CN104746349A - Preparation method of negative-ion down feather material and negative-ion down feather quilt - Google Patents

Preparation method of negative-ion down feather material and negative-ion down feather quilt Download PDF

Info

Publication number
CN104746349A
CN104746349A CN201310750502.1A CN201310750502A CN104746349A CN 104746349 A CN104746349 A CN 104746349A CN 201310750502 A CN201310750502 A CN 201310750502A CN 104746349 A CN104746349 A CN 104746349A
Authority
CN
China
Prior art keywords
anion
down feather
preparation
fiber
negative
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310750502.1A
Other languages
Chinese (zh)
Inventor
李裕高
梅山标
宋春常
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Shuixing Home Textile Co Ltd
Original Assignee
Shanghai Shuixing Home Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Shuixing Home Textile Co Ltd filed Critical Shanghai Shuixing Home Textile Co Ltd
Priority to CN201310750502.1A priority Critical patent/CN104746349A/en
Publication of CN104746349A publication Critical patent/CN104746349A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method of a negative-ion down feather material and a negative-ion down feather quilt. Down feather fibers are compounded by using a negative ion generation agent and a negative ion far infrared finishing agent so that down feather fibers can absorb negative-ion materials very well under the condition of not adding a penetrating agent and a binding agent; and meanwhile, the negative-ion down feather material has good durability so that the down feather quilt can release negative ions for a long period and the additional value is improved. According to the preparation method, the function of releasing negative ions by the down feather quilt is realized, the air quality can be improved and the down feather has an antibacterial function; the additional value is greatly improved; and the quality and grades of related home textile products are improved, so that the product quality has a qualitative leap.

Description

A kind of preparation method of anion down feather material and anion down feather quilt
Technical field
The present invention relates to a kind of down feather material, be specifically related to a kind of anion down feather material.
Background technology
Air is by countless molecule, former molecular, after the molecule in air or atom lose or obtain electronics, just forms charged particle, is called ion; Positively charged is cation, and electronegative is anion.Anion to the health of people, longevity and ecological significant impact, by domestic and international medical circle expert is verified by clinical practice.Pollute few place in forest, beach, waterfall, countryside etc., containing a large amount of anion air, its concentration is seriously polluted urban hundred times, here people can feel with fresh air, breathe happy, relaxation and happiness, relaxed and joyful, convalescence center is all located at around mountain forest, beach, waterfall basic reason that Here it is, this is the effect that numerous anion air produces.Therefore anion air is referred to as " long-lived element " or " air vitamin " by people.In addition, the anion produced by oxygen in air has higher activity and very strong redox.This interaction energy destroys the cell membrane of bacterium or the activity of cellular plasm organized enzyme, thus reaches object that is antibacterial and sterilization.As can be seen here, suck appropriate anion every day, of great advantage to health.Therefore in recent years anion in the extensive use of each field.
Eider down is good natural heat insulating material formed, has light weight, and soft, the advantages such as good heat preservation performance, eiderdown quilt is also the preferably selection of consumer's insulated bed Bed linens.But the chemical composition of eider down is a kind of protein, and with animal fat, through degreasing repeatedly, cleaning in processing procedure, still impurity and bacterium can not be eliminated completely.Eiderdown quilt will be caused in use will to there will be breed bacteria produce stink like this, and there will be user and occur the problems such as allergic symptom, this greatly affects the use crowd of eiderdown quilt.
Summary of the invention
Cannot eliminate for the eider down adopted in existing eiderdown quilt the problem that impurity and bacterium bring completely, the object of the present invention is to provide one to have negative ion-releasing function, and the preparation method of the obvious anion down feather material of antibacterial effect.
As the second object of the present invention, the present invention is based on this anion down feather material, a kind of anion down feather quilt is also provided.
In order to achieve the above object, the present invention adopts following technical scheme:
A kind of preparation method of anion down feather material, this preparation method uses anion propellant and negative ion far-infrared finishing agent to carry out composite to down fiber, under the condition not adding bleeding agent and adhesive, down fiber is made to absorb anion material, obtained anion down feather fiber.
In the preferred embodiment of this preparation method, when using anion propellant and negative ion far-infrared finishing agent to carry out composite to down fiber, adjusted to ph is to 6-7.5, and bath raio: 1:10, temperature 50-60 DEG C, is then incubated 10-30min, obtained anion down feather fiber.
Further, described anion propellant is Kayacera anion propellant; Described negative ion far-infrared finishing agent is JLSUN888 negative ion far-infrared finishing agent.
