KR20110119130A - Capacitive overlay touch screen panel integrated with window and mathod for manufacturing there of - Google Patents

Capacitive overlay touch screen panel integrated with window and mathod for manufacturing there of Download PDF

Info

Publication number
KR20110119130A
KR20110119130A KR1020100038644A KR20100038644A KR20110119130A KR 20110119130 A KR20110119130 A KR 20110119130A KR 1020100038644 A KR1020100038644 A KR 1020100038644A KR 20100038644 A KR20100038644 A KR 20100038644A KR 20110119130 A KR20110119130 A KR 20110119130A
Authority
KR
South Korea
Prior art keywords
pattern layer
conductive
window
electrode pattern
forming
Prior art date
Application number
KR1020100038644A
Other languages
Korean (ko)
Other versions
KR101133967B1 (en
Inventor
조동현
최원영
남영구
강용재
Original Assignee
주식회사 모린스
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 모린스 filed Critical 주식회사 모린스
Priority to KR1020100038644A priority Critical patent/KR101133967B1/en
Publication of KR20110119130A publication Critical patent/KR20110119130A/en
Application granted granted Critical
Publication of KR101133967B1 publication Critical patent/KR101133967B1/en

Abstract

PURPOSE: A window integrated capacitive overlay touch screen panel and a method for manufacturing the same are provided to improve the productivity by simplifying the manufacturing process. CONSTITUTION: A transparent conductive electrode pattern(20) is arranged on the upper part of a window panel substrate and the window area. A non-conductive color pattern(30) arranged in the edge part of the substrate divides the window area. A metal electrode pattern arranged on the edge part of the substrate divides the window area on the conductive electrode pattern layer and the insulation pattern layer. An insulating layer pattern layer(50) is arranged by remaining a bonding area of an FPCB(Flexible Printed Circuit Board)(60) on the upper part of the metal electrode pattern layer.

Description

윈도우 일체형 정전용량방식 터치스크린 패널 및 그 제조방법{CAPACITIVE OVERLAY TOUCH SCREEN PANEL INTEGRATED WITH WINDOW AND MATHOD FOR MANUFACTURING THERE OF}CAPACITIVE OVERLAY TOUCH SCREEN PANEL INTEGRATED WITH WINDOW AND MATHOD FOR MANUFACTURING THERE OF

본 발명은 윈도우 일체형 정전용량방식 터치스크린 패널 및 그 제조방법에 관한 것으로, 더욱 상세하게는 윈도우 패널 기판에 ITO층의 증착과 패터닝 및 컬러층의 인쇄와 패터닝의 순으로 공정을 거쳐 적층을 형성시킴으로써, ITO층의 저항을 낮추고, 투명도를 높여 센싱감도와 광 특성을 향상시킨 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널 및 그 제조방법에 관한 것이다.
The present invention relates to a window-integrated capacitive touch screen panel and a method of manufacturing the same. More particularly, the present invention relates to a window panel substrate in which a laminate is formed through a process of deposition and patterning of an ITO layer and printing and patterning of a color layer. The present invention relates to a window integrated capacitive touch screen panel characterized by lowering resistance of the ITO layer and increasing transparency to improve sensing sensitivity and optical characteristics.

일반적으로 터치스크린은 저항막(Resistive)방식, 정전용량(Capacitive)방식, 초음파(SAW)방식, 적외선(IR)방식 등과 같이 다양한 방식들이 적용되고 있으며, 이러한 방식들 중에서 저항막방식, 정전용량방식이 가장 널리 적용되고 있다.
In general, various types of touch screens are applied, such as resistive, capacitive, ultrasonic (SAW), and infrared (IR) methods. Among these methods, resistive, capacitive, and the like are used. This is most widely applied.

저랑막 방식은 투명전극이 코팅되어 있는 두 장의 기판을 합착시킨 구조로서, 손가락 등의 압력을 가해 상부와 하부의 전극층이 서로 접촉되면, 전기적 신호가 발생되어 위치를 인지하는 방식으로 정확도가 높고, 소형화에 유리하고 가격이 저렴한 장점이 있는 반면에 제작하기가 어려운 문제점이 있다. 또한 정전용량방식은 사람의 몸에서 발생하는 정전기를 감지해 구동하는 방식으로, 내구성이 강하고, 반응시간이 짧고, 투과성이 좋은 반면 가격이 높은 것이 단점이지만, 정전용량방식이 저항막 방식에 비해 투과율이 우수하고, 동시에 두 곳이상을 인식하는 멀티터치 기능을 갖춰 빠르게 확산될 것으로 전망되고, 근래 애플의 아이폰이 정전용량 방식 터치스크린 패널을 휴대폰에 채용하기 시작하면서 이 방식을 채택하는 시장이 급성장할 것으로 기대되고 있다.
The mezzanine method is a structure in which two substrates coated with a transparent electrode are bonded together, and when the upper and lower electrode layers contact each other by applying pressure such as a finger, an electrical signal is generated to recognize the position, and thus the accuracy is high. While it is advantageous in miniaturization and low cost, there is a problem that is difficult to manufacture. In addition, the capacitive method is a method of sensing and driving static electricity generated in a human body, which is disadvantageous in terms of durability, short reaction time, and good permeability, but high price, but the capacitance method has a higher transmittance than a resistive film method. It is expected to spread rapidly with its excellent and multi-touch function that recognizes more than one place at the same time. As Apple's iPhone began to adopt capacitive touch screen panels in mobile phones, the market adopting this method will grow rapidly. It is expected to be.

정전용량방식을 채택하는 터치스크린 패널의 특허출원된 내용들을 살펴보면, 국내 등록특허공보 제 10-0942763호는 도 1에 도시된 바와 같이 윈도우 패널(211)과 윈도우 패널(211)의 하부에 부착된 정전용량방식 터치센서(220)를 포함하는 종래의 터치스크린 패널(200)로서, 상기 정전용량방식 터치센서(220)이 유리 또는 PET 필름 기판(216)[도 1(a)]의 상부면에 인듐주석산화물(ITO) 등을 증착하여 투명한 도전성 막(215)을 코팅[도 1(b)]한 다음 포토리소그래피 공정 등을 이용하여 전극 패턴(215)을 형성[도 1(c)]한 후, 투명한 전극 패턴과 전기적으로 연결하기 위한 도전성 회로 배선(214)을 도포[도 1(d)]한 다음 접착제(213, PSA, Pressure Sensitive Adhesive)를 도포[도 1(e)]하고, FPC(218)를 이방 도전성 필름(ACF, anisotropic conductive film)으로 도전성 배선 패턴(214)의 단부에 연결[도 1(f)]한 다음 상기와 같은 과정을 거쳐 제조된 정전용량방식 터치센서(220)를 장식층(212)이 인쇄된 윈도우 패널(211)과 합착하여 제조한 터치스크린 패널(200)[도 1(i)]이 알려져 있지만 상기와 같은 터치스크린 패널(200)은 불투명한 장식층(212)이 형성된 윈도우 패널(211)[도 1(g)][도 1(h)]과 정전용량방식 터치센서(220)를 합착하기 위해 접착제를 도포하여야 하고, 터치센서를 윈도우 패널에 부착시 발생하는 기포 발생이나 이물 혼입과, 합착 과정에서 발생되는 정렬 불량 등의 문제점들을 지적한 바 있다.
Looking at the patent applications of the touch screen panel adopting the capacitive method, Korean Patent Publication No. 10-0942763 is attached to the window panel 211 and the lower portion of the window panel 211 as shown in FIG. A conventional touch screen panel 200 including a capacitive touch sensor 220, wherein the capacitive touch sensor 220 is on the upper surface of the glass or PET film substrate 216 (FIG. 1 (a)). After depositing indium tin oxide (ITO) or the like to coat the transparent conductive film 215 [FIG. 1 (b)], and then forming the electrode pattern 215 using a photolithography process [FIG. 1 (c)], A conductive circuit wiring 214 for electrically connecting with the transparent electrode pattern (FIG. 1 (d)), followed by an adhesive 213 (PSA, Pressure Sensitive Adhesive) [FIG. 1 (e)], and an FPC ( 218 is connected to an end of the conductive wiring pattern 214 with an anisotropic conductive film (ACF) (Fig. 1 (f)). Next, the touch screen panel 200 (FIG. 1 (i)) manufactured by bonding the capacitive touch sensor 220 manufactured by the above process to the window panel 211 on which the decorative layer 212 is printed is manufactured. Although known, the touch screen panel 200 may include the window panel 211 (FIG. 1 (g)] [FIG. 1 (h)) and the capacitive touch sensor 220 in which an opaque decorative layer 212 is formed. In order to adhere, adhesives have to be applied, and problems such as bubble generation or foreign matter mixing when the touch sensor is attached to the window panel, and misalignment occurring during the bonding process have been pointed out.

