CN102671770B - 一种异极矿与石英的浮选分离方法 - Google Patents

一种异极矿与石英的浮选分离方法 Download PDF

Info

Publication number
CN102671770B
CN102671770B CN 201210131704 CN201210131704A CN102671770B CN 102671770 B CN102671770 B CN 102671770B CN 201210131704 CN201210131704 CN 201210131704 CN 201210131704 A CN201210131704 A CN 201210131704A CN 102671770 B CN102671770 B CN 102671770B
Authority
CN
China
Prior art keywords
flotation
smithsonite
quartz
mineral
carbonate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201210131704
Other languages
English (en)
Other versions
CN102671770A (zh
Inventor
陈建华
魏宗武
穆枭
陈晔
李玉琼
蓝丽红
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangxi University
Original Assignee
Guangxi University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangxi University filed Critical Guangxi University
Priority to CN 201210131704 priority Critical patent/CN102671770B/zh
Publication of CN102671770A publication Critical patent/CN102671770A/zh
Application granted granted Critical
Publication of CN102671770B publication Critical patent/CN102671770B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种异极矿与石英的浮选分离方法,浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿。采用本发明能够有效将异极矿与石英及碳酸盐脉石矿物浮选分离,在给矿锌含量为11.92~14.10%条件下,经过2~3浮选分离,获得锌含量为21.26~23.80%、回收率为72.51~75.67%的异极矿精矿。

Description

一种异极矿与石英的浮选分离方法
一、技术领域
本发明涉及一种矿物浮选分离方法,特别是一种异极矿与石英的浮选分离方法。
二、背景技术
在异极矿与石英及碳酸盐脉石矿物浮选分离过程中,由于异极矿与石英的可浮性接近,又由于在破碎、磨矿过程中碳酸盐矿物易于形成矿泥影响异极矿的浮选性能,致使异极矿难于与石英及碳酸盐脉石矿物分离;即使偶有能将其浮选分离,不仅工艺流程结构复杂,药剂种类及用量多、生产成本高,而选矿指标不高,因此也限制了异极矿的开发和利用。
三、发明内容
本发明的目的在于提供一种异极矿与石英的浮选分离方法,它能够回收异极矿,使异极矿获得较高的品位和回收率。
本发明采用以下技术方案达到上述目的:一种异极矿与石英的浮选分离方法,采用水玻璃及硫酸锌作为异极矿的抑制剂,用石灰作pH调整剂、用醚胺作石英及碳酸盐脉石矿物的捕收剂,具体步骤和药剂制度如下:
(1)浮选时矿浆pH值为10~11,
(2)用硫酸锌及水玻璃作为异极矿的抑制剂,
(3)用醚胺作石英及碳酸盐脉石矿物的捕收剂,
(4)浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿,
(5)药剂用量为:
Figure BDA0000159729920000021
使用时,将所述药剂先配制成以下重量百分浓度:
本发明所述的异极矿为含结晶水的硅酸锌或氢氧化锌矿物。
本发明的突出优点在于:
1、能够将异极矿与石英及碳酸盐脉石矿物浮选分离,获得锌含量为21.26~23.80%,回收率达到72.51~75.67%的异极矿精矿。
2、本发明流程结构简单,药剂用量少,能耗少,能够对资源综合回收。
四、具体实施方式
实施例1
1.矿物原料:
所用矿物原料中锌含量为11.92%,硅含量为25.30%、碳酸钙含量为24.14%、物相分析表明,锌主要以异极矿形式存在,脉石矿物主要以碳酸盐及二氧化硅矿物形式存在。
2.浮选药剂及操作条件:
Figure BDA0000159729920000031
使用时,将所述药剂先配制成以下重量百分浓度:
Figure BDA0000159729920000032
浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿。试验表明采用以上工艺和药剂条件能够有效将异极矿回收,在给矿锌含量为11.92%条件下,经过两次浮选丢弃泡沫后,获得了锌含量为21.26%,回收率达到72.51%的异极矿精矿。
实施例2
1.矿物原料:
所用矿物原料中锌含量为14.10%,硅含量为28.72%、碳酸钙含量为27.64%、物相分析表明,锌主要以异极矿形式存在,脉石矿物主要以碳酸盐及二氧化硅矿物形式存在。
2.浮选药剂及操作条件:
Figure BDA0000159729920000041
使用时,将所述药剂先配制成以下重量百分浓度:
Figure BDA0000159729920000042
浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿。按上述工艺参数进行了试验,表明采用以上工艺和药剂条件能够有效将异极矿回收,在给矿锌含量为14.10%条件下,经过三次浮选丢弃泡沫后,获得了锌含量为23.80%,回收率达到75.67%的异极矿精矿。
实施例3
1.矿物原料:
所用矿物原料中锌含量为12.56%,硅含量为29.66%、碳酸钙含量为25.81%、物相分析表明,锌主要以异极矿形式存在,脉石矿物主要以碳酸盐及二氧化硅矿物形式存在。
2.浮选药剂及操作条件:
使用时,将所述药剂先配制成以下重量百分浓度:
Figure BDA0000159729920000052
浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿。按上述工艺参数进行了试验,表明采用以上工艺和药剂条件能够有效将异极矿回收,在给矿锌含量为12.56%条件下,经过三次浮选丢弃泡沫后,获得了锌含量为22.11%,回收率达到74.73%的异极矿精矿。

Claims (2)

1.一种异极矿与石英的浮选分离方法,其特征在于,该方法采用水玻璃及硫酸锌作为异极矿的抑制剂,用石灰作pH调整剂、用醚胺作石英及碳酸盐脉石矿物的捕收剂,具体步骤和药剂制度如下:
(1)浮选时矿浆pH值为10~11,
(2)用硫酸锌及水玻璃作为异极矿的抑制剂,
(3)用醚胺作石英及碳酸盐脉石矿物的捕收剂,
(4)浮选过程中,将水玻璃及硫酸锌加入到磨矿机将矿石磨至矿物单体解离后,再加石灰调节矿浆pH值为10~11,然后加醚胺对石英及碳酸盐矿物进行浮选,浮选泡沫作为尾矿丢弃,经过2~3次浮选,浮选槽内即为异极矿精矿,
(5)药剂用量为:
Figure FDA0000159729910000011
2.根据权利要求1所述的异极矿与石英的浮选分离方法,其特征在于,使用时将所述药剂先配制成以下重量百分浓度:
CN 201210131704 2012-05-02 2012-05-02 一种异极矿与石英的浮选分离方法 Expired - Fee Related CN102671770B (zh)