CN104213201A - Dry cocoon shell reeling method - Google Patents

Dry cocoon shell reeling method Download PDF

Info

Publication number
CN104213201A
CN104213201A CN201410440163.1A CN201410440163A CN104213201A CN 104213201 A CN104213201 A CN 104213201A CN 201410440163 A CN201410440163 A CN 201410440163A CN 104213201 A CN104213201 A CN 104213201A
Authority
CN
China
Prior art keywords
hours
cocoon
silk floss
silk
clear water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410440163.1A
Other languages
Chinese (zh)
Other versions
CN104213201B (en
Inventor
林泽银
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huang Ping Fumin sericulture Co., Ltd.
Original Assignee
GUIZHOU HUANGPING COUNTY HAIXIANG SILK CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUIZHOU HUANGPING COUNTY HAIXIANG SILK CO Ltd filed Critical GUIZHOU HUANGPING COUNTY HAIXIANG SILK CO Ltd
Priority to CN201410440163.1A priority Critical patent/CN104213201B/en
Publication of CN104213201A publication Critical patent/CN104213201A/en
Application granted granted Critical
Publication of CN104213201B publication Critical patent/CN104213201B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a dry cocoon shell reeling method, which comprises the following operating steps of impregnating dry cocoon shells for 24 hours in clear water, and draining the water; impregnating the impregnated cocoon shells for 4 to 5 hours in lime water at mass concentration of 0.08 to 0.12 percent; boiling the cocoon shells for 20 to 40 hours by using alkaline water at mass concentration of 0.2 percent; impregnating the boiled cocoon shells for 2 to 3 hours by circulating clear water, and flushing the cocoon shells by using clear water; spin-drying the cocoon shells for 5 to 8 hours to obtain available silk floss by using a washing machine. According to the method, 40 to 60 kilograms of silk floss can be processed every day, the quality of the silk floss is the same as that of conventional purely-manually processed silk floss, the silk floss is white and soft, and related silk floss detection requirements are completely met.