따라서, 국내 등록특허공보 제 10-0942763호는 상기한 바와 같은 문제점들을 개선하기 위한 방안으로 도 2에 도시된 바와 같이, 투명한 재질의 윈도우 패널 기판(311)과, 상기 기판에 투명한 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 비도전성 불투명 장식층(312)과, 상기 기판의 윈도우부(WA)와 장식층의 상부에 걸쳐서 배치된 ITO 등을 이용한 투명한 도전성 전극 패턴층(313)과, 상기 투명한 도전성 전극 패턴층(313)의 상부 테두리부에 배치된 도전성 회로 배선층(314)을 포함하고, 상기 투명한 도전성 전극 패턴층(313)의 상부에 배치된 반사 방지층(315)과, 상기 반사 방지층(315)의 상부에 배치된 비산방지층(316)을 더 포함하는 것을 특징으로 하는 윈도우 패널 일체형 정전용량방식 터치 센서을 제안한 바 있지만, 도 2에 도시된 바와 같은 윈도우 패널 일체형 정전용량방식 터치 센서는 도전성 전극 패턴층(313)을 형성시킬 때 보다 나은 특성을 얻기 위하여 ITO 증착시에 250℃ 이상의 높은 열을 가하게 되면, ITO 증착층 내부에 형성된 불투명 장식층(312)이 고온의 열에 의해 용해되면서 ITO 패턴층의 전기적, 광학적 특성에 손상이 가는 것은 물론이고 외부 디자인을 손상시켜 제품으로서의 가치를 상실하게 된다.
Accordingly, Korean Patent Publication No. 10-0942763 discloses a window panel substrate 311 made of a transparent material and a transparent window portion WA on the substrate, as shown in FIG. 2 as a method for improving the above problems. ) Is a transparent conductive electrode using a non-conductive opaque decorative layer 312 disposed on one side edge portion E of the substrate, and ITO or the like disposed over the window portion WA and the decorative layer of the substrate. An anti-reflective layer including a pattern layer 313 and a conductive circuit wiring layer 314 disposed on an upper edge portion of the transparent conductive electrode pattern layer 313 and disposed on the transparent conductive electrode pattern layer 313. 315 and a window panel-integrated capacitive touch sensor, which further includes a scattering prevention layer 316 disposed on the anti-reflection layer 315, have been proposed. The right panel integrated capacitive touch sensor has an opaque decorative layer 312 formed inside the ITO deposition layer when high heat of 250 ° C. or higher is applied during ITO deposition to obtain better characteristics when forming the conductive electrode pattern layer 313. ) Dissolves due to high temperature heat and damages the electrical and optical properties of the ITO pattern layer as well as damages the external design and loses its value as a product.

따라서, 상기와 같은 문제점을 해결하기 위한 방안으로 본 발명은 종래의 정전용량방식 터치스크린 패널이 패널 기판에 컬러 패턴층을 형성시킨 다음 ITO층을 증착시키는 것과는 달리 패널 기판에 ITO를 증착시킨 다음 컬러 패턴층을 형성시킴으로써, 기판에 ITO의 증착시에 250℃ 이상의 높은 열을 가하여 ITO의 증착특성을 향상시켜 투과율을 높여 센싱감도와 광 특성을 향상시킨 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널 및 그 제조방법을 제공함을 과제로 한다.
Therefore, in order to solve the above problems, the present invention is different from the conventional capacitive touch screen panel that forms a color pattern layer on a panel substrate and then deposits an ITO layer on the panel substrate, and then color By forming a pattern layer, a window-integrated capacitive touch screen panel is characterized by applying high heat of 250 ° C. or more to the substrate to improve the deposition characteristics of the ITO to increase the transmittance, thereby improving the sensing sensitivity and the light characteristics. And the subject is providing the manufacturing method.

그리고 종래의 정전용량방식 터치스크린 패널이 패널 기판에 컬러 패턴을 형성시킨 다음 ITO를 증착시킨 구조에서 평탄도 및 컬러 패턴의 두께 차이로 인한 단차에 의해 ITO 패턴층에 균열하고 인쇄 단차면에 일정한 두께의 ITO층을 형성하지 못하여 균일한 저항을 얻기 어려운데 반해 본 발명은 패널 기판에 직접 ITO를 증착시킴으로써, ITO 패턴층에 균열이 발생하지 아니하여 ITO 패턴층의 저항을 일정하게 형성시켜 전기적 특성을 향상시킨 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널 및 그 제조방법을 제공함을 다른 과제로 한다.
In the conventional capacitive touch screen panel, a color pattern is formed on a panel substrate, and then ITO is deposited, cracked in the ITO pattern layer by a step due to a difference in flatness and color pattern, and a constant thickness on the printing step surface. While it is difficult to obtain uniform resistance because the ITO layer is not formed, the present invention deposits ITO directly on the panel substrate, thereby preventing cracks in the ITO pattern layer, thereby forming a constant resistance of the ITO pattern layer to improve electrical characteristics. Another object of the present invention is to provide a window integrated capacitive touch screen panel and a manufacturing method thereof.

상기의 과제를 달성하기 위한 본 발명은 윈도우 패널 기판(10)과,The present invention for achieving the above object is a window panel substrate 10,

상기 윈도우 패널 기판의 상부에 영상센서의 터치 영역인 윈도우부(WA)에 걸쳐서 배치된 투명한 도전성 전극 패턴층(20)과,A transparent conductive electrode pattern layer 20 disposed over the window portion WA, which is a touch region of the image sensor, on the window panel substrate;

상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 비도전성 컬러 패턴층(30)과,A non-conductive color pattern layer 30 disposed on one side edge portion E of the substrate such that the window portion WA is partitioned on the conductive electrode pattern layer;

상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 금속전극 패턴층(40)과,A metal electrode pattern layer 40 disposed on one side edge portion E of the substrate such that a window portion WA is partitioned on the conductive electrode pattern layer;

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 연성회로기판(FPCB)이 본딩되는 구획을 남겨두고 배치된 절연막 패턴층(50) 및 An insulating film pattern layer 50 disposed on the conductive electrode pattern layer and the metal electrode pattern layer, leaving a section in which a flexible printed circuit board (FPCB) is bonded;

금속전극 패턴층과 연결되게 본딩된 연성회로기판(60, FPCB),A flexible printed circuit board 60 (FPCB) bonded to the metal electrode pattern layer;

을 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널을 과제 해결 수단으로 한다.
The integrated window capacitive touch screen panel comprising a as a problem solving means.

