SE8008081L - ACID ZINC PLETING SOLUTIONS AND METHOD USING ETHOXILATED / PROPOXILATED MULTIPLE ALCOHOLS - Google Patents
ACID ZINC PLETING SOLUTIONS AND METHOD USING ETHOXILATED / PROPOXILATED MULTIPLE ALCOHOLSInfo
- Publication number
- SE8008081L SE8008081L SE8008081A SE8008081A SE8008081L SE 8008081 L SE8008081 L SE 8008081L SE 8008081 A SE8008081 A SE 8008081A SE 8008081 A SE8008081 A SE 8008081A SE 8008081 L SE8008081 L SE 8008081L
- Authority
- SE
- Sweden
- Prior art keywords
- solutions
- acid zinc
- propoxilated
- ethoxilated
- pleting
- Prior art date
Abstract
The problem of low "cloud point" and of foaming associated with the conventional grain-refining agents used in aqueous acid zinc electroplating solutions are reduced or avoided by employing as the grain- refining agent a polyhydric alcohol having three or more hydroxyl groups substituted with one or more oxyalkylene groups and which is soluble in the zinc plating solution. The use of these grain-refining agents also permits continuous operation at higher bath temperatures than is presently possible without deterioration or clouding of the plating solutions, and plating at lower temperatures than is presently possible.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US9548379A | 1979-11-19 | 1979-11-19 |
Publications (1)
Publication Number | Publication Date |
---|---|
SE8008081L true SE8008081L (en) | 1981-05-20 |
Family
ID=22252215
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SE8008081A SE8008081L (en) | 1979-11-19 | 1980-11-18 | ACID ZINC PLETING SOLUTIONS AND METHOD USING ETHOXILATED / PROPOXILATED MULTIPLE ALCOHOLS |
Country Status (10)
Country | Link |
---|---|
JP (1) | JPS5841357B2 (en) |
AU (1) | AU536353B2 (en) |
BE (1) | BE886216A (en) |
BR (1) | BR8007548A (en) |
CH (1) | CH647009A5 (en) |
ES (1) | ES496940A0 (en) |
FR (1) | FR2470169B1 (en) |
GB (1) | GB2064585B (en) |
IT (1) | IT1142191B (en) |
SE (1) | SE8008081L (en) |
Families Citing this family (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4515663A (en) * | 1984-01-09 | 1985-05-07 | Omi International Corporation | Acid zinc and zinc alloy electroplating solution and process |
IT1206252B (en) * | 1986-03-03 | 1989-04-14 | Omi Int Corp | ELECTROLYTE FOR THE ELECTRODEPOSITION OF ZINC ALLOYS |
GB2266894A (en) * | 1992-05-15 | 1993-11-17 | Zinex Corp | Modified tin brightener for tin-zinc alloy electroplating bath |
CN102471910B (en) * | 2009-07-30 | 2016-01-20 | 巴斯夫欧洲公司 | For the metal plating compositions comprising inhibitor that imporosity submicroscopic feature is filled |
US20110108115A1 (en) * | 2009-11-11 | 2011-05-12 | International Business Machines Corporation | Forming a Photovoltaic Device |
JP5552042B2 (en) | 2010-12-27 | 2014-07-16 | インターナショナル・ビジネス・マシーンズ・コーポレーション | Program analysis method, system and program |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB602591A (en) * | 1945-02-12 | 1948-05-31 | Du Pont | Improvements in or relating to the electro-deposition of metals |
GB895156A (en) * | 1959-03-19 | 1962-05-02 | Metal & Thermit Corp | Electrodeposition of copper |
JPS4840543B1 (en) * | 1970-04-24 | 1973-12-01 | ||
DE2160081A1 (en) * | 1970-12-03 | 1972-08-03 | Popescu geb. Micsunescu, Francine, Paris | Process for the production of brighteners for baths for electroplating, the brighteners thus obtained and baths for the use of these brighteners |
JPS5249297B2 (en) * | 1973-05-24 | 1977-12-16 |
-
1980
- 1980-11-14 GB GB8036594A patent/GB2064585B/en not_active Expired
- 1980-11-17 CH CH850380A patent/CH647009A5/en not_active IP Right Cessation
