- CN103464615A CN103464615A CN2013104656388A CN201310465638A CN103464615A CN 103464615 A CN103464615 A CN 103464615A CN 2013104656388 A CN2013104656388 A CN 2013104656388A CN 201310465638 A CN201310465638 A CN 201310465638A CN 103464615 A CN103464615 A CN 103464615A
- Authority
- CN
- China
- Prior art keywords
- screw
- die
- pin
- stretching
- iii
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Images
Landscapes
- Shaping Metal By Deep-Drawing, Or The Like (AREA)
Abstract
一种接线盒拉伸模具,包括上模板、拉伸凹模、内导柱、螺钉Ⅰ、拉伸凸模、螺钉Ⅱ、销钉Ⅰ、导套、导柱、下模板、螺钉Ⅲ、销钉Ⅱ、销钉Ⅲ、螺钉Ⅳ、推料杆、推料板、凸模固定板、压边圈;所述的下模板的上方还装有通过螺钉Ⅲ和销钉Ⅱ紧固的凸模固定板,推料杆自下而上依次穿过所述的下模板和所述的凸模固定板,并与压边圈相连,所述的推料杆的下端与推料板的上端面连接,所述的拉伸凸模被销钉Ⅲ和螺钉Ⅳ固定于所述的凸模固定板的上方。应用本发明拉伸过程中,压边力稳定,分布均匀,使材料流动性好,成品表面光滑,无明显凹凸痕迹。
Description
技术领域
本发明涉及一种机械工件生产,尤其涉及一种接线盒拉伸模具。
背景技术
我厂生产的接线盒,在完成落料工序后,要对该工件料进行拉伸、加工,现有技术中,,拉伸为接线盒的制造过程中较为重要的工艺,决定了工件成型质量的优劣,目前,改善材料的流动性已成为设计和制作拉伸模具的重要工作内容,我厂在接线盒的拉伸阶段,采用现有结构的模具和工艺,会出现基准不稳定,作用在压边圈上的压边力分布不均匀,压边力不够稳定的问题,易导致工件出现明显凹凸痕迹,光滑度低。
发明内容
为解决现有技术存在的上述问题,本发明改进了拉伸模具结构,以增加单边间隙的合理性和稳定性,解决压边力分布不均的问题。
本发明采用如下技术方案:
一种接线盒拉伸模具,包括上模板、拉伸凹模、内导柱、螺钉Ⅰ、拉伸凸模、螺钉Ⅱ、销钉Ⅰ、导套、导柱、下模板、螺钉Ⅲ、销钉Ⅱ、销钉Ⅲ、螺钉Ⅳ、推料杆、推料板、凸模固定板、压边圈;
拉伸凹模一侧设有导孔,该导孔与内导柱同轴滑动配合,所述的拉伸凹模通过螺钉Ⅰ和销钉Ⅰ安装于上模板的下方,导套固定于所述的上模板的下方,导柱固定于下模板的上方,所述的导套与导柱相对滑动配合;
所述的下模板的上方还装有通过螺钉Ⅲ和销钉Ⅱ紧固的凸模固定板,推料杆自下而上依次穿过所述的下模板和所述的凸模固定板,并与压边圈相连,所述的推料杆的下端与推料板的上端面连接,所述的拉伸凸模被销钉Ⅲ和螺钉Ⅳ固定于所述的凸模固定板的上方。
所述的一种接线盒拉伸模具的模具钢材料选用微合金Cr12MoV模具钢,模具钢的热处理工艺为:热轧后加热到1050‐1150℃进行固溶处理,快冷到600℃转入400-700℃炉中使之等温转变,机加工后加热到900-950℃油淬,最后在150-200℃回火。
组成所述的一种接线盒拉伸模具的各独立部件采用数控机床加工。
本发明的有益效果是:凸模和凹模的材料选用微合金Cr12MoV模具钢,保证了模具硬度,模具钢采用上述热处理工艺,减少了碳排放,淬透性可提高一倍以上;数控机床加工模具的独立工件,提高了独立工件的精度;独立工件高精度加工及整体结构设计优化,提高了本发明单边间隙的合理性和稳定性,使凸模和凹模的间隙保持在0.01—0.02mm之间,采用以上技术方案,使经落料工艺后的工件,拉伸成型,且拉伸过程中,压边力稳定,分布均匀,使材料流动性好,成品表面光滑,无明显凹凸痕迹。
附图说明
图1是本发明的主视图;
图2是下模板的俯视图。
其中:2011、上模板,2021、拉伸凹模,2031、内导柱、2041、螺钉Ⅰ、2051、拉伸凸模、2042、螺钉Ⅱ、2061、销钉Ⅰ、2071、导套、2032、导柱、2081、下模板、2043、螺钉Ⅲ、2062、销钉Ⅱ、2063、销钉Ⅲ、2044、螺钉Ⅳ、2091、推料杆、2101、推料板、2111、凸模固定板、2121、压边圈。
具体实施方式:
下面结合具体实施例对本发明进一步说明:
一种接线盒拉伸模具,包括上模板2011、拉伸凹模2021、内导柱2031、螺钉Ⅰ2041、拉伸凸模2051、螺钉Ⅱ2042、销钉Ⅰ2061、导套2071、导柱2032、下模板2081、螺钉Ⅲ2043、销钉Ⅱ2062、销钉Ⅲ2063、螺钉Ⅳ2044、推料杆2091、推料板2101、凸模固定板2111、压边圈2121;