Description

A kind of method of bar cocoon shell filature
Technical field
The present invention relates to a kind of method of bar cocoon shell filature.
Background technology
Silk, is matured silkworm secretion silk liquid concretionary continuous fiber when cocooing, also claims natural silk.It is the same with wool, and be one of animal fiber of utilizing the earliest of the mankind, the strand taken out from single silk cocoon is called silk, and it borrows silk gum to bond coated forming by two filaments.Extracted out by the silk of several silk cocoon, by means of the strand of silk gum bonding parcel, the silk of removing silk gum, is called refining silk.With them for raw material, just available loom is processed into the fabric of each veriety.Usually said mulberry silk, plant mulberry exactly and support the silk extracted out in the cocoon of silkworm knot, yellowish in this silk color and luster is white, feel is fine and smooth, smooth, the distinctive smell of the animal fiber having one light.The quilt particularly soft made with mulberry silk, next to the skin, the manual stacked cocoon silk quilt made is more durable.
But in the rural area of China, silk cocoon is processing like this, after being boiled by silk cocoon plain boiled water, after soaking certain hour, with regard to tearing cocoon shell, for each person every day at most can tearing about 0.5 jin, such method of operating, sometimes hand is all worn, very arduous, and working efficiency is not high.
Summary of the invention
For the deficiencies in the prior art part, the present invention aims to provide a kind of method of dried cocoon shell filature, and main purpose is the working (machining) efficiency improving silk flosssilk wadding, reduces labour intensity.
The object of the invention is to be achieved through the following technical solutions:
The method of this kind of bar cocoon shell filature, comprises following operating procedure:
(1) soak dried cocoon shell after 24 hours with clear water, leak dry;
(2) with containing mass percent concentration being 0.08%-0.12% limewash immersion 4-5 hours;
(3) 20-40 minute is boiled with the buck slow fire that mass percentage concentration is 0.2%;
(4) use circulation cleaning water soaking 2-3 hours, then rinse well with clear water, obtain semi-finished product;
(5) semi-finished product are put into washing machine and dry 5-8 minutes, obtain available silk flosssilk wadding.
The invention has the beneficial effects as follows: adopt the method, within one day, can process 40-60 kilograms of silk flosssilk waddings, the quality of the method processing silk flosssilk wadding reaches original pure manual crudy, and this silk flosssilk wadding is not only pure white but also soft, meets the related request that silk flosssilk wadding detects completely.
Other advantages of the present invention, target and feature will be set forth to a certain extent in the following description, and to a certain extent, based on will be apparent to those skilled in the art to investigating hereafter, or can be instructed from the practice of the present invention.Target of the present invention and other advantages can be realized by description below and claims and be obtained.
Detailed description of the invention
Below will be described in detail the preferred embodiments of the present invention.Should be appreciated that preferred embodiment only in order to the present invention is described, instead of in order to limit the scope of the invention.
Implement place: Huangping County, the Sericulture developing history of Huangping County is very long, and the masses have and oneself breed silkworms, and oneself is come by dried cocoon shell after tearing becomes silk flosssilk wadding, silk flosssilk wadding to be made into cocoon silk quilt.
Embodiment one
The present embodiment comprises following operating procedure:
(1) get 50 kilograms of dried cocoon shells, soak dried cocoon shell after 24 hours with clear water, leak dry;
(2) with containing mass percent concentration be that 0.10% limewash soaks 5 hours;
(3) 30 minutes are boiled with the buck slow fire that mass percentage concentration is 0.2%;
(4) use circulation cleaning water soaking 2.5 hours, then rinse well with clear water;
(5) dry 6 minutes with washing machine, just become available silk flosssilk wadding.
Embodiment two
The present embodiment comprises following operating procedure:
(1) get 30 kilograms of dried cocoon shells, soak dried cocoon shell after 24 hours with clear water, leak dry;
(2) with containing mass percent concentration be that 0.08% limewash soaks 4 hours;
(3) 20 minutes are boiled with the buck slow fire that mass percentage concentration is 0.2%;
(4) use circulation cleaning water soaking 2 hours, then rinse well with clear water;
(5) dry 5 minutes with washing machine, obtain available silk flosssilk wadding.
Embodiment three
The present embodiment comprises following operating procedure:
(1) get 80 kilograms of dried cocoon shells, soak dried cocoon shell after 24 hours with clear water, leak dry;
(2) with containing mass percent concentration be that 0.12% limewash soaks 5 hours;
(3) 40 minutes are boiled with the buck slow fire that mass percentage concentration is 0.2%;
(4) use circulation cleaning water soaking 3 hours, then rinse well with clear water;
(5) dry 8 minutes with washing machine, obtain available silk flosssilk wadding.
By adopting above-mentioned processing method, greatly can improve working (machining) efficiency, the bright and clean softness of the silk floss simultaneously obtained, the scope of application is wide.
What finally illustrate is, above embodiment is only in order to illustrate technical scheme of the present invention and unrestricted, although with reference to preferred embodiment to invention has been detailed description, those of ordinary skill in the art is to be understood that, can modify to technical scheme of the present invention or equivalent replacement, and not departing from aim and the scope of the technical program, it all should be encompassed in the middle of right of the present invention.

Claims (1)

1. a method for bar cocoon shell filature, is characterized in that: comprise following operating procedure:
(1) soak dried cocoon shell after 24 hours with clear water, leak dry;
(2) by the cocoon shell that obtains after step (1) process with containing mass percent concentration being 0.08%-0.12% limewash immersion 4-5 hours;
(3) 20-40 minute is boiled with the buck slow fire that mass percentage concentration is 0.2% again;
(4) use circulation cleaning water soaking 2-3 hours, then rinse well with clear water, obtain semi-finished product;
(5) semi-finished product are put into washing machine, utilize washing machine to dry 5-8 minutes, just become available silk flosssilk wadding.
CN201410440163.1A 2014-09-01 2014-09-01 A kind of method of dry cocoon shell filature Expired - Fee Related CN104213201B (en)