SU531659A1 - Method for heat treatment of deformed alloys from nickel-based alloyed powders - Google Patents

Method for heat treatment of deformed alloys from nickel-based alloyed powders

Info

Publication number
SU531659A1
SU531659A1 SU2009395A SU2009395A SU531659A1 SU 531659 A1 SU531659 A1 SU 531659A1 SU 2009395 A SU2009395 A SU 2009395A SU 2009395 A SU2009395 A SU 2009395A SU 531659 A1 SU531659 A1 SU 531659A1
Authority
SU
USSR - Soviet Union
Prior art keywords
nickel
heat treatment
alloyed powders
based alloyed
alloys
Prior art date
Application number
SU2009395A
Other languages
Russian (ru)
Inventor
Олег Хикметович Фаткуллин
Генриэтта Сергеевна Крыкина
Николай Николаевич Журавлев
Фаина Львовна Гущина
Маргарита Дмитриевна Красавина
Original Assignee
Предприятие П/Я Г-4361
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я Г-4361 filed Critical Предприятие П/Я Г-4361
Priority to SU2009395A priority Critical patent/SU531659A1/en
Application granted granted Critical
Publication of SU531659A1 publication Critical patent/SU531659A1/en

Description

3 pOiBarfHbix оплааоБ из легиро.ва ных порош ков на основе ншкел , включающий закалку и ступенчатое старение, отличающийс  тем, что, с целью ловыщени  жаролрочности, закалку осуществл ют ступенчато, причем5 первую ступень закалки лравод т при темпе 4 ратуре 1200-1230° С, вторую - при 1100- 1120° С, .первую ступень старени  осущестзл ют Прм температуре 900-920° С, вторую - при 790-820° С с выдержкой на каждой ступени старени  2-3 ч, а охлаждение после каждой ступени провод т с печью.3 pOiBarfHbix opa-bB from nshkel-based alloyed powders, including quenching and step aging, characterized in that, in order to increase the heat resistance of the flares, the quenching is carried out stepwise, and the second at 1100-120 ° C; the first stage of aging is Prm at a temperature of 900-920 ° C; the second at 790-820 ° C with an exposure at each stage of aging 2-3 h, and cooling after each stage is carried out with a stove.

SU2009395A 1974-03-27 1974-03-27 Method for heat treatment of deformed alloys from nickel-based alloyed powders SU531659A1 (en)