CN102676967A - 一种热镀锌***中冷却装置 - Google Patents
一种热镀锌***中冷却装置 Download PDFInfo
- Publication number
- CN102676967A CN102676967A CN2012101013014A CN201210101301A CN102676967A CN 102676967 A CN102676967 A CN 102676967A CN 2012101013014 A CN2012101013014 A CN 2012101013014A CN 201210101301 A CN201210101301 A CN 201210101301A CN 102676967 A CN102676967 A CN 102676967A
- Authority
- CN
- China
- Prior art keywords
- cooling
- cooling tower
- vertical air
- deflector roll
- cooling device
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种热镀锌***中冷却装置,涉及镀锌设备技术领域,包括一冷却塔,所述冷却塔顶端一侧设有第一转向辊,所述冷却塔顶端另一侧设有第二转向辊,所述冷却塔中间位置设有垂直风冷机构,所述冷却塔顶端设有水平风冷机。本发明设计新颖,结构简单,通过水平及垂直风冷机进行交叉冷却,使得冷却效果更佳,制造成本相对也低,能满足生产需要。
Description
技术领域
本发明涉及镀锌设备技术领域,具体涉及一种热镀锌***中冷却装置。
背景技术
钢铁在空气、水或土壤中很容易生锈,甚至完全损坏,每年因腐蚀造成的钢铁损失占整个钢铁产量的很大一部分,使得钢铁资源的严重浪费。另一方面,现今路桥建设、电气行业、建筑业、造船业、车辆制造业、家具行业,尤其是在国家大力发展交通的背景下,针对高架铁路、高速公路、桥梁的建设中过程中使用的钢铁大部分都是要在钢铁表面镀上较厚的纯锌层,能在各种恶劣的环境中使用。现在常用的镀锌方法是热浸镀锌和电镀锌这两种。使用电镀锌这种方法制成的镀锌钢材因锌层很薄,使用寿命很短,成本较高,污染相对较大,近年来发展缓慢;使用热浸镀锌这种方法制成的镀锌钢材它是在锌呈液体的状态下,经过了相当复杂的物理、化学作用之后,在钢铁上不仅镀上较厚的纯锌层,而且还生成一种锌-铁合金层,因此用热浸镀锌所制成的钢材比电镀锌制成的钢材更加适用于在各种恶劣的气候环境中使用,因此热浸镀锌制品在工业(如化工设备、石油加工、海洋勘探、金属结构、电力输送、造船等),农业(如:喷灌、暖房)、建筑(如:水及煤气输送、电线套管、脚手架、房屋等)、桥梁建设、高速公路中的钢材用料等方面。目前我国热浸镀锌吹镀的做法之一是:工人站在锌锅边,手工钳住需要镀锌的钢材,把钢材放入锌锅内,等镀锌完成后再把锌锅中的钢材提到锌锅外,进行吹镀这道工序。这样镀锌存在严重的安全问题,镀锌钢材的产量也不高,而且很难准确的控制锌层的厚度等问题,镀锌设备落后,不能满足市场需要。
发明内容
本发明所要解决的技术问题在于提供一种结构简单,冷却效果好的热镀锌***中冷却装置。
本发明所要解决的技术问题采用以下技术方案来实现:
一种热镀锌***中冷却装置,包括一冷却塔,所述冷却塔顶端一侧设有第一转向辊,所述冷却塔顶端另一侧设有第二转向辊,所述冷却塔中间位置设有垂直风冷机构,所述冷却塔顶端设有水平风冷机。
所述的水平风冷机位于第一转向辊与第二转向辊之间。
所述的垂直风冷机构设有四组。
所述的垂直风冷机构包括支架及设于支架上的垂直风冷机。
本发明的有益效果是:本发明设计新颖,结构简单,通过水平及垂直风冷机进行交叉冷却,使得冷却效果更佳,制造成本相对也低,能满足生产需要。
附图说明
图1为本发明结构示意图。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本发明。
如图1所示,一种热镀锌***中冷却装置,包括一冷却塔1,冷却塔1顶端一侧设有第一转向辊2,冷却塔1顶端另一侧设有第二转向辊3,冷却塔1中间位置设有垂直风冷机构,冷却塔1顶端设有水平风冷机4,水平风冷机4位于第一转向辊2与第二转向辊3之间,垂直风冷机构设有四组,每组垂直风冷机构包括支架6及设于支架6上的垂直风冷机5。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (4)
1.一种热镀锌***中冷却装置,包括一冷却塔,所述冷却塔顶端一侧设有第一转向辊,所述冷却塔顶端另一侧设有第二转向辊,所述冷却塔中间位置设有垂直风冷机构,所述冷却塔顶端设有水平风冷机。
2.根据权利要求1所述的一种热镀锌***中冷却装置,其特征在于:所述的水平风冷机位于第一转向辊与第二转向辊之间。
3.根据权利要求1所述的一种热镀锌***中冷却装置,其特征在于:所述的垂直风冷机构设有四组。
4.根据权利要求1所述的一种热镀锌***中冷却装置,其特征在于:所述的垂直风冷机构包括支架及设于支架上的垂直风冷机。