拉伸凹模2021一侧设有导孔,该导孔与内导柱2031同轴滑动配合,所述的拉伸凹模2021通过螺钉Ⅰ2041和销钉Ⅰ2061安装于上模板2011的下方,导套2071固定于所述的上模板2011的下方,导柱2032固定于下模板2081的上方,所述的导套2071与导柱2032相对滑动配合;
所述的下模板2081的上方还装有通过螺钉Ⅲ2043和销钉Ⅱ2062紧固的凸模固定板2111,推料杆2091自下而上依次穿过所述的下模板2081和所述的凸模固定板2111,并与压边圈2121相连,所述的推料杆2091的下端与推料板2101的上端面连接,所述的拉伸凸模2051被销钉Ⅲ2063和螺钉Ⅳ2044固定于所述的凸模固定板2111的上方。
接线盒拉伸加工过程如下:
1、将接线盒拉伸模具固定在200T的油压机上;
2、经落料工艺加工后的接线盒工件的料板置于压边圈2121的上表面;
3、开动油压机,拉伸凹模2021随上模板2011下行至与压边圈2121压紧,拉伸凹模2021继续下行,压边圈2121随动下行,拉伸凸模2051固定不动,接线盒工件料板将拉伸凸模2051覆盖,被拉伸出拉伸凸模2051的形状;
4、工件成型后,方箱推动推料板2101及其上方的推料杆2091,将压边圈2121复位。
Claims (2)
1.一种接线盒拉伸模具,其特征在于:包括上模板(2011)、拉伸凹模(2021)、内导柱(2031)、螺钉Ⅰ(2041)、拉伸凸模(2051)、螺钉Ⅱ(2042)、销钉Ⅰ(2061)、导套(2071)、导柱(2032)、下模板(2081)、螺钉Ⅲ(2043)、销钉Ⅱ(2062)、销钉Ⅲ(2063)、螺钉Ⅳ(2044)、推料杆(2091)、推料板(2101)、凸模固定板(2111)、压边圈(2121);
拉伸凹模(2021)一侧设有导孔,该导孔与内导柱(2031)同轴滑动配合,所述的拉伸凹模(2021)通过螺钉Ⅰ(2041)和销钉Ⅰ(2061)安装于上模板(2011)的下方,导套(2071)固定于所述的上模板(2011)的下方,导柱(2032)固定于下模板(2081)的上方,所述的导套(2071)与导柱(2032)相对滑动配合;
所述的下模板(2081)的上方还装有通过螺钉Ⅲ(2043)和销钉Ⅱ(2062)紧固的凸模固定板(2111),推料杆(2091)自下而上依次穿过所述的下模板(2081)和所述的凸模固定板(2111),并与压边圈(2121)相连,所述的推料杆(2091)的下端与推料板(2101)的上端面连接,所述的拉伸凸模(2051)被销钉Ⅲ(2063)和螺钉Ⅳ(2044)固定于所述的凸模固定板(2111)的上方。
2.根据权利要求1所述的一种接线盒拉伸模具,其特征在于:模具钢材料选用微合金Cr12MoV模具钢,模具钢的热处理工艺为:热轧后加热到1050-1150℃进行固溶处理,快冷到600℃转入400-700℃炉中使之等温转变,机加工后加热到900-950℃油淬,最后在150-200℃回火。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013104656388A CN103464615A (zh) | 2013-09-30 | 2013-09-30 | 一种接线盒拉伸模具 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013104656388A CN103464615A (zh) | 2013-09-30 | 2013-09-30 | 一种接线盒拉伸模具 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN103464615A true CN103464615A (zh) | 2013-12-25 |
Family
ID=49789780
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2013104656388A Pending CN103464615A (zh) | 2013-09-30 | 2013-09-30 | 一种接线盒拉伸模具 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN103464615A (zh) |
Citations (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101798657A (zh) * | 2010-04-01 | 2010-08-11 | 戚正风 | 微合金化工模具钢及其热处理方法 |
CN202192165U (zh) * | 2011-08-16 | 2012-04-18 | 刘玲 | 一种带凸缘的阶梯盒形件拉伸模具结构 |
CN202667450U (zh) * | 2012-07-17 | 2013-01-16 | 上海赛科利汽车模具技术应用有限公司 | 热冲压拉深试验模具 |
