CN101191273A - 四面弹力麂皮绒 - Google Patents

四面弹力麂皮绒 Download PDF

Info

Publication number
CN101191273A
CN101191273A CNA2007101913708A CN200710191370A CN101191273A CN 101191273 A CN101191273 A CN 101191273A CN A2007101913708 A CNA2007101913708 A CN A2007101913708A CN 200710191370 A CN200710191370 A CN 200710191370A CN 101191273 A CN101191273 A CN 101191273A
Authority
CN
China
Prior art keywords
ptt
spandex
fiber
elastic fiber
urethane elastic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2007101913708A
Other languages
English (en)
Inventor
陆文峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YANGZHOU JIYUAN TEXTILE CO Ltd
Original Assignee
YANGZHOU JIYUAN TEXTILE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YANGZHOU JIYUAN TEXTILE CO Ltd filed Critical YANGZHOU JIYUAN TEXTILE CO Ltd
Priority to CNA2007101913708A priority Critical patent/CN101191273A/zh
Publication of CN101191273A publication Critical patent/CN101191273A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种四面弹力麂皮绒,属于纺织面料技术领域,主要特点是经纱以海岛丝为氨纶芯丝的包丝,使海岛丝成为有弹性的海岛丝;纬纱以PTT聚酯作为氨纶芯丝的包丝,从而使PTT具有良好的拉伸与回复、柔软、蓬松和易染、易洗涤等先进性能充分展现出来,少量氨纶在内,增强PTT的回弹性,本发明利用PTT纤维比锦纶纤维更好的抗污染性,比尼龙更好的抗静电性,加上蓬松性、回弹性和染色性以及除防污性能好,易于染色、手感柔软、富有弹性,伸长率同氨纶纤维一样好的性能和氨纶按配比包覆制备麂皮绒,充分发挥两种纤维的优势,增加PTT纤维可以降低原料成本以及能耗等加工成本,添加氨纶则可以保证回弹性,织成麂皮绒则避免了薄型面料的劣势。

