CN105040914A - 宠物屋屋顶油毡附着工艺 - Google Patents

宠物屋屋顶油毡附着工艺 Download PDF

Info

Publication number
CN105040914A
CN105040914A CN201510448832.4A CN201510448832A CN105040914A CN 105040914 A CN105040914 A CN 105040914A CN 201510448832 A CN201510448832 A CN 201510448832A CN 105040914 A CN105040914 A CN 105040914A
Authority
CN
China
Prior art keywords
malthoid
linoleum
roofing
pet house
roof
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510448832.4A
Other languages
English (en)
Inventor
傅立春
劳宝根
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujian Liancheng Hangkai Wood Industry Co Ltd
Original Assignee
Fujian Liancheng Hangkai Wood Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fujian Liancheng Hangkai Wood Industry Co Ltd filed Critical Fujian Liancheng Hangkai Wood Industry Co Ltd
Priority to CN201510448832.4A priority Critical patent/CN105040914A/zh
Publication of CN105040914A publication Critical patent/CN105040914A/zh
Pending legal-status Critical Current

Abstract

本发明公开了宠物屋屋顶油毡附着工艺,包括如下步骤:步骤一,根据屋面大小裁好油毡;步骤二,将裁好后的油毡铺设在屋面上;步骤三,对油毡进行加热处理,使油毡上的沥青软化并附着在屋面上;步骤四,冷却油毡直至固化。本发明整个铺设过程非常简单,通过对油毡进行加热使沥青***,油毡在重力的作用下会自动和屋面贴合,无需人工强行压制,***后的沥青将渗透进屋顶表面,冷却后沥青将被牢牢的吸附在屋面,结合强度非常高,并且经软化铺设完成后油毡的平整度将和原屋面一致,因此适合任何屋面形状的宠物屋。由于没有采用胶水,因此环保,无需压制,无需晾干,且对屋面基础的要求低。

