CN104815852B - 热连轧层流冷却带钢头部不冷却长度的控制方法 - Google Patents
热连轧层流冷却带钢头部不冷却长度的控制方法 Download PDFInfo
- Publication number
- CN104815852B CN104815852B CN201510258485.9A CN201510258485A CN104815852B CN 104815852 B CN104815852 B CN 104815852B CN 201510258485 A CN201510258485 A CN 201510258485A CN 104815852 B CN104815852 B CN 104815852B
- Authority
- CN
- China
- Prior art keywords
- strip steel
- length
- head
- cool down
- unit
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
热连轧层流冷却带钢头部不冷却长度的控制方法,属于冶金工业生产自动控制领域,即在带钢进入精轧机组F7时,脉冲发生器开始动作,二级计算机通过延时计算公式计算出延时时间,带钢进入层流冷却区阀架后,一级计算机根据二级计算机的喷水指令控制阀架喷水阀的开闭操作,实现带钢头部的不冷却控制。本发明充分利用计算机控制技术的先进性和可操作性的特点,在层流冷却控制中使用,节约了投资,改善了头部不冷却长度控制的稳定性,带钢头部的切损率明显降低,避免了因带钢头部温度低造成卷取机堆钢的问题,取得了良好的效益。
Description
技术领域
本发明属于冶金工业生产自动控制领域,热连轧带钢层流冷却头部不冷却长度的控制技术。
背景技术
2250生产线层流冷却带钢头部不冷却长度控制不够稳定。当不冷长度较长时,带钢头部性能无法达到机械控制要求,成品切除量大,生产成本高。当不冷长度非常短,甚至头部完全冷却时,极易造成卷取机堆钢,从而影响生产效率,企业经济效益遭受损失。故此,层流冷却头部不冷却长度的控制技术成为我们重点研究的问题。
发明内容
本发明目的是为了使热轧带钢层流冷却头部不冷却长度控制稳定,且控制长度在1~1.5米之间,既保证带钢头部切损量不大,同时又能满足卷取机能够正常卷取,不会出现废钢故障。
热连轧层流冷却带钢头部不冷却长度的控制方法,即在带钢进入精轧机组F7时,脉冲发生器开始动作,二级计算机通过延时计算公式计算出延时时间,带钢进入层流冷却区阀架后,一级计算机根据二级计算机的喷水指令控制阀架喷水阀的开闭操作,实现带钢头部的不冷却控制;
延时计算公式:delaytime =(int)( f_NSPLeng*1000) % (int)( f_SectionLeng*1000) /1000/f_Speed+ delaytimecrr ;
其中:delaytime为延时时间(单位是秒);f_NSPLeng为头部不冷长度设定值(单位是米);f_SectionLeng为跟踪段的长度,薄规格带钢为4.56米,厚规格带钢为2.28米;f_Speed为带钢实际速度(单位:米/秒);delaytimecrr为延时时间修正值(单位:秒);
头部不冷却长度设定值为1~1.5米;延时时间修正值为0.2~0.5。
本发明解决了热轧带钢层流冷却头部不冷长度控制不稳定的问题。
太钢热连轧厂层流冷却使用该发明,效果如下:
(1)带钢头部不冷长度控制更加稳定。
(2)避免了卷取机堆钢的废钢事故。
(3)带钢头部切损率明显下降,取得的直接经济效益每年200万元左右。
具体实施方式
下表为部分钢种的头部不冷长度设定值f_NSPLeng(m)和延时修正给定值delaytimeccr (s):
(1)由二级计算机完成头部不冷长度的设定计算及下送工作。
如表1所示,头部不冷却长度通过转化成延时时间得以实现,延时时间的计算过程如下:
delaytime =((int)( f_NSPLeng*1000)) % ((int)( f_SectionLeng *1000)) /1000/f_Speed+ delaytimecrr (公式1)
delaytime为延时时间,f_NSPLeng为头部不冷长度设定值,f_SectionLeng为跟踪段的长度,薄规格带钢为4.56米,厚规格带钢为2.28米, f_Speed为带钢实际速度,delaytimecrr为延时时间修正值。
由于在精轧机组中,带钢易产生抖动、受阻、温度等异常波动,从而使带钢的实际速度存在波动,而钢种规格不同产生的速度波动情况也不同,速度波动直接对delaytime造成影响,故使用delaytimecrr 对delaytime进行修正。delaytimecrr 延时修正值如表中所示。
在程序当中,若delaytime > 0,执行Time::Wait(delaytime)的延时下送工作。
(2)二级计算机执行延时后,一级计算机根据接到的指令指挥现场阀的打开操作,从而保证带钢头部的不冷却控制。
Claims (1)
1.热连轧层流冷却带钢头部不冷却长度的控制方法,即在带钢进入精轧机组F7时,脉冲发生器开始动作,二级计算机通过延时计算公式计算出延时时间,带钢进入层流冷却区阀架后,一级计算机根据二级计算机的喷水指令控制阀架喷水阀的开闭操作,实现带钢头部的不冷却控制;
延时计算公式:delaytime =((int)( f_NSPLeng*1000)) % ((int)( f_SectionLeng*1000)) /1000/f_Speed+ delaytimecrr ;
其中:delaytime为延时时间, 单位是秒;f_NSPLeng为头部不冷长度设定值,单位是米;f_SectionLeng为跟踪段的长度,单位是米;薄规格带钢跟踪段的长度为4.56米,厚规格带钢跟踪段的长度为2.28米;f_Speed为带钢实际速度,单位是米/秒;delaytimecrr为延时时间修正值,单位是米;
头部不冷却长度设定值为1~1.5米;延时时间修正值为0.2~0.5米。