Further, described down fiber carry out composite before, carry out the eider down preliminary treatment of following operation successively: 1. raw material go stalk; 2. then dedust is husky; 3. then essence is divided; 4. previous cleaning; 5. wash; 6. clean; 7. dewater.
Further, during described previous cleaning, with cold wash, washing 4-15 minute.
Further, during described washing, with the clever 10-30g/L that deoils; Cleaning agent 15-20g/L; PH value 6.5-7.5, temperature 40-60 DEG C, process 30-40min.
Further, during described cleaning, clean water 20-25 time, each 5min, bath raio 1:20.
Further, described obtained anion down feather fiber is delivered on conveyer belt and is dried, and carries out ultraviolet sterilization.
As the second object of the present invention, a kind of anion down feather quilt, it comprises quilt cover and is filled in the down filler in quilt cover, and described down filler is the anion down feather fiber that above-mentioned preparation method is formed.
Utilize the preparation method of anion down feather material provided by the invention, can be formed and there is negative ion-releasing function, and the obvious anion down feather fiber of antibacterial effect.This anion down feather fiber simultaneously, can be applicable in home textile product, can prepare anion down feather quilt, it not only has negative ion-releasing function, antibacterial effect is obvious simultaneously, to candida albicans, Escherichia coli, the bacteriostasis rate of gold-coloured staphylococci reaches more than 98%, and have long-lasting, in addition quilt in use breed bacteria can not produce stink, also can improve consumer and use eiderdown quilt allergic phenomena, considerably increase the use crowd of eiderdown quilt.
Detailed description of the invention
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, setting forth the present invention further with instantiation below.
Example 1
Anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 is adopted to carry out composite to the eider down of process in this example, thus can under the condition not adding bleeding agent and adhesive, make down fiber well can absorb anion material, there is good persistence simultaneously, thus obtained anion down feather fiber.Use this anion down feather fibroplastic eiderdown quilt energy long-acting negative ion release, improve its added value.
Based on this principle, the process being prepared anion down feather fiber of this example is as follows:
1. eider down preliminary treatment
Raw material goes stalk → dedust husky → smart point → previous cleaning → washing → cleaning → dehydration.
(1) previous cleaning technique: cold wash, washs 4 minutes;
(2) washing process: Zhejiang development of evil in febrile disease special efficacy is deoiled spirit, FT-101,10g/L, Shanghai Wei Hao eider down cleaning agent, 15g/L, pH value 6.5, temperature 40 DEG C, process 40min;
(3) clean: clean water 20 times, each 5min, bath raio 1:20.
2. the preparation of anion down feather fiber
The eider down good to preliminary treatment adopts anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 to carry out composite, adjusted to ph to 6, bath raio: 1:10, and temperature 50 C, is then incubated 30min, obtained anion down feather fiber.
3. drying and processing
The anion down feather fiber prepared is delivered on conveyer belt and dries, containing ultraviolet sterilization apparatus in drying unit, reach effective bactericidal effect.
Because down fiber chemical composition is a kind of protein, and with animal fat, therefore its to the absorption of auxiliary agent and persistence all difficult, adopt the anion propellant Kayacera of Nippon Kayaku Colors company and the negative ion far-infrared finishing agent JLSUN888 of Beijing Jie Ershuan High Seience Technology Co., Ltd. to carry out composite in this example.Composite auxiliary agent particle diameter is very little, and 50-100nm, is evenly distributed, and can be deep in the cell membrane of eider down, then forms hydrogen bond with the NH2 base in protein molecule, makes the combination that auxiliary agent can be stable with down fiber.The anion down feather fiber prepared thus, generates the gel layer containing nano particle or micropore, makes fabric anion releasing, have antibacterial functions simultaneously under the state of friction.
The anion down feather fiber prepared by above-mentioned technique, test has following technical performance index by experiment:
Anion down feather fiber anion burst size: >=2000/cm3;
Anion down feather fiber is to gold-coloured staphylococci, candida albicans, colibacillary bacteriostasis rate: >=98%.
Thus, utilize this anion down feather fiber as filler, be filled in the anion down feather that formed in quilt cover by the function of not only anion releasing, air quality can be improved, eider down is also made to have antibacterial functions, substantially increase its added value, improve the quality of relevant home textile product and the raising of class, make its product quality achieve qualitative leap.
This anion down feather is tested by experiment has following technical performance index:
Anion down feather quilt, in use after 1 year, anion burst size: >=1800/cm3;
Anion down feather in use breed bacteria can not be produced stink, also can improve consumer and use eiderdown quilt allergic phenomena.