Description

四面弹力麂皮绒
技术领域
本发明涉及一种四面弹力麂皮绒,是一种高挡服装面料,属于纺织面料技术领域。
背景技术
随着生活水平的提高,人们对服装舒适性的要求越来越高,近两年采用氨纶、PA66等高弹丝弹性纤维的纺织品大受欢迎,这些纤维可以给服装面料带来良好的弹性舒适性能。与此同时,人们对麂皮绒、桃皮绒等服装、服饰、家纺面料也有了舒适度的更高要求。现有麂皮绒以氨纶为原料,但是,仅仅利用氨纶为原料进行麂皮绒的生产,不仅存在着原料价格过高和加工技术中的整形、印染成本较高等问题,而且在综合性能上也有不尽如人意的地方。
发明内容
本发明的目的是解决仅利用氨纶为原料进行麂皮绒生产,不仅存在着原料价格过高和加工技术中的整形、印染成本较高等问题,而且在综合性能上也有不尽如人意的地方等不足,提供一种弹力高,穿着舒适,综合性能好,可大幅度降低能耗和生产成本的四面弹力麂皮绒。
本发明的目的是通过以下技术方案实现的,一种四面弹力麂皮绒,包括经纱和纬纱,其特征是所述经纱和纬纱均采用氨纶为芯丝,作为经纱的氨纶芯丝以海岛丝为包丝、作为纬纱的氨纶芯丝以PTT聚酯为包丝的两种包覆丝织造。
所述的PTT聚酯为聚对苯二甲酸丙二醇酯,纬纱原料氨纶与PTT的质量配比为1∶3.8~4.2。
述的经纱原料氨纶与海岛丝的质量配比为1∶6~7.2。
本发明以氨纶作为芯丝,经纱是海岛丝包覆氨纶芯丝,纬纱是PTT包覆氨纶芯丝,PTT紧紧包覆氨纶,从而使PTT具有良好的拉伸与回复、柔软、蓬松和易染、易洗涤等先进性能充分展现出来。少量氨纶在内,增强PTT的回弹性。本发明利用PTT纤维、即聚对苯二甲酸丙二醇酯比锦纶纤维更好的抗污染性,比尼龙更好的抗静电性,加上蓬松性、回弹性和染色性以及除防污性能好,易于染色、手感柔软、富有弹性,伸长率同氨纶纤维一样好的性能,将聚对苯二甲酸丙二醇酯和氨纶按配比包覆丝制备麂皮绒,则可以充分发挥两种纤维的优势,增加PTT纤维可以降低原料成本以及能耗等加工成本,添加氨纶则可以保证回弹性,织成麂皮绒则避免了薄型面料的劣势。
本发明弹力高,穿着寿命长,具有抗皱性和耐化学性,不褪色,抗污染,易于洗涤干燥,在生产过程中可大幅度降低能耗,是一种高附加值、功能型环境友好型生态纺织产品,由于氨纶的生产成本较高,在长丝生产过程中会产生对人体皮肤有害的物质,因此,用PTT通力丝来替代部分氨纶制备包覆丝,具有非常重要的经济和环保价值。
本发明达到了人体适宜的最佳弹性,并具有柔软性、蓬松心、抗污性、低静电性和高弹性稳定,弹性回复指标的伸长率为10%,拉伸30次的弹性回复率达54.5%,优于同类氨纶产品27%的弹性回复率,染色温度为100℃,比采用PET等其它原料的麂皮绒产品低30-40℃,且染料耗量少、渗透性好,能量消耗小。色牢度:耐洗、耐汗渍(酸、碱)、耐水、耐摩擦达到4级,柔软的手感,良好的干爽性和新的悬垂性,悬垂性达30%。
具体实施方式
结合实施例进一步说明本发明,本发明的经纱和纬纱均采用氨纶为芯丝,经纱以海岛丝包覆氨纶芯丝,氨纶与海岛丝的质量配比为1∶6~7.2,增加海岛丝的弹性,纬纱以PTT聚酯包覆氨纶芯丝,氨纶与PTT聚酯的配比为质量1∶3.8~4.2,两种包覆丝织造四面弹力麂皮绒;所述的PTT聚酯为聚对苯二甲酸丙二醇酯。
PTT聚酯成为综合性能上超过尼龙的最新一代、最有前途的纤维材料之一。但PTT的弹性不如氨纶,仅为氨纶弹性的60%,而且目前的复丝细度也较粗,它的细度还远远没有达到氨纶丝的细度,故对开发薄型面料来说有一定难度。而氨纶不经过高温处理则弹性回复率较差,高温处理温度要求又较高。利用PTT和氨纶的各自特点,采用PTT和氨纶包覆丝技术制备麂皮绒,则可以充分发挥了两种纤维的优势,增加PTT纤维可以降低原料成本以及能耗等加工成本,添加氨纶则可以保证回弹性,织成麂皮绒则避免了薄型面料的劣势。
生产工艺流程是原材料→整经→浆纱→并轴→分绞→穿综→绕筘→织造→检验→入库。
1、原材料选用美国产的海岛丝、PTT聚酯和国产的氨纶涤纶丝。
2、整经,在日产津田驹整经机上整经,该设备可加工高密度类的产品,能在超高速的情况下整经机也能保持恒定的张力,就经丝与经丝之间张力几乎无差异,使整片经纱保持了恒定的张力。
3、织造,织造采用国际上最先进的日产ZAX-E型喷气织机,该种设备具有全电脑控制,自动化程度高,并能自动控制引纬送经量、布面质量,该设备有独特的拉伸、喷咀设计,适应弹性纤维生产要求,辅助喷咀技能保证织造的有效进行,而且能节能降耗。
4、后整理,机织布→退浆(德国THEN)→水洗→开幅→定型(德国MONFORTS)→磨毛(意大利LEFA)→染色→水洗→功能性整理。

Claims (3)

1.一种四面弹力麂皮绒,包括经纱和纬纱,其特征是所述经纱和纬纱均采用氨纶为芯丝,作为经纱的氨纶芯丝以海岛丝为包丝、作为纬纱的氨纶芯丝以PTT聚酯为包丝的两种包覆丝织造,。
2.根据权利要求1所述的四面弹力麂皮绒,其特征是所述的PTT聚酯为聚对苯二甲酸丙二醇酯,纬纱原料氨纶与PTT的质量配比为1∶3.8~4.2。
3.根据权利要求1所述的四面弹力麂皮绒,其特征是所述的经纱原料氨纶与海岛丝的质量配比为1∶6~7.2。
CNA2007101913708A 2007-12-17 2007-12-17 四面弹力麂皮绒 Pending CN101191273A (zh)