그리고 본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법은 도전성 전극막(20a)과 비도전성 컬러 코팅막의 패터닝 공정에 따라 아래와 같이 두 가지의 제조방법으로 구분되어진다.
In addition, the manufacturing method of the window-integrated capacitive touch screen panel according to the present invention is classified into the following two manufacturing methods according to the patterning process of the conductive electrode film 20a and the non-conductive color coating film.

본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제1 제조방법은 윈도우 패널 기판(10)에 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성하는 도전성 전극막 형성/패터닝 단계(P100)와;In the first manufacturing method of the window-integrated capacitive touch screen panel according to the present invention, the conductive electrode film forming the conductive electrode pattern layer 20 by removing the conductive electrode film 20a at regular intervals from the window panel substrate 10 is formed. Forming / patterning step (P100);

상기 도전성 전극 패턴층(20)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시킨 다음 비도전성 컬러 패턴층(30)을 형성시키는 비도전성 컬러 코팅막 형성/패터닝 단계(P200)와;Forming / patterning a non-conductive color coating film for forming a non-conductive color coating film 30a using a non-conductive ink or non-conductive compound on the conductive electrode pattern layer 20 and then forming the non-conductive color pattern layer 30. Step P200;

상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(P300)와;A metal electrode film forming / patterning step (P300) for forming a metal electrode film 40a on the conductive electrode pattern layer and then forming a metal electrode pattern layer 40;

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(P400) 및;An insulating film formation / patterning step (P400) of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming the insulating film pattern layer 50;

상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(P500);An FPCB bonding step (P500) of bonding a flexible printed circuit board (60, FPCB) to be connected to the metal electrode pattern layer;

를 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법을 다른 과제 해결 수단으로 한다.
Method for manufacturing a window-integrated capacitive touch screen panel, characterized in that it comprises another problem solving means.

그리고 본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제2 제조방법은 윈도우 패널 기판(10)에 도전성 전극막(20a)을 형성시키는 단계(S101)와;The second manufacturing method of the window integrated capacitive touch screen panel according to the present invention includes forming a conductive electrode film 20a on the window panel substrate 10 (S101);

상기 도전성 전극막(20a)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시키는 단계(S102)와;Forming a non-conductive color coating film (30a) using a non-conductive ink or a non-conductive compound on the conductive electrode film (20a) (S102);

상기 비도전성 컬러 코팅막(30a)을 패턴층(30)으로 형성시키는 비도전성 컬러 코팅막 패터닝 단계(S201)와;A non-conductive color coating film patterning step of forming the non-conductive color coating film 30a as a pattern layer 30 (S201);

상기 도전성 전극막(20a)을 패턴층(20)으로 형성시키는 도전성 전극막 패터닝 단계(S202)와;A conductive electrode film patterning step of forming the conductive electrode film 20a as a pattern layer 20 (S202);

상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(S300)와;Forming a metal electrode film 40a on the conductive electrode pattern layer and then forming / patterning a metal electrode pattern layer 40 (S300);

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(S400) 및;An insulating film formation / patterning step of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming an insulating film pattern layer 50;

상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(S500);An FPCB bonding step (S500) of bonding a flexible circuit board 60 (FPCB) to be connected to the metal electrode pattern layer;

를 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법을 또 다른 과제 해결 수단으로 한다.
Method for manufacturing a window-integrated capacitive touch screen panel, characterized in that it comprises another problem solving means.

상기의 과제 해결 수단에 의한 본 발명은 윈도우 패널 기판에 ITO를 증착시킨 다음 컬러 패턴층을 형성시켜 윈도우 일체형 정전용량방식 터치스크린 패널을 제조함으로써, 제조방법이 간편하여 생산성이 향상되고, 기판에 ITO의 증착시에 250℃ 이상의 높은 열을 가하여 ITO를 증착시켜 투과율을 높이고, ITO 패턴층에 균열이 발생하지 아니하여 ITO 패턴층의 저항을 낮추어 센싱감도와 광 특성을 향상시켜 각종 전자제품의 개발에 일조할 수 있을 것으로 기대된다.
According to the present invention by the above problem solving means to produce a window-integrated capacitive touch screen panel by depositing ITO on the window panel substrate and then forming a color pattern layer, the production method is simple, productivity is improved, ITO on the substrate During the deposition, the ITO is deposited by applying high heat of 250 ℃ or higher to increase the transmittance, and there is no crack in the ITO pattern layer, which lowers the resistance of the ITO pattern layer to improve the sensing sensitivity and optical properties to develop various electronic products. It is expected to help.

도 1은 종래의 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 도면이고,
도 2는 종래의 다른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 도면이며,
도 3은 통상적인 터치스크린 패널(TSP)의 일례를 보여주는 사시도이고,
도 4는 본 발명의 실시예에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 도면이며,
도 5는 본 발명의 실시예에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 공정블럭도이고,
도 6은 본 발명의 다른 실시예에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 도면이며,
도 7은 본 발명의 다른 실시예에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제조공정을 나타낸 공정블럭도에 관한 것이다.
1 is a view showing a manufacturing process of a conventional window integrated capacitive touch screen panel,
2 is a view showing a manufacturing process of another conventional window integrated capacitive touch screen panel,
3 is a perspective view showing an example of a conventional touch screen panel (TSP),
4 is a view showing a manufacturing process of a window integrated capacitive touch screen panel according to an embodiment of the present invention,
5 is a process block diagram illustrating a manufacturing process of a window integrated capacitive touch screen panel according to an exemplary embodiment of the present invention.
6 is a view showing a manufacturing process of a window integrated capacitive touch screen panel according to another embodiment of the present invention,
7 is a process block diagram illustrating a manufacturing process of a window integrated capacitive touch screen panel according to another exemplary embodiment of the present invention.

이하, 본 발명의 바람직한 실시예를 첨부한 도면인 도 3 내지 도 7에 의거하여 상세히 설명하며, 도면 및 상세한 설명에서 이 분야의 종사자들이 용이하게 알 수 있는 구성 및 작용에 대한 도시 및 언급은 간략히 하거나 생략하였고, 특히, 도면의 도시에 있어서 요소들 사이의 크기 비가 다소 상이하게 표현되거나 서로 결합되는 부품들 사이의 크기가 상이하게 표현된 부분도 있으나, 이와 같은 도면의 표현 차이는 이 분야의 종사자들이 용이하게 이해할 수 있는 부분들이므로 별도의 설명을 생략한다.
Hereinafter, with reference to the accompanying drawings, preferred embodiments of the present invention will be described in detail with reference to Figures 3 to 7, the figures and references to the construction and operation that can be easily understood by those skilled in the art in the drawings and detailed description will be briefly described. In particular, in the drawings of the drawings, the size ratio between the elements is somewhat different, or there are parts in which the sizes are different between the parts coupled to each other, but the difference in representation of such drawings is due to those skilled in the art. Since these parts are easily understood, a separate description is omitted.