CN102962347A (zh) * | 2012-07-02 | 2013-03-13 | 大连益联金属成型有限公司 | 散热片拉延模 |
CN202910142U (zh) * | 2012-11-15 | 2013-05-01 | 上海贤众汽车零部件有限公司 | 油底壳拉伸装置 |
CN203044653U (zh) * | 2012-11-29 | 2013-07-10 | 冯英 | 新型拉深模 |
CN203091527U (zh) * | 2012-12-13 | 2013-07-31 | 宁波太尔炊具有限公司 | 一种用于加工直伸铝制不粘锅的模具 |
-
2013
- 2013-09-30 CN CN2013104656388A patent/CN103464615A/zh active Pending
Patent Citations (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101798657A (zh) * | 2010-04-01 | 2010-08-11 | 戚正风 | 微合金化工模具钢及其热处理方法 |
CN202192165U (zh) * | 2011-08-16 | 2012-04-18 | 刘玲 | 一种带凸缘的阶梯盒形件拉伸模具结构 |
CN102962347A (zh) * | 2012-07-02 | 2013-03-13 | 大连益联金属成型有限公司 | 散热片拉延模 |
CN202667450U (zh) * | 2012-07-17 | 2013-01-16 | 上海赛科利汽车模具技术应用有限公司 | 热冲压拉深试验模具 |
CN202910142U (zh) * | 2012-11-15 | 2013-05-01 | 上海贤众汽车零部件有限公司 | 油底壳拉伸装置 |
CN203044653U (zh) * | 2012-11-29 | 2013-07-10 | 冯英 | 新型拉深模 |
CN203091527U (zh) * | 2012-12-13 | 2013-07-31 | 宁波太尔炊具有限公司 | 一种用于加工直伸铝制不粘锅的模具 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103639227A (zh) | 一种制造超薄壁微小圆筒件的模具与方法 | |
CN103464613B (zh) | 一种隔热罩的生产专用模具组 | |
CN203578539U (zh) | 一种隔热罩落料冲孔复合模具 | |
CN105080995A (zh) | 花键套挤压成形工艺 | |
CN103464614A (zh) | 一种接线盒的生产专用模具组 | |
CN203578514U (zh) | 一种锥体工件落料模具 | |
CN103495657B (zh) | 一种隔热罩端盖拉伸模具 | |
CN103480746A (zh) | 一种锥体工件拉伸模具 | |
CN203578540U (zh) | 一种管夹落料冲孔复合模具 | |
CN103495658A (zh) | 一种隔热罩落料冲孔复合模具 | |
CN103567294A (zh) | 一种风扇罩拉伸切边复合模具 | |
CN103464611A (zh) | 一种隔热罩成型模具 | |
CN103495659A (zh) | 一种管夹拉伸模具 | |
CN103464615A (zh) | 一种接线盒拉伸模具 | |
CN105478588A (zh) | 一种防工件磨损的中铰链垫片弯曲模 | |
CN205309079U (zh) | 一种防工件磨损的中铰链垫片弯曲模母模组件 | |
CN103480743A (zh) | 一种隔热罩压筋模具 | |
CN103480741A (zh) | 一种锥体工件切边冲孔复合模具 | |
CN203578546U (zh) | 一种风扇罩拉伸切边复合模具 | |
CN204320936U (zh) | 一种拉深模具 | |
CN205147058U (zh) | 一种防工件磨损的中铰链垫片弯曲模 | |
CN203578544U (zh) | 一种管夹的生产专用模具组 | |
CN103464612B (zh) | 一种接线盒上表面翻孔模具 | |
CN103495656A (zh) | 一种管夹一次成型模具 | |
CN103480724A (zh) | 一种隔热罩压百叶模具 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
C12 | Rejection of a patent application after its publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20131225 |