KR920012547A - Manufacturing method of ultra low shrink polyester - Google Patents

Manufacturing method of ultra low shrink polyester Download PDF

Info

Publication number
KR920012547A
KR920012547A KR1019900022538A KR900022538A KR920012547A KR 920012547 A KR920012547 A KR 920012547A KR 1019900022538 A KR1019900022538 A KR 1019900022538A KR 900022538 A KR900022538 A KR 900022538A KR 920012547 A KR920012547 A KR 920012547A
Authority
KR
South Korea
Prior art keywords
manufacturing
ultra low
low shrink
shrink polyester
polyester
Prior art date
Application number
KR1019900022538A
Other languages
Korean (ko)
Inventor
박종식
서종원
최수명
Original Assignee
공정곤
동양나이론 주식회사
배도
동양 폴리에스터 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 공정곤, 동양나이론 주식회사, 배도, 동양 폴리에스터 주식회사 filed Critical 공정곤
Priority to KR1019900022538A priority Critical patent/KR920012547A/en
Publication of KR920012547A publication Critical patent/KR920012547A/en

Abstract

내용 없음No content

Description

초저수축성 폴리에스터 사의 제조방법Manufacturing method of ultra low shrink polyester

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

Claims (1)

극한점도 0.62의 폴리에스터 중합물을 방사속도 7,000m/분 이상으로 고속방사하여 오일링한 다음, 제 1 고뎃로울러와 제 2 고뎃로울러 사이에서 1-1.5%의 오버피드를 주어 190℃ 이상 230℃ 미만으로 스팀열처리 하는 것을 특징으로 하는 저수축 폴리에스테르 필라멘트사의 제조방법.Oiling the polyester polymer with an ultimate viscosity of 0.62 at a spinning speed of 7,000 m / min or more at high speed, and then giving an overfeed of 1-1.5% between the first and second high rollers, and the temperature is 190 ° C. or more and less than 230 ° C. Process for producing low-shrink polyester filament yarn, characterized in that the steam heat treatment. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019900022538A 1990-12-29 1990-12-29 Manufacturing method of ultra low shrink polyester KR920012547A (en)