본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 일실시예를 첨부된 도면인 도 3 및 도 4를 중심으로 상세히 설명하면 다음과 같다.
An embodiment of a window integrated capacitive touch screen panel according to the present invention will be described in detail with reference to FIGS. 3 and 4.

통상적인 터치스크린 패널은 도 3에 도시된 바와 같이 전면에 화상이 보이는 투명한 영상센서의 터치 영역인 윈도우부(WA)와, 이 윈도우부(WA)를 둘러싼 테두리부(E)로 구분되고, 윈도우부(WA)는 손가락 등에 의한 터치 입력을 받아들이는 영역이고, 테두리부(E)는 휴대폰 메이커의 상표나 로고 등을 인쇄하거나 또는 불투명한 도전성 배선 패턴을 은폐하는 기능을 한다.
A typical touch screen panel is divided into a window portion WA, which is a touch area of a transparent image sensor in which an image is seen in front, and an edge portion E surrounding the window portion WA, as shown in FIG. A portion WA is an area for receiving a touch input by a finger or the like, and the edge portion E functions to print a trademark or logo of a cellular phone maker or to conceal an opaque conductive wiring pattern.

본 발명의 특징에 의하면, 본 발명은 윈도우 패널 기판(10)과,According to a feature of the invention, the invention is a window panel substrate 10,

상기 윈도우 패널 기판의 상부에 영상센서의 터치 영역인 윈도우부(WA)에 걸쳐서 배치된 투명한 도전성 전극 패턴층(20)과,A transparent conductive electrode pattern layer 20 disposed over the window portion WA, which is a touch region of the image sensor, on the window panel substrate;

상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 비도전성 컬러 패턴층(30)을 포함한다.
The non-conductive color pattern layer 30 is disposed on one side edge portion E of the substrate so that the window portion WA is partitioned on the conductive electrode pattern layer.

그리고 상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 금속전극 패턴층(40)과,A metal electrode pattern layer 40 disposed on one side edge portion E of the substrate such that a window portion WA is partitioned on the conductive electrode pattern layer;

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 연성회로기판(FPCB)이 본딩되는 구획을 남겨두고 배치된 절연막 패턴층(50) 및 An insulating film pattern layer 50 disposed on the conductive electrode pattern layer and the metal electrode pattern layer, leaving a section in which a flexible printed circuit board (FPCB) is bonded;

금속전극 패턴층과 연결되게 본딩된 연성회로기판(60, FPCB),A flexible printed circuit board 60 (FPCB) bonded to the metal electrode pattern layer;

을 포함하는 것을 특징으로 한다.
Characterized in that it comprises a.

또한 본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 제1 제조방법은 윈도우 패널 기판(10)에 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성하는 도전성 전극막 형성/패터닝 단계(P100)와;In addition, the first manufacturing method of the window-integrated capacitive touch screen panel according to the present invention removes the conductive electrode film 20a at regular intervals from the window panel substrate 10 to form the conductive electrode pattern layer 20. A film forming / patterning step (P100);

상기 도전성 전극 패턴층(20)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시킨 다음 비도전성 컬러 패턴층(30)을 형성시키는 비도전성 컬러 코팅막 형성/패터닝 단계(P200)와;Forming / patterning a non-conductive color coating film for forming a non-conductive color coating film 30a using a non-conductive ink or non-conductive compound on the conductive electrode pattern layer 20 and then forming the non-conductive color pattern layer 30. Step P200;

상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(P300)와;A metal electrode film forming / patterning step (P300) for forming a metal electrode film 40a on the conductive electrode pattern layer and then forming a metal electrode pattern layer 40;

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(P400) 및;An insulating film formation / patterning step (P400) of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming the insulating film pattern layer 50;

상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(P500);An FPCB bonding step (P500) of bonding a flexible printed circuit board (60, FPCB) to be connected to the metal electrode pattern layer;

를 포함하는 단계를 거쳐 제조되어진다.
It is prepared through a step comprising a.

이하, 본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널의 적층구조를 구성하는 각 적층체와 본 발명에 따른 제1 제조방법에 대해 상세히 설명하면 아래의 내용과 같다.
Hereinafter, each laminated body constituting the laminated structure of the window-integrated capacitive touch screen panel according to the present invention and the first manufacturing method according to the present invention will be described in detail.

본 발명에서 상기 윈도우 패널 기판(10)은 SiO2를 주성분으로 하는 유리 재질로 이루어질 수 있다. 윈도우 패널 기판(10)은 반드시 이에 한정되는 것은 아니며 투명한 플라스틱 재로 형성될 수도 있다. 기판(10)을 형성하는 플라스틱 재는 절연성 유기물일 수 있는데 폴리에테르술폰(PES, polyethersulphone), 폴리아크릴레이트(PAR, polyacrylate), 폴리에테르 이미드(PEI, polyetherimide), 폴리에틸렌 나프탈레이트(PEN, polyethyelenen napthalate), 폴리에틸렌 테레프탈레이트(PET, polyethyeleneterepthalate), 폴리페닐렌 설파이드(polyphenylene sulfide : PPS), 폴리아릴레이트(polyallylate), 폴리이미드(polyimide), 폴리카보네이트(PC, polycarbonate), 셀룰로오스 트리 아세테이트(TAC), 셀룰로오스 아세테이트 프로피오네이트(cellulose acetate propionate : CAP)로 이루어진 그룹으로부터 선택되는 것이 바람직하다.
In the present invention, the window panel substrate 10 may be made of a glass material mainly containing SiO 2 . The window panel substrate 10 is not necessarily limited thereto and may be formed of a transparent plastic material. The plastic material forming the substrate 10 may be an insulating organic material, such as polyethersulphone (PES), polyacrylate (PAR, polyacrylate), polyetherimide (PEI), polyethylene naphthalate (PEN, polyethyelenen napthalate) ), Polyethylene terephthalate (PET, polyethyeleneterepthalate), polyphenylene sulfide (PPS), polyallylate, polyimide, polycarbonate (PC, polycarbonate), cellulose triacetate (TAC), It is preferably selected from the group consisting of cellulose acetate propionate (CAP).

그리고 상기 도전성 전극 패턴층(20)은 영상센서의 터치 영역인 윈도우부(WA)에 손가락을 접촉시키면 사람의 몸에서 발생하는 정전기를 감지해서 전기신호로 연결하는 작용을 한다.
In addition, the conductive electrode pattern layer 20 detects static electricity generated in a human body by connecting a finger to the window portion WA, which is a touch area of the image sensor, and connects the electrical signal to an electric signal.

상기 도전성 전극 패턴층(20)은 도전성 전극막 형성/패터닝 단계(P100)에서 윈도우 패널 기판(10)에 영상센서의 터치영역인 윈도우부(WA)의 상부에 걸쳐서 배치된 투명한 도전성 전극막(20a)을 형성시킨 다음 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성시킨다.
The conductive electrode pattern layer 20 is a transparent conductive electrode film 20a disposed over the upper portion of the window portion WA, which is a touch area of the image sensor, on the window panel substrate 10 in the forming / patterning of the conductive electrode film P100. ), And then the conductive electrode film 20a is removed at regular intervals to form the conductive electrode pattern layer 20.

