SU542742A1 - Raw mix for portland cement clinker - Google Patents

Raw mix for portland cement clinker

Info

Publication number
SU542742A1
SU542742A1 SU2118912A SU2118912A SU542742A1 SU 542742 A1 SU542742 A1 SU 542742A1 SU 2118912 A SU2118912 A SU 2118912A SU 2118912 A SU2118912 A SU 2118912A SU 542742 A1 SU542742 A1 SU 542742A1
Authority
SU
USSR - Soviet Union
Prior art keywords
portland cement
cement clinker
raw mix
mix
raw
Prior art date
Application number
SU2118912A
Other languages
Russian (ru)
Inventor
Юрий Михайлович Бутт
Владимир Васильевич Тимашев
Владимир Леонтьевич Шестаков
Борис Владимирович Алексеев
Original Assignee
Московский Ордена Ленина И Ордена Трудового Красного Знамени Химикотехнологический Институт Им. Д.И. Менделеева
Сибирский Научно-Исследовательский И Проектный Институт Цементной Промышленности
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Московский Ордена Ленина И Ордена Трудового Красного Знамени Химикотехнологический Институт Им. Д.И. Менделеева, Сибирский Научно-Исследовательский И Проектный Институт Цементной Промышленности filed Critical Московский Ордена Ленина И Ордена Трудового Красного Знамени Химикотехнологический Институт Им. Д.И. Менделеева
Priority to SU2118912A priority Critical patent/SU542742A1/en
Application granted granted Critical
Publication of SU542742A1 publication Critical patent/SU542742A1/en

Description

глинистым и х елезосодержащии комтонеиты, отличающа с  тем, что, с целью повышеии  размолоспособности клинкера, она дополиительно Содержит двуокись титана, двуокись циркони  и борный ангидрид, при следующем соотнощении комтоиентов, вес. %:clayey and iron-containing comtonite, characterized in that, in order to increase the grindability of clinker, it additionally contains titanium dioxide, zirconium dioxide and boric anhydride, with the following ratio of components, %:

Известковый комиовент74-79Limy komiovent74-79

Глинистый компонент19-24Clay component19-24

ЖелезосодержащийIron-containing

компонент0,5-2component 0.5-2

0,,0 0,6-1,0 0.3-0,5.0, 0 0.6-1.0 0.3-0.5.

Источники информации, прин тые во внимание при экспертизе;Sources of information taken into account in the examination;

1.Авторское свидетельство СССР К 438623, кл. С 04В 7/38, 1972.1. USSR author's certificate K 438623, cl. C 04B 7/38, 1972.

2.Авторское свидетельство СССР № 342842, кл. С 04В 7/24, 1970.2. USSR author's certificate number 342842, cl. From 04B 7/24, 1970.

SU2118912A 1975-03-31 1975-03-31 Raw mix for portland cement clinker SU542742A1 (en)