CN102828419A - Production method of anti-creasing shirts - Google Patents

Production method of anti-creasing shirts Download PDF

Info

Publication number
CN102828419A
CN102828419A CN2012103489260A CN201210348926A CN102828419A CN 102828419 A CN102828419 A CN 102828419A CN 2012103489260 A CN2012103489260 A CN 2012103489260A CN 201210348926 A CN201210348926 A CN 201210348926A CN 102828419 A CN102828419 A CN 102828419A
Authority
CN
China
Prior art keywords
production method
creasing
parts
fabrics
agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012103489260A
Other languages
Chinese (zh)
Inventor
解吉平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Original Assignee
KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY filed Critical KUNSHAN ZHOUSHI HUIHONG GARMENT FACTORY
Priority to CN2012103489260A priority Critical patent/CN102828419A/en
Publication of CN102828419A publication Critical patent/CN102828419A/en
Pending legal-status Critical Current

Abstract

The invention discloses a production method of anti-creasing shirts. The production method comprises the following steps: carrying out liquid ammonia treatment on full-cotton worsted fabrics; pre-shrinking the fabrics with a pre-shrinking machine; padding the fabrics in an impregnation liquid containing an anti-creasing agent, wherein the pressure is 1.5-2kg/cm<2> and the liquid take-up rate is 60-70%; drying and tailoring the treated fabrics and making clothes with the fabrics; and ironing and setting for 10-20 minutes at 140-150 DEG C by adopting a drying and setting machine. According to the invention, the anti-creasing agent is formed by the following components in parts by weight: 45-55 parts of waterborne polyurethane, 15-20 parts of bis[monoethyl(3,5-di-tert-butyl-4-hydroxylbenzyl) phosphonate, 35-40 parts of chitosan, 2-5 parts of silane coupling agent and 0.5-1.2 parts of sodium polyacrylate dispersing agent; and water is added to the anti-creasing agent to prepare the 15-45% impregnation liquid. The anti-creasing agent can be firmly bonded with the shirt fabrics and is strong in durability, so the shirts have excellent anti-creasing effect.