또한 상기 도전성 전극 패턴층(20)은 인듐주석산화물(ITO), 인듐아연산화물(IZO), 아연산화물(ZnO), 인듐아연주석산화물(IZTO), 카드뮴주석산화물(CTO), PEDOT(poly(3,4-ethylenedioxythiophene)), 탄소나노튜브(CNT), 실버나노와이어(silver nano wire) 중에서 1종을 선택한 도전성 화합물을 사용하여 도전성 전극막(20a)을 증착시킨 후 포토리소그래피, 에칭 또는 레이저 가공하여 투명한 도전성 전극 패턴층(20)을 형성시키는 것이 바람직하다.
In addition, the conductive electrode pattern layer 20 may be formed of indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium zinc oxide (IZTO), cadmium tin oxide (CTO), or PEDOT (poly (3). , 4-ethylenedioxythiophene)), carbon nanotubes (CNT), silver nano wire (silver nano wire) using a conductive compound selected from the deposition of the conductive electrode film (20a) and then photolithography, etching or laser processing It is preferable to form the transparent conductive electrode pattern layer 20.

그리고 상기 컬러 패턴층(30)은 윈도우 패널 기판(20)의 중앙부에 투명한 터치 영역인 윈도우부(WA)가 구획되도록 윈도우 패널 기판(20)의 테두리부에 불투명한 장식층을 형성하는 작용을 하며, 컬러 코팅막 형성/패터닝 단계(P200)에서 도전성 전극 패턴층(20)의 상부에 잉크 또는 화합물을 사용하여 컬러 코팅막(30a)을 형성시킨 다음 컬러 코팅막(30a)을 영상센서의 터치 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부에 배치되게 컬러 패턴층(30)을 형성시킨다.
In addition, the color pattern layer 30 functions to form an opaque decorative layer on the edge of the window panel substrate 20 so that the window portion WA, which is a transparent touch area, is partitioned at the center of the window panel substrate 20. In operation P200, the color coating layer 30a is formed on the conductive electrode pattern layer 20 using an ink or a compound, and then the color coating layer 30a is formed on the touch window part of the image sensor. The color pattern layer 30 is formed to be disposed at the edge of one surface of the substrate so as to be partitioned.

그리고 금속전극 패턴층(40)은 영상센서의 터치 윈도우부(WA)에서 발생하는 터치에 의해 도전성 전극 패턴층(20)에서 발생하는 전기적 신호를 FPCB 및 IC chip으로 전달하는 역할을 하며, 금속전극 코팅막 형성/패터닝 단계(P300)에서 도전성 전극 패턴층과 컬러 패턴층의 상부에 금속전극 코팅막(40a)을 형성시킨 다음 이 금속전극 코팅막(40a)을 영상센서의 터치 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부에 배치된 금속전극 패턴층(40)을 형성시킨다.
In addition, the metal electrode pattern layer 40 transfers an electrical signal generated from the conductive electrode pattern layer 20 to the FPCB and the IC chip by a touch generated from the touch window part WA of the image sensor. In the coating film forming / patterning step (P300), the metal electrode coating film 40a is formed on the conductive electrode pattern layer and the color pattern layer, and the metal electrode coating film 40a is partitioned so that the touch window part WA of the image sensor is partitioned. The metal electrode pattern layer 40 disposed on the edge of one surface of the substrate is formed.

또한 상기 금속전극 패턴층(40)은 스크린인쇄, 증착 같은 방법으로 형성시키며 일반적으로 Ag를 주로 이용하지만 용도 및 구현 방법에 따라 Mg, Al, Pt, Au, Ni, Cr, Pd, Mo 같은 소재 중에서 1종을 선택하여 금속전극 패턴층(40)을 형성시키는 것이 바람직하다.
In addition, the metal electrode pattern layer 40 is formed by a method such as screen printing and vapor deposition. Generally, Ag is mainly used. It is preferable to select one kind to form the metal electrode pattern layer 40.

그리고 상기 절연막 패턴층(50)은 그 하부에 있는 복수의 층들을 외부 전기적, 물리적, 화학적 충격으로부터 차단시켜 오염을 방지하고 내구성을 높여주는 작용을 하며, 절연막 형성/패터닝단계(P400)은 영상센서의 터치영역인 윈도우부(WA)에 걸쳐서 배치된 절연막 코팅막(50a)을 형성시킨 다음 절연막 코팅막(50a)을 영상센서의 터치영역인 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부에 배치되게 절연막 패턴층(50)을 형성시킨다.
The insulating film pattern layer 50 prevents contamination and enhances durability by blocking a plurality of layers under the external electrical, physical and chemical shocks. The insulating film forming / patterning step (P400) includes an image sensor. An insulating film coating film 50a disposed over the window portion WA, which is a touch area of the substrate, is formed, and then the insulating film coating film 50a is disposed on an edge of one surface of the substrate so that the window portion WA, which is a touch area of the image sensor, is partitioned. The insulating film pattern layer 50 is formed.

또한 상기 절연막 패턴층(50)은 절연화합물을 사용하여 스크린 인쇄, 증착, 스핀 코팅(spin coating)법 또는 커튼 플로우(curtain flow)법 으로 형성하여 열 또는 UV 건조 방식으로 절연막을 형성시키는 것이 바람직하다.
In addition, the insulating film pattern layer 50 is preferably formed by screen printing, vapor deposition, spin coating or curtain flow using an insulating compound to form an insulating film by thermal or UV drying. .

본 발명에서 사용가능한 절연화합물은 구체적으로 우레탄(Urethane), 폴리에스테르(Polyester), 아크릴(Acrylic) 등의 유기 화합물 또는 알루미나(Al2O3), 실리카(SiO2), 마그네시아(MgO) 등의 무기 화합물 중에서 1종 또는 그 이상을 선택하여 사용하는 것이 바람직하다.
Insulating compounds usable in the present invention are specifically organic compounds such as urethane, polyester, acrylic, or alumina (Al 2 O 3 ), silica (SiO 2 ), magnesia (MgO), etc. It is preferable to select and use 1 type or more from an inorganic compound.

그리고 연성회로기판(60, FPCB)은 금속전극 패턴층과 연결되어 IC 칩(chip)으로 전기적 신호를 전달하는 작용을 한다.
In addition, the flexible printed circuit board 60 (FPCB) is connected to the metal electrode pattern layer to transmit an electrical signal to the IC chip.

그리고 본 발명에 따른 윈도우 일체형 정전용량방식 터치스크린 패널은 각 적층체의 두께가 윈도우 패널 기판(10)이 0.3㎜~3㎜, 도전성 전극 패턴층(20)이 100Å~1000Å 컬러 패턴층(30)이 0.3㎛~30㎛, 금속전극 패턴층(40)이 0.2㎛~20㎛이고, 절연막 패턴층(50)이 0.5㎛~50㎛인 것이 바람직하지만, 각 적층체의 두께는 상기에서 한정한 범위에만 반드시 적용되지 아니하고, 설계조건에 따라 적절히 조정되어 질 수 있다.
In the window integrated capacitive touch screen panel according to the present invention, each laminate has a thickness of 0.3 mm to 3 mm for the window panel substrate 10 and a 100 mW to 1000 mW color pattern layer 30 for the conductive electrode pattern layer 20. Although it is preferable that the 0.3 micrometer-30 micrometers, the metal electrode pattern layer 40 are 0.2 micrometer-20 micrometers, and the insulating film pattern layer 50 is 0.5 micrometer-50 micrometers, the thickness of each laminated body is the range defined above. It is not necessarily applied only to the design and can be adjusted according to the design conditions.

