CN103571286A - 一种彩色粉末涂料的制备方法 - Google Patents

一种彩色粉末涂料的制备方法 Download PDF

Info

Publication number
CN103571286A
CN103571286A CN201310513904.XA CN201310513904A CN103571286A CN 103571286 A CN103571286 A CN 103571286A CN 201310513904 A CN201310513904 A CN 201310513904A CN 103571286 A CN103571286 A CN 103571286A
Authority
CN
China
Prior art keywords
add
stir
preparation
30min
powder coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310513904.XA
Other languages
English (en)
Inventor
张书佳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Vocational and Technical College of Industry and Trade
Original Assignee
Anhui Vocational and Technical College of Industry and Trade
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Vocational and Technical College of Industry and Trade filed Critical Anhui Vocational and Technical College of Industry and Trade
Priority to CN201310513904.XA priority Critical patent/CN103571286A/zh
Publication of CN103571286A publication Critical patent/CN103571286A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种彩色粉末涂料的制备方法,包括以下步骤:配制基料;配制浆料;浆料与基料混合。本发明配方合理,配制方便,贮存运输方便,涂膜干燥后能形成连续性的涂层,涂层具有良好的延伸率及断裂强度,耐酸、耐碱性好,耐候性优异、施工方便、无环境污染。

Description

一种彩色粉末涂料的制备方法
技术领域
本发明属于涂料技术领域,具体涉及一种彩色粉末涂料的制备方法。
背景技术
随着人们对健康的认识,越来越意识到环保的重要,涂料的高档化,功能化,环保化也逐渐被市场接受,然而涂料市场竞争一直很激烈,随着消费结构的改变,功能和环保涂料呼之欲出,是市场的热点;众所周知,人们70%的时间在室内渡过,因此室内空气的清洁度将直接影响到人们的健康。近几年,随着人民生活水平不断提高,居住环境不断改善,室内装饰日趋豪华、美观的同时,因装修引起的室内污染影响人体健康的问题越来越多,调查表明:68%的疾病起因与室内空气的污染有关,80%的癌症与居住环境有关。因此,高效持久地净化室内有害气体,保持清新健康的生活、工作环境成了人们越来越迫切追求的目标。
现有的涂料大多为液态,而这种液态涂料存在贮存运输不便的缺点。
发明内容
本发明的目的在于针对现有技术的不足,提供一种配制工艺简单的彩色粉末涂料的制备方法。
本发明的上述目的是通过如下方案实现的:
一种彩色粉末涂料的制备方法,包括以下步骤:
(1)配制基料:取1/5的水加入反应釜中搅拌,转速控制在30-40转/分,将2/3的消泡剂,再加入防腐剂,搅拌10min;加入色浆、BA-154乳液、聚醋酸乙烯乳掖,搅拌30min;
(2)配制浆料:在另一搅拌槽中,将其余的水加入,开动搅拌,转速300转/分,依次加入三聚磷酸钠、偏硼酸钡、剩余的消泡剂、氧化镁,搅拌10min;再加入膨润土,搅拌30min后加入高岭土,再搅拌10min;最后加入填料碳酸钙,搅拌约30min后出料;料浆放入胶体磨中循环研磨25-30min;
(3)浆料与基料混合:在150转/分的转速下搅拌30min;加氨水调pH值至8.2-8.3;继续搅拌40min,即可出料、过滤、装捅。
上述粉末涂料包括以下重量份的组分:
聚醋酸乙烯乳液10-30份
BA-154乳液5-10份
水30-50份
轻质碳酸钙1-1.5份
三聚磷酸钙1-1.5份
膨润土1-1.5份
氧化镁0.1-1份
高岭土2-4份
偏硼酸钡1-3份
防腐剂0.05-0.1份
复合消泡剂0.5~1份
氨水适量。
与现有技术相比较,本发明具有的有益效果为:
本发明配方合理,配制方便,贮存运输方便,涂膜干燥后能形成连续性的涂层,涂层具有良好的延伸率及断裂强度,耐酸、耐碱性好,耐候性优异、施工方便、无环境污染。
具体实施方式
为便于理解本发明,本发明列举实施例如下。本领域技术人员应该明了,所述实施例仅仅用于帮助理解本发明,不应视为对本发明的具体限制。
如无具体说明,本发明的各种原料均可以通过市售得到;或根据本领域的常规方法制备得到。除非另有定义或说明,本文中所使用的所有专业与科学用语与本领域技术熟练入员所熟悉的意义相同。此外任何与所记载内容相似或均等的方法及材料皆可应用于本发明方法中。
除非另外说明,本文中所使用的所有专业与科学用语与本领域技术熟练人员所熟悉的意义相同。
此外任何与所记载内容相似或均等的方法及材料皆可应用于本发明方法中。
一种彩色粉末涂料的制备方法,包括以下步骤:
(1)配制基料:取1/5的水加入反应釜中搅拌,转速控制在30-40转/分,将2/3的消泡剂,再加入防腐剂,搅拌10min;加入色浆、BA-154乳液、聚醋酸乙烯乳掖,搅拌30min;
(2)配制浆料:在另一搅拌槽中,将其余的水加入,开动搅拌,转速300转/分,依次加入三聚磷酸钠、偏硼酸钡、剩余的消泡剂、氧化镁,搅拌10min;再加入膨润土,搅拌30min后加入高岭土,再搅拌10min;最后加入填料碳酸钙,搅拌约30min后出料;料浆放入胶体磨中循环研磨25-30min;
(3)浆料与基料混合:在150转/分的转速下搅拌30min;加氨水调pH值至8.2-8.3;继续搅拌40min,即可出料、过滤、装捅。
上述粉末涂料包括以下重量份的组分:
聚醋酸乙烯乳液10-30份
BA-154乳液5-10份
水30-50份
轻质碳酸钙1-1.5份
三聚磷酸钙1-1.5份
膨润土1-1.5份
氧化镁0.1-1份
高岭土2-4份
偏硼酸钡1-3份
防腐剂0.05-0.1份
复合消泡剂0.5~1份
氨水适量。
申请人声明,所属技术领域的技术人员在上述实施例的基础上,将上述实施例某组分的具体含量点值,与发明内容部分的技术方案相组合,从而产生的新的数值范围,也是本发明的记载范围之一,本申请为使说明书简明,不再罗列这些数值范围。

