JPS6371326A - Fastening device for optical insert divided into two parts - Google Patents
Fastening device for optical insert divided into two partsInfo
- Publication number
- JPS6371326A JPS6371326A JP21665086A JP21665086A JPS6371326A JP S6371326 A JPS6371326 A JP S6371326A JP 21665086 A JP21665086 A JP 21665086A JP 21665086 A JP21665086 A JP 21665086A JP S6371326 A JPS6371326 A JP S6371326A
- Authority
- JP
- Japan
- Prior art keywords
- insert
- optical insert
- lower insert
- fastening device
- ring
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【発明の詳細な説明】
産業上の利用分野
本発明は、射出(圧縮)成形用金型で用いられるプラス
チック用オプティカルインサート(以下0、I 、 と
略称する)の締結装置に関するものである。DETAILED DESCRIPTION OF THE INVENTION Field of Industrial Application The present invention relates to a fastening device for a plastic optical insert (hereinafter abbreviated as 0, I, ) used in an injection (compression) mold.
従来の技術
近年、射出(圧縮)成形によるプラスチ、クレンズの生
産が成されている。成形手法の改良と高稍贋な金型があ
いまって、今後とも発展が予想される。レンズ金型で使
用されている0、工、は数ミクロンの形状精度とともに
、温度調節効果を高めるために同心円や渦巻状の温度調
節溝がO,1,内部に設けられている。この温度調節溝
を0.1.内部に形成するため、従来、0.1.を上下
に分割し。BACKGROUND OF THE INVENTION In recent years, plastics and cleanses have been produced by injection (compression) molding. The combination of improved molding methods and highly defective molds is expected to continue to develop. The 0, machining used in the lens mold has a shape accuracy of several microns, and concentric or spiral temperature adjustment grooves are provided inside the 0,1 in order to enhance the temperature adjustment effect. This temperature adjustment groove is 0.1. Conventionally, 0.1. Divide into upper and lower parts.
第3図に示すように各々のインサー)9 、12に適轟
な温度調節溝13を加工し、ロー付けにて2分割された
インサートを一体にしている。ここで10はロー付部を
示し、11はローのたまり部を示す。かかる手段によれ
ば、合わせ面全体がロー付けされているので温度調節水
の漏れがなく、金型の剛性にすぐれており、極めて信頼
性が高いものである。As shown in FIG. 3, appropriate temperature regulating grooves 13 are machined in each of the inserts 9 and 12, and the two divided inserts are integrated by brazing. Here, 10 indicates a soldering part, and 11 indicates a brazing part. According to this method, since the entire mating surfaces are brazed, there is no leakage of temperature control water, the mold has excellent rigidity, and is extremely reliable.
発明が解決しようとする問題点
しかしながら、従来のこの工法では、高度なロー付焼入
技術が必要であり、納期、コストの点で生産用金型とし
ての工法としては十分満足できるものではなかった。Problems to be solved by the invention However, this conventional construction method required advanced brazing and hardening technology, and was not fully satisfactory as a construction method for production molds in terms of delivery time and cost. .
即ち、従来のように上、下のインサートをロー付により
締結する方法では、ロー付けのシール性を確実にするた
め、ロー付けのたまり形状や寸法調整の配慮がかなり必
要で金型構造的に複雑であった。また、複雑な温度調節
溝に異物がつまっても、容易に取除くことはできないと
いう問題点を有していた。In other words, in the conventional method of fastening the upper and lower inserts by brazing, in order to ensure the sealing performance of the brazing, considerable consideration must be given to the shape of the brazing pool and dimensional adjustment, which causes problems with the mold structure. It was complicated. Another problem is that even if foreign matter gets stuck in the complicated temperature adjustment groove, it cannot be easily removed.
本発明は上記問題点に鑑み、簡単な構成で、温度調節溝
に異物がつまっても、容易に取除くことができる2分割
オプティカルインサートの締結装置を提供することを目
的とする。SUMMARY OF THE INVENTION In view of the above problems, it is an object of the present invention to provide a fastening device for a two-part optical insert that has a simple configuration and can be easily removed even if foreign matter becomes clogged in the temperature adjustment groove.
問題点を解決するための手段
上記目的を達するため、本発明の0.工、の締結装置は
、従来のロー付けにかわジ0リングと引張りボルトにて
上インサートと下インサートとを締結するものである。Means for Solving the Problems In order to achieve the above object, the present invention provides 0. This fastening device fastens the upper and lower inserts using a gage O-ring and a tension bolt instead of conventional brazing.
作 用
本発明は上記したように、0リングを介したことにより
上、下のインサートの取付け、取外しが容易で、生産中
の溝の掃除、変更も容易にでき、製品形状が少し変わっ
ても上インサートのみI41シ替えることができ、下イ
ンサートの共用化も可能である。Function: As described above, the present invention allows the upper and lower inserts to be easily installed and removed by using the O-ring, and the grooves can be easily cleaned and changed during production, and even if the product shape changes slightly, the present invention can be easily installed and removed. Only the upper insert can be replaced, and the lower insert can also be shared.
