KR960021288A - 제강용 티밍 래들 - Google Patents

제강용 티밍 래들 Download PDF

Info

Publication number
KR960021288A
KR960021288A KR1019940034162A KR19940034162A KR960021288A KR 960021288 A KR960021288 A KR 960021288A KR 1019940034162 A KR1019940034162 A KR 1019940034162A KR 19940034162 A KR19940034162 A KR 19940034162A KR 960021288 A KR960021288 A KR 960021288A
Authority
KR
South Korea
Prior art keywords
steelmaking
slag
ladle
life
timing
Prior art date
Application number
KR1019940034162A
Other languages
English (en)
Other versions
KR0135350B1 (ko
Inventor
이상완
이상욱
Original Assignee
김만제
포항종합제철 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김만제, 포항종합제철 주식회사 filed Critical 김만제
Priority to KR1019940034162A priority Critical patent/KR0135350B1/ko
Publication of KR960021288A publication Critical patent/KR960021288A/ko
Application granted granted Critical
Publication of KR0135350B1 publication Critical patent/KR0135350B1/ko

Abstract

제강용 티밍 래들을 계속 사용시 슬래그(S)의 위치가 하향됨으로써 프리보드(53)가 공기중에 노출되면 산화가 급격히 진행됨으로써 프리보드(53)의 수명이 감소되고 이로 인하여 티밍 래들 전체의 수명이 감소됨을 방지하기 위하여, 슬래그(S)에 의한 침식을 균일하게 하기 위하여 테이퍼부(1)가 형성됨가 아울러 각각 탄소함량이 2~10%와 15~25%인 제1, 2내화물(2)(3)이 테이퍼부(1)를 통해 결합된 상태로 슬래그(s)가 접촉되는 부분을 형성함으로써 제강용 티밍 래들의 수명이 향상된다.

Description

제강용 티밍 래들
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 본 발명에 따른 제강용 티밍 래들을 도시한 부분 확대도,
제2도는 본 발명에 따른 제강용 티밍 래들의 용손상태를 도시한 상태도.

Claims (2)

  1. 제강용 티밍 래들에 있어서, 슬래그(S)에 의한 침식을 균일하게 하기 위하여 티밍 래들에 용강을 최초 수강 시와 최후 수강 시의 연장선에 해당하는 데이퍼부(1)가 형성됨과 아울러 각각 탄소 함량이 2~10%와 15~25%인 제1, 2내화물(2)(3)이 테이퍼부(1)를 통해 결합된 상태로 슬래그(S)가 접촉되는 부분을 형성함을 특징으로 하는 제강용 티밍 래들.
  2. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019940034162A 1994-12-14 1994-12-14 슬래그 라인용 벽체 라이닝 구조를 가진 제강용 티밍 래들 KR0135350B1 (ko)