CN102453973A CN2010105289999A CN201010528999A CN102453973A CN 102453973 A CN102453973 A CN 102453973A CN 2010105289999 A CN2010105289999 A CN 2010105289999A CN 201010528999 A CN201010528999 A CN 201010528999A CN 102453973 A CN102453973 A CN 102453973A
Authority
CN
China
Prior art keywords
fiber
protein
parts
animal
plant protein
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010105289999A
Other languages
English (en)
Inventor
吴裕礼
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010105289999A priority Critical patent/CN102453973A/zh
Publication of CN102453973A publication Critical patent/CN102453973A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Artificial Filaments (AREA)

Abstract

本发明涉及一种动植物蛋白共聚纤维,该纤维的组份及含量为(重量比):牛奶酪蛋白质10~40份,豆酪素蛋白质10~40份,丙烯腈10~90份。本发明纤维具有羊毛绒手感、高贵,真丝一样的光泽,蛋白质纤维的吸湿、滑爽、透气和色泽艳丽,又有一定聚丙烯腈纤维的强度,可作为羊毛绒的替代品,减少过多的山羊数量,有利于生态的保护。

Description

动植物蛋白共聚纤维
技术领域
本发明属于高档服装(内、外衣)用的纺织新型材料技术领域,具体涉及一种动植物蛋白质(牛奶酪蛋白质和植物蛋白为大豆蛋白质和花生、谷物类蛋白质)与丙烯腈接枝共聚纤维及制造方法。
背景技术
蛋白纤维从纤维家族的分类来讲,属于酪素类纤维,世界各国一直将它作为课题来研究,我国在20世纪50年代、70年代曾分别对再生蛋白质纤维进行过初步的探索,但未获成功。90年代,四川省曾对蚕蛹再生蛋白纤维进行了研制,虽然纤维实现了小批量生产,但蛋白质含量较低,且在织造和印染加工中存在很多问题,严重影响了该类产品的开发和技术推广。东华大学、上海金山石化总公司曾对酪素/丙烯腈接枝共聚物的纺丝进行过研究,但亦停留于理论探讨,未见其产品:复旦大学和东华大学曾对再生丝素溶液的纺丝进行过研究,亦未能实现工业化生产。国外从19世纪、20世纪初即开始对再生蛋白质纤维进行研究。1936年意大利科学家、1938年英国ICI公司、1939年con product refinind公司曾分别探讨从牛乳、花生蛋白质、玉米、大豆豆粕中提取蛋白质,再进行纺丝。20世纪40年代初,美、英研制了酷系纤维、1945年美、英又研究了大豆蛋白质纤维;1938年美国通用汽车公司从豆粕中提取并且制作了大豆蛋白质纤维,但大多因为纤维性能键槽较差,无法进行纺织加工而中断研究。1969年日本东洋纺公司成功开发出了牛奶蛋白质纤维,以其良好的品质受到纺织业的欢迎。
发明内容
本发明所要解决的技术问题是提供一种动植物蛋白质(牛奶酪蛋白质和植物蛋白为大豆蛋白质)与丙烯腈接枝共聚纤维,并赋予该纤维优秀的(服装用)性能和功能,为中国乃至世界提供一种新型、高档的纺织材料。
本发明是通过以下技术方案来实现的,一种动植物蛋白共聚纤维,其组份及含量如下:(重量比)
牛奶酪蛋白质                    10~40份
豆酪素蛋白质                    10~40份
丙烯腈                          10~90份
本发明与现有技术相比具有以下有益效果:该纤维有羊毛绒一样的手感、高贵,真丝一样的光泽,蛋白质纤维的吸湿、滑爽、透气和色泽艳丽,又有一定聚丙烯腈纤维的强度,可作为羊毛绒的替代品,减少过多的山羊数量,有利于生态的保护。
具体实施方式:
实施例1
将70g牛奶干酪素和60g大豆蛋白质干粉放入270g丙烯腈中常温溶胀3小时后,放入60%的氯化锌水溶液中进行搅拌,在60℃中溶解8小时后搅拌降温到12℃,加入过硫酸钠1.01g,亚硫酸钠1.26g,反应1小时,分子量5万~6万,熟成脱泡后进行湿法纺丝,所得纤维的纤度0.8~6d tex,强力2.5~3.5CN/dtex,伸长15~30%,纤维公定回潮率3~8%。
实施例2
将100g牛奶干酪素和30g大豆蛋白质干粉放入250g丙烯腈中常温溶胀4小时后,放入60%的氯化锌水溶液中进行搅拌,在60℃中溶解8小时后搅拌降温到12℃,加入过硫酸钠1.01g,亚硫酸钠1.26g,反应1小时,分子量5万~6万,熟成脱泡后进行湿法纺丝,所得纤维的纤度0.8~6d tex,强力2.5~3.5CN/dtex,伸长15~30%,纤维公定回潮率3~8%。

