Beneficial effect: glass is carried out tempering process by physics mode so that it is by under big External Force Acting the most not Can be the most broken, protection LCD and the safety of user;Use three secondary net India side formulas, reduce and printing process produces pin hole light leak And variable color.
Detailed description of the invention
In order to the technological means of the present invention, creation characteristic, reach purpose and be easy to understand with effect, it is expanded on further The present invention.
The manufacture method of a kind of mobile phone capacitive touch screen cover-plate glass, it is characterised in that described method includes following step Rapid:
A. sawing sheet: large stretch of glass-cutting is become the specification of 20-30mm bigger than product, enters next process;
B. molding: according to having design drawing, carries out trimming, fluting, edge grinding to the glass after sawing sheet;
C. plain grinding: glass carries out plain grinding, improves surface smoothness;
D. tempering: glass is carried out tempering process;
F. wire mark: after glass is carried out the wire mark of one side, carry out high-temperature baking;
G. plated film: plate anti-radiation film at glass another side;
H. inspection: the above-mentioned product completed is tested.
Further, rank or punching can be begined a theatrical performance with finishing impression after described step B molding.
Further, described D step tempering is to use the glass after plain grinding is put into heating furnace, and heating makes it 600 Celsius Degree, then to its carry out high pressure cooling air be cooled to room temperature rapidly.
Further, the wire mark of described F step is to use the mode of three superpositions to print, first to glass glass one side Glass carries out impurity cleaning, then carries out wire mark color sample for the first time, carries out 60-80 degree Celsius of baking 30min-50min, then enters Row second time wire mark color sample, rebake 30min-50min, after room temperature again after transparent protective film of net, in baking 10min-20min。
Further, electrostatic precipitation operation will be entered before described each three wire marks.
The ultimate principle of the present invention and principal character and advantages of the present invention have more than been shown and described.The technology of the industry Personnel are it should be appreciated that the present invention is not restricted to the described embodiments, without departing from the spirit and scope of the present invention, and this Bright also having various changes and modifications, these changes and improvements both fall within scope of the claimed invention.Application claims Protection domain is defined by appending claims and equivalent thereof.

Claims (5)

1. the manufacture method of a mobile phone capacitive touch screen cover-plate glass, it is characterised in that said method comprising the steps of:
A. sawing sheet: large stretch of glass-cutting is become the specification than the mobile phone big 20-30dmm of figure paper size, enters next process;
B. molding: according to having design drawing, carries out trimming, fluting, edge grinding operation to the glass after sawing sheet;
C. plain grinding: glass carries out plain grinding, improves surface smoothness;
D. tempering: glass is carried out tempering process;
F. wire mark: after glass is carried out the wire mark of one side, carry out high-temperature baking;
G. plated film: plate anti-radiation film at glass another side;
H. inspection: the above-mentioned product completed is tested.
2. the manufacture method of mobile phone capacitive touch screen cover-plate glass as claimed in claim 1, it is characterised in that described B walks Rank or punching can be begined a theatrical performance with finishing impression after rapid molding.
3. the manufacture method of mobile phone capacitive touch screen cover-plate glass as claimed in claim 1, it is characterised in that described D walks Rapid tempering is to use the glass after plain grinding is put into heating furnace, and heating makes its 600 degrees Celsius, then it is carried out high pressure cooling air It is cooled to room temperature rapidly.
4. the manufacture method of mobile phone capacitive touch screen cover-plate glass as claimed in claim 1, it is characterised in that described F walks Rapid wire mark is to use the mode of three superpositions to print glass one side, first glass is carried out impurity cleaning, then carries out Wire mark color sample for the first time, carries out 60-80 degree Celsius of baking 30min-50min, then carries out using the silk screen of small-bore to carry out Wire mark color sample for the second time, rebake 30min-50min, after room temperature again after transparent protective film of wire mark, in baking 10min-20min。
5. the manufacture method of mobile phone capacitive touch screen cover-plate glass as claimed in claim 4, it is characterised in that described every time Electrostatic precipitation operation will be entered before three wire marks.
CN201610192656.7A 2016-03-29 2016-03-29 A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass Pending CN106170027A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201610192656.7A CN106170027A (en) 2016-03-29 2016-03-29 A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201610192656.7A CN106170027A (en) 2016-03-29 2016-03-29 A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass

Publications (1)

Publication Number Publication Date
CN106170027A true CN106170027A (en) 2016-11-30

Family

ID=57358886

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201610192656.7A Pending CN106170027A (en) 2016-03-29 2016-03-29 A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass

Country Status (1)