Description

The production method of wrinkle resistant shirt
Technical field
The present invention relates to a kind of production method of wrinkle resistant shirt.
Background technology
The general wrinkle resistance of fabric is poor, natural fabric especially, and for example cotton, woolen knitwear are easy to wrinkling distortion under wet environment.Simultaneously, textiles is to lightening development, and this kind fabric is wrinkling more easily, and Machine Washable property is poor, for improving its application performance, need carry out anti-crease finishing.Crease-shedding finishing agent in the market mostly is the resin type finishing agent, and mostly contains formaldehyde, uses harmful for a long time.
Chinese patent CN102535172A discloses a kind of manufacturing approach of crease resistant fabric, and it adopts magnetron sputtering technique that the aqueous polyurethane crease-shedding finishing agent is covered on the fabric, and this is higher to equipment requirements, and cost is higher.
Summary of the invention
The technical problem that the present invention will solve provides a kind of production method of wrinkle resistant shirt, to overcome the above-mentioned defective that prior art exists.
For solving the problems of the technologies described above, the production method of the wrinkle resistant shirt of the present invention comprises the steps:
1) the cotton worsted fabric is carried out Liquid Ammonia Treatment;
2) with preshrinking machine lining is carried out preshrunk and handle, steam pressure is 2-3kg/m 2, steam consumption is 50-70kg/h;
3) lining is padded processing in containing the maceration extract of anti-creasing agent, pressure 1.5-2kg/cm 2, liquid carrying rate 60-70%;
4) to the lining after handling dry, cutting, clothing;
5) employing is baked and banked up with earth setting machine 140-150 ℃ of whole down boiling hot typing 10-20 minute;
Said anti-creasing agent is made up of the component of following weight portion:
Aqueous polyurethane 45-55 part,
Two (3,5-di-t-butyl-4-hydroxyl) benzylphosphonic acid mono ethyl ester 15-20 part,
Shitosan 35-40 part,
Silane coupler 2-5 part,
Sodium Polyacrylate dispersant 0.5-1.2 part,
And add water and be made into the padding liquid that mass concentration is 15-45%.
Said cotton worsted fabric is 120 a high-accuracy cotton yarn knitted fabric.
Said Sodium Polyacrylate dispersant preferred viscosities 200-300mPas.
Anti-creasing agent can adopt general mixed method, preferably adopts following method preparation:
Aqueous polyurethane, two benzylphosphonic acid mono ethyl ester and shitosan are mixed, slowly add silane coupler and Sodium Polyacrylate dispersant then simultaneously, feeding intake in 1-2 hour finishes, and continues to mix 20-30 minute.
Anti-creasing agent preferably is made into the maceration extract of mass content 30-40%.
Anti-creasing agent of the present invention can with the shirt fabric strong bonded, durability is strong, makes shirt have good anti-wrinkle effect.
The specific embodiment
Embodiment 1
The preparation of anti-creasing agent:
55 parts of aqueous polyurethanes,
Two (3,5-di-t-butyl-4-hydroxyl) 15 parts of benzylphosphonic acid mono ethyl esters,
35 parts of shitosans,
2 parts of silane couplers,
0.5 part of Sodium Polyacrylate dispersant,
With aqueous polyurethane, two (3; 5-di-t-butyl-4-hydroxyl) benzylphosphonic acid mono ethyl ester and shitosan mix, and slowly add silane coupler and Sodium Polyacrylate dispersant then simultaneously, and feeding intake in 1 hour finishes; Continue to mix 20 minutes, adding water then, to be made into mass concentration be 15% padding liquid.
The production of wrinkle resistant shirt:
1) the cotton worsted fabric is carried out Liquid Ammonia Treatment;
2) with preshrinking machine lining is carried out preshrunk and handle, steam pressure is 2kg/m 2, steam consumption is 50kg/h;
3) lining is padded processing in containing the maceration extract of anti-creasing agent, pressure 1.5kg/cm 2, liquid carrying rate 60%;
4) to the lining after handling dry, cutting, clothing;
5) employing is baked and banked up with earth setting machine 140 ℃ of whole down boiling hot typings 20 minutes.
Embodiment 2
The preparation of anti-creasing agent:
45 parts of aqueous polyurethanes,
Two (3,5-di-t-butyl-4-hydroxyl) 20 parts of benzylphosphonic acid mono ethyl esters,
40 parts of shitosans,
5 parts of silane couplers,
1.2 parts of Sodium Polyacrylate dispersants,
With aqueous polyurethane, two (3; 5-di-t-butyl-4-hydroxyl) benzylphosphonic acid mono ethyl ester and shitosan mix, and slowly add silane coupler and Sodium Polyacrylate dispersant then simultaneously, and feeding intake in 2 hours finishes; Continue to mix 30 minutes, adding water then, to be made into mass concentration be 40% padding liquid.
The production of wrinkle resistant shirt:
1) the cotton worsted fabric is carried out Liquid Ammonia Treatment;
2) with preshrinking machine lining is carried out preshrunk and handle, steam pressure is 3kg/m 2, steam consumption is 70kg/h;
3) lining is padded processing in containing the maceration extract of anti-creasing agent, pressure 2kg/cm 2, liquid carrying rate 70%;
4) to the lining after handling dry, cutting, clothing;
5) employing is baked and banked up with earth setting machine 150 ℃ of whole down boiling hot typings 10 minutes.
The anti-wrinkle effect of the wrinkle resistant shirt of the present invention is excellent, and has good wash durability, through repeatedly still having good wrinkle resistance after the washing.

Claims (5)

1. the production method of wrinkle resistant shirt is characterized in that, comprises the steps:
1) the cotton worsted fabric is carried out Liquid Ammonia Treatment;
2) with preshrinking machine lining is carried out preshrunk and handle, steam pressure is 2-3kg/m 2, steam consumption is 50-70kg/h;
3) lining is padded processing in containing the maceration extract of anti-creasing agent, pressure 1.5-2kg/cm 2, liquid carrying rate 60-70%;
4) to the lining after handling dry, cutting, clothing;
5) employing is baked and banked up with earth setting machine 140-150 ℃ of whole down boiling hot typing 10-20 minute;
Said anti-creasing agent is made up of the component of following weight portion:
Aqueous polyurethane 45-55 part,
Two (3,5-di-t-butyl-4-hydroxyl) benzylphosphonic acid mono ethyl ester 15-20 part,
Shitosan 35-40 part,
Silane coupler 2-5 part,
Sodium Polyacrylate dispersant 0.5-1.2 part,
And add water and be made into the padding liquid that mass concentration is 15-45%.
2. the production method of wrinkle resistant shirt according to claim 1 is characterized in that, said cotton worsted fabric is 120 a high-accuracy cotton yarn knitted fabric.
3. the production method of wrinkle resistant shirt according to claim 1 is characterized in that, said anti-creasing agent is made into the maceration extract of mass content 30-40%.
4. the production method of wrinkle resistant shirt according to claim 1 is characterized in that, said Sodium Polyacrylate dispersant viscosity is 200-300mPas.
5. the production method of wrinkle resistant shirt according to claim 1; It is characterized in that; Said anti-creasing agent adopts following method preparation: aqueous polyurethane, two benzylphosphonic acid mono ethyl ester and shitosan are mixed; Slowly add silane coupler and Sodium Polyacrylate dispersant then simultaneously, feeding intake in 1-2 hour finishes, and continues to mix 20-30 minute.
CN2012103489260A 2012-09-19 2012-09-19 Production method of anti-creasing shirts Pending CN102828419A (en)