PH12018501689B1 - Sulfuration treatment method, sulfide production method, and hydrometallurgical process for nickel oxide ore - Google Patents
Sulfuration treatment method, sulfide production method, and hydrometallurgical process for nickel oxide oreInfo
- Publication number
- PH12018501689B1 PH12018501689B1 PH12018501689A PH12018501689A PH12018501689B1 PH 12018501689 B1 PH12018501689 B1 PH 12018501689B1 PH 12018501689 A PH12018501689 A PH 12018501689A PH 12018501689 A PH12018501689 A PH 12018501689A PH 12018501689 B1 PH12018501689 B1 PH 12018501689B1
- Authority
- PH
- Philippines
- Prior art keywords
- sulfuric acid
- acidic solution
- acid acidic
- added
- nickel
- Prior art date
Abstract
Provided is a method with which it is possible, when causing a sulfuration reaction to occur from a sulfuric acid acidic solution containing at least nickel through use of a sulfuration agent and generating a nickel sulfide, to suitably control the grain size of the generated sulfide while maintaining high reaction efficiency. The sulfuration treatment method according to the present invention comprises supplying a sulfuric acid acidic solution that contains nickel to a reactor, adding hydrogen sulfide gas to the sulfuric acid acidic solution, and generating nickel sulfide, wherein unreacted gas among the hydrogen sulfide gas added to the sulfuric acid acidic solution is recovered, sodium hydroxide is added to the recovered hydrogen sulfide gas, sodium hydrosulfide is generated, and the resulting solution of sodium hydrosulfide is added to sulfuric acid acidic solution. At this time, when the sodium hydrosulfide solution is added, the grain size of the generated nickel sulfide is set to 50 æm or higher by 50 pcnt particle size (D50) by controlling the amount of sodium hydrosulfide solution added to the reactor to which the sulfuric acid acidic solution is supplied.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2016024712A JP6213586B2 (en) | 2016-02-12 | 2016-02-12 | Sulfidation treatment method, sulfide production method, and nickel oxide ore hydrometallurgy method |
PCT/JP2017/003684 WO2017138421A1 (en) | 2016-02-12 | 2017-02-02 | Sulfuration treatment method, sulfide production method, and wet smelting method for nickel oxide ore |
Publications (2)
Publication Number | Publication Date |
---|---|
PH12018501689A1 PH12018501689A1 (en) | 2019-05-27 |
PH12018501689B1 true PH12018501689B1 (en) | 2019-05-27 |
Family
ID=59563555
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PH12018501689A PH12018501689B1 (en) | 2016-02-12 | 2018-08-08 | Sulfuration treatment method, sulfide production method, and hydrometallurgical process for nickel oxide ore |
Country Status (5)
Country | Link |
---|---|
JP (1) | JP6213586B2 (en) |
AU (1) | AU2017218246B2 (en) |
CU (1) | CU20180089A7 (en) |
PH (1) | PH12018501689B1 (en) |
WO (1) | WO2017138421A1 (en) |
Families Citing this family (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP6747620B2 (en) * | 2018-03-07 | 2020-08-26 | 住友金属鉱山株式会社 | Ni/Co sulfide manufacturing method and iron quality stabilizing system |
JP7035735B2 (en) * | 2018-04-03 | 2022-03-15 | 住友金属鉱山株式会社 | Method for producing nickel-cobalt mixed sulfide from low nickel grade oxide ore |
JP7196630B2 (en) * | 2019-01-22 | 2022-12-27 | 住友金属鉱山株式会社 | Method and equipment for recovering valuable metals from aqueous sulfuric acid solution |
CN110127629B (en) * | 2019-04-25 | 2020-11-17 | 南京聚拓化工科技有限公司 | Device and process for preparing sulfuric acid from sulfide by wet process |
JP7293873B2 (en) * | 2019-05-30 | 2023-06-20 | 住友金属鉱山株式会社 | Method for producing nickel sulfide, hydrometallurgical method for nickel oxide ore |
