CN101726395B - 焊缝密性的测试方法 - Google Patents
焊缝密性的测试方法 Download PDFInfo
- Publication number
- CN101726395B CN101726395B CN200910155511XA CN200910155511A CN101726395B CN 101726395 B CN101726395 B CN 101726395B CN 200910155511X A CN200910155511X A CN 200910155511XA CN 200910155511 A CN200910155511 A CN 200910155511A CN 101726395 B CN101726395 B CN 101726395B
- Authority
- CN
- China
- Prior art keywords
- tightness
- vacuum
- weld
- testing
- welding line
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种焊缝密性的测试方法,包括如下步骤:选取透明的真空箱,该真空箱通过管道与抽真空机相连通,并在真空箱上设置有能显示真空箱内真空度的真空压力表;选取需要检测的焊缝,并在需要被检测的焊缝左右各200mm区域清理干净,然后涂上肥皂液,再将真空箱覆盖在涂有肥皂液的焊缝上;压紧真空箱,开启抽真空阀门,在真空表上显示真空度在0.015-0.02MPa范围内时,观察焊缝表面是否有气泡冒出,如发现有气泡冒出,确定焊缝不合格,应修补后重新检查;如没有发现有气泡冒出,确定焊缝合格。本发明的优点在于:能降低船坞密性测试工作量,能有效地提高缩短船台生产周期;优化密性作业环境,高空封闭作业可以在平地敞开做,使操作更安全,并且测试方法简单可靠,即测试准确、操作方便,有效地提高了密性的工作效率。
Description
技术领域
本发明涉及到一种用于造船船板上的焊缝密性的测试方法。
背景技术
众所周知,船舶建造过程中,为防止各种舱室之间相互渗漏,在船体结构中设置了水密舱壁板,检验这些舱壁板是否渗漏,则是通过密性测试来进行的,传统的密性作业阶段是放在船台上或船坞内,等分段合拢后再进行大舱密性的,而对需要进行密性的焊缝,在分段涂装前必须在焊缝上用胶带粘贴宽度为100mm左右,待密性结束后,涂装再进行补漆工作,而补漆前又必须将焊缝两侧(150mm)范围内进行打磨,然后用手工刷涂。就这一项作业不仅费时、费力同时增加了高空作业及密闭舱室作业的危险性,对焊缝质量控制方面带来许多困难,最重要的是延长了船台或船坞内的作业周期,从而降低生产效率,所以这种测试方法还有待于改进。
发明内容
本发明所要解决的技术问题是针对现有技术的现状提供一种测试准确、操作方便、安全且检测效率高的焊缝密性的测试方法。
本发明解决上述技术问题而采用的技术方案为:本焊缝密性的测试方法,其特征在于:包括如下步骤:a、选取透明的真空箱,该真空箱通过管道与抽真空机相连通,并在真空箱上设置有能显示真空箱内真空度的真空压力表;b、选取需要检测的焊缝,并在需要被检测的焊缝左右各200mm区域清理干净,然后涂上肥皂液,再将真空箱覆盖在涂有肥皂液的焊缝上;c、压紧真空箱,开启抽真空阀门,在真空表上显示真空度在0.015-0.02Mpa范围内时,观察焊缝表面是否有气泡冒出,d、如发现有气泡冒出,确定焊缝不合格,应修补后重新检查;如没有发现有气泡冒出,确定焊缝合格。
作为改进,在部件、组件和片体上的焊缝可分段进行测试。
再改进,所述测试方法可应用于深熔焊缝、全焊透角焊缝及角焊缝密性的测试。
