CN102247990A - 钼基顶头 - Google Patents

钼基顶头 Download PDF

Info

Publication number
CN102247990A
CN102247990A CN2011101399246A CN201110139924A CN102247990A CN 102247990 A CN102247990 A CN 102247990A CN 2011101399246 A CN2011101399246 A CN 2011101399246A CN 201110139924 A CN201110139924 A CN 201110139924A CN 102247990 A CN102247990 A CN 102247990A
Authority
CN
China
Prior art keywords
loose joint
tappet
mandril
push rod
molybdenum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011101399246A
Other languages
English (en)
Inventor
***
章建新
沈卫强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU WUJIN STAINLESS STEEL PIPE GROUP CO Ltd
Original Assignee
JIANGSU WUJIN STAINLESS STEEL PIPE GROUP CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU WUJIN STAINLESS STEEL PIPE GROUP CO Ltd filed Critical JIANGSU WUJIN STAINLESS STEEL PIPE GROUP CO Ltd
Priority to CN2011101399246A priority Critical patent/CN102247990A/zh
Publication of CN102247990A publication Critical patent/CN102247990A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种用于不锈钢热穿孔的钼基顶头,包括顶头、空心的顶杆、以及连接顶头和顶杆的活接,所述的活接包括与顶头螺纹连接的顶头活接和与顶杆螺纹连接的顶杆活接,顶头活接与顶杆活接螺纹连接,所述的顶头活接和顶杆活接为空心管,所述的顶头活接的管壁具有至少一个通孔。本发明的钼基顶头结构简单,在顶头活接管壁上增设通孔,用于排出部分冷却水,达到降低顶头温度的作用,同时适当的冷却水有利于不锈钢管内壁快速冷却达到固溶强化的目的,提高产品的合格率。

Description

钼基顶头
技术领域
本发明涉及不锈钢热穿孔设备技术领域,尤其是一种钼基顶头。
背景技术
钼基顶头采用钼粉原料添加稀土材料,经过混料、成型、外形加工、高温烧结等工序加工制成,钼合金具有良好的导热、导电性和低的膨胀系数,在高温下(1100~1650℃)仍然具有较高的强度,主要用于不锈钢、钎钢、轴承钢和高温合金钢等无缝钢管在高温恶劣环境下的热轧穿孔工作。
钼基顶头在热轧穿孔工作时,在高温高压和剧烈摩擦的恶劣环境下,钼基顶头的温度过高产生粘性,划伤钢管内孔且使钢管内壁出现裂纹,产生次品,因不锈钢材价格较高,一旦出现次品,损失将非常大。因此在穿孔时需要对钼基顶头进行冷却,现有技术采用水冷方式,但还是不能很好的冷却钼基顶头。
发明内容
本发明要解决的技术问题是:克服现有技术中之不足,提供一种钼基顶头,冷却效果更好。
本发明解决其技术问题所采用的技术方案是:一种钼基顶头,包括顶头、空心的顶杆、以及连接顶头和顶杆的活接,所述的活接包括与顶头螺纹连接的顶头活接和与顶杆螺纹连接的顶杆活接,顶头活接与顶杆活接螺纹连接,所述的顶头活接和顶杆活接为空心管,所述的顶头活接的管壁具有至少一个通孔。
进一步地,所述的通孔数量为三个。
本发明的有益效果是,本发明的钼基顶头结构简单,在顶头活接管壁上增设通孔,用于排出部分冷却水,达到降低顶头温度的作用,同时适当的冷却水有利于不锈钢管内壁快速冷却达到固溶强化的目的,提高产品的合格率。
附图说明
下面结合附图对本发明进一步说明。
图1是本发明的钼基顶头的最佳实施例的结构示意图。
图中:1.顶头,2.顶头活接,21.通孔,3.顶杆活接,4.顶杆。
具体实施方式
如图1所示,本发明的钼基顶头的最佳实施例,一种钼基顶头,包括顶头1、空心的顶杆4、以及连接顶头1和顶杆4的活接,活接包括与顶头1螺纹连接的顶头活接2和与顶杆4螺纹连接的顶杆活接3,顶头活接2与顶杆活接3螺纹连接,顶头活接2和顶杆活接3为空心管,顶头活接2的管壁具有至少一个通孔21。最佳方案,通孔21数量为三个。
在实际生产时,空心的顶杆4内通入冷却水管路,可通过控制水压来调节冷却效率,大部分水通过空心的顶杆4流出,部分水通过顶头活接2上的通孔21流出,使顶头1内外都受到冷却,同时也使不锈钢管内壁冷却,有利于内壁快速冷却固溶强化,减少废次品,提高产品的合格率。

Claims (2)

1.一种钼基顶头,包括顶头(1)、空心的顶杆(4)、以及连接顶头(1)和顶杆(4)的活接,所述的活接包括与顶头(1)螺纹连接的顶头活接(2)和与顶杆(4)螺纹连接的顶杆活接(3),顶头活接(2)与顶杆活接(3)螺纹连接,其特征是:所述的顶头活接(2)和顶杆活接(3)为空心管,所述的顶头活接(2)的管壁具有至少一个通孔(21)。
2.如权利要求1所述的钼基顶头,其特征是:所述的通孔(21)数量为三个。
CN2011101399246A 2011-05-27 2011-05-27 钼基顶头 Pending CN102247990A (zh)