그리고 본 발명에 따른 제2 제조방법은 상기 제1 제조방법과는 달리 도 3 및 도 6, 도 7에 도시된 바와 같이, 비도전성 컬러 코팅막과 도전성 전극막을 패터닝시키는 단계의 순서를 달리한 제조한 방법으로, 윈도우 패널 기판(10)에 도전성 전극막(20a)을 형성시키는 단계(S101)와;And unlike the first manufacturing method according to the second manufacturing method according to the present invention, as shown in Figs. 3, 6, and 7, the non-conductive color coating film and the conductive electrode film patterning step By forming a conductive electrode film 20a on the window panel substrate 10 (S101);

상기 도전성 전극막(20a)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시키는 단계(S102)와;Forming a non-conductive color coating film (30a) using a non-conductive ink or a non-conductive compound on the conductive electrode film (20a) (S102);

상기 비도전성 컬러 코팅막(30a)을 패턴층(30)으로 형성시키는 비도전성 컬러 코팅막 패터닝 단계(S201)와;A non-conductive color coating film patterning step of forming the non-conductive color coating film 30a as a pattern layer 30 (S201);

상기 도전성 전극막(20a)을 패턴층(20)으로 형성시키는 도전성 전극막 패터닝 단계(S202)와;A conductive electrode film patterning step of forming the conductive electrode film 20a as a pattern layer 20 (S202);

상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(S300)와;Forming a metal electrode film 40a on the conductive electrode pattern layer and then forming / patterning a metal electrode pattern layer 40 (S300);

상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(S400) 및;An insulating film formation / patterning step of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming an insulating film pattern layer 50;

상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(S500);An FPCB bonding step (S500) of bonding a flexible circuit board 60 (FPCB) to be connected to the metal electrode pattern layer;

를 포함하는 것을 특징으로 한다.
Characterized in that it comprises a.

상기 비도전성 컬러 코팅막 패터닝 단계(S201)는 영상센서의 터치 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치되게 비도전성 컬러 패턴층(30)을 형성시킨다.
In the non-conductive color coating film patterning step (S201), the non-conductive color pattern layer 30 is formed to be disposed on the edge portion E of the substrate so that the touch window portion WA of the image sensor is partitioned.

그리고 도전성 전극막 패터닝 단계(S202)는 영상센서의 터치영역인 윈도우부(WA)의 상부에 걸쳐서 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성시킨다.
In the conductive electrode film patterning step S202, the conductive electrode film 20a is removed at regular intervals over the window portion WA, which is the touch area of the image sensor, to form the conductive electrode pattern layer 20.

이하, 공정은 상기 제1 제조방법과 동일한 방법에 의해 실시되므로 여기서는 그 설명을 생략하기로 한다.
Hereinafter, since the process is carried out by the same method as the first manufacturing method, a description thereof will be omitted here.

이하, 본 발명에 따른 실시예를 들면서 상세히 설명하는바, 본 발명이 다음의 실시 예에 의해서만 반드시 한정되는 것은 아니다.
Hereinafter, the present invention will be described in detail with reference to Examples. However, the present invention is not necessarily limited to the following Examples.

1. 윈도우 일체형 정전용량방식 터치스크린 패널의 제조
1. Manufacturing of Integrated Window Capacitive Touch Screen Panel

(실시예 1)(Example 1)

0.7㎜ 두께의 Glass 기판(10)에 영상센서의 터치 윈도우부(WA)의 상부에 걸쳐서 인듐주석산화물(ITO)을 이용하여 증착한 다음 300℃로 가열하여 150Å 두께의 투명한 ITO 전극막(20a)을 형성시킨 후 이 ITO 전극막(20a)을 일정 간격으로 제거하여 ITO 패턴층(20)을 형성시킨 다음 그 상부에 잉크를 사용하여 1㎛ 두께의 컬러 코팅막(30a)을 형성시켜 100℃에서 건조시킨 후, 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부에 배치되게 비도전성 컬러 패턴층(30)을 형성시키고, 상기 ITO 패턴층과 비도전성 컬러 패턴층의 상부에 금속전극 코팅막(40a)을 1㎛ 두께로 형성시킨 다음 이 금속전극 코팅막(40a)을 영상센서의 터치 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부에 배치된 금속전극 패턴층(40)을 형성시킨 다음 상기 절연막 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 1㎛ 두께로 형성시켜 100℃에서 건조시킨 다음 이 절연막(50a)을 연성회로기판(FPCB)이 본딩되는 구획을 남겨두고 배치된 절연막 패턴층(50)을 형성시킨 후 상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시켜 윈도우 일체형 정전용량방식 터치스크린 패널을 제조하였다.
A glass substrate 10 having a thickness of 0.7 mm was deposited using indium tin oxide (ITO) over the upper portion of the touch window WA of the image sensor, and then heated to 300 ° C. to form a 150 Å thick transparent ITO electrode film 20a. After forming the ITO electrode film 20a at regular intervals to form the ITO pattern layer 20, and then to form a color coating film 30a of 1㎛ thickness using ink on the top and dried at 100 ℃ After forming the non-conductive color pattern layer 30, the non-conductive color pattern layer 30 is formed on the edge of the substrate so that the window part WA is partitioned, and the metal electrode coating layer 40a is formed on the ITO pattern layer and the non-conductive color pattern layer. ) To a thickness of 1 μm, and then the metal electrode coating layer 40 a to form a metal electrode pattern layer 40 disposed on one edge of the substrate such that the touch window WA of the image sensor is partitioned. Images of the insulating film pattern layer and the metal electrode pattern layer The insulating film 50a was formed to a thickness of 1 μm, dried at 100 ° C., and then the insulating film 50a was formed to form an insulating film pattern layer 50 arranged to leave a section to which the flexible printed circuit board FPCB was bonded. The flexible integrated circuit board 60 (FPCB) was bonded to be connected to the metal electrode pattern layer to manufacture a window integrated capacitive touch screen panel.

(비교예 1)(Comparative Example 1)

0.7㎜ 두께의 Glass 기판(10)에 영상센서의 터치 윈도우부(WA)의 상부에 걸쳐서 먼저, 비도전성 잉크를 사용하여 1㎛ 두께의 컬러 코팅막(30a)을 형성시켜 100℃에서 건조시킨 후 비도전성 컬러 패턴층(30)을 형성시킨 다음 그 상부에 인듐주석산화물(ITO)을 이용하여 증착한 다음 120℃로 가열하여 투명한 ITO 전극막(20a)을 형성시킨 후 이 ITO 전극막(20a)을 일정 간격으로 제거하여 ITO 패턴층(20)을 형성시키고, 이후의 공정은 상기 실시예 1과 동일한 방법에 의해 윈도우 일체형 정전용량방식 터치스크린 패널을 제조하였다.
On the 0.7 mm thick glass substrate 10 over the upper part of the touch window portion WA of the image sensor, first, a color coating film 30a having a thickness of 1 μm was formed using non-conductive ink and dried at 100 ° C., and then After forming the exclusive color pattern layer 30, it is deposited by using indium tin oxide (ITO) on top of it, and then heated to 120 DEG C to form a transparent ITO electrode film 20a, and then the ITO electrode film 20a is formed. The ITO pattern layer 20 was formed by removing the ITO pattern layer at regular intervals, and the subsequent process was performed by the same method as in Example 1 to manufacture a window integrated capacitive touch screen panel.

