CN101580661A - 触摸屏保护油墨 - Google Patents

触摸屏保护油墨 Download PDF

Info

Publication number
CN101580661A
CN101580661A CNA200910040022XA CN200910040022A CN101580661A CN 101580661 A CN101580661 A CN 101580661A CN A200910040022X A CNA200910040022X A CN A200910040022XA CN 200910040022 A CN200910040022 A CN 200910040022A CN 101580661 A CN101580661 A CN 101580661A
Authority
CN
China
Prior art keywords
touch screen
portions
screen protective
protective ink
polyvinyl chloride
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA200910040022XA
Other languages
English (en)
Inventor
刘恒全
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA200910040022XA priority Critical patent/CN101580661A/zh
Publication of CN101580661A publication Critical patent/CN101580661A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种触摸屏保护油墨,采用下列原材料混合后制成;各种原材料按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:100-250份;聚氯乙烯A:100-300份;聚氯乙烯B:150-300份;C23H16n8Cu:1-3份;非移性高分子聚酯可塑剂:20-60份;偏苯三甲酸二异壬酯:120-300份;邻苯二甲酸丁苄酯:20-70份;邻苯二甲酸二辛酯:30-80份。触摸屏保护油墨用于触摸屏制作原材料中的ITO膜与ITO玻璃表面保护作用。通过印刷后加热固化或紫外光照后起到保护作用,使用完后可剥离;使用后剥离下时没有残胶亮边,韧性好,无变色,好剥离,无漏空,无残留等。可用于市场上所有的ITO膜与ITO玻璃。

Description

触摸屏保护油墨
技术领域
本发明涉及油墨,具体涉及一种触摸屏保护油墨。
背景技术
在现有技术中,要在触摸屏制作原材料中的ITO膜与ITO玻璃表面,采用油墨印刷后加热固化进行保护;现有的油墨在使用剥离时,存在如下缺点:有残胶亮边,韧性不好,不好剥离,有残留等问题。
发明内容
本发明的目的在于,针对现有技术的上述缺陷,提供一种触摸屏保护油墨;这种油墨使用后剥离时没有残胶亮边,韧性好,无变色,好剥离,无漏空,无残留。
本发明提供的技术方案如下:提供一种触摸屏保护油墨,采用下列原材料混合后制成;各种原材料按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:100-250份;聚氯乙烯树脂A:100-300份;聚氯乙烯树脂B:150-300份;色浆:1-3份;非移性高分子聚酯可塑剂:20-60份;偏苯三甲酸二异壬酯:120-300份;邻苯二甲酸丁苄酯:20-70份;邻苯二甲酸二辛酯:30-80份;稀释剂、流平剂、增粘剂10-30份。
本发明具有如下优点:触摸屏保护油墨用于触摸屏制作原材料中的ITO膜与ITO玻璃表面保护作用。通过印刷后加热固化或紫外光照后起到保护作用,使用完后可剥离;使用后剥离下时没有残胶亮边,韧性好,无变色,好剥离,无漏空,无残留等。可以适用与市场上所有的ITO膜与ITO玻璃。
具体实施方式
实施例一:取下列原材料混合制成;按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:180-200份;聚氯乙烯树脂A:170-250份;聚氯乙烯树脂B:200-300份;色浆:2-3份;非移性高分子聚酯可塑剂:30-50份;偏苯三甲酸二异壬酯:180-250份;邻苯二甲酸丁苄酯:40-60份;邻苯二甲酸二辛酯:40-70份。
实施例二:采用下列原材料混合后制成;按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:190份;聚氯乙烯树脂A:200份;聚氯乙烯树脂B:250份;色浆:2份;非移性高分子聚酯可塑剂:44份;偏苯三甲酸二异壬酯:202份;邻苯二甲酸丁苄酯:50份;邻苯二甲酸二辛酯:42份;稀释剂、流平剂、增粘剂10-30份。

Claims (3)

1、一种触摸屏保护油墨,其特征在于,采用下列原材料混合后制成;原材料按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:100-250份;聚氯乙烯树脂A:100-300份;聚氯乙烯树脂B:150-300份;色浆:1-3份;非移性高分子聚酯可塑剂:20-60份;偏苯三甲酸二异壬酯:120-300份;邻苯二甲酸丁苄酯:20-70份;邻苯二甲酸二辛酯:30-80份,稀释剂、流平剂、增粘剂10-30份。
2、根据权利要求1所述的触摸屏保护油墨,其特征在于;采用下列原材料混合后制成;按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:180-200份;聚氯乙烯树佛A:170-250份;聚氯乙烯树佛B:200-300份;色浆:2-3份;非移性高分子聚酯可塑剂:30-50份;偏苯三甲酸二异壬酯:180-250份;邻苯二甲酸丁苄酯:40-60份;邻苯二甲酸二辛酯:40-70份;流平剂、增粘剂10-30份。
3、根据权利要求2所述的触摸屏保护油墨,其特征在于;采用下列原材料混合后制成;按份数计;其中:氯乙烯-醋酸乙烯酯共聚氟树脂:190份;聚氯乙烯树脂A:200份;聚氯乙烯树脂B:250份;色浆:2份;非移性高分子聚酯可塑剂:44份;偏苯三甲酸二异壬酯:202份;邻苯二甲酸丁苄酯:50份;邻苯二甲酸二辛酯:42份。稀释剂、流平剂、增粘剂20份。
CNA200910040022XA 2009-06-05 2009-06-05 触摸屏保护油墨 Pending CN101580661A (zh)