CN102260390A - 可自然分解的环保器具及其制造方法 - Google Patents
可自然分解的环保器具及其制造方法 Download PDFInfo
- Publication number
- CN102260390A CN102260390A CN2010101883386A CN201010188338A CN102260390A CN 102260390 A CN102260390 A CN 102260390A CN 2010101883386 A CN2010101883386 A CN 2010101883386A CN 201010188338 A CN201010188338 A CN 201010188338A CN 102260390 A CN102260390 A CN 102260390A
- Authority
- CN
- China
- Prior art keywords
- environmental protection
- natural decomposition
- manufacture method
- protection utensil
- thermoplastic material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种可自然分解的环保器具及其制造方法,该制造方法包括下列步骤:(1)将50%的热塑性塑料材料、40%的竹粉纤维及10%的加工黏着助剂混合;(2)将上述材料的混合物放入造粒机造粒;(3)将经过造粒后的产品再放入烤箱烘烤;(4)再将经过烘烤的产品放入注塑机成型;及(5)最后即为成品。
Description
技术领域
本发明涉及一种可自然分解的环保器具及其制造方法,其主要是应用于制作可自然分解的环保容器的技术上。
背景技术
一般传统的环保美耐皿树脂餐具内含玉米粉,所以成本高,而且容易产生细菌及发霉。此外,以可食用的玉米作为制作原料,不但浪费粮食,而且又不环保,为其既存尚待克服解决的问题与缺陷。
发明内容
本发明的目的在于提供一种可自然分解的环保器具,以解决现有技术中存在的上述问题。
本发明的另一目的在于提供一种可自然分解的环保器具的制造方法。
本发明提供一种可自然分解的环保器具,包括:
热塑性塑料材料,含量占50%;竹粉纤维,具有高强度补强及韧度,含量占40%;加工黏着助剂,具有黏着性,含量占10%。
本发明提供一种可自然分解的环保器具制造方法,包括下列步骤:
(1)将50%的热塑性塑料材料、40%的竹粉纤维及10%的加工黏着助剂混合;
(2)将上述材料的混合物放入造粒机造粒;
(3)将经过造粒后的产品再放入烤箱烘烤;
(4)再将经过烘烤的产品放入注塑机成型;及
(5)最后即为成品。
本发明对照现有技术的有益技术效果在于:热塑本发明所使用的竹粉纤维为制作竹器用品剩下的废料,由于竹子的生长速度远比一般的树木快,所以可以减少砍伐树木的数量,具有节能减碳的效益,而且竹子本身并非粮食(竹笋才是),故不会浪费粮食,可以废物再利用,同时本发明所使用的原料和加工黏着助剂均为有机物,绝对不含八大重金属及N系磷苯二甲酸,丢弃掩埋后,本材质会通过自然界中的微生物分解,不会对地球的环境造成二次污染。
本发明所提供的制作方法制作出来的可自然分解的环保容器,适用于微波炉等加热,使用过后的废弃环保容器可以回收再利用,重新制作成餐具、栈板、音箱等,资源回收再利用。
附图说明
图1:为本发明的可自然分解的环保器具的制作流程示意图。
图2:为本发明的可自然分解的环保器具的截面图。
具体实施方式
为使熟悉此项技术的人员易于深入了解本发明的装置内容以及所能达成的有益效果,兹列举一具体实施例,并配合附图详细介绍说明如下。
本发明提供一种可自然分解的环保器具及其制造方法,敬请参阅图1,其所示为本发明的可自然分解的环保器具的制作流程示意图,与图2,其所示为本发明的可自然分解的环保器具的截面图。
本发明的可自然分解的环保器具主要包括:热塑性塑料材料,如:PP(聚丙烯)或PE(聚乙烯)或PS(聚苯乙烯)或ABS(丙烯腈-丁二烯-苯乙烯共聚物),含量占50%;竹粉纤维,具有高强度补强及韧度,含量占40%;加工黏着助剂(Adjuvant),具有黏着性,含量占10%。
本发明的可自然分解的环保器具的制作流程如下:
一、将50%的热塑性塑料材料,如:PP、PE、PS或ABS、40%的竹粉纤维及10%的加工黏着助剂(Adjuvant)混合;
二、将混合物放入造粒机内搅拌捏合,再经过高速造粒,将滚动的产品切成均匀的颗粒;
三、再放入烤箱(温度在100~150℃)烘烤;
四、再放入注塑机(温度在150℃)成型;
五、最后即为成品。
综上所述的本发明提供了一种可自然分解的环保器具及其制造方法,经过本发明人实际制作完成以及反复操作测试后,证实的确可以达到本发明所预期的功能效益。
Claims (6)
1.一种可自然分解的环保器具,包括:
热塑性塑料材料,含量占50%;竹粉纤维,含量占40%;加工黏着助剂,含量占10%。
2.如权利要求1所述的可自然分解的环保器具制造方法,其中:所述热塑性塑料材料为聚丙烯、聚乙烯、聚苯乙烯、或丙烯腈-丁二烯-苯乙烯共聚物。
3.一种可自然分解的环保器具制造方法,包括下列步骤:
(1)将50%的热塑性塑料材料、40%的竹粉纤维及10%的加工黏着助剂混合;
(2)将上述材料的混合物放入造粒机造粒;
(3)将经过造粒后的产品再放入烤箱烘烤;
(4)再将经过烘烤的产品放入注塑机成型;及
(5)最后即为成品。
4.如权利要求3所述的可自然分解的环保器具制造方法,其中热塑性塑料材料为聚丙烯、聚乙烯、聚苯乙烯、或丙烯腈-丁二烯-苯乙烯共聚物。
5.如权利要求3所述的可自然分解的环保器具制造方法,其中该步骤(3)的烘烤的温度在100~150℃。
6.如权利要求3所述的可自然分解的环保器具制造方法,其中该步骤(4)的成型的温度为150℃。