CN104874826A - 一种厚铜线路板的钻孔制作方法 - Google Patents

一种厚铜线路板的钻孔制作方法 Download PDF

Info

Publication number
CN104874826A
CN104874826A CN201510222489.1A CN201510222489A CN104874826A CN 104874826 A CN104874826 A CN 104874826A CN 201510222489 A CN201510222489 A CN 201510222489A CN 104874826 A CN104874826 A CN 104874826A
Authority
CN
China
Prior art keywords
boring
circuit board
thick copper
copper circuit
drill bit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201510222489.1A
Other languages
English (en)
Other versions
CN104874826B (zh
Inventor
王淑怡
彭卫红
阙玉龙
朱拓
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Suntak Multilayer PCB Co Ltd
Original Assignee
Shenzhen Suntak Multilayer PCB Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Suntak Multilayer PCB Co Ltd filed Critical Shenzhen Suntak Multilayer PCB Co Ltd
Priority to CN201510222489.1A priority Critical patent/CN104874826B/zh
Publication of CN104874826A publication Critical patent/CN104874826A/zh
Application granted granted Critical
Publication of CN104874826B publication Critical patent/CN104874826B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种厚铜线路板的钻孔方法,涉及线路板制作技术领域。所述钻孔方法采用转速为20-30krmp,进刀速度为20-30mm/s,退刀速度为220-300mm/s的钻咀钻孔;所述的钻咀由钻杆和钻头连接组成,钻头包括切削刀片和排屑槽,所述的排屑槽在钻头的钻入端沿轴向设有凹槽;所述线路板内层线路的铜厚≧3OZ。本发明采用有凹槽缺口的钻咀,钻头钻孔端的凹槽缺口一方面可以切断钻孔铜丝,另一方面有利于在钻孔过程中,将切割出来的铜丝及时的利用凹槽排出,避免堵孔、钻孔铜拉丝等问题。