2. 윈도우 일체형 정전용량방식 터치스크린 패널의 평가
2. Evaluation of Window Integrated Capacitive Touch Screen Panel

상기의 방법에 의해 제조한 실시예 1 및 비교예 1의 윈도우 일체형 정전용량방식 터치스크린 패널에서 ITO 패턴층의 비저항특성과 광 투과율을 측정한 결과는 아래 [표 1]의 내용과 같다.
The results of measuring the resistivity and light transmittance of the ITO pattern layer in the window integrated capacitive touch screen panel of Example 1 and Comparative Example 1 manufactured by the above method are shown in Table 1 below.

항목Item 실시예 1Example 1 비교예 1Comparative Example 1 비저항(10-4Ω-cm)Specific resistance (10 -4 Ω-cm) 1.41.4 5.25.2 ITO층 광 투과율(%)ITO layer light transmittance (%) 9797 9292

상기 [표 1]의 내용에 의하며, 실시예 1은 비교예 1에 비해 비저항이 낮으며, ITO층의 광 투과율이 우수한 것으로 확인되었다.
Based on the contents of [Table 1], Example 1 has a lower specific resistance than Comparative Example 1, it was confirmed that the excellent light transmittance of the ITO layer.

비교예 1과 동일한 순서로 공정을 진행할 경우에는 컬러 코팅막의 형성시 100℃에서 건조시키고, 패턴층을 형성시킨 다음 ITO 전극막을 증착시킨 후 300℃에서 건조시킴에 따라 컬러층의 패턴이 용해되면서 ITO 전극막에 좋지 않은 영향을 미칠 뿐만 아니라 제품 외부 디자인이 훼손되어 제품으로서의 가치를 상실하게 된다.
When the process is performed in the same order as in Comparative Example 1, when the color coating film is formed, it is dried at 100 ° C., a pattern layer is formed, and then an ITO electrode film is deposited and dried at 300 ° C., so that the pattern of the color layer is dissolved. Not only does it adversely affect the electrode film, but the external design of the product is compromised, resulting in loss of value as a product.

상술한 바와 같은, 본 발명의 바람직한 실시예를 상기한 설명 및 도면에 따라 도시하였지만, 이는 예를 들어 설명한 것에 불과하며 본 발명의 기술적 사상을 벗어나지 않는 범위 내에서 다양한 변화 및 변경이 가능하다는 것을 이 분야의 통상적인 기술자들은 잘 이해할 수 있을 것이다.
As described above, although the preferred embodiment of the present invention has been shown in accordance with the above description and drawings, this is merely an example and various changes and modifications can be made without departing from the spirit of the present invention. Those skilled in the art will appreciate.

본 발명은 제조방법이 간편하여 생산성이 향상되고, 윈도우 패널 기판에 ITO의 증착시에 250℃ 이상의 높은 열을 가하여 ITO를 증착시켜 투과율을 높이고, ITO 패턴층에 균열이 발생하지 아니하여 ITO 패턴층의 저항을 낮추어 센싱감도와 광 특성을 향상시킴으로써, 산업상 파급효과가 클 것으로 기대된다.
In the present invention, the production method is simple, the productivity is improved, and when the ITO is deposited on the window panel substrate, ITO is deposited by applying high heat of 250 ° C. or higher to increase the transmittance, and the ITO pattern layer is not cracked in the ITO pattern layer. It is expected that the ripple effect of the industry will be great by improving the sensing sensitivity and optical properties by lowering the resistance of.

10 : 윈도우 패널 기판 20 : 도전성 전극 패턴층
30 : 비도전성 컬러 패턴층 40 : 금속전극 패턴층
50 : 절연막 패턴층 60 : FPCB
10 window panel substrate 20 conductive electrode pattern layer
30: non-conductive color pattern layer 40: metal electrode pattern layer
50: insulating film pattern layer 60: FPCB

Claims (13)

