포리졸 접착제Polyazole adhesive
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
포리비닐알콜(PVA)와 물을 용해하여 온도 조절 탱크에서 촉매와 반응하고 초산비닐단량체(CH2=COHCOCH3)와 유화제를 반응하여 중합반응 시킨다. 이때 중요한 것은 시간과 온도의 조절에 있다. 중합반응 시킬때 반드시 진공펌프와 진공 보조탱크를 설치한다.Polyvinyl alcohol (PVA) and water are dissolved to react with the catalyst in a temperature control tank, and the vinyl acetate monomer (CH2 = COHCOCH3) is reacted with an emulsifier to polymerize. The important thing here is to control the time and temperature. When the polymerization reaction is carried out, a vacuum pump and a vacuum auxiliary tank must be installed.
Claims (1)
본문에서 상술한 바와 같이 PVA 용액과 물에 대한 비율 PVA 용액 10% 물 90%첨가. 반응시간과 온도를 조절하여 촉미제(과산화 벤조일)과 초산비닐 모노마를 첨가 반응시켜 포리졸의 제조 방법 및 그 조성물.Add PVA solution 10% water 90% water to PVA solution and water as described above in the text. A method for producing a polyazole and a composition thereof by controlling a reaction time and temperature to add and react a stimulant (benzoyl peroxide) with vinyl monoma acetate.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.