CN103387825B - 一种分枝井夹壁墙固化液及其制备方法 - Google Patents
一种分枝井夹壁墙固化液及其制备方法 Download PDFInfo
- Publication number
- CN103387825B CN103387825B CN201310337075.4A CN201310337075A CN103387825B CN 103387825 B CN103387825 B CN 103387825B CN 201310337075 A CN201310337075 A CN 201310337075A CN 103387825 B CN103387825 B CN 103387825B
- Authority
- CN
- China
- Prior art keywords
- solid solution
- furane resin
- parts
- solidifying liquid
- formula
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
温度 | 固化时间 | 抗压强度MPa | |
实施例1 | 40℃ | 24h | 8.8 |
实施例1 | 60℃ | 24h | 11.6 |
实施例1 | 80℃ | 24h | 16.8 |
实施例1 | 60℃ | 48h | 13.4 |
实施例2 | 40℃ | 24h | 8.0 |
实施例2 | 60℃ | 24h | 10.6 |
实施例2 | 80℃ | 24h | 12.0 |
实施例2 | 60℃ | 48h | 10.8 |
Claims (7)