Claims (2)

1.一种彩色粉末涂料的制备方法,其特征在于,包括以下步骤:
(1)配制基料:取1/5的水加入反应釜中搅拌,转速控制在30-40转/分,将2/3的消泡剂,再加入防腐剂,搅拌10min;加入色浆、BA-154乳液、聚醋酸乙烯乳掖,搅拌30min;
(2)配制浆料:在另一搅拌槽中,将其余的水加入,开动搅拌,转速300转/分,依次加入三聚磷酸钠、偏硼酸钡、剩余的消泡剂、氧化镁,搅拌10min;再加入膨润土,搅拌30min后加入高岭土,再搅拌10min;最后加入填料碳酸钙,搅拌约30min后出料;料浆放入胶体磨中循环研磨25-30min;
(3)浆料与基料混合:在150转/分的转速下搅拌30min;加氨水调pH值至8.2-8.3;继续搅拌40min,即可出料、过滤、装捅。
2.如权利要求1所述的一种彩色粉末涂料的制备方法,其特征在于,所述粉末涂料包括以下重量份的组分:
聚醋酸乙烯乳液10-30份
BA-154乳液5-10份
水30-50份
轻质碳酸钙1-1.5份
三聚磷酸钙1-1.5份
膨润土1-1.5份
氧化镁0.1-1份
高岭土2-4份
偏硼酸钡1-3份
防腐剂0.05-0.1份
复合消泡剂0.5~1份
氨水适量。
CN201310513904.XA 2013-10-25 2013-10-25 一种彩色粉末涂料的制备方法 Pending CN103571286A (zh)