実施例
以下、本発明の一実施例について図面を参照しながら説
明する。第1図は本発明の一実施例における2分割オプ
ティカルインサート締結装置の断面図を示すものである
。第1図において、1は上インサート、2は下インサー
ト、3は温度調節溝、4は上、下インサート1,2の間
に介在するOリング、6は上、下インサート1.2を結
合するための取付ボルト、6は凹形成形レンズである。EXAMPLE Hereinafter, an example of the present invention will be described with reference to the drawings. FIG. 1 shows a sectional view of a two-part optical insert fastening device according to an embodiment of the present invention. In Fig. 1, 1 is an upper insert, 2 is a lower insert, 3 is a temperature adjustment groove, 4 is an O-ring interposed between upper and lower inserts 1 and 2, and 6 is a connector that connects upper and lower inserts 1.2. The mounting bolt 6 is a concave lens.
まず、下インサート2にOリング4を挿入し、上インサ
ート1と下インサート2とをはめ合わせて、取付ボルト
6にて上インサート1と下インサート2とを締結する。First, the O-ring 4 is inserted into the lower insert 2, the upper insert 1 and the lower insert 2 are fitted together, and the upper insert 1 and the lower insert 2 are fastened together with the mounting bolt 6.
生産中に異物(ゴミ、スケール、錆)が温度調節溝3に
付着したり、温度調節効果を改善するため、温度調節溝
3の追加加工をしたい場合、取付ポルト5を外し、上イ
ンサート1と下インサート2とを分離させることにより
可能となる。If foreign matter (dust, scale, rust) adheres to the temperature control groove 3 during production, or if you wish to additionally process the temperature control groove 3 to improve the temperature control effect, remove the mounting port 5 and insert the upper insert 1. This becomes possible by separating the lower insert 2.
また、第2図の第2の実施例に示すように、外径が両端
で同程度のレンズであれば、下インサート2はそのまま
で上インサート7に新しいレンズ形状8の形状加工を施
せば新機種にも対応が容易である。すなわち、製品部の
インサートのみを交換すれば、0.1.が構成できるの
で下インサート2の共用化が図れる。In addition, as shown in the second embodiment of FIG. 2, if the outer diameter of the lens is the same at both ends, the lower insert 2 can be left as it is, and the upper insert 7 can be shaped into a new lens shape 8. It is easy to adapt to different models. In other words, if only the insert in the product section is replaced, the cost will be 0.1. Since the lower insert 2 can be configured, the lower insert 2 can be shared.
発明の効果
以上のように本発明は、上、下のインサートを0リング
を用いボルトにて締結することにより、0.1.のメン
テナンスが容易で、必要あれば、温度調節溝の変更も容
易にできるものである。また、形状部のみのインサート
を新しく製作することにより、下インサートの共用化が
図れ、その実用的効果は大である。Effects of the Invention As described above, the present invention provides a 0.1. Maintenance is easy, and the temperature control grooves can be easily changed if necessary. Furthermore, by manufacturing a new insert with only the shaped portion, the lower insert can be shared, which has a great practical effect.
第1図は本発明の一実施例における2分割オプティカル
インサートの締結装置の断面図、第2図は本発明の他の
実施例における2分割オプティカルインサートの締結装
置の上インサートのみを付は変えたO、1.の断面図、
第3図は従来のロー付による0、工、の締結部を示す断
面図である。
1・・・・・・上インサート、2・・・・・・下インサ
ート、3・・・・・・温度調節溝、4・・・・・・Oリ
ング、6・・・・・・取付ボルト。
代理人の氏名 弁理士 中 尾 敏 男 ほか1名/
−ミー上インV−ト
2− 下インブー上
3− 蓋、友稠地溝
第 2 図 7− 上インプート9−
−一一インブート
10 −−一 ローイ寸師
11−m−ローのたコリ師Fig. 1 is a cross-sectional view of a fastening device for a two-part optical insert in one embodiment of the present invention, and Fig. 2 is a cross-sectional view of a fastening device for a two-part optical insert in another embodiment of the present invention, in which only the upper insert has been changed. O, 1. A cross-sectional view of
FIG. 3 is a cross-sectional view showing a fastening part of 0 and 2 by conventional brazing. 1...Top insert, 2...Bottom insert, 3...Temperature adjustment groove, 4...O-ring, 6...Mounting bolt . Name of agent: Patent attorney Toshio Nakao and 1 other person/
-Mie Upper Input 2- Lower Input Upper 3- Lid, Todomoe Graben No. 2 Figure 7- Upper Input 9-
-11 Inboot 10 -1 Roi Sunshi 11-m-Roi no Takorishi
Claims (1)
カルインサートと、第1のオプティカルインサートに嵌
合し着脱可能なレンズ形状に形成された第2のオプティ
カルインサートとを備え、第2のオプティカルインサー
トにOリングを介して、第1のオプティカルインサート
と第2のオプティカルインサートとを取付ボルトで結合
させてなる2分割オプティカルインサートの締結装置。a first optical insert having a base in which a temperature adjustment groove is formed; a second optical insert formed in a lens shape that fits into the first optical insert and is detachable; A fastening device for a two-part optical insert, which connects a first optical insert and a second optical insert with a mounting bolt via an O-ring.