JP7355186B1 (en) | 2022-08-29 | 2023-10-03 | 住友金属鉱山株式会社 | Particle size control method for nickel-cobalt mixed sulfide |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP5506136B2 (en) * | 2006-12-25 | 2014-05-28 | 住友金属鉱山株式会社 | Method for chlorine leaching of mixed sulfides containing nickel and cobalt |
JP5435058B2 (en) * | 2012-03-06 | 2014-03-05 | 住友金属鉱山株式会社 | Neutralization treatment method and neutralization treatment plant |
JP5807689B2 (en) * | 2014-01-28 | 2015-11-10 | 住友金属鉱山株式会社 | Sulfide production equipment and method |
-
2016
- 2016-02-12 JP JP2016024712A patent/JP6213586B2/en active Active
-
2017
- 2017-02-02 WO PCT/JP2017/003684 patent/WO2017138421A1/en active Application Filing
- 2017-02-02 AU AU2017218246A patent/AU2017218246B2/en active Active
- 2017-02-02 CU CUP2018000089A patent/CU20180089A7/en unknown
-
2018
- 2018-08-08 PH PH12018501689A patent/PH12018501689B1/en unknown
Also Published As
Publication number | Publication date |
---|---|
WO2017138421A1 (en) | 2017-08-17 |
JP6213586B2 (en) | 2017-10-18 |
CU20180089A7 (en) | 2018-10-04 |
PH12018501689A1 (en) | 2019-05-27 |
AU2017218246B2 (en) | 2019-01-31 |
JP2017141499A (en) | 2017-08-17 |
AU2017218246A1 (en) | 2018-08-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
PH12018501689A1 (en) | Sulfuration treatment method, sulfide production method, and hydrometallurgical process for nickel oxide ore | |
MX2017009005A (en) | An electrochemical process for preparing a compound comprising a metal or metalloid and a peroxide, ionic or radical species. | |
MX2016008349A (en) | Process for recycling li-ion batteries. | |
CU24633B1 (en) | METHOD FOR EFFICIENTLY RECOVERING IRON, SCANDIUM AND ALUMINUM FROM A LATERITE-NICKEL LIMONITE MINERAL | |
MX2019008901A (en) | Highly reactive, dust-free and free-flowing lithium sulphide and method for the production thereof. | |
JO3218B1 (en) | Production of high purity precipitated calcium carbonate | |
PH12016501637A1 (en) | Method for producing nickel powder | |
MX2023008385A (en) | Methods and apparatuses for production of carbon, carbide electrodes, and carbon compositions. | |
PH12019501841A1 (en) | Method for producing sulfide, and method for hydrometallurgically refining nickle oxide ore | |
PH12017501778A1 (en) | Method for manufacturing nickel and cobalt mixed sulfide and nickel oxide ore hydrometallurgical method | |
FI20175928A1 (en) | Process for recovering components from pickling acid residue | |
PH12017500172A1 (en) | Method for producing pellets and method for producing iron-nickel alloy | |
MY187291A (en) | Process for the production of copper sulfide | |
WO2016048709A3 (en) | Method for reducing iron oxide to metallic iron using coke oven gas | |
PH12016501890A1 (en) | Method for producing nickel powder | |
PH12017501317A1 (en) | Method for producing nickel powder | |
PH12018500427A1 (en) | Scandium oxide manufacturing method | |
PH12017501582A1 (en) | Method for producing nickel sulfide and hydromettalurgical method for nickel oxide ore | |
PH12018500584A1 (en) | Method for manufacturing nickel powder, and method for operating reaction facility | |
EA033556B1 (en) | Method of producing carbon-coated lithium transition metal phosphates | |
PH12020500468A1 (en) | Leaching treatment method and hydrometallurgical method for nickel oxide ore | |
CN104674018A (en) | Method for chemical copper removal of wet lead | |
CL2015003082A1 (en) | Hydrometallurgical process for leaching of copper ores and products containing them, and reactive mixture used in it | |
MY188939A (en) | Recycling process of wastewater containing ammonium ion and preparation method of metal oxide | |
PH12018501872A1 (en) | Method for producing nickel powder |