Example 2
The process being prepared anion down feather fiber of this example is as follows:
1. eider down preliminary treatment
Raw material goes stalk → dedust husky → smart point → previous cleaning → washing → cleaning → dehydration.
(1) previous cleaning technique: cold wash, washs 8 minutes;
(2) washing process: Zhejiang development of evil in febrile disease special efficacy is deoiled spirit, FT-101,15g/L, Shanghai Wei Hao eider down cleaning agent, 16g/L, pH value 6.8, temperature 45 C, process 36min;
(3) clean: clean water 22 times, each 5min, bath raio 1:20.
2. the preparation of anion down feather fiber
The eider down good to preliminary treatment adopts anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 to carry out composite, adjusted to ph to 6.5, bath raio: 1:10, and temperature 52 DEG C, is then incubated 28min, obtained anion down feather fiber.
3. drying and processing
The anion down feather fiber prepared is delivered on conveyer belt and dries, containing ultraviolet sterilization apparatus in drying unit, reach effective bactericidal effect.
The anion down feather fiber prepared by above-mentioned technique, test has following technical performance index by experiment:
Anion down feather fiber anion burst size: >=3000/cm3;
Anion down feather fiber is to gold-coloured staphylococci, candida albicans, colibacillary bacteriostasis rate: >=98%.
Thus, the anion down feather of formation is tested by experiment and is had following technical performance index:
Anion down feather quilt, in use after 1 year, anion burst size: >=2000/cm3;
Anion down feather in use breed bacteria can not be produced stink, also can improve consumer and use eiderdown quilt allergic phenomena.
Example 3
The process being prepared anion down feather fiber of this example is as follows:
1. eider down preliminary treatment
Raw material goes stalk → dedust husky → smart point → previous cleaning → washing → cleaning → dehydration.
(1) previous cleaning technique: cold wash, washs 10 minutes;
(2) washing process: Zhejiang development of evil in febrile disease special efficacy is deoiled spirit, FT-101,20g/L, Shanghai Wei Hao eider down cleaning agent, 17g/L, pH value 7.0, temperature 55 DEG C, process 35min;
(3) clean: clean water 23 times, each 5min, bath raio 1:20.
2. the preparation of anion down feather fiber
The eider down good to preliminary treatment adopts anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 to carry out composite, adjusted to ph to 7.0, bath raio: 1:10, and temperature 55 DEG C, is then incubated 25min, obtained anion down feather fiber.
3. drying and processing
The anion down feather fiber prepared is delivered on conveyer belt and dries, containing ultraviolet sterilization apparatus in drying unit, reach effective bactericidal effect.
The anion down feather fiber prepared by above-mentioned technique, test has following technical performance index by experiment:
Anion down feather fiber anion burst size: >=3500/cm3;
Anion down feather fiber is to gold-coloured staphylococci, candida albicans, colibacillary bacteriostasis rate: >=98%.
Thus, the anion down feather of formation is tested by experiment and is had following technical performance index:
Anion down feather quilt, in use after 1 year, anion burst size: >=2500/cm3
Anion down feather in use breed bacteria can not be produced stink, also can improve consumer and use eiderdown quilt allergic phenomena.
Example 4
The process being prepared anion down feather fiber of this example is as follows:
1. eider down preliminary treatment
Raw material goes stalk → dedust husky → smart point → previous cleaning → washing → cleaning → dehydration.
(1) previous cleaning technique: cold wash, washs 12 minutes;
(2) washing process: Zhejiang development of evil in febrile disease special efficacy is deoiled spirit, FT-101,25g/L, Shanghai Wei Hao eider down cleaning agent, 18g/L, pH value 7.2, temperature 58 DEG C, process 32min;
(3) clean: clean water 23 times, each 5min, bath raio 1:20.
2. the preparation of anion down feather fiber
The eider down good to preliminary treatment adopts anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 to carry out composite, adjusted to ph to 7.0, bath raio: 1:10, and temperature 58 DEG C, is then incubated 20min, obtained anion down feather fiber.
3. drying and processing
The anion down feather fiber prepared is delivered on conveyer belt and dries, containing ultraviolet sterilization apparatus in drying unit, reach effective bactericidal effect.
The anion down feather fiber prepared by above-mentioned technique, test has following technical performance index by experiment:
Anion down feather fiber anion burst size: >=3500/cm3;
Anion down feather fiber is to gold-coloured staphylococci, candida albicans, colibacillary bacteriostasis rate: >=98%.