윈도우 패널 기판(10)과,
상기 윈도우 패널 기판의 상부에 영상센서의 터치 영역인 윈도우부(WA)에 걸쳐서 배치된 투명한 도전성 전극 패턴층(20)과,
상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 비도전성 컬러 패턴층(30)과,
상기 도전성 전극 패턴층의 상부에 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 금속전극 패턴층(40)과,
상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 연성회로기판(FPCB)이 본딩되는 구획을 남겨두고 배치된 절연막 패턴층(50) 및
금속전극 패턴층과 연결되게 본딩된 연성회로기판(60, FPCB),
을 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널.
A window panel substrate 10,
A transparent conductive electrode pattern layer 20 disposed over the window portion WA, which is a touch region of the image sensor, on the window panel substrate;
A non-conductive color pattern layer 30 disposed on one side edge portion E of the substrate such that the window portion WA is partitioned on the conductive electrode pattern layer;
A metal electrode pattern layer 40 disposed on one side edge portion E of the substrate such that a window portion WA is partitioned on the conductive electrode pattern layer;
An insulating film pattern layer 50 disposed on the conductive electrode pattern layer and the metal electrode pattern layer, leaving a section in which a flexible printed circuit board (FPCB) is bonded;
A flexible printed circuit board 60 (FPCB) bonded to the metal electrode pattern layer;
Integrated window capacitive touch screen panel comprising a.
제 1항에 있어서,
상기 윈도우 패널 기판(10)은 유리 또는 PET 필름인 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널.
The method of claim 1,
The window panel substrate 10 is a window integrated capacitive touch screen panel, characterized in that the glass or PET film.
제 1항에 있어서,
상기 도전성 전극 패턴층(20)은 인듐주석산화물(ITO), 인듐아연산화물(IZO), 아연산화물(ZnO), 인듐아연주석산화물(IZTO), 카드뮴주석산화물(CTO), PEDOT(poly(3,4-ethylenedioxythiophene)), 탄소나노튜브(CNT), 실버나노와이어(silver nano wire) 중에서 1종을 선택하여 형성시킨 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널.
The method of claim 1,
The conductive electrode pattern layer 20 may be formed of indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium zinc oxide (IZTO), cadmium tin oxide (CTO), or PEDOT (poly (3, 4-ethylenedioxythiophene)), carbon nanotube (CNT), silver nano wire (silver nano wire) is a window integrated capacitive touch screen panel, characterized in that formed by selecting one type.
제 1항에 있어서,
상기 금속전극 패턴층(40)은 스크린인쇄, 증착 같은 방법으로 형성시키며 Ag를 주로 이용하지만 용도 및 구현 방법에 따라 Mg, Al, Pt, Au, Ni, Cr, Pd, Mo 같은 소재 중에서 1종을 선택하여 형성시킨 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널.
The method of claim 1,
The metal electrode pattern layer 40 is formed by a method such as screen printing and vapor deposition, and mainly uses Ag. However, the metal electrode pattern layer 40 may be formed of one of materials such as Mg, Al, Pt, Au, Ni, Cr, Pd, and Mo depending on the use and implementation method. Integrated window capacitive touch screen panel, characterized in that formed by selecting.
제 1항에 있어서,
상기 절연막 코팅층(50)은 절연화합물을 사용하여 스크린 인쇄, 증착, 스핀 코팅(spin coating)법 또는 커튼 플로우(curtain flow)법에 의해 코팅층을 형성시킨 다음 열 또는 UV로 건조하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널.
The method of claim 1,
The insulating film coating layer 50 is a window, characterized in that the coating layer is formed by screen printing, vapor deposition, spin coating method or curtain flow method using an insulating compound and then dried by heat or UV Integrated capacitive touch screen panel.
윈도우 패널 기판(10)에 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성하는 도전성 전극막 형성/패터닝 단계(P100)와;
상기 도전성 전극 패턴층(20)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시킨 다음 비도전성 컬러 패턴층(30)을 형성시키는 비도전성 컬러 코팅막 형성/패터닝 단계(P200)와;
상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(P300)와;
상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(P400) 및;
상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(P500);
를 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
A conductive electrode film formation / patterning step (P100) for removing the conductive electrode film 20a on the window panel substrate 10 at regular intervals to form the conductive electrode pattern layer 20;
Forming / patterning a non-conductive color coating film for forming a non-conductive color coating film 30a using a non-conductive ink or non-conductive compound on the conductive electrode pattern layer 20 and then forming the non-conductive color pattern layer 30. Step P200;
A metal electrode film forming / patterning step (P300) for forming a metal electrode film 40a on the conductive electrode pattern layer and then forming a metal electrode pattern layer 40;
An insulating film formation / patterning step (P400) of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming the insulating film pattern layer 50;
An FPCB bonding step (P500) of bonding a flexible printed circuit board (60, FPCB) to be connected to the metal electrode pattern layer;
Method of manufacturing a window integrated capacitive touch screen panel comprising a.
윈도우 패널 기판(10)에 도전성 전극막(20a)을 형성시키는 단계(S101)와;
상기 도전성 전극막(20a)의 상부에 비도전성 잉크 또는 비도전성 화합물을 사용하여 비도전성 컬러 코팅막(30a)을 형성시키는 단계(S102)와;
상기 비도전성 컬러 코팅막(30a)을 패턴층(30)으로 형성시키는 비도전성 컬러 코팅막 패터닝 단계(S201)와;
상기 도전성 전극막(20a)을 패턴층(20)으로 형성시키는 도전성 전극막 패터닝 단계(S202)와;
상기 도전성 전극 패턴층의 상부에 금속전극막(40a)을 형성시킨 다음 금속전극 패턴층(40)을 형성시키는 금속전극막 형성/패터닝 단계(S300)와;
상기 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 절연막 패턴층(50)을 형성시키는 절연막 형성/패터닝단계(S400) 및;
상기 금속전극 패턴층과 연결되게 연성회로기판(60, FPCB)을 본딩시키는 FPCB 본딩단계(S500);
를 포함하는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
Forming a conductive electrode film 20a on the window panel substrate 10 (S101);
Forming a non-conductive color coating film (30a) using a non-conductive ink or a non-conductive compound on the conductive electrode film (20a) (S102);
A non-conductive color coating film patterning step of forming the non-conductive color coating film 30a as a pattern layer 30 (S201);
A conductive electrode film patterning step of forming the conductive electrode film 20a as a pattern layer 20 (S202);
Forming a metal electrode film 40a on the conductive electrode pattern layer and then forming / patterning a metal electrode pattern layer 40 (S300);
An insulating film formation / patterning step of forming an insulating film 50a on the conductive electrode pattern layer and the metal electrode pattern layer, and then forming an insulating film pattern layer 50;
An FPCB bonding step (S500) of bonding a flexible circuit board 60 (FPCB) to be connected to the metal electrode pattern layer;
Method of manufacturing a window integrated capacitive touch screen panel comprising a.
제 6항에 있어서,
상기 도전성 전극막 형성/패터닝 단계(P100)는 윈도우 패널 기판(10)에 영상센서의 터치영역인 윈도우부(WA)의 상부에 걸쳐서 배치된 투명한 도전성 전극막(20a)을 형성시킨 다음 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method of claim 6,
In the forming / patterning of the conductive electrode film P100, a transparent conductive electrode film 20a disposed over the window portion WA, which is a touch area of the image sensor, is formed on the window panel substrate 10, and then the conductive electrode film is formed. Method for manufacturing a window-integrated capacitive touch screen panel, characterized in that to form a conductive electrode pattern layer 20 by removing the (20a) at a predetermined interval.
제 6항에 있어서,
상기 비도전성 컬러 코팅막 형성/패터닝 단계(P200)는 도전성 전극 패턴층(20)의 상부에 비도전성 컬러 코팅막(30a)을 형성시킨 다음 비도전성 컬러 코팅막(30a)을 영상센서의 터치영역인 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치되게 비도전성 컬러 패턴층(30)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method of claim 6,
In the forming / patterning of the non-conductive color coating film (P200), a non-conductive color coating film 30a is formed on the conductive electrode pattern layer 20, and then the non-conductive color coating film 30a is a window portion which is a touch area of the image sensor. A non-conductive color pattern layer (30) is formed to be disposed on one side edge portion (E) of the substrate so as to partition (WA).
제 7항에 있어서,
상기 비도전성 컬러 코팅막 패터닝 단계(S201)는 영상센서의 터치 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치되게 비도전성 컬러 패턴층(30)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method of claim 7, wherein
In the non-conductive color coating film patterning step (S201), the non-conductive color pattern layer 30 is formed to be disposed on the edge portion E of the substrate so that the touch window part WA of the image sensor is partitioned. Method for manufacturing a window integrated capacitive touch screen panel.
제 7항에 있어서,
상기 도전성 전극막 패터닝 단계(S202)는 영상센서의 터치영역인 윈도우부(WA)의 상부에 걸쳐서 도전성 전극막(20a)을 일정 간격으로 제거하여 도전성 전극 패턴층(20)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method of claim 7, wherein
The conductive electrode film patterning step (S202) may form the conductive electrode pattern layer 20 by removing the conductive electrode film 20a at regular intervals over the window portion WA, which is a touch area of the image sensor. Method of manufacturing a window integrated capacitive touch screen panel.
제 6항 또는 제 7항 중 어느 한 항에 있어서,
상기 금속전극 코팅막 형성/패터닝 단계(P300)(S300)는 도전성 전극 패턴층과 비도전성 컬러 패턴층의 상부에 금속전극 코팅막(40a)을 형성시킨 다음 이 금속전극 코팅막(40a)을 영상센서의 터치영역인 윈도우부(WA)가 구획되도록 상기 기판의 일면 테두리부(E)에 배치된 금속전극 패턴층(40)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method according to any one of claims 6 to 7,
In the forming / patterning of the metal electrode coating film (P300) (S300), the metal electrode coating film 40a is formed on the conductive electrode pattern layer and the non-conductive color pattern layer, and then the metal electrode coating film 40a is touched by the image sensor. And forming a metal electrode pattern layer (40) disposed at one edge (E) of the substrate so that the window (WA), which is an area, is partitioned.
제 6항 또는 제 7항 중 어느 한 항에 있어서,
상기 절연막 형성/패터닝단계(P400)(S400)는 도전성 전극 패턴층과 금속전극 패턴층의 상부에 절연막(50a)을 형성시킨 다음 이 절연막(50a)을 연성회로기판(FPCB)이 본딩되는 구획을 남겨두고 배치된 절연막 패턴층(50)을 형성시키는 것을 특징으로 하는 윈도우 일체형 정전용량방식 터치스크린 패널의 제조방법.
The method according to any one of claims 6 to 7,
In the insulating film forming / patterning step (P400) (S400), an insulating film 50a is formed on the conductive electrode pattern layer and the metal electrode pattern layer, and then the insulating film 50a is divided into sections where the flexible printed circuit board (FPCB) is bonded. A method of manufacturing a window-integrated capacitive touch screen panel, comprising: forming an insulating layer pattern layer (50) left over.
KR1020100038644A 2010-04-26 2010-04-26 Capacitive overlay touch screen panel integrated with window and mathod for manufacturing there of KR101133967B1 (en)