与现有技术相比,本发明的优点在于:首先,符合工序阶段前移的特点,降低船坞密性测试工作量,能有效地提高缩短船台(船坞)生产周期;其次是,优化密性作业环境,高空封闭作业可以在平地敞开做,使操作更安全,并且测试方法简单可靠,即测试准确、操作方便,有效地提高了密性的工作效率,还有,能减少船台(坞内)脚手架工作,降低为密性测试所化费的成本,即节约了生产成本;再次是,能保证分段出涂装车间的油漆完整性,对已做通气密性测试的焊缝可以进行冲砂油漆,减少船台,船坞补漆工作量。综上所述,本测试方法,具有测试准确、操作方便、安全且检测效率高,是一种价得推广应用的技术,值得重视。
具体实施方式
以下结合实施例对本发明作进一步详细描述。
本实施例的焊缝密性的测试方法,包括如下步骤:a、选取透明的真空箱,该真空箱通过管道与抽真空机相连通,并在真空箱上设置有能显示真空箱内真空度的真空压力表;b、选取需要检测的焊缝,并在需要被检测的焊缝左右各200mm区域清理干净,然后涂上肥皂液,再将真空箱覆盖在涂有肥皂液的焊缝上;c、压紧真空箱,开启抽真空阀门,在真空表上显示真空度在0.015-0.02Mpa范围内时,观察焊缝表面是否有气泡冒出,d、如发现有气泡冒出,确定焊缝不合格,应修补后重新检查;如没有发现有气泡冒出,确定焊缝合格。在部件、组件和片体上的焊缝可分段进行测试,这样更方便,并且,本测试方法可应用于深熔焊缝、全焊透角焊缝及分角焊缝密性的测试,应用范围更广。
以下对本发明作进一步说明:
一、目的:
1、查焊缝的密性,保证分段涂装的完整性。
2、低现场施工难度,改善施工环境。
3、对深熔焊和全焊透角焊缝不能实施角焊缝密性测试的一种补充。
4、减少船台(坞内)脚手架工作,降低密性测试成本。
5、证分段出涂装车间的油漆完整性,对已做通气密测试的焊缝可以进行冲砂油漆,减少船台,船坞补漆工作量。
二.范围:
非自动焊对接焊缝,角焊缝等。
三.测试程序
真空密性测试是对角焊缝,对接焊缝(非自动焊缝)表面喷涂肥皂液,同时将真空箱罩住被检焊缝,开启球阀(真空阀门),目测焊缝渗漏情况。
1.为能看清焊缝渗漏情况,真空箱必须是透明的。
2.在真空箱上安装压缩空气注入管接头和真空压力表接头。
3.真空测试压力为0.015~0.02Mpa。
4.在被检查焊缝左右各~200mm区域清理干净,并涂上肥皂液。将真空箱覆盖在涂有肥皂液的焊缝上。
5.压紧真空箱开启球阀,观察真空表上真空度是否满足要求。在满足真空度要求的前提下,观察焊缝表面是否有气泡冒出,如有:说明焊缝有渗漏,应修补后重复检查;如无;说明焊缝没有渗漏。
6.所有抽真空检查的焊缝都要报QC认可并做记录。
四.工装制作:
该工装主要是用于船体分段角焊缝及外板焊缝密性测试。参考船体分段各种角度的角焊缝及外板线型,制作了凹、凸、平、及各种角度的角焊缝的真空箱。
Claims (3)
1.一种焊缝密性的测试方法,其特征在于:包括如下步骤:a、选取透明的真空箱,该真空箱通过管道与抽真空机相连通,并在真空箱上设置有能显示真空箱内真空度的真空压力表;b、选取需要检测的焊缝,并在需要被检测的焊缝左右各200mm区域清理干净,然后涂上肥皂液,再将真空箱覆盖在涂有肥皂液的焊缝上;c、压紧真空箱,开启抽真空阀门,在真空表上显示真空度在0.015Mpa时,观察焊缝表面是否有气泡冒出,d、如发现有气泡冒出,确定焊缝不合格,应修补后重新检查;如没有发现有气泡冒出,确定焊缝合格。
2.根据权利要求1所述焊缝密性的测试方法,其特征在于:在部件、组件和片体上的焊缝为分段进行测试。
3.根据权利要求1或2所述焊缝密性的测试方法,其特征在于:所述测试方法可应用于深熔焊缝、全焊透角焊缝及角焊缝密性的测试。