Thus, the anion down feather of formation is tested by experiment and is had following technical performance index:
Anion down feather quilt, in use after 1 year, anion burst size: >=2500/cm3;
Anion down feather in use breed bacteria can not be produced stink, also can improve consumer and use eiderdown quilt allergic phenomena.
Example 5
The process being prepared anion down feather fiber of this example is as follows:
1. eider down preliminary treatment
Raw material goes stalk → dedust husky → smart point → previous cleaning → washing → cleaning → dehydration.
(1) previous cleaning technique: cold wash, washs 15 minutes;
(2) washing process: Zhejiang development of evil in febrile disease special efficacy is deoiled spirit, FT-101,30g/L, Shanghai Wei Hao eider down cleaning agent, 20g/L, pH value 7.5, temperature 60 C, process 30min;
(3) clean: clean water 25 times, each 5min, bath raio 1:20.
2. the preparation of anion down feather fiber
The eider down good to preliminary treatment adopts anion propellant Kayacera and negative ion far-infrared finishing agent JLSUN888 to carry out composite, adjusted to ph to 7.5, bath raio: 1:10, and temperature 60 C, is then incubated 10min, obtained anion down feather fiber.
3. drying and processing
The anion down feather fiber prepared is delivered on conveyer belt and dries, containing ultraviolet sterilization apparatus in drying unit, reach effective bactericidal effect.
The anion down feather fiber prepared by above-mentioned technique, test has following technical performance index by experiment:
Anion down feather fiber anion burst size: >=4000/cm3;
Anion down feather fiber is to gold-coloured staphylococci, candida albicans, colibacillary bacteriostasis rate: >=98%.
Thus, the anion down feather of formation is tested by experiment and is had following technical performance index:
Anion down feather quilt, in use after 1 year, anion burst size: >=3000/cm3;
Anion down feather in use breed bacteria can not be produced stink, also can improve consumer and use eiderdown quilt allergic phenomena.
From upper example, this programme not give only the function of eiderdown quilt anion releasing, also can improve air quality, eider down is also made to have antibacterial functions, substantially increase its added value, improve the quality of relevant home textile product and the raising of class, make its product quality achieve qualitative leap.
More than show and describe general principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (9)

1. the preparation method of an anion down feather material, it is characterized in that, described preparation method uses anion propellant and negative ion far-infrared finishing agent to carry out composite to down fiber, under the condition not adding bleeding agent and adhesive, down fiber is made to absorb anion material, obtained anion down feather fiber.
2. the preparation method of a kind of anion down feather material according to claim 1, it is characterized in that, when using anion propellant and negative ion far-infrared finishing agent to carry out composite to down fiber, adjusted to ph is to 6-7.5; bath raio: 1:10; temperature 50-60 DEG C, is then incubated 10-30min, obtained anion down feather fiber.
3. the preparation method of a kind of anion down feather material according to claim 1 and 2, is characterized in that, described anion propellant is Kayacera anion propellant; Described negative ion far-infrared finishing agent is JLSUN888 negative ion far-infrared finishing agent.
4. the preparation method of a kind of anion down feather material according to claim 1, is characterized in that, described down fiber carry out composite before, carry out the eider down preliminary treatment of following operation successively: 1. raw material go stalk; 2. then dedust is husky; 3. then essence is divided; 4. previous cleaning; 5. wash; 6. clean; 7. dewater.
5. the preparation method of a kind of anion down feather material according to claim 4, is characterized in that, during described previous cleaning, with cold wash, and washing 4-15 minute.
6. the preparation method of a kind of anion down feather material according to claim 4, is characterized in that, during described washing, with the clever 10-30g/L that deoils; Cleaning agent 15-20g/L; PH value 6.5-7.5, temperature 40-60 DEG C, process 30-40min.
7. the preparation method of a kind of anion down feather material according to claim 4, is characterized in that, during described cleaning, and clean water 20-25 time, each 5min, bath raio 1:20.
8. the preparation method of a kind of anion down feather material according to claim 1, is characterized in that, described obtained anion down feather fiber is delivered on conveyer belt and dried, and carries out ultraviolet sterilization.
9. an anion down feather quilt, it comprises quilt cover and is filled in the down filler in quilt cover, it is characterized in that, the anion down feather fiber that described down filler is formed for preparation method according to any one of claim 1 to 8.
CN201310750502.1A 2013-12-31 2013-12-31 Preparation method of negative-ion down feather material and negative-ion down feather quilt Pending CN104746349A (en)