Country Link
CN (1) CN106170027A (en)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106946447A (en) * 2017-02-16 2017-07-14 芜湖荣茂电子材料有限公司 A kind of processing technology of mobile phone glass
CN107651863A (en) * 2017-09-29 2018-02-02 广东星弛光电科技有限公司 A kind of preparation method for the hand-set lid coated glass for ending blue light
CN109151113A (en) * 2018-08-28 2019-01-04 余泽军 A kind of manufacture craft of mobile phone glass cover board
CN109542271A (en) * 2018-11-26 2019-03-29 重庆津油纳米光学科技有限公司 A kind of production method of touch screen
CN110228949A (en) * 2018-03-05 2019-09-13 蓝思科技(长沙)有限公司 A kind of small size cover board manufacture craft

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2009019965A1 (en) * 2007-08-03 2009-02-12 Nippon Electric Glass Co., Ltd. Hardened glass substrate and method for manufacturing the same
CN103713768A (en) * 2013-12-10 2014-04-09 黄彩娟 Cover plate structure, touch panel structure and protective panel structure of display device
CN104253883A (en) * 2013-06-27 2014-12-31 王荷琴 Manufacture method of mobile phone glass

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2009019965A1 (en) * 2007-08-03 2009-02-12 Nippon Electric Glass Co., Ltd. Hardened glass substrate and method for manufacturing the same
CN104253883A (en) * 2013-06-27 2014-12-31 王荷琴 Manufacture method of mobile phone glass
CN103713768A (en) * 2013-12-10 2014-04-09 黄彩娟 Cover plate structure, touch panel structure and protective panel structure of display device

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106946447A (en) * 2017-02-16 2017-07-14 芜湖荣茂电子材料有限公司 A kind of processing technology of mobile phone glass
CN107651863A (en) * 2017-09-29 2018-02-02 广东星弛光电科技有限公司 A kind of preparation method for the hand-set lid coated glass for ending blue light
CN110228949A (en) * 2018-03-05 2019-09-13 蓝思科技(长沙)有限公司 A kind of small size cover board manufacture craft
CN109151113A (en) * 2018-08-28 2019-01-04 余泽军 A kind of manufacture craft of mobile phone glass cover board
CN109151113B (en) * 2018-08-28 2020-10-09 安徽徽昂光电科技有限公司 Manufacturing process of mobile phone glass cover plate
CN109542271A (en) * 2018-11-26 2019-03-29 重庆津油纳米光学科技有限公司 A kind of production method of touch screen

Similar Documents

Publication Publication Date Title
CN106170027A (en) A kind of manufacture method of mobile phone capacitive touch screen cover-plate glass
CN101462426B (en) Technology for printing sheet material with 3-D pattern
CN105183237B (en) A kind of manufacturing method of the touch screen with IR induction zone
CN101941337A (en) Display glass printing technology and refrigerator door shaping method using finished products formed thereby
CN102582340A (en) Tempered glass decorative plate printed with three-dimensional patterns and printing process thereof
CN106891635B (en) A kind of transfer processing method of surrounding curved surface 3D cover board
CN105034561A (en) Glass thermal transferring apparatus for display device and method thereof
CN103722965A (en) Preparation method of thermal transfer printing glass
CN101429841A (en) 2mm silk-screen strengthened glass and wood plank combined kitchen cabinet door board production technology
CN204009275U (en) A kind of crooked liquid crystal display device and display device thereof
CN102603175A (en) Device and method for producing toughened glass
CN205890165U (en) Press machine with device induced drafts
CN202453649U (en) Low-pressure-drying preliminary drying device
CN204322722U (en) A kind of silk-screen drying line
CN104281310A (en) Touch panel structure, manufacturing method of touch panel structure and touch device of touch panel structure
CN203059426U (en) Low-iron super-white printing oven glass door plate
CN203128411U (en) Full-automatic control system for balancing wind pressure of glass toughening cooling wind grid
CN205601352U (en) Synchronous silk screen printing frock of monolithic polychrome
CN206633597U (en) A kind of full-automatic printing equipment
CN106587650B (en) A kind of local bad reworking method of silk printing glass
CN109177551A (en) It is a kind of on glass cover-plate simultaneously silk-screen IR and the technique to bit line
CN202448654U (en) Toughened glass decorating plate printed with three-dimensional image
Xie et al. Weight loss phenomenon of paper and the mechanism for negligible damage of heat-induced inkless eco-printing
CN204320627U (en) A kind of size coat machine with hot blast function of exchange
CN106290028A (en) A kind of method of testing characterizing CCL powder body material Mohs' hardness

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20161130

RJ01 Rejection of invention patent application after publication