Description

一种厚铜线路板的钻孔制作方法
技术领域
本发明涉及线路板制作技术领域,尤其涉及一种厚铜线路板的钻孔制作方法。
背景技术
线路板生产时,一般采用含树脂量为72%且容易压合及成本较低的半固化片,在外层线路制作工序,如无特殊要求,锡圈直径为0.35mm(锡圈为位于孔位置线路上的铜环,钻孔孔径为1.8mm~1.95mm)。针对此类普通设计的板,通常使用如下参数制作:
采用普通钻咀,钻孔时,一次性钻穿,转速、进刀速、退刀速分别为35krpm、36mm/s、340mm/s。
但针对内层线路厚铜(≥3OZ)设计的多层线路板,铜厚太大,钻咀在切割铜层时,产生的钻污不能及时排出,产生的热量过大,且由于铜具有韧性,钻孔容易出现铜拉丝、孔内热膨胀变形现象,造成断层、铜层错位等问题,且钻咀对铜层的拉扯作用,导致孔内壁铜层偏移或产生缺口;同时,由于热量和冲击力的作用,容易产生断钻咀问题。此外,厚铜板钻孔,还容易出现外层线路图形锡圈和基材分离的问题,而含树脂量为72%的半固化片,压合后,容易产生填树脂量不足或空洞问题。
发明内容
针对上述问题,本发明提供一种厚铜线路板的钻孔方法,具体方案如下:
一种厚铜线路板的钻孔制作方法,所述钻孔制作方法采用转速为20-30krmp,进刀速度为20-30mm/s,退刀速度为220-300mm/s的钻咀钻孔;所述的钻咀由钻杆和钻头连接组成,钻头包括切削刀片和排屑槽,所述的排屑槽在钻头的钻入端沿轴向设有凹槽;所述线路板内层线路的铜厚≧3OZ。
进一步的,所述的钻咀钻孔采用分次进行,每次钻孔的深度为1-2mm。
优选的,所述的凹槽从钻入端沿轴向上宽度逐渐减小。
优选的,所述的凹槽从钻入端沿轴向深度逐渐减小,凹槽的最大深度为切削刀片厚度的1/3-1/2。
优选的,所述切削刀片为螺旋刀片,切削刀片至少为两条。
优选的,所述钻头的钻径为1.8-1.95mm。
进一步的,所述线路板外层线路对应钻孔位置的锡圈直径≧0.42mm。
进一步的,所述线路板中用于压合的半固化片的含胶量为76-80%。
本发明采用有缺口的凹槽钻咀,钻头上的凹槽一方面可以切断钻孔铜丝,另一方面有利于在钻孔过程中,将切割出来的铜丝及时的利用凹槽排出,避免堵孔、钻孔铜拉丝等问题。
采用多次分段钻孔的方法,及时散去钻孔热量,及时排出钻孔钻污,进一步避免堵孔、孔铜丝拉问题。
将钻孔转速、进刀速度相对现有工艺降低10~40%,降低钻孔的冲击拉扯作用力。
退刀速度相对现有工艺降低10~40%,防止退刀速过快造成的拉扯作用力造成外层锡圈脱离的问题,与此同时,在现有锡圈大小基础上,加大锡圈,增大锡圈和板材的结合面积,进一步保证钻孔时锡圈的附着性。
采用含胶量76~80%的半固化片进行压合(也可以使用不同类型的半固化片结合使用,将含胶量较高的半固化片靠近图形层,含胶量较低的半固化片夹于含胶量较高的半固化片当中),充分保证厚铜线路板层间树脂的填充效果。
因此,本发明通过线路板本身半固化片及锡圈设计,为钻孔做前铺垫工作,采用改进的钻咀、调整钻孔参数,有效改善了厚铜板钻孔铜拉丝、铜层偏移及缺口、排钻污难、外层锡圈易脱落的问题。
附图说明
图1为本发明钻咀钻头的钻入端结构图。
具体实施方式
为了更充分理解本发明的技术内容,下面结合具体实施例对本发明的技术方案进一步介绍和说明。
实施例
如图1所示的钻咀,钻咀由钻杆和钻头连接组成,钻头钻径为1.9mm,包括双螺旋的切削刀片1,切削刀片1双螺旋形成两条螺旋形的排屑槽4,排屑槽4在钻头的钻入端2沿轴向设有凹槽3。凹槽3的横截面为三角形,延伸至钻头的钻入端2。凹槽3从钻头的钻入端2沿轴向宽度逐渐减小、深度逐渐减小,凹槽3的最大深度为切削刀片1厚度的1/2,宽度最小端与切削刀片1的表面连接。钻头的钻入端2与钻咀的轴向夹角为67.5°。
应用上述钻咀制作线路板钻孔,线路板为6层铜线路的压合板,内层线路铜厚5OZ,外层线路对应钻孔位置锡圈直径0.45mm。线路板总厚度为5mm,用于压合的半固化片的含胶量为76-80%。
钻孔方法为:将线路板置于钻咀下方,外层线路的锡圈中心位于钻头的正下方,设定钻咀钻孔的转速为25krmp,进刀速度为25mm/s,退刀速度为260mm/s。每一个钻孔分5次进行,每次控深钻孔的深度达到1mm后,钻咀退刀,然后再进行下一次控深钻1mm深,直至钻穿线路板。
以上所述仅以实施例来进一步说明本发明的技术内容,以便于读者更容易理解,但不代表本发明的实施方式仅限于此,任何依本发明所做的技术延伸或再创造,均受本发明的保护。

Claims (8)

1.一种厚铜线路板的钻孔制作方法,其特征在于,所述钻孔制作方法采用转速为20-30krmp,进刀速度为20-30mm/s,退刀速度为220-300mm/s的钻咀钻孔;所述的钻咀由钻杆和钻头连接组成,钻头包括切削刀片和排屑槽,所述的排屑槽在钻头的钻入端沿轴向设有凹槽;所述线路板内层线路的铜厚≧3OZ。
2.根据权利要求1所述厚铜线路板的钻孔制作方法,其特征在于,所述的钻咀钻孔采用分次进行,每次钻孔的深度为1-2mm。
3.根据权利要求1所述厚铜线路板的钻孔制作方法,其特征在于,所述的凹槽从钻入端沿轴向上宽度逐渐减小。
4.根据权利要求3所述厚铜线路板的钻孔制作方法,其特征在于,所述的凹槽从钻入端沿轴向深度逐渐减小,凹槽的最大深度为切削刀片厚度的1/3-1/2。
5.根据权利要求4所述厚铜线路板的钻孔制作方法,其特征在于,所述切削刀片为螺旋刀片,切削刀片至少为两条。
6.根据权利要求5所述厚铜线路板的钻孔制作方法,其特征在于,所述钻头的钻径为1.8-1.95mm。
7.根据权利要求1所述厚铜线路板的钻孔制作方法,其特征在于,所述线路板外层线路对应钻孔位置的锡圈直径≧0.42mm。
8.根据权利要求7所述厚铜线路板的钻孔制作方法,其特征在于,所述线路板中用于压合的半固化片的含胶量为76-80%。
CN201510222489.1A 2015-05-04 2015-05-04 一种厚铜线路板的钻孔制作方法 Expired - Fee Related CN104874826B (zh)