MY137675A - Control of hot rolled product cross section under localized temperature disturbances - Google Patents

Control of hot rolled product cross section under localized temperature disturbances

Info

Publication number
MY137675A
MY137675A MYPI20061814A MY137675A MY 137675 A MY137675 A MY 137675A MY PI20061814 A MYPI20061814 A MY PI20061814A MY 137675 A MY137675 A MY 137675A
Authority
MY
Malaysia
Prior art keywords
weld joint
roll
control
hot rolled
rolled product
Prior art date
Application number
Inventor
Pong David Teng
Maylor Thomas George
Raftsjo Erik Mats
Original Assignee
Pong David Teng
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Pong David Teng filed Critical Pong David Teng
Priority to MYPI20061814 priority Critical patent/MY137675A/en
Publication of MY137675A publication Critical patent/MY137675A/en

Abstract

A METHOD OF ROLLING A CONTINUOUS WELDED BILLET HAVING WELD JOINTS AT SUCCESSIVE LOCATIONS ALONG THE BILLET AND WHEREIN THE CONTINUOUS WELDED BILLET IS ADVANCED THROUGH ROLL PAIRS OF SUCCESSIVE ROLL STANDS. THE ROLLING CONDITIONS IN TWO SUCCESSIVE STANDS ARE ADJUSTED SO THAT WHEN A WELD JOINT IS BETWEEN THE TWO STANDS COMPRESSION IS PRODUCED AT THE WELD JOINT CAUSING AN INCREASE OF CROSS-SECTIONAL AREA AT THE WELD JOINT; THE ROLLING CONDITION INVOLVES SUPERIMPOSING AN INCREASE IN ROLL SPEED IN THE UPSTREAM ROLL STAND COMPARED TO THE DOWNSTREAM ROLL STAND BASED ON TRACKING INFORMATION OF THE WELD JOINT.
MYPI20061814 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances MY137675A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Publications (1)

Publication Number Publication Date
MY137675A true MY137675A (en) 2009-02-27

Family

ID=45689176

Family Applications (1)

Application Number Title Priority Date Filing Date
MYPI20061814 MY137675A (en) 2006-04-20 2006-04-20 Control of hot rolled product cross section under localized temperature disturbances

Country Status (1)

Country Link
MY (1) MY137675A (en)

Similar Documents

Publication Publication Date Title
HK1094555A1 (en) Control of hot rolled product cross section under localized temperature disturbances
CN104874606B (en) The production method of high chromium content ferrite stainless steel seamless steel pipe
MY180966A (en) Winding/unwinding device and method for winding/unwinding a metal product in a rolling line
WO2012013456A3 (en) Apparatus and method for production of metal elongated products.
US5720196A (en) Hot-rolling method of steel piece joint during continuous hot-rolling
WO2011018217A3 (en) Device and method for producing a thin hot-rolled strip
MX341910B (en) Method for producing rolling stock by means of a combined continuous casting and rolling system, control device for a combined continuous casting and rolling system, and combined continuous casting and rolling system.
CA2651739A1 (en) Method and device for producing a metal strip by continuous casting
EP1479457A4 (en) Method of manufacturing seamless steel pipe
MY137675A (en) Control of hot rolled product cross section under localized temperature disturbances
ZA200005828B (en) Process for reducing the scrap length during the rolling of metal bands joined together by means of welded seams and tandem train for implementation of the process.
MX2010001998A (en) Economic secondary descaling.
TW200722749A (en) Device for the ultrasonic testing of hot rolled material
WO2011030273A3 (en) Plant for rolling tubes
CN109092902A (en) The first rolling mill is prevented to sting the milling method of steel skidding
Morioka et al. Development of manufacturing technology for high alloy steel seamless pipe by Mannesmann process
WO2008142803A1 (en) Method, and apparatus, for piercing and rolling seamless pipe
WO2010066230A3 (en) Method for producing seamless tubes by means of a three-roll bar rolling mill
WO2009146676A3 (en) Method and device for continuous joining
Kleiner et al. Die-less forming of sheet metal parts
UA92241C2 (en) Method of continuous longitudinal rolling of pipes in multiple-stand mill on mandrel
UA82972C2 (en) Method of plugless continuous longitudinal rolling of pipes in multistand mill
Morioka et al. Development of manufacturing technology for high alloy steel seamless pipe by Mannesmann process
RU2006108529A (en) METHOD FOR LUBRICATION OF ROLLED MATERIAL
RU2438808C2 (en) Method of tube rolling on mandrel