CN102140296A - 一种耐磨木器涂料 - Google Patents

一种耐磨木器涂料 Download PDF

Info

Publication number
CN102140296A
CN102140296A CN 201010550292 CN201010550292A CN102140296A CN 102140296 A CN102140296 A CN 102140296A CN 201010550292 CN201010550292 CN 201010550292 CN 201010550292 A CN201010550292 A CN 201010550292A CN 102140296 A CN102140296 A CN 102140296A
Authority
CN
China
Prior art keywords
parts
coating
abrasion
woodenware
resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010550292
Other languages
English (en)
Inventor
周雪良
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUJIANG LONGJING HONGBEI INTERIOR DECORATION CO Ltd
Original Assignee
WUJIANG LONGJING HONGBEI INTERIOR DECORATION CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUJIANG LONGJING HONGBEI INTERIOR DECORATION CO Ltd filed Critical WUJIANG LONGJING HONGBEI INTERIOR DECORATION CO Ltd
Priority to CN 201010550292 priority Critical patent/CN102140296A/zh
Publication of CN102140296A publication Critical patent/CN102140296A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种耐磨木器涂料,其按下列原料按照重量配比搅拌制成:55-60份环氧树脂,10-15份硬脂酸锌,15份聚四氟乙烯,5份滑石粉,10-15份樟脑油,9份三乙醇胺,5份丙酮,20份乙二醇,11份碱木木质素,12份纳米氧化钛浆料,5份消泡剂,4份润湿剂。本发明的产品经试验证明,涂抹后表面耐磨性增强、对人畜安全、环境保护等不构成影响,材料和工艺相对较低,广泛用于室内、外木器防护等方面。

Description

一种耐磨木器涂料
技术领域
本发明涉及一种耐磨木器涂料,属于涂料技术领域。
技术背景
目前传统的木器涂料,不论是油性的还是水性的,都以石油化工产品为原料,加工、合成的高分子树脂。这些涂料含有超过50%的挥发性有机化合物和对人体有害的成分,如苯、甲醛等,不仅对操作人员和施工人员的身体造成伤害,同时也对周围的环境造成严重的污染,破坏生态。并且现有的一些木器涂料很容易磨损,不能很好的保护木器。
发明内容
本发明目的在于克服现有技术的缺点与不足,提供一种保护木器不磨损的耐磨木器涂料。
为了达到上述目的,本发明采用一个技术方案是:一种耐磨木器涂料按下列原料按照重量配比搅拌制成:55-60份环氧树脂,10-15份硬脂酸锌,15份聚四氟乙烯,5份滑石粉,10-15份樟脑油,9份三乙醇胺,5份丙酮,20份乙二醇,11份碱木木质素,12份纳米氧化钛浆料,5份消泡剂,4份润湿剂。
本发明的产品经试验证明,涂抹后表面耐磨性增强、对人畜安全、环境保护等不构成影响,材料和工艺相对较低,广泛用于室内、外木器防护等方面。
具体实施方式
本发明所述的实例是对本发明的说明而不能限制本发明,在与本发明相当的含义和范围内的任何改变和调整,都应认为是在本发明的范围内。
实施例1
一种耐磨木器涂料按下列原料按照重量配比搅拌制成:55-60份环氧树脂,10-15份硬脂酸锌,15份聚四氟乙烯,5份滑石粉,10-15份樟脑油,9份三乙醇胺,5份丙酮,20份乙二醇,11份碱木木质素,12份纳米氧化钛浆料,5份消泡剂,4份润湿剂。

Claims (1)

1.一种耐磨木器涂料,其特征在于它主要是由下列原料按照重量配比搅拌制成:55-60份环氧树脂,10-15份硬脂酸锌,15份聚四氟乙烯,5份滑石粉,10-15份樟脑油,9份三乙醇胺,5份丙酮,20份乙二醇,11份碱木木质素,12份纳米氧化钛浆料,5份消泡剂,4份润湿剂。
CN 201010550292 2010-11-19 2010-11-19 一种耐磨木器涂料 Pending CN102140296A (zh)