CN103525146A - 一种不易爆色uv光固化涂料及其制备方法 - Google Patents
一种不易爆色uv光固化涂料及其制备方法 Download PDFInfo
- Publication number
- CN103525146A CN103525146A CN201310457284.2A CN201310457284A CN103525146A CN 103525146 A CN103525146 A CN 103525146A CN 201310457284 A CN201310457284 A CN 201310457284A CN 103525146 A CN103525146 A CN 103525146A
- Authority
- CN
- China
- Prior art keywords
- parts
- coating
- low possibility
- phosphine oxide
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种不易爆色UV光固化涂料,由下列重量份的原料制成:氨基甲酸酯丙烯酸酯60-65、α-羟基异丁酰苯2-3、二缩三丙二醇二丙烯酸酯12-15、甘油松香酯3-4、松节油1-2、聚甲基丙烯酸羟乙酯2-3、乙烯焦油1-2、聚乙烯醇4-6、烷基酚聚氧乙烯醚1-2、磷酸三丁酯1-2、2,4,6—三甲基苯甲酰基二苯基氧化膦5-7、对苯二酚1-2、分散助剂4-5。本发明涂料具有特别好的柔韧性、较好的耐磨性、不易黄变、附着力强、固化速度快,解决了印刷品易爆色的问题,广泛应用于烟包纸张和酒盒等包装盒的印刷,有机物挥发少,安全环保,且不易开裂,配方成本较低,应用前景很好。
Description
技术领域
本发明属于涂料领域,尤其涉及一种不易爆色UV光固化涂料及其制备方法。
背景技术
随着市场经济的发展,涂料领域发生了巨大变化,其中UV 涂料具有固化速度快、节能、常温固化、性能优越、绿色环保等优点,其上光速度快,膜层光亮度高,干燥后膜面坚固耐热,折光效果好,使底材产生强烈的主体感,已广泛应用于化工、机械、电子轻工、通讯等领域。由于其环保优势,UV 固化已获得了相关环境法规的强有力支持和工业界的密切关注,UV 辐射固化材料在市场需求高速增长的同时,UV 辐射固化体系正同多种技术结合,以克服某些缺陷,满足实际的应用。现在印刷行业中,UV 能使包装取得一些特殊的效果:高光泽度、良好的油墨保护特性、可加控制的滑爽性和耐摩擦性、低气味或没有气味、低萃取物或无法检出萃取物,以及对油墨的保护作用。
目前的UV固化材料各种各样,但是还是不同程度的存在着一些问题,例如:有机物污染、黄变、易爆色、不耐低温、成本高、耐腐蚀性差等一系列问题,都需要针对不同的用途继续改良,降低生产成本,扩大用途。
发明内容
本发明的目的在于提供一种附着力强、韧性好、不易爆色的UV光固化涂料及其制备方法。
本发明的技术方案如下:
一种不易爆色UV光固化涂料,其特征在于由下列重量份的原料制成:氨基甲酸酯丙烯酸酯60-65、α-羟基异丁酰苯2-3、二缩三丙二醇二丙烯酸酯12-15、甘油松香酯3-4、松节油1-2、聚甲基丙烯酸羟乙酯2-3、乙烯焦油1-2、聚乙烯醇4-6、烷基酚聚氧乙烯醚1-2、磷酸三丁酯1-2、2,4,6—三甲基苯甲酰基二苯基氧化膦5-7、对苯二酚1-2、分散助剂4-5;
所述分散助剂由以下重量份的原料制成: 竹炭粉4-5、玉石粉2-3、玫瑰精油1-2、抗坏血酸1-2、季戊四醇三丙烯酸酯4-5、醇酯十二3-4、硅烷偶联剂KH550 1-2、乙酸乙酯14-18;制备方法是将竹炭粉、玉石粉放入10-15%盐酸溶液中泡3-4小时,取出,用去离子水洗涤多次,烘干,加入至乙酸乙酯中,研磨得20-40μm浆料,向浆料中加入其它剩余成分,加热至50-55℃,搅拌40-50分钟;继续升温至70-75℃,搅拌反应1-2小时,即得。