Claims (1)

1.一种动植物蛋白共聚纤维,其特征是:其组份及含量如下:(重量比)
牛奶酪蛋白质                    10~40份
豆酪素蛋白质                    10~40份
丙烯腈                          10~90份 。
CN2010105289999A 2010-10-30 2010-10-30 动植物蛋白共聚纤维 Pending CN102453973A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010105289999A CN102453973A (zh) 2010-10-30 2010-10-30 动植物蛋白共聚纤维

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010105289999A CN102453973A (zh) 2010-10-30 2010-10-30 动植物蛋白共聚纤维

Publications (1)

Publication Number Publication Date
CN102453973A true CN102453973A (zh) 2012-05-16

Family

ID=46037630

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010105289999A Pending CN102453973A (zh) 2010-10-30 2010-10-30 动植物蛋白共聚纤维

Country Status (1)

Country Link
CN (1) CN102453973A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104005134A (zh) * 2014-05-04 2014-08-27 广东都市丽人实业有限公司 腈纶混纺暖智能纱线的制备方法及内衣制品
CN107217327A (zh) * 2017-07-07 2017-09-29 苏州市晨彩纺织研发有限公司 一种添加有蛋白纤维的纺织面料及其制备方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104005134A (zh) * 2014-05-04 2014-08-27 广东都市丽人实业有限公司 腈纶混纺暖智能纱线的制备方法及内衣制品
CN107217327A (zh) * 2017-07-07 2017-09-29 苏州市晨彩纺织研发有限公司 一种添加有蛋白纤维的纺织面料及其制备方法

Similar Documents

Publication Publication Date Title
CN101333718B (zh) 牛仔布经线用dty双色涤纶丝
CN101307502A (zh) 菠萝叶纤维的制备方法
CN104195650A (zh) 一种可纺性柔软椰壳细纤维生产工艺及其制品应用
CN104372439B (zh) 生物基蛋白复合纤维及其制备方法
CN108950867B (zh) 一种高强度抗皱水刺无纺布的生产工艺
CN102747477A (zh) 天丝混纺纱及其在涡流纺上的制备方法
CN102304781A (zh) 鸡毛再生蛋白粘胶纤维及其制备方法和应用
CN103437013B (zh) 一种由芳纶1414废丝短纤维制备纱线的方法
CN111334880B (zh) 光致变色莱赛尔纤维及其制备方法
CN105297215A (zh) 一种阻燃抗静电改性的聚酯混纺再生棉纱及其制备方法
CN105908501A (zh) 采用再生棉纱生产抗菌毛巾的方法
CN103361803A (zh) 一种低缩水率的竹纤维纺织制品及其制备方法
CN1156619C (zh) 大豆分离蛋白改性的聚乙烯醇纤维及制法
CN102453973A (zh) 动植物蛋白共聚纤维
Trivedy et al. Production of Pink Colored Silk Fabric Dyed Using a" Green" Dye-Fed Silkworm Approach.
CN100999848A (zh) 羊毛与改性涤纶混纺呢绒面料及其工艺
CN102330250A (zh) 一种具有超强粘着力面料及其生产方法
CN106012083B (zh) 一种环保亲肤涤纶欧根纱面料的制备方法
CN105442147A (zh) 一种抗紫外远红外生态面料的制备方法
CN109629235B (zh) 超细桑蚕丝纤维真丝围巾面料
CN1233889C (zh) 动植物蛋白质与丙烯腈接枝共聚纤维的制造方法
CN1257318C (zh) 动物蛋白质与丙烯腈接枝共聚纤维的制造方法
CN101608360A (zh) 一种大豆蛋白纤维及其在家纺面料中的应用
CN111321499B (zh) 基于超细桑蚕丝纤维/柞蚕丝纤维的真丝围巾面料的制备方法
CN106192042B (zh) 一种黄秋葵有色粘胶纤维的制备方法及所得家居服

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20120516