- 1980-11-18 SE SE8008081A patent/SE8008081L/en not_active Application Discontinuation
- 1980-11-18 BE BE2/58861A patent/BE886216A/en not_active IP Right Cessation
- 1980-11-18 ES ES496940A patent/ES496940A0/en active Granted
- 1980-11-18 AU AU64493/80A patent/AU536353B2/en not_active Ceased
- 1980-11-18 IT IT50187/80A patent/IT1142191B/en active
- 1980-11-19 JP JP55162102A patent/JPS5841357B2/en not_active Expired
- 1980-11-19 FR FR8024575A patent/FR2470169B1/en not_active Expired
- 1980-11-19 BR BR8007548A patent/BR8007548A/en not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
IT8050187A0 (en) | 1980-11-18 |
AU6449380A (en) | 1981-05-28 |
CH647009A5 (en) | 1984-12-28 |
GB2064585B (en) | 1983-11-09 |
FR2470169B1 (en) | 1985-09-27 |
ES8204769A1 (en) | 1982-05-01 |
ES496940A0 (en) | 1982-05-01 |
AU536353B2 (en) | 1984-05-03 |
BR8007548A (en) | 1981-06-02 |
JPS5841357B2 (en) | 1983-09-12 |
FR2470169A1 (en) | 1981-05-29 |
JPS5693889A (en) | 1981-07-29 |
GB2064585A (en) | 1981-06-17 |
BE886216A (en) | 1981-05-18 |
IT1142191B (en) | 1986-10-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES514752A0 (en) | "PROCEDURE TO INHIBIT THE DETERIORATION EFFECTS OF DISSOLVED OXYGEN CONTAINED IN AN AQUEOUS FLUID". | |
DE3575328D1 (en) | LIQUID SPACER COMPOSITION FOR CEMENTING A HOLE. | |
GR861438B (en) | Liquid detergent and decalcifying agents and method for their preparation | |
DE3582118D1 (en) | AQUEOUS EMULSION OF AN ACRYLIC ACID COPOLYMER. | |
BR8400691A (en) | APPLICATION OF ALCOHOLS, AS WELL AS HIGHLY VISCOSE TECHNICAL CONCENTRATES | |
SE7900619L (en) | METAL LUBRICANT | |
ES531995A0 (en) | PARENTERAL FORMULATION OF NIMODIPINE, A PROCEDURE FOR ITS PREPARATION, AS WELL AS ITS USE IN THE FIGHT AGAINST DISEASES | |
TR24208A (en) | BILHASSA USED IN COSMETIC PREPARATIONS - MAGA CUSTOMIZED WATER | |
DE59009494D1 (en) | Aqueous, storage stable, low foaming wetting agent. | |
IT7822831A0 (en) | IMPROVED KINETIC METHOD FOR THE DETERMINATION OF GLUCOSE CONCENTRATIONS WITH GLUCOSE DEHYDROGENASE. | |
SE8008081L (en) | ACID ZINC PLETING SOLUTIONS AND METHOD USING ETHOXILATED / PROPOXILATED MULTIPLE ALCOHOLS | |
DE3582755D1 (en) | METHOD FOR PRODUCING LOW SALT, LIQUID, AQUEOUS PREPARATIONS OF FIBER REACTIVE DYES. | |
ES2056957T3 (en) | USE OF POLYGLYCOLETERES AS FOAM INHIBITING ADDITIVES FOR CLEANING AGENTS. | |
DE3767920D1 (en) | METHOD FOR PRODUCING ALKYLOLIGOGLYCOSIDES. | |
ATE90217T1 (en) | LIQUID DEHALOGENING AGENTS. | |
JPS6438021A (en) | Non aqueous solution of doxorubicin hydrochloride | |
AU538612B2 (en) | Salt of furosemide or piretanide as acid component and penbutolol or (-)-3-(4-3-(3,4-dimethoxyphenylethylamino)-2- hydroxypropoxy)-phenyl)-crotonitrile as base component | |
NL7016694A (en) | Bath for electroplating bright nickel coat - ing | |
BR8305985A (en) | APPLICATION OF ORGANIC COMPOUNDS WITH LOW MOLECULAR WEIGHT AS WELL AS WATER CONCENTRATES OF HIGHLY VISCOSE TECHNICAL SURFACES | |
DK0431465T3 (en) | Aqueous dialysis and rinsing solution | |
RO93391A (en) | PROCEDURE FOR THE PREPARATION OF DOBUTAMINE DAMAGES | |
SE8700716L (en) | POLYOXYL-CYCLEED POLYHYDROXY COMPOUNDS ADDED IN ZINC ALLOY ELECTROLYTS | |
SE8006764L (en) | PREPARATION OF 2,5-DICETOGLUCONIC ACID | |
FI873483A (en) | OXIRANPSEUDOOLIGOSACKARIDER, FOERFARANDE FOER DERAS FRAMSTAELLNING, DERAS ANVAENDNING OCH PHARMACEUTISKA PREPARAT. | |
JPS53103936A (en) | Electroplating solution |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
NAV | Patent application has lapsed |
Ref document number: 8008081-5 Effective date: 19870212 |