CN102328278A - 一种钛及钛合金带卷抛丸去除氧化皮的方法 - Google Patents

一种钛及钛合金带卷抛丸去除氧化皮的方法 Download PDF

Info

Publication number
CN102328278A
CN102328278A CN201110183788A CN201110183788A CN102328278A CN 102328278 A CN102328278 A CN 102328278A CN 201110183788 A CN201110183788 A CN 201110183788A CN 201110183788 A CN201110183788 A CN 201110183788A CN 102328278 A CN102328278 A CN 102328278A
Authority
CN
China
Prior art keywords
titanium
titanium alloy
speed
shot blasting
strip
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201110183788A
Other languages
English (en)
Inventor
曹占元
苏鹤洲
史亚鸣
张彦民
张宝柱
李志敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yunnan Titanium Industry Co Ltd
Original Assignee
Yunnan Titanium Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yunnan Titanium Industry Co Ltd filed Critical Yunnan Titanium Industry Co Ltd
Priority to CN201110183788A priority Critical patent/CN102328278A/zh
Publication of CN102328278A publication Critical patent/CN102328278A/zh
Pending legal-status Critical Current

Abstract

一种钛及钛合金带卷抛丸去除氧化皮的方法,本发明采用2~8台抛丸机将直径为0.2~2.0mm的耐磨钢球以25~98m/s的速度、20~100Hz的频率抛打在以3~30m/min的速度运行的钛带上表面和下表面,从而把钛带表面的氧化皮打脱落。本发明具有能够实现打开长度上千米、收裹成圆环卷状的钛及钛合金带的处理,运行过程为物理过程,不存在化学反应失控的安全风险,也不存在环境污染,具有金属损耗少的显著优点。

Description

一种钛及钛合金带卷抛丸去除氧化皮的方法
技术领域
本发明属于钛及钛合金带表面加工处理的技术领域。
背景技术
现有的钛板单板轧制的生产形式中,钛板表面氧化皮的去除是采用碱爆除鳞法,即把钛及钛合金平板浸入熔融的碱液中,使TiO2与NaOH发生反应,从而去除钛板表面的氧化皮。碱爆除鳞法存在的缺陷是,一是不能实现收裹成圆环状的、打开长度达上千米的钛及钛合金带卷的处理,二是存在较大的安全风险,三是环境污染严重,四是金属损耗高。
发明内容
本发明的目的就是为了解决碱爆除鳞法不能处理打开长度上千米、收裹成圆环卷状的钛及钛合金带卷表面氧化层的问题,提供一种高效、安全、环境友好、金属损耗小的钛及钛合金带卷表面除鳞去氧化层的方法。
本发明的目的是通过如下技术方案实现的:
一种钛及钛合金带卷抛丸去除氧化皮的方法,本发明采用2~8台抛丸机将直径为0.2~2.0mm的耐磨钢球以25~98m/s的速度、20~100Hz的频率抛打在以3~30m/min的速度运行的钛带上表面和下表面,从而把钛带表面的氧化皮打脱落。
本发明的有益效果是:能够实现打开长度上千米、收裹成圆环卷状的钛及钛合金带卷的处理,运行过程为物理过程,不存在化学反应失控的安全风险,也不存在环境污染,具有金属损耗少的显著优点。
具体实施方式
实施例一    一种钛及钛合金带卷抛丸去除氧化皮的方法,本发明采用4台抛丸机将直径为0.5mm的耐磨钢球以45m/s的速度、35Hz的频率抛打在以8m/min的速度运行的钛带上表面和下表面,从而把钛带表面的氧化皮打脱落。
实施例二    一种钛及钛合金带卷抛丸去除氧化皮的方法,本发明采用2台抛丸机将直径为0.3mm的耐磨钢球以50m/s的速度、55Hz的频率抛打在以12m/min的速度运行的钛带卷上表面和下表面,从而把钛带表面的氧化皮打脱落。
实施例三   一种钛及钛合金带卷抛丸去除氧化皮的方法,本发明采用6台抛丸机将直径为0.6mm的耐磨钢球以60m/s的速度、60Hz的频率抛打在以20m/min的速度运行的钛带卷上表面和下表面,从而把钛带表面的氧化皮打脱落。

Claims (1)

1.一种钛及钛合金带卷抛丸去除氧化皮的方法,其特征是,采用2~8台抛丸机将直径为0.2~2.0mm的耐磨钢球以25~98m/s的速度、20~100Hz的频率抛打在以3~30m/min的速度运行的钛带上表面和下表面,从而把钛带表面的氧化皮打脱落。
CN201110183788A 2011-07-01 2011-07-01 一种钛及钛合金带卷抛丸去除氧化皮的方法 Pending CN102328278A (zh)