KR870001130A - 기포 콘크리트의 충전재의 제조방법 - Google Patents

기포 콘크리트의 충전재의 제조방법 Download PDF

Info

Publication number
KR870001130A
KR870001130A KR1019850005256A KR850005256A KR870001130A KR 870001130 A KR870001130 A KR 870001130A KR 1019850005256 A KR1019850005256 A KR 1019850005256A KR 850005256 A KR850005256 A KR 850005256A KR 870001130 A KR870001130 A KR 870001130A
Authority
KR
South Korea
Prior art keywords
filler
crushed
manufacturing
foam concrete
metros
Prior art date
Application number
KR1019850005256A
Other languages
English (en)
Inventor
이철제
Original Assignee
이철제
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이철제 filed Critical 이철제
Priority to KR1019850005256A priority Critical patent/KR870001130A/ko
Publication of KR870001130A publication Critical patent/KR870001130A/ko

Abstract

내용 없음.

Description

기포 콘크리트의 충전재의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (3)

  1. 플라이애쉬와 100-120메쉬로 분쇄된 규사와 소석회를 혼합하고 이에 식물성레진을 100-120메쉬로 분쇄하여 메트로스, 폴티비닐알콜, 소듐라오릴썰페이드를 혼합하여 첨가하는 것을 특징으로 하는 기포 콘크리트의 충전재의 제조방법.
  2. 정구범위 제1항에 있어서 발포스치로폴입자 또는 발포스치로폴을 파쇄하여 배합하는 것.
  3. 청구범위 제1항 및 제2항에 있어서 식물성 레진, 메트로스, 폴리비닐알콜, 소듐라오릴썰페이드의 배합을 8:1:2:1로 하여 이에 70%의 물을 투입 60-70℃로 가열한 것을 파쇄스치로폴에 도포하는 것.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019850005256A 1985-07-23 1985-07-23 기포 콘크리트의 충전재의 제조방법 KR870001130A (ko)