SU1258328A3 - Коррозионностойка ферритна нержавеюща сталь - Google Patents

Коррозионностойка ферритна нержавеюща сталь Download PDF

Info

Publication number
SU1258328A3
SU1258328A3 SU2917251A SU2917251A SU1258328A3 SU 1258328 A3 SU1258328 A3 SU 1258328A3 SU 2917251 A SU2917251 A SU 2917251A SU 2917251 A SU2917251 A SU 2917251A SU 1258328 A3 SU1258328 A3 SU 1258328A3
Authority
SU
USSR - Soviet Union
Prior art keywords
nitrogen
carbon
stainless steel
niobium
titanium
Prior art date
Application number
SU2917251A
Other languages
English (en)
Inventor
Джон Никол Томас
Хьюмз Маккунн Томас
Original Assignee
Аллегени Ладлам Стил Корпорейшн (Фирма)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Аллегени Ладлам Стил Корпорейшн (Фирма) filed Critical Аллегени Ладлам Стил Корпорейшн (Фирма)
Application granted granted Critical
Publication of SU1258328A3 publication Critical patent/SU1258328A3/ru

Description

Изобретение относитс  к черной металлургии, в частности к ферритным нержавеющим стал м.
Целью изобретени   вл етс  снижение себестоимости получени  стали при суммарном содержании углерода и азота более 0,0275 мас,% и сохранение при этом высокой коррозионной стойкости и механических свойств.
Сталь получают путем аргонокисло- родного обезуглероживани  и примен ю дл  свариваемых деталей, имеющих ТОЛ1ЦИНУ не более 1,7В мм (предпочтительно не более 1,24 мм)j особенно дл  свариваемьк конденсаторных труб, толщина которых составл ет 0,66- 0,97 мм.
Редактор А.Лежнина Заказ 5044/60
Составитель В.Яковлев
Техред М.Ходан-ич Корректор А.Обручар
Тираж 567Подписное
ЕКНИПН Государственного комитета СССР
по делам изобретений и открытий 113035,, Москва, Ж-35, Раушска  наб., д. 4/5
11роизводственно-полиграфич - ское предпри тие, г.Ужгород, ул .Проектна , 4
Полученные слитки нагревают до 1125 С, в гор чем состо нии прокатывают на лист ТОЛ1ЦИНОЙ 3,18 мм, отжигают при 1060-1125 С, в холодном состо нии прокатывают на лист толщиной 1,57-1,65 мм и отжигают при 1060- 1125 С. Затем одни образцы подвергают испытаг:лю на стойкость против коррозии , а другие сваривают при помощи дуги вольфрамовым электродом
в среде инертного газа и испытывают на стойкость.
Испытанные образцы имеют свойст- ва, сходные со свойствами ферритной нержавеющей стали, полученной вакуумной плавкой.

Claims (1)

  1. КОРРОЗИОННО-СТОЙКАЯ ФЕРРИТНАЯ НЕРЖАВЕЮЩАЯ СТАЛЬ, содержащая хром, молибден, марганец, никель, кремний, алюминий, железо, а также углерод и азот и по крайней мере один компонент для стабилизации углерода и азота, выбранный из группы, включающей титан и ниобий, отличаю-
    щ а я с я тем, что, с целью сниже- ния себестоимости получения стали при суммарном содержании углерода и азота более 0, 0275 мас.% и сохранения при этом высокой коррозионной стойкости и механических свойств, стабилизирующие компоненты составляют % Ti % Nb б“- + 8~ =1,0-4,0(% С +% N) при следующем тов, мас.%: соотношении компонен- Хром 28,75-29,52 Молибден 4,00-4,20 Марганец 0,24-0,43 Никель 0,29-0,54 Кремний 0,28-0.45 s Алюминий 0,01-0,055 (/ Титан 0,19-0,66 Ниобий 0,32-0,53 Чмт Углерод 0,0301-0.0640 Азот '0,0201-0,0270 Железо Остальное ьс
    сл Q0 сэ ю Q0
SU2917251A 1980-01-03 1980-05-06 Коррозионностойка ферритна нержавеюща сталь SU1258328A3 (ru)