JPS64209A - Production of fine gold particles - Google Patents

Production of fine gold particles

Info

Publication number
JPS64209A
JPS64209A JP15477587A JP15477587A JPS64209A JP S64209 A JPS64209 A JP S64209A JP 15477587 A JP15477587 A JP 15477587A JP 15477587 A JP15477587 A JP 15477587A JP S64209 A JPS64209 A JP S64209A
Authority
JP
Japan
Prior art keywords
soln
particle size
iodide
alkali hydroxide
gold
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP15477587A
Other languages
Japanese (ja)
Other versions
JPH01209A (en
Inventor
Motoyuki Nakanishi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tanaka Kikinzoku Kogyo KK
Original Assignee
Tanaka Kikinzoku Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tanaka Kikinzoku Kogyo KK filed Critical Tanaka Kikinzoku Kogyo KK
Priority to JP62-154775A priority Critical patent/JPH01209A/en
Priority claimed from JP62-154775A external-priority patent/JPH01209A/en
Publication of JPS64209A publication Critical patent/JPS64209A/en
Publication of JPH01209A publication Critical patent/JPH01209A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To produce singly dispersed fine gold particles having a narrow particle size distribution by adding an amphoteric surfactant to an aq. soln. contg. iodoauric acid ions and by further adding alkali hydroxide to the aq. soln. to decompose gold iodide.
CONSTITUTION: An amphoteric surfactant such as acrylic acid amine is added to an aq. soln. contg. iodoauric acid ions prepd. by dissolving gold iodide in an aq. potassium iodide soln. or by other method. Alkali hydroxide is then added to the aq. soln. to decompose gold iodide. The proper concn. of the alkali hydroxide is about 0.1W6N. The pref. reaction temp. is about 20W70°C and the particle size of formed particles can be controlled by changing the temp. condition. The reaction is terminated at ≥about 12.5, preferably ≥about 13 pH. Thus, singly dispersed fine gold particles of ≤several μm particle size are obtd.
COPYRIGHT: (C)1989,JPO&Japio
JP62-154775A 1987-06-22 Method for producing gold particles Pending JPH01209A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP62-154775A JPH01209A (en) 1987-06-22 Method for producing gold particles

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP62-154775A JPH01209A (en) 1987-06-22 Method for producing gold particles

Publications (2)

Publication Number Publication Date
JPS64209A true JPS64209A (en) 1989-01-05
JPH01209A JPH01209A (en) 1989-01-05

Family

ID=

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4675128A (en) * 1984-12-31 1987-06-23 Henkel Kommanditgesellschaft Auf Aktien Alkane sulfonates as viscosity regulators
US4880569A (en) * 1985-06-21 1989-11-14 Lever Brothers Company Concentrated liquid detergent composition containing anionic surfactants having non-terminal sulfonate groups
CN1054780C (en) * 1994-10-20 2000-07-26 中国科学院山西煤炭化学研究所 Method of preparing coated superfine powder with metal surfactant by phase transfer

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4675128A (en) * 1984-12-31 1987-06-23 Henkel Kommanditgesellschaft Auf Aktien Alkane sulfonates as viscosity regulators
US4880569A (en) * 1985-06-21 1989-11-14 Lever Brothers Company Concentrated liquid detergent composition containing anionic surfactants having non-terminal sulfonate groups
CN1054780C (en) * 1994-10-20 2000-07-26 中国科学院山西煤炭化学研究所 Method of preparing coated superfine powder with metal surfactant by phase transfer

Similar Documents

Publication Publication Date Title
AU4944885A (en) Biooxidising subterranean water using hydrogen peroxide
AU582315B2 (en) Composition and method for metal surface refinement
BR0114684A (en) Method for making a dry alkali metal or ammonium salt of a carboxylic acid
AU5290986A (en) Method for producing foamable compositions
US3856507A (en) Recovery of gold from solution in aqua regia
JPS64209A (en) Production of fine gold particles
JPS64208A (en) Production of fine gold particles
JPS64211A (en) Production of fine gold particles
JPS64210A (en) Production of fine gold particles
ES471032A1 (en) Purification process
ES447641A1 (en) Method for producing L({30 )-tartaric acid
DE3664929D1 (en) Process for treating rare-earth ores
GB1485067A (en) Effluent treatment process
ATE211768T1 (en) IMPROVED METHOD FOR PRODUCING L-ASPARAGIC ACID
JPS5551705A (en) Production of nitridosulfate
JPS5244052A (en) Factory waste water processing method
ES8501381A1 (en) Fine crystalline isoxicam.
JPS64707A (en) Manufacture of barium ferrite powder
JPS5767136A (en) Dephosphorizing method for ore
IN183010B (en)
JPS54130499A (en) Production of needle-like goethite
JPS6475493A (en) Method for treating product having high boiling point in production of organohalosilane
ES2033810T3 (en) PROCEDURE FOR THE EXTRACTION OF AN ORGANIC LIQUID COMPRISING A NITROGENATED ORGANIC BASE, OF AN AQUEOUS BROTH OF PARTICLES OF MINERAL MATERIAL AND PROCEDURE FOR THE PRODUCTION OF ALKALINE METAL CARBONATE.
JPS5217380A (en) Production process of cation exchange resin