SU704746A1 - Method of electrospark trueing of grinding wheels - Google Patents

Method of electrospark trueing of grinding wheels

Info

Publication number
SU704746A1
SU704746A1 SU772480197A SU2480197A SU704746A1 SU 704746 A1 SU704746 A1 SU 704746A1 SU 772480197 A SU772480197 A SU 772480197A SU 2480197 A SU2480197 A SU 2480197A SU 704746 A1 SU704746 A1 SU 704746A1
Authority
SU
USSR - Soviet Union
Prior art keywords
trueing
electrospark
grinding wheels
grinding
editing
Prior art date
Application number
SU772480197A
Other languages
Russian (ru)
Inventor
Рафик Балабекович Мартиросян
Сергей Рубенович Маркарян
Рубен Ваганович Князян
Original Assignee
Ереванский политехнический институт им.К.Маркса
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ереванский политехнический институт им.К.Маркса filed Critical Ереванский политехнический институт им.К.Маркса
Priority to SU772480197A priority Critical patent/SU704746A1/en
Application granted granted Critical
Publication of SU704746A1 publication Critical patent/SU704746A1/en

Description

(54) СПОСОБ ЭЛЕКТРОЭРОЗИОННОЙ ПРАВКИ ШЛИФОВАЛЬНЫХ КРУГОВ(54) METHOD FOR ELECTROEROSION EDITION OF GRINDING GRAPES

ба; на фиг. 2 - узел 1 на фиг. 1 fe увеличенном масштабе; на фиг.З схема правки по данному способу.ba; in fig. 2 — node 1 in FIG. 1 fe on a larger scale; on fig.Z scheme edits in this way.

- инструмент 1 с нанесенным токонепровод щим покрытием 2 на вспомогательную обращенную к счлифоВсшьному кругу 3 поверхность установлен под углом -об к радиусу круга в точке касани  вершины токонепровод щего покрыти  с заправл емой поверхностью шлифовального круга. Диэлектрическую жидкость 4 через сопло 5 подают на вращающийс  шливофальный круг, В процессе правки по мере зерен электрод - инструмент подают вперед микрометрическим устройством б/ закрепленным на кожухе 7 Шлифовального станка. Электрод - инструмент и шлифовальный круг изолирован друг от друга.и подключены к :элёkтpoиcкpoвoмy ,генератору. Одно временно с электроискровой правкой происходит шлифование детали 8. - tool 1 with applied non-conductive coating 2 on the auxiliary surface facing to the grinding wheel 3 is set at an angle - to the radius of the circle at the point of contact of the top of the non-conductive coating with the surface of the grinding wheel. The dielectric fluid 4 is fed through a nozzle 5 to a rotating shlyofalny circle. During the editing process, as the grains, the tool serves forward with a micrometer device b fixed to the casing 7 of the Grinder. Electrode - the tool and the grinding wheel are isolated from each other. And connected to: electric generator, generator. Simultaneously with the electric spark editing, grinding of the part 8 takes place.

tt

Оптимальные результаты электроэрозионной правки достигаютс  при (. 30, при прочих равных параметрах правки. Уменьшение угла приводит к некоторому снижению производительности . процесса правки, а увеличение к снижению зерноудержани .Optimal EDM results are achieved at (. 30, all other parameters being equal. Editing results in a slight decrease in the productivity of the dressing process, and increases in grain retention.

Данный способ электроэрозионной правки позвол ет вскрывать зерна с особым расположением св зки вокруг Hftk: затылок на задней поверхностиThis method of electroerosive straightening makes it possible to open grains with a special arrangement of the ligament around Hftk: the back of the head on the back surface

зерна и лунка у передней поверхности .Затылок повышает жесткость закреп|лени  зерна, а лунка выполн ет роль стружечной канавки.the grain and the hole at the front surface. The nipple increases the stiffness of the grain, and the hole acts as a chip groove.

Применение насто щего способа электроэроэионной правки позвол ет снизить силы резани  при шлифовании правленным кругом соответственно в 1,3 и 1,1 раза и повысить стойкость шлифовальных кругов в 1,2 и 1,7 раза.The use of this method of electric power editing makes it possible to reduce cutting forces during grinding with a directed circle, respectively, 1.3 and 1.1 times and to increase the durability of grinding wheels by 1.2 and 1.7 times.

Claims (1)

1. Авторское свидетельство .СССР № 380425, кл. В 23 Р 1/12, 1971.1. Copyright certificate. USSR № 380425, cl. B 23 P 1/12, 1971. Фиг.1 Фиг.1Figure 1 figure 1
SU772480197A 1977-04-27 1977-04-27 Method of electrospark trueing of grinding wheels SU704746A1 (en)