Description

宠物屋屋顶油毡附着工艺
技术领域
本发明涉及宠物屋屋顶油毡附着工艺。
背景技术
油毡是用动物的毛或植物纤维制成的毡或厚纸坯,浸透沥青后所成的建筑材料,具有韧性,且不透水,用来做屋顶、地下室墙壁、地基等的防水、防潮层。油毡运输存放时需卷起以减少空间,油毡上下面贴有塑料薄膜制成的隔离薄膜,防止卷绕时沥青相互粘连在一起,使用时揭去隔离薄膜即可。
宠物屋在制作完成后多采用屋顶附着油毡的方法来进行防水,传统的附着工艺,采用胶水将油毡粘合在宠物屋顶上,该工艺具有如下缺点:
一、胶水气味重,甲醛含量超标,不环保,影响宠物的生活环境;
二、作业时间长,效率低,每一平方米屋面的面积从上胶水到胶水晾干至少需要10分钟;
三、难度大,上油毡时需整块平整铺开,不能有凸起,并用木板施加压力使之和胶水完全粘合,否则胶水不均匀容易空鼓和脱胶;
四、油毡边沿的胶水粘合附着效果差,容易脱胶。
五、对屋面要求高,首先要求屋面基层表面坚硬,否则施压时容易塌陷,再者需干燥、无尘、无油污、无凸起和无凹陷等,否则将影响胶水的粘合性能。
鉴于此,本发明人专门研制出一种无需胶水的宠物屋屋顶油毡附着工艺,本案由此产生。
发明内容
本发明的目的在于提供宠物屋屋顶油毡附着工艺,环保,工艺简单,无需胶水即可将油毡牢靠的附着在屋顶上,且对屋面基础的要求低。
为了实现上述目的,本发明的技术方案如下:
宠物屋屋顶油毡附着工艺,包括如下步骤:
步骤一,根据屋面大小裁好油毡;
步骤二,将裁好后的油毡铺设在屋面上;
步骤三,对油毡进行加热处理,使油毡上的沥青软化并附着在屋面上;
步骤四,冷却油毡直至固化。
进一步,步骤二铺设时,油毡需和屋面贴合,保证油毡平整无拱起。
进一步,步骤三采用液化气打火枪喷射的火焰对油毡进行来回均匀加热。
进一步,步骤三加热处理的加热温度为60-70度,加热时间为每平方米3-4分钟。
进一步,步骤三加热完成后,观察软化后的油毡是否有拱起或褶皱,如有采用木板轻轻压平。
进一步,步骤四采用自然风冷。
进一步,步骤一中裁剪的油毡面积大于屋面面积,步骤二铺设时需保证油毡伸出屋面四周的距离一致,步骤三加热完成后,将伸出屋面的油毡向内卷并吸附在屋顶屋檐内侧。
采用上述方案后,本发明整个铺设过程非常简单,通过对油毡进行加热使沥青***,油毡在重力的作用下会自动和屋面贴合,无需人工强行压制,***后的沥青将渗透进屋顶表面,冷却后沥青将被牢牢吸附在屋面,结合强度非常高,并且经软化铺设完成后油毡的平整度将和原屋面一致,因此适合任何屋面形状的宠物屋。由于没有采用胶水,因此环保,无需压制,无需晾干,且对屋面基础的要求低。
具体实施方式
为了进一步解释本发明的技术方案,下面通过具体实施例来对本发明进行详细阐述。
本发明揭示的宠物屋屋顶油毡附着工艺,包括如下步骤:
步骤一,根据屋面大小裁好油毡,油毡的面积最好略大于屋面;
步骤二,将裁好后的油毡铺设在屋面上,铺设时,用手将油毡和屋面贴合,保证油毡平整无拱起,其中需保证油毡四周离屋面四周的距离一致。
步骤三,采用液化气打火枪喷射的火焰对油毡进行来回均匀加热,使油毡上的沥青软化并附着在屋面上。油毡的加热温度为60-70度,一般加热时间为每平方米3-4分钟时即可,此时油毡的柔软度最适合屋面的铺设,不会因沥青太硬而无法渗透进屋面,又不会因沥青太软而局部滴落,或局部塌落。
打火枪喷射的火焰具有范围广的特点,因此加热更加均匀,并可缩短加热时间,再者打火枪喷射的火焰的冲击力能使油毡更快的附着在屋面上。
加热完成后,需观察软化后的油毡是否有拱起或褶皱,如有采用木板轻轻压平即可。再将伸出屋面四周的油毡向内卷其,使其吸附在屋顶的屋檐内侧,因此在屋檐内的包边可免遭风雨的腐蚀,进一步增强包边的附着性能,且包边内敛更加美观。
步骤四,采用自然风冷却油毡,直至固化,由于是自然风冷,因此无需人工操作,此时宠物屋可置于原地,也可移置其它位置进行冷却,不会占用作业场地,因此不会影响后续宠物屋油毡的铺设,提高了作业效率。
本实施例整个铺设过程非常简单,通过对油毡进行加热使沥青***,油毡在重力的作用下会自动和屋面贴合,无需人工强行压制,***后的沥青将渗透进屋顶表面,冷却后沥青将被牢牢的吸附在屋面,结合强度非常高,并且经软化铺设完成后油毡的平整度将和原屋面一致,因此适合任何屋面形状的宠物屋。由于没有采用胶水,因此环保,无需压制,无需晾干,且对屋面基础的要求低。
以上仅为本发明的较佳实施例,并非对本发明的保护范围的限定。凡依本案的设计思路所做的等同变化,均落入本案的保护范围。

Claims (7)

1.宠物屋屋顶油毡附着工艺,其特征在于:宠物屋屋顶油毡附着工艺,包括如下步骤:
步骤一,根据屋面大小裁好油毡;
步骤二,将裁好后的油毡铺设在屋面上;
步骤三,对油毡进行加热处理,使油毡上的沥青软化并附着在屋面上;
步骤四,冷却油毡直至固化。
2.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤二铺设时,油毡需和屋面贴合,保证油毡平整无拱起。
3.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤三采用液化气打火枪喷射的火焰对油毡进行来回均匀加热。
4.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤三加热处理的加热温度为60-70度,加热时间为每平方米3-4分钟。
5.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤三加热完成后,观察软化后的油毡是否有拱起或褶皱,如有采用木板轻轻压平。
6.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤四采用自然风冷。
7.如权利要求1所述的宠物屋屋顶油毡附着工艺,其特征在于:步骤一中裁剪的油毡面积大于屋面面积,步骤二铺设时需保证油毡伸出屋面四周的距离一致,步骤三加热完成后,将伸出屋面的油毡向内卷并吸附在屋顶屋檐内侧。
CN201510448832.4A 2015-07-28 2015-07-28 宠物屋屋顶油毡附着工艺 Pending CN105040914A (zh)