所述的不易爆色UV光固化涂料的制备方法,其特征在于包括以下步骤:将除2,4,6—三甲基苯甲酰基二苯基氧化膦外的其它成分混合,升温至60-70℃,在800-1000转/分下搅拌20-25分钟,降温到40℃以下再加入2,4,6—三甲基苯甲酰基二苯基氧化膦,继续搅15-20分钟,即得。
本发明的有益效果
本发明涂料具有特别好的柔韧性、较好的耐磨性、不易黄变、附着力强、固化速度快,解决了印刷品易爆色的问题,广泛应用于烟包纸张和酒盒等包装盒的印刷,有机物挥发少,安全环保,且不易开裂,配方成本较低,应用前景很好。
具体实施方式
一种不易爆色UV光固化涂料,由下列重量份(公斤)的原料制成:氨基甲酸酯丙烯酸酯63、α-羟基异丁酰苯2、二缩三丙二醇二丙烯酸酯14、甘油松香酯3、松节油1、聚甲基丙烯酸羟乙酯3、乙烯焦油1、聚乙烯醇5、烷基酚聚氧乙烯醚1.5、磷酸三丁酯1.4、2,4,6—三甲基苯甲酰基二苯基氧化膦6、对苯二酚1.5、分散助剂4;
所述分散助剂由以下重量份(公斤)的原料制成: 竹炭粉4、玉石粉2、玫瑰精油2、抗坏血酸1.5、季戊四醇三丙烯酸酯4.6、醇酯十二3.5、硅烷偶联剂KH550 1.4、乙酸乙酯16;制备方法是将竹炭粉、玉石粉放入14%盐酸溶液中泡3小时,取出,用去离子水洗涤5次,烘干,加入至乙酸乙酯中,研磨得25μm浆料,向浆料中加入其它剩余成分,加热至53℃,搅拌44分钟;继续升温至72℃,搅拌反应2小时,即得。
所述的不易爆色UV光固化涂料的制备方法,包括以下步骤:将除2,4,6—三甲基苯甲酰基二苯基氧化膦外的其它成分混合,升温至70℃,在900转/分下搅拌23分钟,降温到30℃再加入2,4,6—三甲基苯甲酰基二苯基氧化膦,继续搅16分钟,即得。
该不易爆色UV光固化涂料可以采用滚涂、淋涂、喷涂的施工方式进行施工。按以上方案制得的涂料涂装在木板上附着力都好于二级,耐75%乙醇24 小时以上,耐碱24小时以上、耐酸48小时以上,耐受零下40 度和40度的冷热循环10 次不发生开裂,耐15%食盐水60 小时以上,硬度可在2HB 到3H 间调节,耐磨指数在4000转以上。
Claims (2)
1.一种不易爆色UV光固化涂料,其特征在于由下列重量份的原料制成:氨基甲酸酯丙烯酸酯60-65、α-羟基异丁酰苯2-3、二缩三丙二醇二丙烯酸酯12-15、甘油松香酯3-4、松节油1-2、聚甲基丙烯酸羟乙酯2-3、乙烯焦油1-2、聚乙烯醇4-6、烷基酚聚氧乙烯醚1-2、磷酸三丁酯1-2、2,4,6—三甲基苯甲酰基二苯基氧化膦5-7、对苯二酚1-2、分散助剂4-5;
所述分散助剂由以下重量份的原料制成: 竹炭粉4-5、玉石粉2-3、玫瑰精油1-2、抗坏血酸1-2、季戊四醇三丙烯酸酯4-5、醇酯十二3-4、硅烷偶联剂KH550 1-2、乙酸乙酯14-18;制备方法是将竹炭粉、玉石粉放入10-15%盐酸溶液中泡3-4小时,取出,用去离子水洗涤多次,烘干,加入至乙酸乙酯中,研磨得20-40μm浆料,向浆料中加入其它剩余成分,加热至50-55℃,搅拌40-50分钟;继续升温至70-75℃,搅拌反应1-2小时,即得。
2.根据权利要求1所述的不易爆色UV光固化涂料的制备方法,其特征在于包括以下步骤:将除2,4,6—三甲基苯甲酰基二苯基氧化膦外的其它成分混合,升温至60-70℃,在800-1000转/分下搅拌20-25分钟,降温到40℃以下再加入2,4,6—三甲基苯甲酰基二苯基氧化膦,继续搅15-20分钟,即得。